Abstract

DEPCT68 One characteristic of this disclosure is an aluminum alloy sheet for can lids, composed of silicon (Si) content of 0.20% by mass or more and 0.47% by mass or less; iron (Fe) content of 0.30% by mass or more and 0.70% by mass or less; copper (Cu) content of 0.11% by mass or more and 0.40% by mass or less; manganese (Mn) content of 0.70% by mass or more and 1.20% by mass or less; magnesium (Mg) content of 1.1% by mass or more and 3.7% by mass or less; and residuals consisting of or incorporating aluminum (Al) and inevitably, impurities. The aluminum alloy sheet has a solidification temperature higher than the solid solution temperature of Mg2Si.
Need to check novelty before this filing date? Find Prior Art

Claims

DEPCT68 1. Aluminum alloy sheet for can lids. The aluminum alloy sheet contains: Silicon (Si) content of 0.20% by mass or more and 0.47% by mass or less; Iron (Fe) content of 0.30% by mass or more and 0.70% by mass or less; Copper (Cu) content of 0.11% by mass or more and 0.40% by mass or less; Manganese (Mn) content of 0.70% by mass or more and 1.20% by mass or less; Magnesium (Mg) content of 1.1% by mass or more and 3.7% by mass or less; and the remaining portion consisting of or incorporating aluminum (AI) and unavoidable impurities, where the aluminum alloy sheet has a solidification temperature higher than the solution temperature of Mg2Si.

2. Aluminum alloy sheets for can lids according to claim 1, where the aluminum alloy sheet contains: a silicon (Si) content of 0.20 percent by mass or more and 0.47 percent by mass or less; an iron (Fe) content of 0.30 percent by mass or more and 0.59 percent by mass or less; copper (Cu) content of 0.11 percent by mass or more and 0.40 percent by mass or less; manganese (Mn) content of 0.70 percent by mass or more and 0.98 percent by mass or less; and magnesium (Mg) content of 1.1 percent by mass or more and 3.3 percent by mass or less, where the initial solidification temperature of Al is higher than the initial crystallization temperature.

3. Aluminum alloy sheets for can lids pursuant to claim 2, where the aluminum alloy sheets are composed of: silicon (Si) content of 0.20 percent by mass or more and 0.39 percent by mass or less; iron (Fe) content of 0.30 percent by mass or more and 0.59 percent by mass or less; The copper (Cu) content must be 0.11% by mass or greater and 0.40% by mass or less; the manganese (Mn) content must be 0.70% by mass or greater and 0.98% by mass or less; and the magnesium (Mg) content must be 1.

1. Aluminum alloy sheets for can lids according to claim 3, where the temperature difference is achieved by lowering the solid solution temperature of Mg2Si from the solidification temperature to 30 °C or more; 4. Aluminum alloy sheets for can lids according to claim 3, where the aluminum alloy sheets consist of: silicon (Si) content of 0.20 percent by mass or more and 0.39 percent by mass or less; iron (Fe) content of 0.30 percent by mass or more and 0.51 percent by mass or less; copper (Cu) content of 0.11 percent by mass or more and 0.40 percent by mass or less; manganese (Mn) content of 0.70 percent by mass or more and 0.92 percent by mass or less; And the magnesium (Mg) content of 1.1 percent by mass or more and 2.9 percent by mass or less, where the temperature difference is achieved by lowering the initial crystallization temperature of the Al crystal from the initial solidification temperature of Al by 1 degree Celsius or more.