Aluminum alloy sheets for can lids.

TH2501001027APending Publication Date: 2026-11-16UACJ CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
TH2501001027
Authority / Receiving Office
TH · TH
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-17
Filing Date
2024-04-16
Publication Date
2026-11-16

Smart Images

  • Figure 2501001027_DRAWING_01
    Figure 2501001027_DRAWING_01
  • Figure 2501001027_DRAWING_02
    Figure 2501001027_DRAWING_02
  • Figure 2501001027_DRAWING_03
    Figure 2501001027_DRAWING_03
Patent Text Reader

Abstract

DEPCT68, one aspect of this disclosure, provides aluminum alloy sheets for can lids, the sheets composed of: 0.20% by mass or more and 0.47% by mass or less of Si; 0.30% by mass or more and 0.59% by mass or less of Fe; 0.11% by mass or more and 0.40% by mass or less of Cu; 0.70% by mass... or greater and 0.98 percent mass or less of Mn and 1.1 percent mass or greater and 3.7 percent mass or less of Mg, where in each of the directions 0 degrees, 45 degrees and 90 degrees to the rolling direction the minimum evaluation value Smin between the evaluation values ​​S is calculated by the following formula (1) which uses 0.2% yield strength sigma0.2, tensile strength sigmaB and average sigmafm of 0.2% yield strength and tensile strength of 330 MPa or greater and 410 MPa or less S = sigmafm / (sigma0.2 / sigmaB) ... (1)
Need to check novelty before this filing date? Find Prior Art

Claims

DEPCT68 1. Aluminum alloy sheet for can lids, composed of: silicon (Si) content of 0.20% by mass or more and 0.47% by mass or less; iron (Fe) content of 0.30% by mass or more and 0.59% by mass or less; copper (Cu) content of 0.11% by mass or more and 0.40% by mass or less; manganese (Mn) content of 0.70% by mass or more and 0.98% by mass or less; magnesium (Mg) content of 1.1% by mass or more and 3.7% by mass or less; and residuals consisting of or including aluminum (Al) and unavoidable impurities, which are present in each of the 0°, 45°, and 90° directions with respect to the rolling direction of the alloy sheet. The minimum evaluation value Smin is the smallest value among the evaluation values ​​S calculated by the subsequent formula (1) using 0.2% yield strength sigma0.2, tensile strength sigmaB and average sigmafm of 0.

2. Yield strength and tensile strength are 330 MPa or more and 410 MPa or less. S = sigma fm / (sigma 0.2 / sigma B) ... (1) 2. Aluminum alloy sheets for can lids according to claim 1, the sheets are composed of: silicon (Si) content of 0.20 percent by mass or more and 0.39 percent by mass or less; manganese (Mn) content of 0.75 percent by mass or more and 0.98 percent by mass or less; and magnesium (Mg) content of 1.4 percent by mass or more and 3.1 percent by mass or less, where the temperature difference between the solidification temperature and the manufacturing temperature The solid solution of Mg2Si is at 30 °C or higher; the initial crystallization temperature is lower than the initial solidification temperature of aluminum. In the L-ST cross-section of the central part in the width direction of the alloy sheet, the ratio of the total area in the L-ST cross-section of Mg2Si particles, where each has an area of ​​0.3 micrometers or more, is 0.2% or less, and the minimum evaluation value Smin is 360 MPa or more and 410 MPa or less.

3. Aluminum alloy sheet for can lids according to claim 1 or 2, where the value obtained by deducting 0.2% yield strength sigma 0.2_90 degrees in the 90 degree direction from the rolling direction from 0.2% yield strength sigma 0.2_0 degrees in the 0 degree direction from the rolling direction is -13 MPa or more and 13 MPa or less.

4. Aluminum alloy sheet for can lids according to claim 1 or 2, where the bending work is a 90 degree bending work on a test piece cut into a strip with a width of 12.5 mm and a length of 200 mm, and then the test piece is reversed to the 0 degree position, the number of circadian bends N is the number of bending works until the test piece... Fracture occurs when bending operations are repeatedly performed in the direction of the bending ridge parallel to the rolling direction, and the number of normalized circular bends Ns obtained by normalization to the number of circular bends N by the sheet thickness t and the subsequent formula (2) is 18 or more Ns=N xt / 0.235 ... (2).