Methods for manufacturing aluminum alloy sheets for can lids.

TH2501001029APending Publication Date: 2026-11-16UACJ CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
TH2501001029
Authority / Receiving Office
TH · TH
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-17
Filing Date
2024-04-16
Publication Date
2026-11-16
Patent Text Reader

Abstract

DEPCT68, one aspect of this disclosure, describes the method of producing aluminum alloy sheets for can lids. The method comprises the process of casting ingots containing Si (0.20% by mass or more and 0.47% by mass or less), Fe (0.30% by mass or more and 0.59% by mass or less), Cu (0.11% by mass or more and 0.40% by mass or less), Mn (0.70% by mass or more and 0.98% by mass or less), and Mg (1.3% by mass or more and 3.7% by mass or less); a homogenization treatment process on the ingots; and a rolling process. In the rolling process, cold rolling is completed without any post-hot rolling treatment on the ingots.
Need to check novelty before this filing date? Find Prior Art

Claims

DEPCT68 1. Method of producing aluminum alloy sheets for can lids, assembly method: Ingot casting process; ingots consist of: silicon (Si) content of 0.20% by mass or more and 0.47% by mass or less; iron (Fe) content of 0.30% by mass or more and 0.59% by mass or less; copper (Cu) content of 0.11% by mass or more and 0.40% by mass or less; manganese (Mn) content of 0.70% by mass or more and 0.98% by mass or less; magnesium (Mg) content of 1.3% by mass or more and 3.7% by mass or less; and residuals consisting of or incorporating aluminum (Al) and unavoidable impurities; ingot homogenization treatment process; And the process of rolling metal billets that is carried out under homogenization treatment, where in the rolling process, cold rolling is completed without creating heat treatment after hot rolling on the billet. 2.Method of producing aluminum alloy sheets for can lids according to claim 1, where in the process of homogenization treatment, homogenization is performed on ingots at a temperature higher than or equal to the solidification temperature of Mg2Si and lower than or equal to the solidification temperature of the aluminum alloy part.

3. Method of producing aluminum alloy sheets for can lids according to claim 2, where in the process of casting, casting is performed on ingots containing: silicon (Si) content of 0.20 percent by mass or more and 0.47 percent by mass or less; iron (Fe) content of 0.30 percent by mass or more and 0.55 percent by mass or less; copper (Cu) content of 0.17 percent by mass or more and 0.25 percent by mass or less; manganese (Mn) content of 0.70 percent by mass or more and 0.98 percent by mass or less; The magnesium content (Mg) is 2.6 percent by mass or more and 3.7 percent by mass or less; and the remainder consisting of or including aluminum (Al) and unavoidable impurities.

4. Method of production of aluminum alloy sheets for can lids according to claim 3, where in the casting process the casting is made on an ingot containing: silicon (Si) content of 0.20 percent by mass or more and 0.30 percent by mass or less; iron (Fe) content of 0.30 percent by mass or more and 0.55 percent by mass or less; copper (Cu) content of 0.17 percent by mass or more and 0.25 percent by mass or less; manganese (Mn) content of 0.70 percent by mass or more and 0.98 percent by mass or less; magnesium (Mg) content of 2.6 percent by mass or more and 3.7 percent by mass or less; And the remainder consists of or includes aluminum (Al) and unavoidable impurities. 5.The method of producing aluminum alloy sheets for can lids according to claim 4, includes subsequent annealing at 270°C or lower to the coating on the sheet material which has been cold-rolled from the metal ingot.

6. The method of producing aluminum alloy sheets for can lids according to claim 5, where the cold-rolling process is performed at a reduction of 90% or less.