Particle composition of refractory material for interior lining.

TH2501002791APending Publication Date: 2026-11-02แซ็งต์-โกแบง ซังเตอร์ เดอ เรอแชร์ช เอต์ เดอตูเดส์ ยูโรเปียน
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
TH2501002791
Authority / Receiving Office
TH · TH
Patent Type
Applications
Current Assignee / Owner
Priority Date
2022-11-02
Filing Date
2023-10-31
Publication Date
2026-11-02
Patent Text Reader

Abstract

DEPCT68 This disclosure pertains to the particle composition of refractory linings, which comprise 0.5 to 10% by weight of calcium titanate, Al2O3, and MgO phases. The calcium titanate, present in the form of CaTiO3, reacts with Al2O3 to form calcium aluminate complexes and / or hyponite phases during sintering / heat treatment in the presence of MgO. The refractory lining, after sintering, exhibits resistance to slag penetration and an increased modulus of cracking.
Need to check novelty before this filing date? Find Prior Art

Claims

DEPCT68 1. The particulate composition of the refractory lining particulate material, comprising 0.1 to 10% by weight of calcium titanate, Al2O3, MgO and a mineral binder, where the calcium titanate phase to be used is present in the form of CaTiO3, and this calcium titanate phase reacts with Al2O3 to form a hyponite phase during sintering in the presence of MgO.

2. The particulate composition of the refractory lining as claimed in Patent 1, comprising: -0.5 to 10% by weight of calcium titanate, where the calcium titanate phase to be used is present in the form of CaTiO3; -60 to 95% by weight of Al2O3, present in the form of grains in the range of 0.25 to 16 mm and fine powder in the range of 1 to 250 µm; -0 to 40%, with 3 to 30% by weight of MgO in granular form recommended in the 0 range.5 to 1 millimeter and fine powder with particle size less than 500 micrometers; -0 to 20% that should be used; 1 to 10% by weight of binder, which should be a mineral binder of a type selected from the group containing SiO2, MgO, CaO, Al2O3, P2O5, Na2O, TiO2 or a combination of them and which the binder particle size should be less than 0.1 millimeters; 3. The particle composition of refractory material for inner lining conforming to one of the preceding reserves, where the addition of calcium titanate is less than 8% by weight, which should be in the range of 2 to 5% by weight; 4. The particle composition of refractory material for inner lining conforming to one of the preceding reserves, which includes a mineralizer, whose particle size of A mineralizer selected from a group containing B2O3, V2O5, TiO2, Y2O3, Fe2O3, CaO, NaCl, AlCl3, MgCl, LiF, ZnF2, BaF2, CaF2, or a combination of them. (5.)The particle composition of refractory material for inner lining conforming to one of the preceding reservations includes one or more drying agents, for example, anhydrous magnesium sulfate (MgSO4), boron oxide (B2O3), amorphous silica gel (SiO2), xanthan gum, acrylic acid or methacrylic acid, a two-component polymerization binder, boric acid, and a phosphate mixture.

6. The particle composition of refractory material for inner lining conforming to one of the preceding reservations, in which 30 to 50% by weight of Al2O3 is present in the form of particles with a particle size of 1 mm or greater. 7.The process for preparing the particle composition of refractory material for interior lining involves the following steps: 1) Preparation of the refractory particle composition conforming to one of the previously specified claims, by a) adding an alumina-magnesia matrix starting material; b) the addition of a binder to the alumina-magnesia matrix starting material; c) the addition of calcium titanate (CaTiO3) to the formed refractory mixture and mixing by hand or using a mixing device; 2) Sintering the refractory particle composition for interior lining at temperatures ranging from 1000 to 1800 °C, preferably above 1300 °C to form a calcium aluminate and / or hyponite complex phase, and at 1600 °C to form an aluminum-magnesium spinel (MgAl2O4).The composition of refractory material for interior lining is obtained from the process specified in Patent 7, where: - the alumina and magnesium phases are present in amounts less than 80% by weight, in the form of aggregates containing alumina-magnesia spinel (MgAl2O4), which should be in the range of 30-40%; and / or - the alumina, magnesium, and sodium phases are present in amounts less than 10% by weight, in the form of aggregates containing sodium-magnesium-aluminum oxide (Al30Mg4Na2O50); and / or - the total amount of impurities SiO2, P2O5, K2O, Na2O, ZnO, Cu2O, FeO / Fe2O3 is less than 3% by weight based on the total weight of the refractory material.