Laminated packaging materials; methods for manufacturing laminated packaging materials and packaging containers incorporating laminated packaging materials.
Patent Information
- Application Number
- TH2501003305
- Authority / Receiving Office
- TH · TH
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-07-20
- Publication Date
- 2026-11-16
Abstract
Claims
DEPCT68 13 / 08 / 2568 1. Laminated packaging material for pouch packaging of liquid food, consisting of an aggregate layer (11; 21) of paper or other material with a cellulose-based composition, the first outermost layer, a liquid barrier layer, a heat-sealable layer (12; 22) composed of a thermoplastic polymer, a barrier layer or barrier multilayer (15; 24) composed of at least one gas barrier material, arranged on the inner side, opposite the aggregate layer (11; 21), and a second innermost heat-sealable liquid barrier layer (15), on the inner side of the barrier layer or barrier multilayer. A second innermost heat-sealable liquid barrier layer (14; 26) is positioned toward the inner side of the packaging container to be formed from the packaging material, where the heat-sealable layer,The second innermost liquid barrier (14; 26) is a pre-fabricated polyethylene film (14; 26) which is a cast and uniaxially oriented film composed of 60 to 100 percent linear low-density polyethylene (LLDPE), preferably 80 to 100 percent LLDPE, or even more desirable 90 to 100 percent LLDPE, a pre-fabricated polyethylene film that also contains Total thickness of 15 to 25 micrometers; elastic modulus of at least 400 MPa in MD, and at least 500 MPa in CD, as measured by ASTM D 882-02 (2018) with an initial strain rate of 0.1 mm / (mm*min); tensile strength greater than 40 MPa, preferably greater than 50 MPa in MD and greater than 100 in CD, as measured by ASTM D638M-14 (2017) at a crosshead rate of 200 mm / min; elongation at break less than 350 percent in MD and less than 100 percent in CD, as measured by ASTM D638M-14 (2017) at a crosshead rate of 200 mm / min; initial sealing temperature, SIT.From 80 to 100 °C as defined by ASTM F1921 (2018) at 2 N, maximum hot bond strength greater than 7 N, as measured by ASTM F1921 (2018), and puncture resistance of 10 N or higher, as measured by ASTM F1306-16 (2016) at a crosshead speed of 500 mm / min.
2. Laminated packaging material as claimed in claim 1, where LLDPE of pre-fabricated polyethylene film (14; 26) has a melt flow rate / melt flow index (MFR / MFI) of 2 to 5 g / 10 min at 2.16 kg, 190 °C, as measured by ASTM D1238 or ISO 1133.
3. Laminated packaging material as claimed in claim 1 or claim 2, where the film Pre-made polyethylene (14; 26) incorporating 60 to 100 percent m-LLDPE, preferably 80 to 100 percent m-LLDPE, more preferably 90 to 100 percent m-LLDPE.
4. Laminated packaging materials as claimed in any of the preceding claims,Where the pre-fabricated polyethylene film (14; 26) has a core layer composed of more than 60 percent by weight of m-LLDPE, a first “skin” layer on one side of the core layer, also composed of LLDPE, preferably m-LLDPE, and which is also adapted for the heat sealing of the film more than the polyethylene of the core layer, and alternatively the pre-fabricated polyethylene film has a second skin layer on the other side of the core layer.
5. Laminated packaging material as claimed in one of the preceding claims, where the pre-fabricated polyethylene film (14; 26) has a total thickness of 16 to 23 micrometers, e.g., from 16 to 20 micrometers.
6. Laminated packaging material as claimed in claim 4, where the core layer of the film Pre-made polyethylene (14; 26) with a thickness of 10 to 16 micrometers, i.e. from 10 to 14 micrometers 7. Laminated packaging material as claimed under any of the claims 4-6, where the thickness of the first layer,and of an optional second skin layer, i.e. from 1 to 3, e.g. from 2 to 3 micrometers.
8. Laminated packaging material as claimed under any of the pre-produced claims, where the pre-produced polyethylene film (14; 26) has an initial sealing temperature, SIT, of 80 to 95 °C, e.g. from 80 to 90 °C, as defined by ASTM F1921 (2018) at 2 N.
9. Laminated packaging material as claimed under any of the pre-produced claims, where the pre-produced polyethylene film (14; 26) has a maximum hot bond strength greater than 8 N, as measured by ASTM F1921 (2018).
10. Laminated packaging material as claimed under any of the pre-produced claims, where the pre-produced polyethylene film (14; 26) has a puncture resistance of 10 N or greater, As measured by ASTM F1306-16 (2016) at a crosshead speed of 500 mm / min,and has an elongation at the bore (i.e. at maximum load) of less than 10 mm.
11. Laminated packaging material as claimed in any of the preceding claims, where the barrier layer or barrier multilayer (14; 26) is laminated to the aggregate layer (11; 21) via a first bonding layer (16; 25) of one or more polymers.
12. Laminated packaging material as claimed in any of the preceding claims, where a prefabricated polyethylene film (14; 26) is laminated to the barrier layer or barrier multilayer (15; 24) via a second bonding layer (17b; 28) of a polymer.
13. Thermoplastics. Laminated packaging materials as claimed in any of the preceding claims, where pre-fabricated polyethylene films (14; 26) have a stretch ratio of 5 to 7 in the machine direction, MD, and from 7 to 10 in the transverse direction,CD 14. Laminated packaging material as claimed in any of the preceding claims, consisting of a cardboard aggregate layer (11) of standard weight from 50 to 140 g / m², i.e. from 50 to 120 g / m² and a barrier multilayer (15), in which the barrier multilayer (15) consists of a paper substrate (15a) which has at least one coating (15b-15d) of a desirable gas barrier material applied to it at a thickness of 2 to 5000 nm (5 µm), to provide a packaging material that Environmentally sustainable and more recyclable 15. Laminated packaging materials as claimed in any of the claims 1 through 13, consisting of a paper core layer (21) of standard weight from 50 to 140 g / m², e.g. from 70 to 120 g / m², e.g. from 70 to 110 g / m², and a barrier layer (24) of aluminum foil,For the purpose of manufacturing pouch packaging 16. Method for the manufacture of laminated pouch packaging materials (10; 20), as defined in one of the preceding claims, which includes the following steps, in any order, of a) lamination (30b, 35b) of continuous fibers of the aggregate layer (11; 21; 34b) of paper, cardboard or other material with cellulose as the main component to the outer side of the continuous fibers of the barrier layer or the multi-layered barrier layer (15; 24; 31b) which are combined. a) Lamination (35c, 37c) of a continuous strand of pre-fabricated inner polyethylene film (14; 26; 38c), which is a heat-sealed, second innermost liquid barrier layer, to the side in, on the other hand, of the barrier layer strands or multi-layered barrier (15; 24; 31b), for example by melt extrusion lamination, with a second bonding layer, in between (17a,17b; 27,28; 36c) of bonding polymer, and c) Extrusion coating (32c,34c) The first outermost (12; 22; 33c) heat-sealable, liquid-tight layer on the outer side of the aggregate layer (11; 21; 31c; 34b), on which the pre-fabricated polyethylene film (14; 26; 38c) is a cast and uniaxially oriented film composed of 60 to 100 percent linear low-density polyethylene (LLDPE), preferably 80 to 100 percent LLDPE, more desirable 90 to 100 percent LLDPE, and the pre-fabricated polyethylene film is also present. Total thickness of 15 to 25 micrometers; elastic modulus of at least 400 MPa in MD, and at least 500 MPa in CD, as measured by ASTM D 882-02 (2018) with a crosshead rate of 10 mm / min; tensile strength greater than 40, preferably greater than 50 MPa, in MD and greater than 100 in CD, as measured by ASTM D638M-14 (2017) with a crosshead rate of 200 mm / min; elongation at break less than 350 percent in MD and less than 100 percent in CD.As measured by ASTM D638M-14 (2017) at a crosshead rate of 200 mm / min, the initial sealing temperature, SIT, is 80 to 100 °C. As determined by ASTM F1921 (2018) at 2 N, the maximum hot bond strength is greater than 7 N, as measured by ASTM F1921 (2018), and the penetration resistance is 10 N or greater, as measured by ASTM F1306-16 (2016) at a crosshead rate of 500 mm / min.
17. The method as requested in claim 16 where procedure a) is performed by wet application with an aqueous dispersion of the adhesive composition, which includes a polymer bonding agent, to the fibers of the aggregate layer (11; 21) or to the fibers of the barrier layer or partition. A multi-layered barrier (15; 24) with a volume of 1 to 5 g / m² of dry weight, and the two fibers are pressed together as they are passed through laminating rollers, without forced drying.
18. Pouch packaging containers (50) for packaging oxygen-sensitive food products, such as liquid food products,Semi-liquid or viscous or water, containing laminated packaging material (10; 20) as defined in any of the claims 1-15,