A method for curing a polythiourethane-based substrate coupled with a wafer having a microstructure.

TH2501004069APending Publication Date: 2026-11-02ESSILOR INTERNATIONAL(COMPAGNIE GENERALE D OPTIQUE)
0 Cites 0 Cited by

Patent Information

Application Number
TH2501004069
Authority / Receiving Office
TH · TH
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-12-21
Publication Date
2026-11-02
Patent Text Reader

Abstract

DEPCT68 The invention describes a method for curing a cast substrate based on polythiorethane, consisting of the provision of a first component A, consisting of a polythiorethane prepolymer A1 containing isocyanate or isothiocyanate end groups with the formula -NCX where X is O or S; the provision of a second component B, consisting of a polythiorethane prepolymer B1 containing thiol end groups or containing at least one polythiol monomer B2; the provision of a microstructured wafer made of a thermoplastic material with an inner and outer surface, where the inner surface of the wafer is microstructured; the mixing of components A and B and the filling of the molding cavity with the resulting mixture, where such cavity is defined by the inner surface of the microstructured wafer and at least part of the mold section; the curing of the mixture and the formation of a polythiorethane-based substrate bonded to the microstructured wafer.
Need to check novelty before this filing date? Find Prior Art

Claims

DEPCT68 1. Method for curing polythiourethane-based cast substrates, comprising the following steps 1), 2), 3), 4), 5), and 6) or 1'), 2'), 3), 4), 5), and 6): 1) Preparation of component one A, comprising a polythiourethane prepolymer A1 with isocyanate or isothiocyanate end groups with the formula -NCX where X is O or S, such prepolymer A1 is prepared from at least one polythiol monomer and at least one polyisocyanate or polyisothiocyanate monomer; 2) Preparation of component two B, comprising a polythiourethane prepolymer B1 with thiol end groups, such prepolymer B1 is prepared from at least one polythiol monomer. All and at least one polyisocyanate or polyisothiocyanate monomer, or: 1') Provision of a first component A incorporating a pre-polythiourethane A1 polymer containing an isocyanate or isothiocyanate end group with the formula -NCX, where X is O or S,The procedure for claim 1 is as follows: 1) Pre-polymer A1, prepared from at least one polythiol monomer and at least one polyisocyanate or polyisothiocyanate monomer; 2) Provision of a second component B, composed of at least one polythiol monomer B2; 3) Provision of a microstructured wafer made of a thermoplastic material with an inner and outer surface, where the inner surface of the wafer has a microstructure; 4) Mixing of the first and second components A and B and filling of the molding cavity with the resulting mixture, where the molding cavity is defined by the inner surface of the microstructured wafer and at least part of the mold section; 5) Curing of the mixture to obtain a polythiourethane-based substrate; and 6) Reattachment of the polythiourethane-based substrate to the microstructured wafer.This consists of the following steps 1) and 2): 1) Preparation of component one A, which comprises a polythiourethane prepolymer A1 containing isocyanate or isothiocyanate end groups with the formula -NCX where X is O or S; such prepolymer A1 is prepared from at least one polythiol monomer and at least one polyisocyanate or polyisothiocyanate monomer; 2) Preparation of component two B, which comprises a polythiourethane prepolymer B1 containing thiol end groups; such prepolymer B1 is prepared from at least one polythiol monomer.

3. A method under one of the preceding claims, where the mixture obtained in step 4) contains at least one catalyst.

4. A method under one of the preceding claims, where the incubation time of step 5) is less than 10 hours, preferably less than 5 hours.

5. A method under one of the preceding claims,Where the amounts of polyisocyanate or polyisothiocyanate monomer and polythiol monomer are adjusted so that the molar ratio of NCX / SH groups for mixtures of polyisocyanate or polyisothiocyanate and polythiol monomers range from 3:1 to 30:1 for the preparation of polythiourethane prepolymer A1 and / or the molar ratio of SH / NCX groups for mixtures of polyisocyanate or polyisothiocyanate and polythiol monomers range from 3:1 to 30:1 for the preparation of polythiourethane prepolymer B1, where X is O or S.

6. A method based on one of the preceding claims, where the substrate is an optical lens substrate.

7. A method based on one of the preceding claims, where the microstructure consists of...

8. A number of microlenses.

9. A method under one of the preceding claims, where the inner surface of the wafer defines a number of concave and / or convex projections.

10. A method under one of the preceding claims, where the microstructured wafer is made of polycarbonate.

11. A method under one of the preceding claims,10. Where the blurring value of the polythiourethane-based substrate with the microstructured wafer bonded to it as defined by ASTM D1003-00 is less than or equal to 6%.

11. According to one of the preceding claims, where the relative visible spectrum transmission factor Tv of the polythiourethane-based substrate with the microstructured wafer bonded to it as defined by ISO 8980-3 is greater than or equal to 74%.

12. According to one of the preceding claims, where no compounds from the mixture prepared in step 4) are diffused into the microstructured wafer during steps 4) and 5).

13. According to one of the preceding claims, where step 4) involves the positioning, in the forming cavity of the casting assembly, of the microstructured wafer in such a way that the outer surface of the wafer contacts the surface of the casting assembly.Where the die assembly for casting is assembled with the said die part; 14. Any of the methods under claims 1 through 13, where step 4) is performed with a two-part die assembly, the first part of which is the said die part and the second part of which is a wafer with the said microstructure; 15. Any of the methods under the preceding claims, where the method does not involve the deposition of the catalytic element on the inner surface of the die part and / or on at least one surface of the filter element after being positioned in the forming cavity;