Random polypropylene copolymer composition with improved impact resistance for pipe applications.

TH2501004193APending Publication Date: 2026-11-09BOREALIS AG +1
0 Cites 0 Cited by

Patent Information

Application Number
TH2501004193
Authority / Receiving Office
TH · TH
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-12-21
Publication Date
2026-11-09
Patent Text Reader

Abstract

DEPCT68 The invention relates to a polypropylene composition consisting of a basic resin (A) and a nucleating agent (B), in which the basic resin (A) contains a bimodal propylene copolymer (PP) with at least one comanomer being ethylene, in which the bimodal propylene copolymer (PP) contains (PP1) the first propylene copolymer component and (PP2) the second propylene copolymer component, and in which the first propylene copolymer component (PP1) differs from the second propylene copolymer component (PP2), and in which the weight ratio of the first propylene copolymer component (PP1), which includes the second propylene copolymer component (PP2), Alternative repolymers to the second propylene copolymer (PP2) component are 30:70 to 70:30, where the polypropylene component has (a) a flow rate of MFR2 (2.16 kg, 230 °C) of 0.15 to 0.50 g / 10 min, determined according to ISO 1133 at 230 °C and a load of 2.16 kg, and (b) a total comonomer content of 3.5 to 5 percent.0 by weight, considering the total weight of the bimodal propylene copolymer (PP) as specified in the invention description; (c) cold soluble xylene (XCS) content equal to or less than 8.2%, considering the total weight of the bimodal propylene copolymer (PP) as specified in ISO 16152; and (d) Charpy notch impact strength at 23 °C of 45.0 kJ / m² to 95.0 kJ / m² and Charpy notch impact strength at 0 °C of at least 6.0 kJ / m², both specified in ISO 179 / eA:2000 using a 1A notch injection molding process for the production of such polypropylene components, products containing such polypropylene components and the use of such polypropylene components for the production of products.
Need to check novelty before this filing date? Find Prior Art

Claims

DEPCT68 1. A polypropylene composition consisting of a base resin (A) and a nucleating agent (B), in which the base resin (A) contains a bimodal propylene copolymer (PP) with at least one comanomer being ethylene, in which the bimodal propylene copolymer (PP) contains (PP1) the first propylene copolymer component and (PP2) the second propylene copolymer component, and in which the first propylene copolymer component (PP1) differs from the other copolymer components. The second propylene copolymer (PP2) and where the weight ratio of the first propylene copolymer (PP1) component, which includes an alternative prepolymer component, to the second propylene copolymer (PP2) component is from 30:70 to 70:30, and where the polypropylene components have (a) a flow rate of MFR2 (2.16 kg, 230 °C) of 0.15 to 0.50 g / 10 min, determined according to ISO 1133 at 230 °C and a load of 2.16 kg, and (b) a total comonomer content of 3.5 to 5.0 percent by weight, considering the total weight of the bimodal propylene copolymer (PP).(c) cold soluble xylene (XCS) content equal to or less than 8.2% by weight of the bimodal propylene copolymer (PP) as specified in ISO 16152, and (d) Charpy notch impact strength at 23 °C of 45.0 kJ / m² to 95.0 kJ / m² and Charpy notch impact strength at 0 °C of at least 6.0 kJ / m², both specified in ISO 179 / eA:2000 using a 1A notch injection molding process.

2. Polypropylene composition according to claim 1 where the weight ratio of the comonomer content of The ratio of the first propylene copolymer component (PP1) to the comonomer content of the bimodal propylene copolymer (PP), both expressed as a percentage by weight, C2PP1 / C2PP is 0.40 to 0.

75.

3. The polypropylene composition according to claim 1 or 2, where the comonomer content of the second propylene copolymer component (PP2) is 4.5 to 9.0 by weight, considering the total weight of theThe second propylene copolymer component (PP2) is defined as described in the specifications of the invention, and / or the weight ratio of the comonomer content of the first propylene copolymer component (PP1) to the comonomer content of the second propylene copolymer component (PP2), both expressed as percentage by weight C2PP1 / C2PP2 is 0.36 to 0.

54.

4. Polypropylene components according to any prior claim. Where the first propylene copolymer component (PP1) has a higher MFR2 than the second propylene copolymer component (PP2) which is desirable, and where the first propylene copolymer component (PP1) has an MFR2 flow rate of 0.4 to 2.0 g / 10 min and / or where the bimodal propylene copolymer (PP) has an MFR2 flow rate of 0.15 to 0.50 g / 10 min.

5. Polypropylene compositions according to one of the preceding claims where the ratio of MFR2 of the bimodal propylene copolymer (PP) to the MFR2 of the first propylene copolymer component (PP1) MFR2 PP / MFR2 PP1 is 0.20 to 0.

50.

6. Polypropylene compositions according to one of the preceding claims.Where the weight ratio of the first propylene copolymer component (PP1), which includes an alternative prepolymer component, to the second propylene copolymer component (PP2) is between 38:62 and 60:

40.

7. Polypropylene compositions under one of the preceding claims with a flexural modulus of 700 to 1,400 MPa as defined in ISO 178 and / or a tensile modulus of 700 to 1,200 MPa as defined in ISO 527-2, using injection molding type 1A.

8. Polypropylene compositions under one of the preceding claims. where the bimodal propylene copolymer (PP) contains soluble xylene (XCS) of 4.0 to 8.0 percent by weight, as defined by ISO 16152 at 25 °C.

9. Polypropylene compositions under any of the preceding claims with a melting temperature (Tm) of 135 to 155 °C as defined by ISO 11357-3 and / or a crystallization temperature (Tc) of not less than 100 °C as defined by ISO 11357-3.

10. Polypropylene compositions under any of the preceding claims where the bimodal propylene copolymer (PP)11. A polypropylene composition according to one of the preceding claims in which the nucleating agent (B) is a polymer of a vinyl compound with the following formula: CH2=CH-CHR1R2 (BI), in which R1 and R2 together form a saturated, unsaturated, or aromatic ring of 5 or 6 members, which may contain substituents or represent alkyl groups composed of 1 to 4 freely occurring carbon atoms, in which case where R1 and R2 form an aromatic ring, the hydrogen atoms of the moity -CHR1R2 are absent.

12. A process for the production of a polypropylene composition according to one of the preceding claims in which a random bimodal propylene copolymer (PP) with at least one commonomer of ethylene is polypolymerized. The polymerizes in a multi-step polymerization process under conditions with (I) a solid catalyst component consisting of magnesium halide, titanium halide and an internal electron donor, and (II) a cocatalyst.This is a multi-step process incorporating (a) a series of steps, including (a) the continuous polymerization of propylene with selected alpha-olefin commonomers of 2 or 4 to 8 carbon atoms, with ethylene preferred in the first polymerization step, by introducing a current of propylene, hydrogen and ethylene into the first polymerization step at a temperature of 60 to 80 °C and a pressure of 3,000 to 6,500 kPa to produce the first propylene copolymer component, where the first propylene copolymer component (PP1) has a flow rate of MFR2 of 0.4 to 2.0 g / 10 min (2.16 kg; 230 °C; (b) The removal of the combined propylene copolymer component one (PP1) from the first polymerization step and the transfer of such current to the second polymerization step. (c)Polymerization of propylene with a selected comonomer of alpha-olefins with 2 or 4 to 8 carbon atoms, with the desired ethylene in the second polymerization step, by introducing a current of propylene, ethylene and, optionally, hydrogen into the said second polymerization step at a temperature of 70 to 90 °C and a pressure of 1,000 to 3,000 kPa to produce a bimodal propylene copolymer (PP) of the said first propylene copolymer component (PP1) and the second propylene copolymer component (PP2). (d) Continuously removing the assembled bimodal propylene copolymer (PP) from the second polymerization step and, optionally, (c) mixing of the aforementioned bimodal propylene copolymer (PP) with additives, and (d) extrusion of the aforementioned bimodal propylene copolymer mixture into pellets with a flow rate of MFR2 (2.16 kg; 230 °C; ISO 1133) of 0.15 to 0.5 g / 10 min, in which the first propylene copolymer component (PP1) differs from the second propylene copolymer component (PP2), and where it is desirable.

12. Has a higher MFR than the second polypropylene copolymer component (PP2).

13. Any polypropylene component under claims 1 through 11 that can be obtained by the process under claim 12.

14. A product which contains any one of the polypropylene components under claims 1 through 11 or claim 13.

15. The use of any one of the polypropylene components under claims 1 through 11 or claim 13 for the manufacture of products.