Abstract

DEPCT68 The method for the recovery of precious metals as disclosed herein comprises the following steps: (S1) leaching of sulfate solution from used battery material; (S2) adding phosphorus compounds to the sulfate solution to precipitate aluminum phosphate; and (S3) separating aluminum phosphate from the sulfate solution by solid-liquid separation, where the sulfate solution contains sulfate metals at a concentration of 90 g / L or higher.
Need to check novelty before this filing date? Find Prior Art

Claims

DEPCT68 1. Method for the restoration of precious metals. A method comprising the following steps: (S1) leaching of sulfate solution from used battery material; (S2) addition of phosphorus compounds to the sulfate solution to precipitate aluminum phosphate; and (S3) separation of aluminum phosphate from the sulfate solution by solid-liquid separation, where the sulfate solution contains metal sulfates at a concentration of 90 g / L or higher.

2. Method of Reputation 1, where the sulfate solution contains aluminum at a concentration of 1 g / L or higher.

3. Method of Reputation 1, where the metal sulfate is at least one sulfate selected from a group comprising nickel, cobalt, manganese, lithium, copper, and aluminum.

4. Method of Reputation 1, where step (S1) includes the battery annealing step.

5. The method of claim 1 in which procedure (S1) includes a procedure for the recovery of deionized lithium using water without carbon dioxide. 6.

7. Method of Claim 1 where the phosphorus compound in step (S2) is added in an amount of 0.1 percent to 7.0 percent by weight, based on the weight of the sulfate solution.

8. Method of Claim 1 where the molar ratio of phosphorus present in the added phosphorus compound to aluminum present in the sulfate solution (molar ratio P / Al) is 0.92 to 1.

72.

9. Method of Claim 1 where the phosphorus compound is sodium phosphate.

10. Method of Claim 1 where step (S2) is 2 to 8 hours.

11. Method of Claim 1 where step (S2) is performed at 25 °C to 95 °C.

12. Method of Claim 1 where the sulfate solution in step (S2) has a pH of 2.0 to 5.

0.

13. Method of Claim 1 where at least 96.0 percent by weight of aluminum is present.

13. The method of claim 1 is further incorporated with step (S4) of the removal of phosphorus present in the sulfate solution. 14.The procedure of claim 13 is that the sulfate solution in step (S4) has a pH of 5.0 or higher.