Steel plates, components, and methods for manufacturing them.

TH2501004899APending Publication Date: 2026-11-09JFE STEEL CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
TH2501004899
Authority / Receiving Office
TH · TH
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-01-30
Filing Date
2024-01-25
Publication Date
2026-11-09
Patent Text Reader

Abstract

DEPCT69 21 / 10 / 2568 provided for high-strength steel plates and components with excellent slow-crack properties and manufacturing methods. The steel plates have a chemical composition containing the following elements in percentage by mass: C: not less than 0.15% and not more than 0.45%, Si: not more than 2.0%, Mn: not more than 4.0%, P: not more than 0.10%, S: not more than 0.010%, soluble Al: not more than 0.50%, N: not more than 0.010%, and B: not less than 0.0008% and not more than 0.0100%, with the remainder being Fe and unintended impurities. The steel plates have a microstructure where the area ratio of martensite to the total microstructure is not less than 85% and not more than 95%, the area ratio of ferrite to the total microstructure is not less than 5% and not more than 15%, and the average crystal grain size... The ferrite density is 10 µm or less, and the density of the number A of the sediment with an equivalent circle diameter of 500 nm or more follows the formula: A (number / sq mm) is less than or equal to 8.5 x 10⁵ x [B].
Need to check novelty before this filing date? Find Prior Art

Claims

DEPCT69 21 / 10 / 2568 1. Steel plates with a chemical composition containing the following elements in % by mass: C: not less than 0.15% and not more than 0.45%; Si: not more than 2.0%; Mn: not more than 4.0%; P: not more than 0.10%; S: not more than 0.01%; dissolved Al: not more than 0.50%; N: not more than 0.010%; and B: not less than 0.0008% and not more than 0.0100%, with the remainder being Fe and unintended impurities, where the steel plate has a steel microstructure in which the area ratio of martensite to the total microstructure is not less than 85% and not more than 95%, the area ratio of ferrite to the total microstructure is not less than 5% and not more than 15%, and the average crystal grain size of ferrite is 10 micrometers or less. Where the density of quantity A of sediment with equivalent circle diameter of 500 nm or more follows the formula (1), A (quantity / sq mm) is less than or equal to 8.5 x 10⁵ x [B] formula (1), where [B] represents the quantity (% by mass) of B.

2. Steel plate according to claim 1, where 50%Or even more so in terms of area ratio.

3. Steel plates according to claim 1 or 2, where the chemical composition is further defined as a percentage by mass with one or more elements selected from the following: Cu: not more than 1.00%, Cr: not more than 1.00%, Nb: not more than 0.10%, Ti: not more than 0.10%, V: not more than 0.50%, Mo: not more than 0.50%, Ni: not more than 1.00%, Sb: not more than 0.10%, Sn: not more than 0.10%, As: not more than 0.10%, Ta: not more than 0.10%, Ca: not more than 0.020%, Mg: not more than 0.020%, Zn: not more than 0.020%, Co: not more than 0.020%, Zr: not more than 0.020%, W: not more than 0.020%, and REM: Not more than 0.020% 4. Steel plates as per any of the claims in Treaties 1 through 3 with a coating on the surface of the steel plate.

5. Components using steel plates as per any of the claims in Treaties 1 through 4.

6. Methods of manufacturing steel plates which include maintaining the state of flat steel billets with the chemical composition as per Treaty 1 or 3.The heating and holding temperature of the flat bar is 1100°C or higher for 30 minutes or more. Then, the flat bar is subjected to hot rolling under conditions of a holding time of not less than 20 seconds and not more than 150 seconds at 900 to 1000°C and a finishing rolling temperature of 850°C or higher. The rolled steel is cooled at an average cooling rate of 40°C / second or more from the finishing rolling temperature to 650°C. The rolled steel is then coiled at a coiling temperature of 650°C or lower to obtain hot-rolled steel sheets. The hot-rolled steel sheets are then cold-rolled at a reduction of 40% or more to obtain cold-rolled steel sheets. Finally, the cold-rolled steel sheets are continuously annealed by heating them from 400°C to annealing temperatures of 830 to 950°C at an average heating rate. 1.0 degrees Celsius / second or more7. A method for producing steel plates according to claim 6 where the continuously annealing steel plate is subjected to surface coating.

8. A method for producing assemblies which includes at least one forming and welding process of the steel plate according to claims 1 to 4.