A method for producing high-yield pressure-hardened parts.
Patent Information
- Application Number
- TH2501004952
- Authority / Receiving Office
- TH · TH
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-01-30
- Filing Date
- 2024-01-19
- Publication Date
- 2026-11-02
Abstract
Claims
DEPCT68 1. The method of pressure hardening which includes the following steps: A) Provision of a coated steel plate (5) made of a metallized steel plate (4), such a metallized steel plate which is incorporated with a heat-treated steel plate (1) coated with a metallized coating (2), on which such a metallized steel plate is superimposed over at least part of the metallized coating by a polymerized coating (3) on one side of such a metallized steel plate. The second side of such a metallized steel plate may be optionally superimposed over at least part of the metallized coating by a polymerized coating (3). The total thickness of such polymerized coating on such a coated steel plate (5) is from 3.0 to 10.0 micrometers of polymer containing no silicone and the nitrogen content of the layer is less than 1% by weight, expressed in relation to the polymerized coating layer; the polymerized coating layer containing a pigment with carbon content from 3 to 30% by weight, expressed in relation to the polymerized coating layer; B) Trimming or cutting of the aforementioned coated steel sheet (5) into blanks; C) Heating of the blanks in a furnace at a set temperature of 850 to 950 degrees Celsius and between 2.00 to 3.40 minutes if the thickest part of the blank is thicker than 0.6 mm and thinner than or equal to 1.5 mm and between 2.50 to 4.50 minutes if the thickest part of the blank is thinner than or equal to 1.5 mm. The above are thicker than 1.5 mm and thinner than 3.0 mm. D) Transferring the hot blank sheet to the press tool. E) Forming the hot blank sheet into parts and press-hardening the parts into press-hardened parts. 2.Methods under Reputation 1 where the blank processed in steps C) through E) is a patched blank and where the following steps are performed after step B) and before step C): B1) Provision of a coated steel sheet (5) of step A) or another coated steel sheet of step A); B2) Trimming or cutting of such coated steel sheet into a patch; B3) Attaching such patch to the top of the blank obtained in step B) where the total polymerization of the surface area between the two sheets is less than 7.0 µm; B4) Spot welding of the blank and patch by means of an electric current flowing through a pair of electrodes to obtain a patched blank; 3. Methods under Reputation 1 or 2 where in step C) the heating temperature is set from 900 to 950 °C; 4. Any of the methods under Reputation 1 through 3. In step A), the elements of the polymer are selected from a list containing C, H, O, N.
6. The method under claim 1 or 4 in which step A) the polymerized coating (3) is obtained from a resin in the form of a dispersion or emulsion in the aqueous phase.
7. The method under claim 5 in which step A) the polymerized coating (3) is obtained from an acrylic resin.
8. The method under claim 1 to 4 in which step A) the polymerized coating (3) is obtained from a resin in the form of a solution in a non-aqueous solvent.
9. The method under claim 7 in which step A) the polymerized coating is obtained from an epoxy or acrylic resin.
10. The method under claim 1 to 4 in which step A) the polymerized coating (3) is assembled with a film bonded by rollers to 10. Metallic surface coating.
10. The method under Reputation 9 in which, in step A) the polymerized coating is incorporated with a film of polyethylene-terephthalate or polyethylene or polybutylene-terephthalate or polypropylene.
11. The method under Reputation 1 through 10 in which, in step A) the pigment is incorporated at least partially with activated carbon.
12. The method under Reputation 1 through 11 in which, in step A) the pigment is incorporated at least partially with graphite.
13. The method under Reputation 11 or 12 in which, in step A) the amount of activated carbon in the polymerized coating is less than 5% by weight relative to that layer.
14. The method under Reputation 1 through 13. Where in step A) the coating is a metallic, aluminum-based coating.
15. The method under either claim 1 or 14 where in step A) the coating is a metallic composition including by weight up to 15% silicone, up to 5% iron, the balancing factor being aluminum and unavoidable impurities. 16.Any of the methods under claims 1 through 13, in which step A) the surface is coated with a zinc-based metal.
17. A vehicle which is assembled with at least one pressure-hardened part obtained by any of the methods under claims 1 through 16.