Hot-rolled thin steel sheets
Patent Information
- Application Number
- TH2501004991
- Authority / Receiving Office
- TH · TH
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-01-31
- Filing Date
- 2024-01-31
- Publication Date
- 2026-11-09
Abstract
Claims
DEPCT69 21 / 10 / 2568 1. Hot-rolled steel sheet with the following chemical composition (in percentage by mass): C: 0.045 to 0.120 percent, Si: 0 to 3.00 percent, Mn: 1.20 to 2.60 percent, Ti: 0.020 to 0.180 percent, Al: 0.010 to 0.400 percent, P: 0.080 percent or less, S: 0.0100 percent or less, N: 0.0050 percent or less, O: 0.010 percent or less, Nb: 0 to 0.100 percent, V: 0 to 1.000 percent, Cu: 0 to 1.000 percent, Cr: 0 to 2.000 percent, Mo: 0 to 3.000 percent. Percentage, Ni: 0 to 0.500 percent, B: 0 to 0.0100 percent, Ca: 0 to 0.0500 percent, Mg: 0 to 0.0500 percent, REM: 0 to 0.100 percent, Bi: 0 to 0.100 percent, Ta: 0 to 0.100 percent, Zr: 0 to 0.500 percent, Co: 0 to 3.000 percent, Zn: 0 to 0.200 percent, W: 0 to 0.200 percent, Sb: 0 to 0.500 percent, As: 0 to 0.050 percent, Sn: 0 to 0.0.50 percent, and the remainder consisting of Fe and impurities, where GAMS / GAMI, which is the ratio of GAMI (the average area of the grain GAM at a depth of 1 / 4 from the surface in the sheet thickness direction) to GAMS (the average area of the grain GAM in the region from the surface to a depth of 200 micrometers in the sheet thickness direction), is 0.70 to 1.05, and in the microstructure at a depth of 1 / 4 from the surface in the sheet thickness direction, the area ratio of regions with GAM greater than 0.6 degrees is 50 percent or more, and the sum of the area ratio of regions with GAM greater than 3.0 degrees and the area ratio... The austenite residue is less than 15 percent, and the standard deviation of the mean area of the grain GAM in the region from the surface to a depth of 200 micrometers in the sheet thickness direction is 0.25 to 0.65 degrees.
2. Hot-rolled thin steel sheets according to claim 1, where the chemical composition includes (in percentage by mass) one or more elements selected from a group consisting of: Nb: 0.001 to 0.100 percent, V: 0.0.001 to 1.000 percent, Cu: 0.001 to 1.000 percent, Cr: 0.001 to 2.000 percent, Mo: 0.001 to 3.000 percent, Ni: 0.001 to 0.500 percent, B: 0.0001 to 0.0100 percent, Ca: 0.0001 to 0.0500 percent, Mg: 0.0001 to 0.0500 percent, REM: 0.001 to 0.100 percent, Bi: 0.001 to 0.100 percent, Ta: 0.001 to 0.100 percent, Zr: 0.001 to 0.500 percent, Co: 0.001 to 3.000 percent, Zn: 0.001 to 0.200 percent. W: 0.001 to 0.200 percent, Sb: 0.001 to 0.500 percent, As: 0.001 to 0.050 percent, and Sn: 0.001 to 0.050 percent.
3. Hot-rolled thin steel sheets according to claim 1 or 2 where in the microstructure at a position of 1 / 4 depth from the surface in the thickness direction, the area ratio of regions with a GAM greater than 0.6 degrees and less than 2.0 degrees is 50 percent or more. 4.Hot-rolled thin steel sheets according to claim 1 or 2 where in the microstructure at a depth of 1 / 4 from the surface in the thickness direction, the area ratio of the region with a GAM of 2.0 degrees or more is 50 percent or more.