High-strength steel plates and the methods for manufacturing the same thing.

TH2501005409APending Publication Date: 2026-11-16JFE STEEL CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
TH2501005409
Authority / Receiving Office
TH · TH
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-06
Filing Date
2024-03-05
Publication Date
2026-11-16

Smart Images

  • Figure 2501005409_DRAWING_01
    Figure 2501005409_DRAWING_01
  • Figure 2501005409_DRAWING_02
    Figure 2501005409_DRAWING_02
  • Figure 2501005409_DRAWING_03
    Figure 2501005409_DRAWING_03
Patent Text Reader

Abstract

DEPCT68 is supplied as a high-strength steel plate with a tensile strength of not less than 1,180 MPa, excellent bending ability and excellent delayed cracking resistance, and a wide suitable free-range when formed from bending of the shear end surface. The steel plate incorporated into the high-strength steel plate will have, by mass, C: 0.030%-0.500%, Si: 0.50%-2.50%, Mn: 1.50%-5.00%, P: not more than 0.100%, S: not more than 0.0200%, Al: not more than 1.000%, N: not more than 0.0100%, O: not more than 0.0100%, and Nb: 0.005%-0.100%, with the following properties: The balanced composition includes Fe and unavoidable impurities; the martensite content is not less than 70%; the residual austenite content is 3%-20%; the total content of ferrite and benetic ferrite is not more than 10%; the instability index k of residual austenite is less than 6.1; and the instability index d of residual austenite in the initial processing stage is less than 5.7.
Need to check novelty before this filing date? Find Prior Art

Claims

DEPCT68 1. High-strength steel plates assembled from steel sheets, in which the steel sheets have a chemical composition including, by mass, C in an amount not less than 0.030% and not more than 0.500%, Si in an amount not less than 0.50% and not more than 2.50%, Mn in an amount not less than 1.50% and not more than 5.00%, P in an amount not more than 0.100%, S in an amount not more than 0.0200%, Al in an amount not more than 1.000%, N in an amount not more than 0.0100%, O in an amount not more than 0.0100%, and Nb in an amount not less than 0.005% and not more than 0.100%, with a balancing effect consisting of Fe and unavoidable impurities; the steel sheets have a microstructure in which the amount of martensite is not less than 70%, and the amount of residual austenite is not less than 3% and not more than... 20%, and the total amount of ferrite and benetic ferrite is no more than 10%, the instability index k of residual austenite is less than 6.1.And the instability index d of the austenite remaining in the initial processing stage is less than 5.

7.

2. High-strength steel plate according to claim 1, where the chemical composition continues to include at least one element selected from The group consists of, by mass, Ti in an amount not exceeding 0.200%, V in an amount not exceeding 0.200%, Ta in an amount not exceeding 0.10%, W in an amount not exceeding 0.10%, B in an amount not exceeding 0.0100%, Cr in an amount not exceeding 1.00%, Mo in an amount not exceeding 1.00%, Ni in an amount not exceeding 1.00%, Co in an amount not exceeding 0.010%, Cu in an amount not exceeding 1.00%, Sn in an amount not exceeding 0.200%, Sb in an amount not exceeding 0.200%, Ca in an amount not exceeding 0.0100%, Mg in an amount not exceeding 0.0100%, REM in an amount not exceeding 0.0100%, Zr in an amount not exceeding 0.100%, and Te in an amount not exceeding... 0.100%, Hf in a quantity not exceeding 0.10%,and Bi in an amount not exceeding 0.200%.

3. High-strength steel plates according to claim 1 or 2, which include a metal coating layer on the surface of the steel plate.

4. Methods for the production of high-strength steel plates according to claim 1 or 2, methods that include: maintaining steel slabs with the chemical composition according to claim 1 or 2 at a slab heating temperature of not less than 1,220°C and subsequently, hot rolling operations to obtain hot-rolled steel sheets; cooling of the hot-rolled steel sheets under conditions of an average cooling rate v1 from 800°C to 600°C of not less than 30°C / second and subsequently, acid etching and cold rolling operations to obtain cold-rolled steel sheets; heat treatment A in which the cold-rolled steel sheets are held at a temperature T1 of not less than 800°C for 10 seconds or more and are further cooled to a cooling stop temperature Ta of not less than 100°C and not higher (Ms point - 80°C), where, in heat treatment A, the average cooling rate v2 from 750°C to 600°C of not less than 20°C / second, the average cooling rate v3 from Ms point to the cooling stop temperature Ta is not higher than 150 degrees Celsius / second,And the tensile force F applied to the cold-rolled steel plate from point Ms to the cooling stop temperature Ta is not less than 5 MPa and not more than 100 MPa; after heat treatment A, heat treatment B is performed in which the cold-rolled steel plate is held at a temperature T2 of not less than the cooling stop temperature Ta and not more than 450 °C for 5 seconds or more and 1,000 seconds or less and is further cooled; after heat treatment B, heat treatment C is performed in which the cold-rolled steel plate is heated to a temperature T3 of not less than 150 °C and not more than 400 °C and is further cooled without being held at T3, where, in heat treatment C,The average cooling rate of v4, from 150°C to 50°C, must be no lower than 1.0°C / second and no higher than 50.0°C / second; And after heat treatment A and before heat treatment C, the processing of the cold-rolled steel sheet to deliver an equivalent plastic stress of not less than 0.10% and not more than 5.00% to the cold-rolled steel sheet, where the point Ms is represented in units of °C and is determined by the formula (a): Ms = 519 - 474 x [%C] - 30.4 x [%Mn] - 12.1 x [%Cr] - 7.5 x [%Mo] - 17.7 x [%Ni] ...(a). In formula (a), [%M] represents the amount of element M in the chemical composition, and where the element M is not present, [%M] has a value of 0.

5. Method for the production of high-strength steel sheets according to claim 4, where the cold-rolled steel sheet is subjected to a metallization treatment operation,