Manufacturing methods for precursors of anode electrode reactants.
Patent Information
- Application Number
- TH2501007113
- Authority / Receiving Office
- TH · TH
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-12-21
- Filing Date
- 2024-04-17
- Publication Date
- 2026-11-02
Abstract
Claims
DEPCT69 1. Method for the production of anode reactive material using a batch reactor, a method consisting of the following steps: (S1) nucleation of the reactant; (S2) nucleation of the nuclei formed in step S1; (S3) further nucleation of the nuclei formed in step S2; (S4) Further growth of the nuclei that were grown in step S3, where the stirring rate in the batch reactor is set to: 200 rpm to 900 rpm during step S2, 800 rpm or less during step S3, and 700 rpm or less during step S4, and the reaction solution is designed to overflow when the batch reactor is full.
2. Method of claim 1, where the co-precipitation reaction is carried out for 1 to 20 hours in step S2.
3. Method of claim 1, where the substrate has an average particle size D50 of 6.5 µm to 13.0 µm after step S3 is completed. 4.
4. Method of Claim 1, where the stirring speed inside the batch reactor during step S1 is between 250 rpm and 1,000 rpm.
5. Method of Claim 1, where the solution of the transition metal compounds is fed into the batch reactor at a flow rate of: 5 ml / min to 40 ml / min during steps S2 and S3, and 2 ml / min to 30 ml / min during step S4.
6. Method of Claim 5, where the solution of the transition metal compounds contains at least one element selected from the group consisting of nickel, cobalt, and manganese.
7. Method of Claim 5, where the solution of the transition metal compounds contains: nickel in an amount of 60 mol to 96 mol; cobalt in an amount of 0 mol to 20 mol; and manganese in amounts from 4% by mol to 40% by mol.
8. Method of claim 1, where a solution of nitrogen-containing compounds is fed at a flow rate of: 1.0 ml / min to 10.
9. Method of Claim 1, where the solution of the basic compound is fed at a flow rate of: 3 ml / min to 35 ml / min during steps S2 and S3, and 2 ml / min to 30 ml / min during step S4.
10. Method of Claim 1, where the reaction solution inside the batch reactor has a pH of 10.5 to 13.5 in step S1.
11. Method of Claim 1, where the reaction solution inside the batch reactor has a pH of 10.5 to 13.0 in steps S2, S3, and S4.
12. Method of Claim 1, where the reaction solution inside the batch reactor has... The ammonia concentration is 3,000 parts per million to 7,000 parts per million in steps S2, S3, and S4.
13. The method of claim 1, where the reaction solution within a batch reactor has a residual nickel concentration of 250 parts per million or less in steps S2, S3, and S4.14.Method of Claim 1, in which the anode reactive material precursors created by following steps S1 to S4 have a Span of 0.38 or less when measured according to the following Equation 1: [Equation 1] Span = (Particle size D90 - Particle size D10) / Average particle size D50.
15. Method of Claim 1, incorporating additional step (S5) of washing and drying the anode reactive material precursors created by following steps S1 to S4.