RBSiC components incorporating SiC coatings, the use of SiC coatings, and methods for manufacturing these components.

TH2501007460APending Publication Date: 2026-11-16SCHUNK INGENIEURKERAMIK GMBH
0 Cites 0 Cited by

Patent Information

Application Number
TH2501007460
Authority / Receiving Office
TH · TH
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-03
Publication Date
2026-11-16
Patent Text Reader

Abstract

DEPCT69 28 / 01 / 2569 The invention relates to a component (1) assembled with a component (2) made of reaction-bonded silicon carbide (RBSiC), a component (2) whose surface (3) is coated with at least some of the coating (4), the coating (4) consisting of silicon carbide (SiC) with a thickness of at least 25 µm. The invention also relates to the use of such SiC coating and to a method for fabricating components assembled with the SiC coating.
Need to check novelty before this filing date? Find Prior Art

Claims

DEPCT69 28 / 01 / 2569 1. Component (1) containing a component (2) made of reaction-bonded silicon carbide (RBSiC), characterized by the fact that the component (2) has a surface (3) coated at least partially with a coating (4), in which the coating (4) consists of silicon carbide (SiC) with a coating thickness of at least 25 µm.

2. Component (1) as claimed in claim 1, characterized by a coating thickness of at least 50 µm, preferably at least 100 µm, preferably at least 300 µm, and preferably at least 500 µm.

3. Component (1) as claimed in either claim 1 or 2, characterized by the fact that the surface (3) has sub-regions aligned in the angular direction. Different areas, where the coating (4) is placed at least in a sub-area pointing in at least two of the six spatial directions. 4.Component (1), as claimed in claim 3, is characterized by the coating (4) being placed in a sub-area pointing in at least three of the six spatial directions, preferably at least four of the six spatial directions, preferably five of the six spatial directions, and preferably all six spatial directions.

5. Component (1), as claimed in one of the preceding claims, is characterized by the coating (4) being placed in at least a sub-area of ​​the body surface (3) which is part of the stiffening structure (5) of component (2), for example, ribs, framing, bracing, tension bars, compression bars, honeycomb, edges or thickening sections.

6. Component (1), as claimed in claim 5, is characterized by the stiffening structure (5) being a frame, scaffolding, or bionic structure. 7.

8. Component (1), as claimed under any of the preceding claims, characterized as silicon carbide (SiC) of coating (4), shall have a purity of 98 percent, preferably 99 percent, and highly desirable 99.9 percent.

9. Component (1), as claimed under any of the preceding claims, characterized as coating (4), shall have a coating thickness of no more than 2 millimeters.

9. Component (1), as claimed under any of the preceding claims, characterized as coating (4), shall have a particle size of no more than 20 micrometers, preferably no more than 10 micrometers, more preferably no more than 7 micrometers, more preferably no more than 4 micrometers, and highly desirable no more than 1 micrometer. 10.Component (1), as claimed under any of the prior claims, is characterized by the fact that Component (2) has an average particle size of at least 25 µm, preferably at least 50 µm, preferably more, preferably at least 70 µm, preferably more, preferably at least 90 µm, and preferably at least 100 µm.

11. Component (1), as claimed under any of the prior claims, is characterized by the fact that Component (2) has a silicon carbide (SiC) purity of less than 99 percent.

12. Component (1), as claimed under any of the prior claims, is characterized by the fact that Component (2) is at least partially 3D printed part or the green body of Component (2) is at least partially based on a 3D printed part. 13.Component (1), as claimed in any of the preceding claims, is characterized to be at least 70 percent, desirable to be 80 percent, desirable to be at least 85 percent, desirable to be at least 90 percent, desirable to be at least 95 percent, and desirable to be at most 100 percent of the surface (3) coated with coating (4).

14. Component (1), as claimed in any of the preceding claims, is characterized to be coating (4) which is either a CVD coating or a PVD coating.

15. Component (1), as claimed in any of the preceding claims, is characterized to be coating (4) which is an anti-corrosion coating.

16. Component (1), as claimed in any of the preceding claims, is characterized to be coating (4) which is uniformly structured. 17.Component (1), as claimed in any of the preceding claims, is characterized as a satellite support.

18. Component (1), as claimed in any of the claims 1 through 16, is characterized as an antenna support.

19. Component (1), as claimed in any of the claims 1 through 16, is characterized as a roller for a continuous kiln or roller kiln.

20. Component (1), as claimed in any of the claims 1 through 16, is characterized as a component part or workpiece holder.

21. Component (1), as claimed under any of the claims 1 through 16, is characterized as Component (1) being the fuel burner or radiation tube in the furnace.

22. Component (1), as claimed under any of the claims 1 through 16, is characterized as Component (1) being the sliding ring or double ring of the gasket assembly.

23. Sliding RingThe application of a (4) coating of silicon carbide (SiC) with a coating thickness of at least 25 µm for coating the surface of body (3) of component (2), made of reaction-bonded silicon carbide (RBSiC), of component (1), for: a) increasing the hardness of the surface of body (3) of component (1); and / or b) increasing the strength of component (1); and / or c) improving the chemical resistance of the surface of body (3) of component (1); and / or d) increasing the thermal stability of component (1).

24. The method for fabricating component (1) is composed of the following steps: a) Fabrication of component (2) by a. Creating a powdered green body from silicon carbide (SiC) and carbon source; b. Performing reaction sintering with infiltration of the green body with silicon (Si) to create a base made of reaction-bonded silicon carbide (RBSiC); b) Coating the surface of body (3) of component (2) with at least 25 µm thickness. Partially with a coating (4) of silicon carbide (SiC) with a coating thickness of at least 25 micrometers.The method as claimed in claim 24, which is characterized by the body surface (3) having sub-regions aligned in different spatial directions, where the coating (4) is coated in at least one sub-region pointing in at least two of the six spatial directions.

26. The method as claimed in either of claim 24 and 25, which is characterized by the body surface (3) of the component (2) intended for coating.

27. The method as claimed in any of Claims 24 to 26, characterized by the green body being produced by 3D printing.

28. The method as claimed in any of Claims 24 to 27, characterized by the coating being formed by CVD or PVD.

29. The method as claimed in any of Claims 24 to 28, characterized by the component (1) being structured as claimed in any of Claims 1 to 22.