Manufacturing method for polycarbonate resin component pellets.

TH2501008798APending Publication Date: 2026-11-09MITSUBISHI ENG PLASTICS CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
TH2501008798
Authority / Receiving Office
TH · TH
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-06-28
Filing Date
2024-06-11
Publication Date
2026-11-09
Patent Text Reader

Abstract

DEPCT69 17 / 03 / 2569 A method for producing polycarbonate resin pellets with excellent transparency in a more stable manner while achieving a high production rate using an extremely high torque twin-screw extruder. This method uses polycarbonate resin pellets with specific molecular weights and particle diameters as raw materials, combined with kneading the pellets under conditions of screw shaft torque density from 9.0 to 17.0 Nm / cm³, screw rotation speed from 400 to 800 rpm, [yield (kg / hr) / screw rotation speed (rpm) / cubic centimeter of distance from the center to the center of the two screw shafts] from 0.015 to 0.026 kg / hr / rpm / cm³, and a non-melting rate in the fins before reaching the binder from 2 to 30%, followed by extrusion of the material from the die and pelletizing.
Need to check novelty before this filing date? Find Prior Art

Claims

DEPCT69 17 / 03 / 2569 1. Method for producing polycarbonate resin pellets from polycarbonate resin granules using a twin-screw extruder, where the polycarbonate resin granules have an average viscosity molecular weight from 11000 to 27000 and a median diameter D50 from 400 to 1500 µm, measured by the wet dispersion method and the composite method. The polycarbonate resin granules were kneaded under the following conditions: the torque density of the screw shafts at the base of each screw ranged from 9.0 to 17.0 Nm / cm³, the screw rotation speed ranged from 400 to 800 rpm, and the value of [yield (kg / hr) divided by screw rotation speed (rpm) divided by cubic centimeters of distance between the center of the two screw shafts] was 0.015 to 0.0.26 kg / hr / rpm / cm³ to achieve a non-melting rate in the fins before reaching the mold holder ranging from 2 to 30%, and extrusion of the material from the mold and granulation of the material.

2. Method of Claim 1, where the removal of volatile matter is carried out under vacuum conditions using a vent with an opening prepared at the end of the kneading zone, with an opening length of 2.0 to 6.0 D (D is the diameter of the cylinder) in the direction of the screw shaft and prepared such that the distance from the furthest point of the vent opening to the end of the screw is 5.0 to 10.0 D.

3. Method of Claim 1 or 2, where the material freshly extruded from the mold has a temperature ranging from 260 °C to 330 °C.

4. Method of one of Claim 1 to 3, where the resulting polycarbonate resin granules have a total light transmittance of 50% or more as specified. The value is measured using the transmitted light according to the JIS K7361 standard.