Polythiol components, polymerizable components for optical materials and applications.

TH2601003593APending Publication Date: 2026-11-16MITSUI CHEMICALSINC 2 5
0 Cites 0 Cited by

Patent Information

Application Number
TH2601003593
Authority / Receiving Office
TH · TH
Patent Type
Applications
Current Assignee / Owner
Priority Date
2018-07-31
Filing Date
2013-08-13
Publication Date
2026-11-16
Patent Text Reader

Abstract

DEPCT69 Polythiol components include polythiol compounds (a) which include at least one of the compounds represented by the following formulas (6) to (8) as the main component (chemical formula) (6) (chemical formula) (7) (chemical formula) (8), and compound (b) in which, in the high-performance liquid chromatography measurement of the polythiol components under specified conditions, the peak area of ​​compound (b) appearing at a retention time from 6.5 min to 8.0 min is equal to or less than 3.0 compared to the peak area of ​​polythiol compound (a) which appears at a retention time from 22.0 min to 28.0 min. The processes for the production of polythiol components, methods for the production of molded products, molded parts, optical parts and lenses are also provided.
Need to check novelty before this filing date? Find Prior Art

Claims

DEPCT69 1. Polythiol composition consists of: a polythiol compound (a) which contains at least one of the compounds represented by the following formulas (6) to (8) as the main component (chemical formula) (6) (chemical formula) (7) (chemical formula) (8), and a compound (b) in which, under the following conditions, the peak area of ​​compound (b), which appears at a retention time of 6.5 min to 8.0 min, is equal to or less than 3.0 compared to the peak area of ​​polythiol compound (a), which appears at a retention time of 22.0 min to 28.0 min (measurement conditions). Column: YMC-Pack ODS-AA-312 (S5, 6 mm x 150 mm). Mobile phase: Acetonitrile / 0.01 Mole-aqueous potassium dihydrogen phosphate solution = 60 / 40 (volume / volume). Column temperature: 40°C. Flow rate: 1.0 mL / min. Detector: UV detector, wavelength 230 nm. Preparation of measurement solution: 160 mg of sample is dissolved and mixed in 10 mL of acetonitrile. Injection volume:

22. The polythiol compound according to claim 1 where the peak area of ​​compound (b), which appears at a retention time from 6.5 minutes to 8.0 minutes, is 0.01 to 3.0, compared to the peak area of ​​100 of polythiol compound (a), which appears at a retention time from 22.0 minutes to 28.0 minutes.

3. The polythiol compound according to claim 1 where the peak area of ​​compound (b), which appears at a retention time from 6.5 minutes to 8.0 minutes, is equal to or less than 2.0, compared to the peak area of ​​100 of polythiol compound (a), which appears at a retention time from 22.0 minutes to 28.0 minutes.

4. The polythiol compound according to claim 1 where the peak area of ​​compound (b), which appears at a retention time from 6.5 minutes to 8.0 minutes, is equal to or greater than 1.

5. Compared to the 100-peak area of ​​the polythiol compound (a), which appears at retention times from 22.0 min to 28.0 min.

5. The polythiol composition according to claim 1 in which compound (b) is composed of compounds with the following IR results measured by the Universal ATR method (IR results): 3300 / cm:NH.Stretching, 2541 per cm : SH Stretching, 1606 per cm : C=N Stretching, 1520 per cm : NH Bending 6. The process for the production of polythiol compounds consists of: a step of reacting 2-mercaptoethanol with an epihalohydrin compound, which is represented by the following formula (1), to obtain a polyalcohol compound, which is represented by the following formula (3) (chemical formula) (1), where X is the halogen atom (chemical formula) (2); a step of reacting the polyalcohol compound, which is represented by the following formula (4) (chemical formula) (4); a step of reacting the polyalcohol compound, which is represented by the following formula (4), to obtain an isothioranium salt, and a step of hydrolyzing the isothioranium salt to obtain a polythiol compound consisting of at least one polythiol compound (a) which is selected from The group consists of compounds represented by the following formulas (6) through (8) as the main component and compound (b) (chemical formula) (6) (chemical formula) (7).(Chemical formula) (8) and the acid washing step of the polythiol components obtained under temperatures of 10°C to 50°C to obtain the following polythiol components, in which, in the high potential liquid chromatography measurement of the polythiol components obtained by the acid washing step under the following conditions, the peak area of ​​compound (b) which appears at a retention time of 6.5 min to 8.0 min is equal to or less than 3.0 compared to the peak area of ​​polythiol (a) which appears at a retention time of 22.0 min to 28.0 min (measurement conditions). Column: YMC-Pack ODS-AA-312 (S5, 6 mm x 150 mm). Mobile phase: Acetonitrile / 0.01 Mole-aqueous potassium dihydrogen phosphate solution = 60 / 40 (volume / volume). Column temperature: 40°C. Flow rate: 1.0 mL / min. Detector: UV detector, wavelength 230 nm. Preparation of measurement solution: 160 mg of sample is dissolved and mixed in 10 mL of acetonitrile. Injection volume: 2 µL. 7.

8. The process for producing polythiol components according to patent 6, where the temperature is between 15°C and 50°C during the acid washing step.

9. The process for producing polythiol components according to patent 6, where the temperature is between 20°C and 50°C during the acid washing step.

10. The process for producing polythiol components according to patent 6, where the temperature is between 30°C and 45°C during the acid washing step.

11. Polymerization-capable components for optical materials comprising: polythiol components according to patent 1; and poly(thio)isocyanate compounds.

12. The method for producing molded products comprising: the step of mixing polythiol components according to patent 1 and poly(thio)isocyanate compounds to obtain polymerization-capable components for optical materials; and the process of injecting the polymerizing component into the mold and solidifying the molded component.

12. The molded product which is obtained by injecting the polymerizing component according to the claim.

10. Solidification; 13. Optical components incorporated into the molded product under claim 12; 14. Lenses incorporated into the optical components under claim 13.