Adhesive sheets, unit panels and video wall displays

The adhesive sheet with specific tensile properties and gel content addresses adhesive seepage and brightness issues in splicing displays, achieving uniform brightness and improved image quality.

TW202631936APending Publication Date: 2026-08-01LINTEC CORP
0 Cites 0 Cited by

Patent Information

Application Number
TW114145259
Authority / Receiving Office
TW · TW
Patent Type
Applications
Current Assignee / Owner
Priority Date
2024-12-27
Filing Date
2025-11-20
Publication Date
2026-08-01

AI Technical Summary

Technical Problem

The connection of multiple unit panels in splicing displays, particularly those using high-brightness Mini-LED or Micro-LED displays, leads to uneven brightness due to gaps between panels, and conventional adhesive layers cause adhesive seepage during laser cutting.

Method used

An adhesive sheet comprising a first adhesive layer, a second adhesive layer, and a core material between them, with specific tensile properties and gel content, preventing adhesive leakage during laser cutting and ensuring uniform brightness.

Benefits of technology

The adhesive sheet enables effective laser cutting of unit panels, reducing gaps and ensuring uniform brightness in splicing displays, enhancing image quality.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The technical problem of the present invention is to provide an adhesive sheet, a unit panel, and a splicing display with good laser cutting processability. This adhesive sheet (1A) is an adhesive sheet (1A) used to manufacture a unit panel (2A) constituting a splicing display. It has a first adhesive layer (12), a second adhesive layer (13), and a core material (14) disposed between the first adhesive layer (12) and the second adhesive layer (13). The elongation at break measured by a tensile test on the adhesive laminate (11) composed of the first adhesive layer (12), the core material (14) and the second adhesive layer (13) at a tensile speed of 200 mm / min is 1000% or less, or the fracture stress measured by the tensile test is 10 MPa or more.