Manufacturing method of non-directional electromagnetic steel sheet
TW202634078APending Publication Date: 2026-08-16JFE STEEL CORP
View PDF 0 Cites 0 Cited by
Patent Information
- Application Number
- TW115104107
- Authority / Receiving Office
- TW · TW
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-02-04
- Filing Date
- 2026-02-03
- Publication Date
- 2026-08-16
Smart Images

Figure 00000000_0000_ABST
Abstract
A method for manufacturing non-directional electromagnetic steel plates with high magnetic flux density is proposed. A method for manufacturing a non-directional electromagnetic steel sheet containing 2.5% by mass or more Si is as follows: after hot rolling of steel raw materials, annealing as needed, and cold rolling once or twice or more with intermediate annealing to produce a cold-rolled steel sheet, during the final annealing of the cold-rolled steel sheet, (1) heating from room temperature to a rapid heating stop temperature in the range of 500°C or higher and below the recrystallization start temperature, at an average heating rate of 150°C / s to 250°C / s, and holding for a specified holding time, and then heating the cold-rolled steel sheet at an average heating rate of 20°C / s or higher until the maximum temperature is reached after the holding time; or (2) heating from room temperature to a rapid heating stop temperature above the recrystallization start temperature, at an average heating rate of 150°C / s to 250°C / s, and holding for a specified holding time, and then heating the cold-rolled steel sheet at an average heating rate of 50°C / s or higher until the maximum temperature is reached after the holding time.
Need to check novelty before this filing date? Find Prior Art