Method for manufacturing a sheet for forming an energy line hardening protective film and a workpiece with the protective film.

TW202637718APending Publication Date: 2026-09-16LINTEC CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
TW115108167
Authority / Receiving Office
TW · TW
Patent Type
Applications
Current Assignee / Owner
Priority Date
2025-03-06
Filing Date
2026-03-06
Publication Date
2026-09-16

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

The energy-curing protective film forming sheet of the present invention comprises: an energy-curing protective film forming film 11 for forming a protective film; a heavy-side peeling film 12 disposed on one side of the aforementioned energy-curing protective film forming film; and a light-side peeling film 13 disposed on the other side of the aforementioned energy-curing protective film forming film; wherein, before energy beam irradiation, the Young's modulus of the aforementioned energy-curing protective film forming film 11 is 6 MPa or more, the peeling force F1 of the aforementioned heavy-side peeling film 12 from the protective film forming film 11 is 100 mN / 100 mm or more to 200 mN / 100 mm or less, the peeling force F2 of the aforementioned light-side peeling film 13 from the protective film forming film 11 is 30 mN / 100 mm or more to 100 mN / 100 mm or less, and the difference (F1-F2) between the aforementioned peeling force F1 and peeling force F2 is 50 mN / 100 mm or more to 160 mN / 100 mm or less.
Need to check novelty before this filing date? Find Prior Art