Method for preparing metal chalcogenide and cathode electrocatalyst containing the metal chalcogenide

TWI938137BActive Publication Date: 2026-09-01NAT YANG MING CHIAO TUNG UNIV
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
TW114149709
Authority / Receiving Office
TW · TW
Patent Type
Patents
Current Assignee / Owner
Filing Date
2025-12-17
Publication Date
2026-09-01
Estimated Expiration
2045-12-16

Smart Images

  • Figure TWG2TB001909125_001
    Figure TWG2TB001909125_001
  • Figure TWG2TB001909125_002
    Figure TWG2TB001909125_002
  • Figure TWG2TB001909125_003
    Figure TWG2TB001909125_003
Patent Text Reader

Abstract

This disclosure provides a method for preparing a metal chalcogenide and a cathode electrocatalyst containing the metal chalcogenide. The method for preparing the metal chalcogenide includes the following steps: providing an ingot sulfur and a foamed nickel in a quartz tube; vacuum sealing the quartz tube and placing it in a tube furnace; and holding the tube furnace at 450°C to 650°C for 60 to 90 minutes and then allowing it to cool naturally.
Need to check novelty before this filing date? Find Prior Art

Claims

1. A method for preparing a metal chalcogenide, comprising the following steps: providing a sulfur ingot and a foamed nickel in a quartz tube; vacuum sealing the quartz tube and placing it in a tube furnace; and holding the tube furnace at 450°C to 650°C for 60 to 90 minutes and then allowing it to cool naturally.

2. The preparation method as described in claim 1, wherein, The metal chalcogenide comprises nickel disulfide (Ni3S2).

3. The preparation method as described in claim 1, wherein, The atomic percentage of sulfur in the sulfur ingot to nickel in the foamed nickel is 1.5-2.5:2.5-3.

5.

4. The preparation method as described in claim 3, wherein, The atomic percentage of sulfur in the sulfur ingot to nickel in the foamed nickel is 1.8-2.2:2.8-3.

2.

5. The preparation method as described in claim 1, wherein, The heating rate of this tubular furnace is 3°C / min to 5°C / min.

6. The preparation method as described in claim 1, wherein, The tubular furnace is held at 500°C to 600°C for 70 to 80 minutes and then naturally cooled.

7. The preparation method as described in claim 1, wherein, The quartz tube has a length in which the sulfur ingot and the foamed nickel are separated by a distance, and the ratio of the distance to the length is greater than or equal to 0.

5.

8. The preparation method as described in claim 7, wherein, The ratio of this distance to this length is greater than or equal to 0.

8.

9. The preparation method as described in claim 7, wherein, The distance is greater than or equal to 8 centimeters.

10. A cathode electrocatalyst comprising a metal chalcogenide as prepared as claimed in claim 1, wherein, The metal chalcogenide comprises nickel disulfide (Ni3S2).

Citation Information

Patent Citations

  • Self-supporting trinickel disulfide electrode and preparation method thereof, and application of self-supporting trinickel disulfide electrode

    CN110518235A

  • Ni3S2 / Ni compound and preparation method thereof

    CN115323430A

  • Synthesis method of oil-soluble trinickel disulfide nanoparticles

    CN119263359A