Method for carbothermic smelting of magnesium and co-production of calcium carbide

By using liquid-phase calcium carbide as a catalyst under controlled conditions, the method enhances magnesium and calcium carbide production efficiency and quality, addressing inefficiencies in traditional carbothermic processes.

AU2020410472B2Pending Publication Date: 2026-11-19ZHENGZHOU UNIV
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
AU2020410472
Authority / Receiving Office
AU · AU
Patent Type
Applications
Current Assignee / Owner
Priority Date
2019-12-17
Filing Date
2020-12-17
Publication Date
2026-11-19
Estimated Expiration
2040-12-17

AI Technical Summary

Technical Problem

Existing carbothermic magnesium production methods using calcium carbide as a catalyst are inefficient and result in significant losses of vaporous calcium, leading to suboptimal yields and product quality.

Method used

Employing liquid-phase calcium carbide as a catalyst in a controlled environment with specific pressure and temperature conditions to manage magnesium vapor condensation, allowing for the production of both magnesium and calcium carbide with reduced losses and improved efficiency.

Benefits of technology

The method achieves twice the production efficiency of traditional solid-phase catalysis, producing high-purity magnesium and calcium carbide with improved yields and quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000001_0000
    Figure 00000001_0000
  • Figure 00000035_0000
    Figure 00000035_0000
  • Figure 00000036_0000
    Figure 00000036_0000
Patent Text Reader

Abstract

A method for carbothermic smelting of magnesium and co-production of calcium carbide, particularly appropriate for carbothermic smelting of magnesium using a mixture of magnesium oxide and calcium oxide as a raw material, and carbon as a reducing agent. Preparing a mixed powder containing magnesium oxide, calcium oxide and a carbon reducing agent; preparing the mixed powder into a pellet furnace charge, and placing same into a reactor provided with a heat source; configuring an absolute pressure P in the reactor to be in a range of 1000 Pa ≤ P ≤ atmospheric pressure, or to be micro-positive pressure, and a reaction temperature T being in a range of 11lg2P+71lgP+1210°C<T<98lg2P-129lgP+1300°C, performing a smelting reaction, cooling to obtain liquid magnesium by means of a condenser connected onto the reactor, and after the smelting reaction is complete, obtaining calcium carbide in the reactor. The present method can completely avoid the safety hazard in carbothermic smelting of magnesium of magnesium vapor and CO gas easily forming magnesium powder when cooling together and causing an explosion, and can significantly reduce magnesium smelting costs; the present method has good application prospects in industry.
Need to check novelty before this filing date? Find Prior Art

Description

will also occur to certain extents. However, the latter two reactions (especially the last one) are mild and provide a small amount of vaporous calcium and CO (compared to the amount of vaporous magnesium produced). When passing through the material layers of blocks, the vaporous calcium will undergo the reaction Ca(g) + 2C(5) ^ CaC2(5) with C at the surface of carbon blocks. When the carbon layers of blocks are thick enough, no vaporous calcium will be discharged from the top of the material layers. After MgO in the melt pool is completely consumed, the reaction CaO(l) + 3C(5) ^ CaC2(l) + CO(g) between CaO and C will start, and as this reaction proceeds, an increasing amount of CaC2 will be present in the melt pool. Because of a higher temperature and faster diffusion of reactants in molten CaC2, especially when both CaO and CaC2 are in a molten state, 2020410472   28 Oct 2026 the reaction CaO,,, + 3C , ^ CaCm (l)           (s)                  2(l) + CO (g) in the melt pool proceeds much faster than the solid-phase reaction CaO(s) + 3 C(s) ^ CaC  + CO, ,. That is, the carbon 2(s)           (g)                   , reduction reaction MgO • CaO + 4C ——2 > Mg + 2CO + CaC2 for magnesium production proceeds much faster under liquid-phase catalysis than under solid-phase catalysis. As can be seen from Figs. 1, 3 and 4, at a molten state of CaC2, i.e., at a melt pool temperature T > 1900 °C and a pressure P in the range of 1000 Pa < P < 10000 Pa, through properly configuring the thickness of the material layers (according to specific values of the reaction temperature and absolute pressure), the magnesium vapor can be controlled so as to leave the material layers at a temperature T lower than T = 98lg2P - 129lgP + 1300 °C and slightly higher than a condensation temperature of the magnesium vapor, Tb = 21.4lg2P + 18.4lgP + 437 °C. That is, the magnesium vapor is controlled so as to leave the material layers at a temperature T in the range of 7812.6 / (11.8 - lgP) - 273 °C < T < 98lg2P - 129lgP + 1300 °C. As a result, liquid magnesium can be obtained by condensation of the magnesium vapor. However, in this case, there may be a small amount of vaporous calcium lost together with gaseous CO. In contrast, at a pressure P > 10000 Pa, through controlling the melt pool temperature as T < 30lg2P + 58lgP + 1215 °C and causing the magnesium vapor to leave the material layers at a temperature T slightly higher than T = 21.4lg2P + 18.4lgP + 437 °C, liquid magnesium can be obtained by condensation of the magnesium vapor and reversing of the smelting reaction can be substantially eliminated, without any loss of vaporous calcium. Similarly, at a pressure P > 10000 Pa, if the melt pool temperature T is > 30lg2P + 58lgP + 1215 °C and the magnesium vapor leaves the material layers at a temperature T > 37lg2P - 73lgP + 580 °C (condensation temperature of vaporous calcium), both liquid magnesium and a minor amount of liquid calcium can be obtained through condensation, without loss of vaporous calcium. Example 4 In S1, the same dolomite as Example 1 with a particle size of 20-50 mm was used and calcined into dolime in a rotary kiln. Each ton of the dolime contained 369.3 kg of magnesium oxide and 617.4 kg of calcium oxide. Semi-coke with a particle size of 2020410472   28 Oct 2026 10-20 mm and fixed carbon content of 82% was obtained from a semi-coke plant. Calcium acetylide with a gas production capacity of 300 l / kg (a CaC2 content of 80%) was obtained from a calcium acetylide plant. According to a calculation, each ton of the dolime was added with 618.2 kg of the semi-coke. That is, a mass ratio of the dolime to the semi-coke was 1: 0.6182. In S2, the calcium acetylide was placed into a graphite smelting chamber of a resistively heated hermetic steel reactor and then heated and melted therein, resulting in the formation of a calcium acetylide melt pool with a depth of about 300 mm. In S3, dolime particles and semi-coke particles were homogenously mixed according to the aforementioned dolime / semi-coke mass ratio, i.e., 1: 0.6182, and added to the melt pool, until an about 500 mm thick unsubmerged material layer emerged above a surface of the melt pool. In S4, with an absolute pressure P in the reactor being set as ~ 20000 Pa and a temperature of the melt pool being maintained at T = 2000 ± 20 °C through adjusting electric heating power, a smelting reaction was run. Meanwhile, the thickness of the material layer was adjusted by material addition so that a magnesium vapor produced left the material layer at a temperature of about 1000 °C. The magnesium vapor entered a condenser connected in series to the reactor and condensed there into liquid magnesium. During the smelting process, once the surface of the melt pool rose beyond a control level, it was discharged from a liquid discharge port in the reactor. After the discharged liquid calcium carbide condensed, it could be sold as a co-product. In average, per hour, this method produced about 13 kg / h of pure magnesium and about 33 kg / h of pure calcium carbide. The production efficiency was about twice that of the solid-phase catalysis approach. The crude liquid magnesium immediately from condensation had a magnesium content of about 95%, the calcium acetylide obtained after the liquid calcium carbide was cooled had a gas production capacity of 270 l / kg, which was equivalent to a calcium carbide content of about 72%. The quality of the crude magnesium was lower than that obtained by the solid-phase approach, but the quality of the calcium acetylide was higher than that obtained by the solid-phase 2020410472   28 Oct 2026 approach. V. Technical Contemplation 5 - Carbothermic Process of Production of Multiple Metals Using Solid-Phase Calcium Carbide Catalyst Studies have found that, not only carbothermic magnesium production from a mixture of magnesium oxide and calcium oxide using calcium carbide as a catalyst is possible, oxides MmO (m represents a ratio of metal atoms to oxygen atoms) of many metals such as Mg, Pb, Sn, Zn, Fe, Mn, Ni, Co, Cr, Mo and V (hereinafter, collectively denoted as M) can react with calcium carbide to produce simple substances of the metals and calcium oxide, and the produced calcium oxide can also further react with carbon to again produce calcium carbide. These smelting reactions can be collectively expressed as the following equations: MmO + CaC2 —— mM + CaO + 2 C CaO + 3C —— CaC + CO A          2 Combining the above two equations, we obtain MmO + C —2 > mM + CO. It can be seen that CaC2 serves as a catalyst in the reactions. The thermodynamic laws of the chemical reactions are qualitatively described in Fig. 5. Thus, using the same method as described above, which uses a mixture of magnesium oxide and calcium oxide as a raw material, carbon as a reducing agent and calcium carbide as a catalyst for magnesium production, oxides of metals such as magnesium, lead, tin, zinc, iron, manganese, nickel, cobalt, chromium, molybdenum and vanadium can be smelted to produce simple substances of the metals. In each production cycle, substantially the same amount of calcium carbide as that of the added calcium carbide catalyst can be produced and reused in its entirety as a catalyst. Example 5 In S1, first-grade magnesite was obtained from an ore mine, with a chemical composition as follows: MgO = 46%, CaO = 0.6%, SiO2 = 1.0%. First-grade calcium acetylide with a CaC2 content of 80% was obtained from a calcium acetylide plant, 2020410472   28 Oct 2026 and high-temperature pitch with a fixed carbon content of 80% was obtained from a chemical plant. To 100 kg of calcined magnesite containing 96.64 kg of the active ingredient MgO, 191.84 kg of the calcium acetylide and 35.97 kg of the pitch were added. They were then mixed and ground to 327.81 kg of a 100 mesh mixed powder. In S2, the aforementioned mixed powder was pressed pillow-shaped pellets with dimensions of 50 mm (length) x 30 mm (width) x 20 mm (height), and the pellets were placed into a graphite smelting chamber contained in a steel hermetic container. The graphite smelting chamber was resistively heated, and a thermal insulation layer was disposed between the smelting chamber and the steel container. A shell and tube condenser was connected in series between an interface for a vacuum pipe on the top of the steel container and a vacuum pump, and a lower portion of the condenser was connected to a hermetic liquid magnesium reservoir. In S3, with an absolute pressure P in the reactor being set as P-1000 Pa and a temperature in the smelting chamber being maintained at T = 1400 ± 20 °C through adjusting electric heating power, a smelting reaction for magnesium production was run. Through an observation window in the liquid magnesium reservoir, liquid magnesium could be seen flowing from the condenser into the liquid magnesium reservoir. In S4, after about 2 hours of the aforementioned smelting reaction for magnesium production, electric heating power had undergone a significant decrease and showed a tendency toward a constant level, indicating that the smelting reaction for magnesium production had substantially ended. After that, with the absolute pressure P in the reactor being set as ~ 3000 Pa, the temperature in the smelting chamber was increased to T = 1750 ± 20 °C to allow a smelting reaction for calcium carbide production to proceed. After about 1 hour of this reaction, heating power again experienced a decrease and showed a tendency toward a constant level, indicating the smelting reaction for calcium carbide production had substantially ended. Argon was introduced to eliminate the vacuum until a vacuum pressure meter on the reactor read zero. A waste discharge port at the bottom of the reactor was opened, and the produced calcium acetylide was discharged and used as a reducing agent for the next production cycle. 2020410472   28 Oct 2026 This method operated in production cycles of about 3 hours. In each cycle, 68.56 kg of crude magnesium was produced. In average, per hour, about 22 kg / h of magnesium was produced. The crude magnesium had a magnesium content of 99.96%. VI. Technical Contemplation 6 - Carbothermic Process of Production of Multiple Metals Using Liquid-Phase Calcium Carbide Catalyst In the method as described above in “Technical Contemplation 5” for carbothermic production of multiple metals, if liquid-phase CaC2 is instead used as the catalyst, not only much faster smelting reaction speeds can be achieved, but also the pulverizing, pelletizing and other steps can be saved, resulting in increased production efficiency, a shortened process flow and reduced product cost. Example 6 In S1, the same magnesite as Example 5 with a particle size of 20-50 mm was used and calcined. Each ton of the calcined magnesite contained 966.4 kg of magnesium oxide. Coke with a particle size of 10-20 mm and a fixed carbon content of 85% was obtained from a coke plant, and calcium acetylide with a gas production capacity of 300 l / kg (a CaC2 content of 80%) was obtained from a calcium acetylide plant. Each ton of the calcined magnesite was added with 338.5 kg of the coke. That is, a mass ratio of the calcined magnesite to the coke was 1: 0.3385. In S2, the calcium acetylide was placed into a graphite smelting chamber of a resistively heated hermetic steel reactor and then heated and melted therein, resulting in the formation of a calcium acetylide melt pool with a depth of about 300 mm. In S3, calcined magnesite particles and coke particles were homogenously mixed according to the aforementioned calcined magnesite / coke mass ratio, i.e., 1: 0.3385, and added to the catalyst melt pool in the smelting chamber, until an about 500 mm thick unsubmerged material layer emerged above a surface of the melt pool. In S4, with an absolute pressure P in the reactor being set as P~ 20000 Pa and a temperature of the melt pool being maintained at T = 2000 ± 20 °C through adjusting electric heating power, a smelting reaction was run. Meanwhile, the thickness of the 2020410472   28 Oct 2026 material layer was adjusted by material addition so that a magnesium vapor produced left the material layer at a temperature of about 1000 °C. The magnesium vapor entered a condenser connected in series to the reactor and condensed there into liquid magnesium. In average, per hour, this method produced an equivalent amount of about 40 kg / h of pure magnesium. The production efficiency was about twice that of the solid-phase catalysis approach. The liquid magnesium immediately from condensation had a magnesium content of about 95%. The quality of the crude magnesium was lower than that obtained by the solid phase approach. Technical contemplations and preferred specific embodiments have been described in detail above. It is to be understood that, those of ordinary skill in the art, without the need for creative effort, can make various modifications and changes, based on the concept of the present invention. Accordingly, all the technical solutions that can be obtained by those skilled in the art by logical analysis, inference or limited experimentation in accordance with the concept of the invention on the basis of the prior art are intended to fall within the protection scope as defined by the claims. Throughout this specification and the claims which follow, unless the context requires otherwise, the word "comprise", and variations such as "comprises" and "comprising", will be understood to imply the inclusion of a stated integer or step or group of integers or steps but not the exclusion of any other integer or step or group of integers or steps. The reference in this specification to any prior publication (or information derived from it), or to any matter which is known, is not, and should not be taken as an acknowledgment or admission or any form of suggestion that that prior publication (or information derived from it) or known matter forms part of the common general knowledge in the field of endeavour to which this specification relates.

Claims

1. A method of carbothermic process of magnesium production and co-production of calcium carbide, comprising steps of:S1: preparing a mixed powder containing magnesium oxide, calcium oxide and a carbon reducing agent;S2: processing the mixed powder into a pelletized furnace feed material and placing it into a reactor equipped with a heat source; andS3: with an absolute pressure P in the reactor being set within a range of 1000 Pa < P < a slightly positive pressure and a reaction temperature T within a range of 30lg2P + 58lgP + 1215°C < T < 98lg2P - 129lgP + 1300 °C, running a smelting reaction, and obtaining liquid magnesium through condensation by a condenser connected to the reactor and calcium carbide within the reactor;wherein the smelting reaction produces a calcium vapor that always reacts with the carbon reducing agent to produce the calcium carbide;wherein the slightly positive pressure refers to a positive pressure not 1000 Pa higher than a local atmospheric pressure.

2. The method of claim 1, wherein the mixed powder, a molar content MC of the carbon reducing agent, a molar content MMgO of the magnesium oxide and a molar content MCaO of the calcium oxide are in a relationship of: MC ~ MMgO + 3MCaO.

3. The method of claim 1, wherein the mixed powder has a degree of fineness of 80 mesh or greater.

4. The method of claim 1, wherein the pelletized furnace feed material has an equivalent diameter of 20 mm to 40 mm.

5. The method of claim 1, wherein an outer layer of the reactor is a hermetic container provided therein with a smelting chamber, with a thermal insulation layer being disposed between the hermetic container and the smelting chamber; and the pelletized furnace feed material is placed within the smelting chamber.2020410472   28 Oct 20266. The method of claim 5, wherein the smelting chamber is constructed from components of a high-temperature resistant material that is resistant to a temperature not lower than 1700 °C.

7. The method of claim 6, wherein the high-temperature resistant material is graphite, silicon carbide, molybdenum disilicide, tungsten, tungsten alloy, molybdenum, molybdenum alloy or high-temperature resistant ceramic.

8. The method of claim 1, wherein the carbon reducing agent is coke, semi-coke, coal, petroleum coke, coal tar, graphite, asphalt or a mixture of any two or more of the above.

9. The method of claim 1, wherein a heating manner of the heat source is electric heating.

Citation Information

Patent Citations

  • Technology for simultaneously preparing metallic magnesium and calcium carbide through carbothermal method

    CN107083491A

  • Process for the continuous production of easily vaporizable metals

    US2920951A

  • Process for manufacture of metallic magnesium

    US4437886A