Method for Preparing Targets for the Production of Radioisotopes or Nuclear Fuels

The spark plasma sintering method addresses the inefficiencies of traditional uranium target production by rapidly forming UAl3 and UAl4 compounds, reducing manufacturing time and enhancing uranium loading for improved radioisotope yields.

AU2025205631B2Pending Publication Date: 2026-11-19CENT NAT DE LA RECH SCI (C N R S) +3
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
AU2025205631
Authority / Receiving Office
AU · AU
Patent Type
Applications
Current Assignee / Owner
Priority Date
2024-07-22
Filing Date
2025-07-21
Publication Date
2026-11-19

AI Technical Summary

Technical Problem

Existing methods for producing radioisotopes like 99Mo using low-enriched uranium targets face challenges such as prolonged manufacturing times, high defect rates due to limited uranium volume fraction, and inefficient uranium loading, leading to increased costs and reduced production yields.

Method used

A spark plasma sintering method is employed to rapidly form UAl3 and/or UAl4 compounds by reacting uranium and aluminum under controlled temperature and pressure conditions, minimizing UAl2 content and optimizing uranium loading.

Benefits of technology

This method significantly reduces manufacturing time, enhances uranium loading, and improves production yields while maintaining target integrity, making it suitable for efficient radioisotope production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000018_0000
    Figure 00000018_0000
  • Figure 00000019_0000
    Figure 00000019_0000
  • Figure 00000019_0001
    Figure 00000019_0001
Patent Text Reader

Abstract

This invention relates to a method for preparing a target for the production of radioisotopes or 5 nuclear fuels comprising a reactive sintering step. (no figures) 20 25 20 56 31 21 J ul 2 02 5 2 0 2 5 A B S T R A C T 2 0 2 5 2 0 5 6 3 1 2 1 J u l 5 2 1 J u l 2 0 2 5 A B S T R A C T 5 2 0 2 5 2 0 5 6 3 1
Need to check novelty before this filing date? Find Prior Art

Description

TITLE: method for preparing targets for the production of radioisotopes or nuclear fuels This invention relates to a method for preparing targets for the production of radioisotopes or nuclear fuels comprising a reactive sintering step. Technetium 99-m (99mTc) is a radioisotope for medical use obtained from the decay of molybdenum 99 (99Mo). To date, it is used in around 80-85% of diagnoses carried out each year using nuclear medicine methods. 99Mo may be produced either by fission of uranium 235 (235U) or by neutron activation reactions of Mo isotopes. The method for producing 99Mo by fission is by far the most widespread, as its yield is much higher than that achieved by activation methods. It also has the advantage of allowing other isotopes used in nuclear medicine, such as iodine 131(131I), xenon 133(133Xe) and yttrium 90(90Y), to be obtained simultaneously. It is used in so-called "experimental" or "research" nuclear reactors (as opposed to power reactors), and is based on the irradiation of "targets" containing uranium enriched in 235U. Historically, the enrichment levels of up to around 90% were used (this is known as highly enriched uranium, or HEU for "High Enriched Uranium"). However, in order to comply with the Nuclear Non-Proliferation Treaty, efforts are currently being made at international level to use targets with a maximum enrichment of 20% (low-enriched uranium, or LEU for "Low Enriched Uranium"). There are different types of target dedicated to the production of radioisotopes by fission. They are distinguished mainly by their geometry and the nature of the uranium-bearing material they contain. One of the most common types is an aluminum alloy sheathing plate with a core made up of a dispersion of uranium-based particles in an aluminum-based matrix. The Uranium-bearing particles most often contain uranium and aluminum (in the form of uranium aluminides, which will be referred to as UAlx and wherein the phases U + UAl2 + UAl3 + UAl4 may be found in variable proportions), but they may also be uranium- and molybdenum-based alloys (or others) or compounds such as uranium silicides (mainly U3Si2). Another common type of target is a tube containing a sheet of uranium-based material (such as metallic uranium). Other more "exotic" concepts based, for example, on the irradiation of liquid solutions containing uranium have also been studied, mainly on a laboratory scale. 2025205631   03 Oct 2026 The most common target geometry is that of plates, typically about 1.3 - 1.5 mm thick, with a surface area of the order of 30-50 x 100-200 mm2. Similar plates, typically around 1.3 - 1.5 mm thick, with a surface area of around 50-70 x 600750 mm2 may be used as nuclear fuel for research reactors. Such plates may be used in flat form or after bending to adapt to different assembly geometries. The method commonly used to manufacture these targets in plate form is known as pictureframing. It includes a preliminary step of pressing the mixture of the two powders (UAlx or other + Al) that will make up the fuel core. This core is then placed in an aluminum alloy frame and this assembly is sheathed by two plates, also in aluminum alloy. The sheathing involves several steps of hot rolling (generally between 440 and 550°C, depending on the type of Al alloy used for the sheath) and then cold rolling. An additional heat treatment (also between 440 and 550°C) may also be performed before cold rolling. As the fuel is held at different temperatures, reactions may occur between the uranium-bearing particles and the aluminum matrix, causing the composition of the fuel core to change. This is particularly the case when the core contains UAlx particles, as their reactivity with the Al matrix is high. To manufacture 99Mo production targets, a UAl2 compound powder is increasingly used as the starting material. This aluminide contains the most uranium (81.5%m, compared with 74.6%m and 68.8%m respectively for UAl3 and UAl4) and also has the highest density (8.1 g.cm-3, compared with 6.8 and 6.1 g.cm-3 respectively for UAl3 and UAl4), which is conducive to increasing the U load of targets (or fuels), and therefore the production of radioisotopes (or neutrons, if it is a fuel). Increasing the U content of targets is particularly important when LEUtype uranium is used. However, the volume fraction of UAl2 in the mixture with the Al powder is usually limited to around 45% (50%vol being a value currently considered the maximum by manufacturers), because redhibitory defects may appear in the targets during rolling when this fraction becomes too high. This is because there is no longer enough Al to accommodate mechanical deformation. In addition, the particle size of the powders used and the shape of the particles may have an impact on the defects encountered at the end of the manufacturing, making it necessary to adapt the rolling range (temperature, pressure, number of passes, reduction rate per pass). The UAl2 phase does not dissolve (or dissolves very poorly) in the alkaline solutions generally used for 99Mo extraction. This is why it is recommended to have as little as possible (of the order of a few %m maximum) in the targets once they have been manufactured. To achieve 2025205631   03 Oct 2026 this, this phase must be converted as far as possible into UAl3 and / or UAl4 during the plates manufacturing method, by reaction between UAl2 and Al: the total time the target is kept at temperature must be in the region of 6 to 10 hours, for a temperature of 540-550°C, and may be as much as twenty hours if the temperature is only 440°C. It is also preferable for this time to be accumulated during the hot rolling operations, so that the volume variations induced by the transformation of the UAlx particles are erased by the rolling. Thus: - the use of the picture-frame method means that the volume fraction of the uranium-bearing phase in the UAlx + Al mixture must be limited, otherwise there is a risk of creating unacceptable defects in the targets (porosity, etc.) and therefore a high scrap rate following the rolling operations; - more generally, this manufacturing method may require a sometimes lengthy development phase for the rolling range, depending on the characteristics of the starting powders (shape, particle size, etc.) and the volume fraction of the uranium-bearing phase; - the increasingly frequent use of the compound UAl2 as the starting uranium-bearing phase (in connection with the transition from HEU to LEU) requires a temperature hold of between a few hours and twenty hours, configured to transform UAl2 into UAl3 + UAl4. These various limitations have repercussions on target production times and costs, as well as on 99Mo production yields. One aim of the invention is therefore to provide a method which does not have the abovementioned disadvantages. In particular, one objective of the invention is to propose a rapid manufacturing method, i.e. one wherein the time required to obtain the targets is significantly reduced compared with the prior art, under moderate temperature and pressure conditions. Another objective of the invention is to propose a method for obtaining UAl2 or virtually UAl2-free targets, which, in particular, in the case of targets configured for 99Mo production, significantly reduces the temperature maintenance time required to obtain an optimised composition of the mixture for extracting this isotope, by chemical dissolution after irradiation. A further objective of the invention is to propose a method that may be quickly and easily adapted to the characteristics of the initial uranium-bearing powder (composition, particle size, etc.) and thus optimize the uranium loading of the powder mixture, and therefore, where appropriate, the radioisotope production yield. 2025205631   03 Oct 2026 OBJECT OF THE INVENTION The invention also relates to a method for preparing a target for the production of radioisotopes or nuclear fuels comprising a sintered compact consisting of or comprising UAl3 and / or UAl4, said method comprising a step (i) of spark plasma sintering (SPS) a powder P consisting of or comprising a uranium source and aluminum or an aluminum alloy to form said sintered compact. The spark plasma sintering, or sintering assisted by electric current (SPS), field assisted sintering technique (FAST) or pulsed electric current sintering (PECS)), is a sintering method that typically combines the effects of the application of uniaxial pressure and a pulsed current of high intensity and low voltage. This current passes through the matrix (made of a conductive material: often graphite or tungsten carbide) and rapidly heats it up by Joule effect and therefore the material (generally in powder form) placed in the latter. In the case of electrically conductive materials, part of the current passes through the powder bed itself. The effects at local level are still poorly understood. In all cases, they result in significantly accelerated material diffusion and sintering compared to conventional sintering (in a resistive furnace). Moreover, since the sintering takes place under load in a matrix of defined dimensions, the dimensions of the sintered object are perfectly controlled. When the powder used is a mixture of two (or more) different materials which tend to react with each other under the effect of temperature, reactive sintering phenomena may occur. Once again, their kinetics are clearly superior to those observed under conventional reactive sintering conditions. For the purposes of this invention, " spark plasma sintering" refers in particular to reactive spark plasma sintering. During spark plasma sintering, the uranium source and the aluminum or aluminum alloy react together to form UAl3 and / or UAl4. In one aspect of the present invention, there is provided a method for preparing a target for the production of radioisotopes comprising a sintered compact consisting of or comprising UAl3 and / or UAl4, said method comprising a step (i) of spark plasma sintering (SPS) a powder P consisting of or comprising a uranium source and aluminum or an aluminum alloy to form said sintered compact, which contains less than 10%mass UAl2; the spark plasma sintering in step (i) being carried out at a temperature Ta of between 400 and 650°C, and at a pressure Pa of between 10 and 400 MPa. 2025205631   03 Oct 2026 According to one embodiment, the method of the present invention is a method for preparing a radioisotope production target or nuclear fuels consisting of or comprising a core consisting of or comprising UAl3 and / or UAl4, and a shell consisting of or comprising Al, said method comprising the following steps: (i) a step of spark plasma sintering (SPS) a powder P consisting of or comprising a source of uranium and aluminum or an aluminum alloy to form a sintered compact consisting of or comprising UAl3 and / or UAl4; (ii) a step of sheathing the sintered compact obtained at the end of step (i) with aluminum or an aluminum alloy to form the target. Aluminum, for example, is A5 quality. Aluminum alloys include the alloys 1100, 6061, AG3NET and AlFeNi. According to a particular embodiment, the uranium source is selected from or comprises at least one element or compound selected from: - U; and -   UAlx, for example UAl2 or any U / UAl2 mixture; - the uranium source being UAl2. By "UAlx" is meant in particular UAl2, UAl3 and / or UAl4, possibly with the addition of U. According to a particular embodiment, the method according to the present invention is a method for preparing a target for producing radioisotopes. According to a particular embodiment, the method according to the present invention is a nuclear fuel preparation method. In a particular embodiment, the source of uranium or aluminum or aluminum alloy contains less than 10% by mass of silicon and typically less than 1% by mass of silicon. According to a particular embodiment, the volume of the power of uranium source relative to the total volume of the powder P is between approximately 30 and approximately 70%, in particular between approximately 40 and 50%. According to a particular embodiment, the size of the particles of the uranium source and / or aluminum or aluminum alloy is between 1 and 250 pm, in particular between 1 and 150 pm, especially between 1 and 100 pm. "Particle size" refers in particular to the largest dimension of the particles. This size may, for example, be measured by scanning electron microscopy (SEM), which is well known to the person skilled in the art. 2025205631   03 Oct 2026 According to a particular embodiment, the size of the uranium source particles is between 1 and 150 pm, in particular between 1 and 100 pm, and / or the size of the aluminum or aluminum alloy particles is between 1 and 50 pm, in particular between 1 and 45 pm. According to a particular embodiment, which sintered compact contains less than 10%m UAl2, in particular less than 9, 8, 7, 6, 5, 4, 3, 2 or 1%m UAl2. According to a particular embodiment, the sintered compact consists of UAl3 and / or UAl4, or comprises UAl3 and / or UAl4, in particular in a minimum total proportion of approximately 90%m. In a particular embodiment, the sintered compact additionally comprises aluminum, in particular up to 40% by volume or less, for example up to 30%, 20% or 10% by volume or less. According to a particular embodiment, the method of the invention comprises, prior to step (i), a step (o) of mixing a uranium source powder and an aluminum or aluminum alloy powder to obtain the powder P, in particular by means of a three-dimensional mixer, for example of the Turbula® type, by attrition or with a mechanical pestle mixer. In a particular embodiment, the sintered compact has the shape of a cylinder, in particular a straight cylinder, more particularly a straight circular cylinder, or a parallelepiped, in particular a rectangular parallelepiped. According to a particular embodiment, the spark plasma sintering in step (i) is carried out at a temperature Ta of between 400 and 650°C, in particular between 500 and 600°C. In a particular embodiment, the temperature Ta is maintained for a period of 0 to 60 minutes, in particular 1 to 10, 15 or 20 minutes. In a particular embodiment, the temperature Ta is reached by a temperature rise of between 10 and 500°C.min-1, for example around 100°C.min-1. According to a particular embodiment, step (i) is carried out at a pressure Pa of between 10 and 400 MPa, in particular between 70 and 80 MPa. According to a particular embodiment, step (i) is carried out at a temperature Ta of between 400 and 650°C, in particular between 500 and 600°C, and under a pressure Pa of between 10 and 400 MPa, in particular between 70 and 80 MPa, the pressure Pa being applied before the temperature Ta. In a particular embodiment, steps (i) and (ii) are performed simultaneously. According to a particular embodiment, step (ii) is carried out by spark plasma sintering, steps (i) and (ii) being simultaneous. According to a particular embodiment, the method according to the present invention is a method as defined above wherein: 2025205631   03 Oct 2026 - Steps (i) and (ii) are simultaneous, or - step (i) is followed, prior to step (ii), by a cooling step (i'), in particular to a temperature Tb of between 10 and 100°C, in particular between 15 and 30°C, for example at a rate of approximately 100°C.min-1. According to a particular embodiment, step (i) is carried out at a temperature Ta of between 400 and 650°C, in particular between 500 and 600°C, and under a pressure Pa of between 10 and 400 MPa, in particular between 70 and 80 MPa, the pressure Pa being applied before the temperature Ta, and in which step (i) is followed, prior to step (ii), by a cooling step (i'), in particular down to a temperature Tb of between 10 and 100°C, in particular between 15 and 30°C, the pressure Pa being released after the temperature Tb has been reached. If required, the temperature Ta may be reached and / or left by applying one or more temperature steps before or after the temperature Ta, which is lower than Ta. Similarly, the pressure Pa may be reached and / or released by applying one or more pressure stages beforehand or afterwards, respectively, which is lower than Pa. In a particular embodiment, the powder P is placed in a spark plasma sintering enclosure (or mold), which is lined with at least one sheet of graphite. According to a particular embodiment, step (i) is followed, prior to step (ii), by a step of demolding the sintered compact obtained by spark plasma sintering. Step (ii) may be carried out by any sheathing method well known to the person skilled in the art. In a particular embodiment, step (ii) is carried out by spark plasma sintering, rolling or hot isostatic pressing. According to a particular embodiment, the sintered compact has the shape of a cylinder, in particular a straight cylinder, more particularly a straight circular cylinder, or a parallelepiped, in particular a rectangular parallelepiped, and in which step (ii) is carried out by spark plasma sintering, through the formation of a closed receptacle of shape and dimensions adapted to said sintered compact, forming the sheathing of the sintered compact. By closed receptacle, we mean in particular a receptacle comprising an opening closed by a cover, or a frame each of whose opposite openings is closed by a cover. In a particular embodiment, the sintered compact has a thickness of between 200 and 1000 pm, the thickness being around 500 pm for example. Alternatively, the sintered compact is in the form of a cylinder with a thickness of up to a centimetric thickness. 2025205631   03 Oct 2026 According to a particular embodiment, the sintered compact has the shape of a cylinder, in particular a straight cylinder, more particularly a straight circular cylinder, or a parallelepiped, in particular a rectangular parallelepiped, said cylinder having a thickness of between 200 and 1000 pm, the thickness being for example approximately 500 pm, and a diameter of between 10 mm and 500 mm, the diameter being for example approximately 35 mm. In a particular embodiment, the sheathing around the sintered compact has a thickness of between 0.2 and 2 mm. According to a particular embodiment, the radioisotope production target is configured to be irradiated in a nuclear reactor in order to produce 99Mo (precursor of 99mTc, used in nuclear medicine) or other radioisotopes, such as iodine 131. In a particular embodiment, the nuclear fuel plate is configured for research reactors. DETAILED DESCRIPTION OF THE INVENTION DEFINITIONS As understood here, the ranges of values in the form of "x-y" or "from x to y" or "(between) x and y" include the bounds x and y, the integers between these bounds, and all the other real numbers between these bounds. For example, "1-5", or "from 1 to 5" or "between 1 and 5" refer to the integers 1, 2, 3, 4 and 5, as well as all other real numbers between 1 and 5. Preferred embodiments include each integer taken individually in the range of values, as well as any subcombination of these integers and any set of real numbers between these integers. For example, the preferred values for “1-5” may comprise the integers 1, 2, 3, 4, 5, 1-2, 1-3, 1-4, 15, 2-3, 2-4, 2-5, etc. As used in this description, the term “about” refers to a range of values within ±10% of a specific value. For example, the term “about 20” comprises the values of 20 ± 10%, i.e., the values of 18 to 22. For the purposes of this description, the percentages refer to percentages by mass in relation to the total mass of the formulation, unless otherwise stated. FIGURES [Fig. 1] is a synoptic of an example of the method covered by the invention, with numbering of the main steps. Steps 6 and 7 are optional in this example. [Fig 2] shows a quantification of the phases present in the UAlx mixture in UAl2 +Al compacts sintered at 552°C, by analysis of X-ray diffraction data using the Rietveld method. 2025205631   03 Oct 2026 [Fig 3] shows a SEM observations of polished sections of UAl2 +Al compacts sintered at 552°C (a) 0 min, (b) 15 min. (a) The light areas correspond to UAl2, black areas to Al and intermediate grey areas to UAl3 and UAl4; (b) The light areas correspond to UAl3, black areas to Al and intermediate grey areas to UAl4. [Fig 4] shows a quantification of the phases present in the UAlx mixture, in UAl2 + Al compacts sintered at 577°C, by analysis of X-ray diffraction data using the Rietveld method. [Fig. 5] shows an SEM observation, in backscattered electron mode, of atomized, coated (in an Al matrix) and polished U-5Al particles. [Fig 6] shows an SEM observation of a polished transverse section of a sintered U-5Al + Al disc sheathed by SPS at 527°C, (a) general view, (b) examination at higher magnification of the area framed in red in image (a). In a particular embodiment, the method according to the invention is carried out using a mixture of UAl2 and Al, for example at a sintering temperature of 552°C. By way of illustration, the following elements are given: Powders used and mixing of these powders (steps 1 and 2, Figure 1): the uranium-bearing powder used is a powder of the compound UAl2 which was obtained by grinding small ingots (mass: a few grams) of this compound, produced by arc smelting. The morphology of the particles is angular, due to the fragile nature of this compound. They range in size from a few pm to around 150 pm. This powder was mixed manually with an aluminum powder with a particle size of less than 44 pm (marketed by STREM Chemicals). A volume ratio of 50 / 50 was used for mixing the two powders. Given that their densities differ by a factor of three (8.1 g.cm-3 and 2.7 g.cm-3 for UAl2 and Al respectively), the mass fraction of UAl2 in the mixture is therefore equal to 75%m (± 2%m). The result is a U-load of around 3.3 g.cm-3 (for a mixture considered to be 100% dense). The quantities used were adapted to obtain discs with a diameter of 10 or 18 mm and a thickness of approximately 500 pm, after sintering. Sintering of the compact (steps 3 and 4, Figure 1): The SPS (Spark Plasma Sintering) furnace used was model HPD-10 from FCT System GMbH. Matrices and pistons made of graphite or tungsten carbide were used. The matrices were fitted with a thermocouple placed in a hole at sample height to monitor the temperature during the sintering cycle. For the pistons with a diameter of 18 mm or more, the temperature was checked using laser pyrometry with a sighting at the center of the disc. The inside of the molds was lined with graphite sheet (Papyex® marketed by MERSEN), 0.2 to 0.4 mm thick (depending on the mold) to facilitate 2025205631   03 Oct 2026 demolding and prevent contamination of the mold by the material to be sintered. Two graphite discs were also placed between the powder bed and the pistons, for the same reasons. A pressure of 76 MPa was applied to the powder bed (i.e. a force of 6 kN for sintering pellets with a diameter of 10 mm, or 19 kN for a diameter of 18 mm). Once this pressure was reached, a temperature rise ramp at 100°C.min-1 was applied until the chosen sintering temperature was reached. The temperature was then held for 0 to 15 minutes. The temperature was reduced at a rate of 100°C.min-1 and the pressure was released at the end of cooling. Table 1 summarizes the sintering temperatures and times of the UAl2 + Al discs, the characteristics of which are described by way of illustration for this particular embodiment and for the particular embodiment below. Table 1: Sintering temperatures and times for the UAl2 + Al discs described for this particular embodiment and for the particular embodiment below. Temperature (°C) Sintering time at selected temperature (min) 552 0 5 10 15 577 0 5 The hot rolling and annealing temperatures used in the picture-frame method of the prior art are generally between 440 and 550°C. Removing the compact from the mold (step 5, Figure 1): lining the molds with graphite sheeting allows the compacts to be easily removed from the mold after sintering. Fragments of graphite sheet sometimes adhere to the surface of samples and may be easily removed by light mechanical polishing. Steps 6 and 7 (Figure 1), which are optional, were not carried out during this series of tests and will be illustrated in a third specific manufacturing embodiment. Characteristics of the compacts obtained: 2025205631   03 Oct 2026 The correct densification of the discs was verified by scanning electron microscopy (SEM) (few pores visible) on polished sections of the discs thus obtained, as well as by density measurement using the Archimedes method. It was also possible to quantify the microstructural changes also revealed by the SEM examinations and by means of X-ray diffraction (XRD) analyses followed by refinement of the diffractograms obtained using the Rietveld method. The results obtained on the four compacts sintered at 552°C are shown in Figure 2. The indicator chosen to monitor the progress of the reactive sintering reactions is the relative mass fraction (in %m) of each aluminide in the UAl2 + UAl3 + UAl4 mixture (UAlx). The accuracy of this value is estimated at a few %m. The results of this quantification are in agreement with the microstructures observed in the SEM (Figure 3). The majority presence of UAl2 (76%m in the UAlx mixture) at 0 minutes and its absence at 15 minutes were confirmed. In fact, after 2 minutes at 552°C, its content has already fallen to just 4.5%m. Increasing the sintering time then leads to the formation of more and more UAl4 at the expense of UAl3. In another particular embodiment, the method according to the invention is carried out using a mixture of UAl2 and Al, for example at a sintering temperature of 577°C. By way of illustration, the following elements are given: The powders used and the compact manufacturing steps are identical to those described above. The only difference is the sintering temperature, i.e. 577°C instead of 552°C. Two sintering stage durations at 577°C are considered: 0 minutes and 5 minutes (see Table 1). Figure 4 shows the quantification of phases in the UAlx mixture based on XRD analysis. From the end of the temperature rise and with a holding time of 0 minutes, the fraction of UAl2 is extremely low (only 3%m) and becomes zero after 5 minutes. In a particular embodiment, the method according to the invention is carried out using a U-5Al (U-Al alloy with 5%m Al) and Al mixture, for example at a sintering and sheathing temperature of 527°C. By way of illustration, the following elements are given: Powders used and mixing of these powders (steps 1 and 2, Figure 1): in this particular embodiment, the uranium-bearing powder used is a U-5Al powder manufactured by centrifugal atomization by the Korea Atomic Energy Research Institute (KAERI), based in South Korea. This powder takes the form of spherical particles with a median diameter of around 60 pm (measured by laser granulometry). Its density was determined by helium pycnometry and is 2025205631   03 Oct 2026 equal to 13.6 g.cm-3 (± 0.1 g.cm-3). According to X-ray diffraction analyses, it contains the phases aU and UAI2 in the following respective mass proportions: 63 %m and 37 %m (values determined at ± 5 %m). Its microstructure is as-solidified and is characterized by the presence of fine UAl2 dendrites in a U matrix (Figure 5). The advantage of such a powder is that it contains significantly more uranium than the compound UAl2. It has been mixed with the same aluminum powder as used in the previous two particular embodiments, in a volume ratio of 40 / 60, instead of 50 / 50. The choice of using a higher volume fraction of Al (60%vol instead of 50%vol) is linked to the fact that increased consumption of Al will be necessary, during reactive sintering, to transform the U into UAlx. Such volume proportions lead to a U-loading of the mixture (assumed to be 100% dense) of around 5.1 g.cm-3 (to be compared with the 3.3 g.cm-3 corresponding to the UAl2 + Al mixture, in 50 / 50 volume proportions). The quantities used were adapted to obtain discs with a diameter of 10 to 35 mm and a thickness of around 500 pm, after sintering. Reactive sintering (step 4, Figure 1): the same pressure (76 MPa) and the same temperature rise and fall ramps (100°C.min-1) were used as in the two previous specific embodiments. The sintering was carried out for 10 minutes at 527°C. The microstructural examinations revealed a high level of reactivity of the U-5Al particles with the Al matrix, but with sometimes significant differences in the progress of the reactions at local level, linked to the availability of Al in the immediate environment of the uranium-bearing particles. According to the XRD analyses, the aluminide fractions obtained at the end of this steps were approximately as follows: 10 %m UAl2 + 80 %m UAl3 + 10 %m UAl4. Sheathing (steps 6 and 7, Figure 1): sheathing tests were carried out on 35 mm diameter discs obtained after the reactive sintering process described above. The various elements of the final object (4) are as follows: - (1) a 40 mm disc made of AG3 grade aluminum alloy (commonly used to manufacture fuel plates), with a total thickness of 0.9 mm, comprising a central part with a diameter of 35 mm, recessed over a height of 0.5 mm, configured to serve as a receptacle for the disc (2), - (2) a disc 35 mm in diameter and 0.5 mm thick obtained by SPS sintering of a U-5Al + Al mixture (the sintered core), - (3) a 40 mm disc made of AG3 alloy, 0.5 mm thick, for use as a cover. As part of these tests, the parts (1) and (3) were machined by milling from a cylindrical bar of aluminum alloy. This explains their ridged surface. They were carefully cleaned and stripped before the SPS sheathing operation, using the method used for the industrial "picture-frame" 2025205631   03 Oct 2026 method in the prior art. The parts (1), (2) and (3) were placed in the matrix of the SPS machine and subjected to a pressure and to a thermal cycle identical to those used for the sintering step described above, setting the holding steps at 527°C for 5 minutes. In the case described here, the sintering and sheathing steps therefore correspond to a total holding time at 527°C of 10 + 5 = 15 minutes. The microstructure obtained after the sheathing step, observed by SEM, shows a very good continuity between the core and the sheath, demonstrating the ability of the SPS method to ensure the welding of the core and of the sheath (Figure 6). It also shows: - that the core thickness has increased from around 500 pm before sheathing to around 700 pm after sheathing, - that on either side of this central part of the core, over a thickness of around 250 pm, the U-5Al particles are completely transformed and the quantity of Al remaining is very small, - that the majority of fully transformed areas correspond to UAl3 (as verified elsewhere by EDS), UAl4 being encountered mainly in the form of a border approximately 10 pm thick at the core / sheath interface. If any U-5Al particles are still partially transformed, the latter may easily be transformed according to the present invention by adding Al and / or by maintaining the applied temperature for longer. The particular embodiments described above have demonstrated the ability of the method of the invention to ensure the reactive sintering of a UAlx + Al mixture with a view to obtaining a sintered mixture containing a reduced quantity of the UAl2 phase during a heat treatment cycle, the total duration of which (rise + plateau + fall included) does not exceed 30 minutes, for temperatures tested of between 527 and 577°C. This temperature range may be extended, but without approaching the melting temperature of Al (around 660°C). As is well known to the person skilled in the art, degrees of freedom open up the possibility of rapidly optimizing this method. This is a major advantage over the picture-frame method, for which the development of the rolling ranges is complex and time-consuming. Three sets of parameters ensuring the flexibility of the method according to the invention are considered below. They cover: - the characteristics of the initial powder mixture; - the sintering conditions; - the sheathing step. The following parameters for the initial powder mix may first be adjusted: 2025205631   03 Oct 2026 - the shape and the particle size of this powder and the Al powder, which will influence both the homogeneity of the UAlx + Al mixture and its reactivity; - the method for mixing these powders; - the method for filling the mold of the SPS machine. 5 The second set of parameters that may be influenced is the pressure sintering cycle, namely: - the creation of intermediate temperature and / or pressure stages; - the use of more advanced parameters such as direct or pulsed current (duration of pulses and pauses, etc.) The reactive sintering is a thermally activated phenomenon, and the higher the temperature, 10 the faster it occurs. The pressure applied also plays a role in reaction kinetics. By adjusting these different parameters, we may optimize the formation of one or other of the uranium aluminides, depending on the desired composition of the final mixture. Thus, an increase in sintering temperature will favor the formation of the UAl4 phase to the detriment of the UAl3 phase. 15 The third set of parameters to be adjusted relates to the sheathing step, which may be carried out by SPS but also by other methods (rolling, hot isostatic pressing, etc.). SPS sheathing offers the same major advantages as SPS sintering, namely speed and flexibility. The important point to remember is that, however it is carried out, this step is likely to lead to a change in the characteristics of the core, which will have been sintered by SPS beforehand (change in 20 thickness, composition, etc.). Whichever method is chosen, it may be necessary to adjust all the target manufacturing steps, up to and including sheathing, in order to obtain a product that complies both with the specifications of the operators of the reactors wherein the targets are irradiated and with those of the plants extracting radioisotopes from the irradiated targets. 25

Claims

1. A method for preparing a target for the production of radioisotopes comprising a sintered compact consisting of or comprising UAl3 and / or UAl4,said method comprising a step (i) of spark plasma sintering (SPS) a powder P consisting of or comprising a uranium source and aluminum or an aluminum alloy to form said sintered compact, which contains less than 10% mass UAl2;the spark plasma sintering in step (i) being carried out at a temperature Ta of between 400 and 650°C, and at a pressure Pa of between 10 and 400 MPa.

2. The method according to claim 1 for preparing a radioisotope production target consisting of or comprising a core consisting of or comprising UAl3 and / or UAl4, and a shell consisting of or comprising Al,said method comprising the following steps:(i) a step of spark plasma sintering (SPS) a powder P consisting of or comprising a source of uranium and aluminum or an aluminum alloy to form a sintered compact consisting of or comprising UAl3 and / or UAl4, which contains less than 10%mass of UAl2;(ii) a step of sheathing the sintered compact obtained at the end of step (i) with aluminum or an aluminum alloy to form the target.

3. The method according to any one of the preceding claims, wherein the uranium source is selected from or comprises at least one element or compound selected from:- U; and-   UAlx, for example UAl2 or any U / UAl2 mixture;the uranium source being UAl2.

4. The method according to any one of the preceding claims, wherein the volume of the powder of uranium source relative to the total volume of the powder P is between approximately 30 and approximately 70%, in particular between approximately 40 and 50%.

5. The method according to any one of the preceding claims, wherein the size of the particles of the uranium source and / or aluminum or aluminum alloy is between 1 and 250 pm, in particular between 1 and 150 pm, in particular between 1 and 100 pm.2025205631   03 Oct 20266. The method according to any one of the preceding claims, which comprises, prior to step (i), a step (o) of mixing a uranium source powder and an aluminum or aluminum alloy powder to obtain the powder P, in particular by means of a three-dimensional mixer, for example of the Turbula® type, by attrition or with a mechanical pestle mixer.

7. The method according to any one of the preceding claims, wherein:- the spark plasma sintering in step (i) is carried out at a temperature Ta of between 500 and 600°C; and / or- step (i) is carried out at a pressure Pa of between 70 and 80 MPa.

8. The method according to claim 1, said method comprising a step (i) of spark plasma sintering (SPS) a powder P consisting of or comprising a uranium source and aluminum or an aluminum alloy to form a sintered compact consisting of or comprising UAl3 and / or UAl4, containing less than 10%mass UAl2, which is sheathed with aluminum or an aluminum alloy to form the target.

9. The method according to claim 2 or 8, wherein the sheathing is carried out by spark plasma sintering, rolling or hot isostatic pressing.

10. The method according to claim 2, 8 or 9, wherein the sheathing around the sintered compact has a thickness of between 0.2 and 2 mm.

Citation Information

Patent Citations

  • Method of manufacturing uranium target to be soluble in basic solution and method of extracting radioactive mo-99 using the same

    US20200368820A1