Wet treatment process for laterite-nickel ore
Patent Information
- Application Number
- AU2025271102
- Authority / Receiving Office
- AU · AU
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-02-25
- Filing Date
- 2025-04-28
- Publication Date
- 2026-09-10
AI Technical Summary
The existing high-pressure leaching process for laterite nickel ore has problems such as long process, poor quality of nickel-cobalt hydroxide products, and low overall scandium recovery rate.
A short-process wet processing technology for laterite nickel ore is adopted, including acid leaching, liquid-solid separation and countercurrent washing. Through one iron and aluminum removal and one nickel and cobalt precipitation treatment, iron and aluminum removal solution and iron and aluminum slag are obtained. The iron and aluminum slag is returned to the acid leaching step. The temperature, time and pH value are optimized to improve the recovery rate of nickel and cobalt and the quality of nickel and cobalt hydroxide products.
It shortens the complex process of traditional two-stage iron and aluminum removal and two-stage nickel and cobalt immersion, reduces production costs and energy consumption, and improves the recovery rate of nickel and cobalt, the overall recovery rate of scandium, and the quality of nickel and cobalt oxide products.
Smart Images

Figure 00000035_0000
Abstract
Citation Information
Patent Citations
Process method for recovering aluminum and scandium
AU2023433480A1
Wet treatment process of laterite nickel ore
CN111424172A
A process for the recovery of value metals from material containing base metal oxides
WO2004101833A1