Composition of ceramic coating and related uses.
The ceramic coating composition with epoxy resin, reinforcing agents, and fillers addresses the issue of excessive coats and man-hours by achieving superior micron thickness and improved adhesion, enhancing durability and reducing surface defects.
Patent Information
- Application Number
- BR102025008640
- Authority / Receiving Office
- BR · BR
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2025-04-30
- Publication Date
- 2026-11-10
AI Technical Summary
Existing ceramic coatings require excessive coats and man-hours for application due to their cross-linked nature, which compromises durability and impact resistance.
A ceramic coating composition comprising epoxy resin, reinforcing agents (quartz and silicon carbide), fillers (precipitated calcium carbonate and glass microspheres), and adhesion agents (3-glycidoxypropyltrimethosilane) is used to achieve superior micron thickness with fewer coats.
The composition provides greater adhesion to substrates, reduces surface defects, and achieves higher micron thickness with fewer applications, thereby reducing man-hours and improving durability.
Description
1 / 9 CERAMIC COATING COMPOSITION AND RELATED USE FIELD OF THE INVENTION
[001] The present invention relates to ceramic coating compositions for application on static structures such as metallic substrates, concrete, wood, among others. The compositions disclosed herein provide micron thicknesses superior to those of the prior art formulations, resulting in a significant reduction in coats and consequently, applicator man-hours. DESCRIPTION OF THE STATE OF THE ART
[002] Ceramic coatings provide different functionalities to a given material. Some illustrative examples include thermal insulation, corrosion and oxidation resistance, electrical conductivity, among others. They are commonly applied in construction materials machinery such as drills, hydroelectric equipment and pipeline transport systems (such as pipeline valves facing abrasive wear), gas turbines for power generation (such as high-temperature blade surfaces), among others.
[003] In this context, the thickness of the ceramic coating (micron thickness) is an important indicator of its performance and functional capacity. For example, ceramic coatings with thermal insulation properties may have a performance increase proportional to their respective thickness. In ceramic coatings with good Petition 870250034949, dated 04 / 30 / 2025, page 5 / 18 2 / 9 electrical conductivity, the thickness significantly increases the material's lifespan in corrosive environments.
[004] Products available in the state of the art employ epoxy resin bases. These are essentially prepolymers or thermosetting polymers containing reactive epoxy groups that allow cross-linking with other components. They are usually mixed with curing components, reacting at room temperature and forming a solid coating. US patent 3876606, for example, discloses a thermosetting epoxy resin for coating metal articles.
[005] US patent 5859153 describes a powder coating that includes an epoxy resin and a novolac (phenolic) compound or resin. The novolac compound is used to enhance the adhesion of the epoxy resin to metallic substrates.
[006] In both cases, their main disadvantages are precisely the cross-linked nature of the resin. Epoxy materials are characterized by high cross-linking density and consequently, high glass transition temperature (Tg). This characteristic gives the material excellent thermal properties, at the expense of durability and impact resistance.
[007] A proposal to overcome this limitation is described in patent EP0659833. This document discloses a two-component formulation comprising epoxy resins, Petition 870250034949, dated 04 / 30 / 2025, page 6 / 18 3 / 9 impact modifier and a mixture of amine curing agents consisting of dicyandiamide, cycloaliphatic amine and polyoxyalkylenamine.
[008] Another approach is disclosed in patent PI0705702 which describes a curing agent for epoxy resins employing a polyoxyalkylene component. This compound aims to increase the ability of the coating composition to receive the application of a finishing composition after prolonged exposure.
[009] As can be observed, none of the above proposals, all proposals in the State of the Art require an excessive number of coats, demanding more man-hours for application.
[010] In this sense, there is a need for solutions that circumvent the disadvantages inherent in the State of the Art, without burdening the coating application process. OBJECTIVES OF THE INVENTION
[011] The present invention overcomes the disadvantages related to the State of the Art by means of a ceramic coating composition comprising (a) an epoxy resin, (b) at least one reinforcing agent, (c) at least one filler and (d) an adhesion agent in the proportions indicated below.
[012] In a preferred embodiment, the ceramic coating composition comprises epoxy resin, quartz, Petition 870250034949, dated 04 / 30 / 2025, page 7 / 18 4 / 9 silicon carbide, 3-glycidoxypropyltrimethosilane, precipitated calcium carbonate, and glass microspheres. The coating layer thickness on the material is achieved with fewer coats, requiring fewer man-hours from applicators. DETAILED DESCRIPTION OF THE INVENTION
[013] It was surprisingly discovered that the ceramic coating composition according to claim 1 allowed for micron thicknesses superior to those of the prior art formulations.
[014] The following terms are described according to the technical understanding of the subject matter and should not be interpreted in a restrictive or limiting manner.
[015] Epoxy resin refers to an industrial polyepoxide selected from aromatic epoxy resins (such as glycidyl ethers of: bisphenol A, bisphenol F or bisphenol A / F); aliphatic or cycloaliphatic polyepoxides, glycidyl ethers of di-, tri- or tetrafunctional open-chain or cyclic branched or unbranched saturated or unsaturated alcohols; hydrogenated bisphenol A, F or A / F liquid resin or glycidylation products of hydrogenated bisphenol A, F or A / F; N-glycidyl derivatives of amides or heterocyclic nitrogen bases (such as triglycidyl cyanurate or triglycidyl isocyanurate or reaction products of epichlorohydrin and hydantoin) and epoxy resins from the oxidation of olefins (such as vinylcyclohexene, Petition 870250034949, dated 04 / 30 / 2025, p. 8 / 18 5 / 9 dicyclopentadiene, cyclohexadiene, cyclododecadiene, cyclododecatriene, isoprene, 1,5-hexadiene, butadiene, polybutadiene or divinylbenzene).
[016] In one embodiment of the invention, the epoxy resin is a bisphenol A-based resin, comprising contents of 30 to 70% by weight. Preferably, the epoxy resin content is 42%.
[017] Reinforcing agents relate to components that provide greater abrasion resistance. These are selected from 2 to 10% quartz and 25 to 40% silica carbide. Preferably, the quartz and silica carbide contents are 5% and 31.6% by weight, respectively.
[018] Fillers are mineral fillers to increase chemical resistance and corrosion barrier properties, as well as mineral fillers for thixotropy. In a preferred embodiment, the filler is precipitated calcium carbonate with contents between 5 and 20% and glass microspheres (content between 3 and 15% by weight). Preferably, the contents of precipitated calcium carbonate and glass microspheres are both 10% by weight.
[019] Bonding agents are compounds added to epoxy resin to increase its adhesion to inorganic components. They can be selected from silanes and titanates. In one embodiment, the bonding agent is 3-glycidoxypropyltrimethosilane with contents between 2 and 7% by weight, preferably 5% by weight. Petition 870250034949, dated 04 / 30 / 2025, page 9 / 18 6 / 9
[020] In the preferred embodiment of application, the ceramic coating composition is suspended in a conventional curing agent. This is selected from polyamine, polyamide, anhydride, modified amine, polyester or phenol bases. Preferably, the curing agent is a mixture of 3-aminoethyl-3,5,5-trimethylcyclohexylamine, 5-amino1,3,3-trimethylcyclohexanemethanamine and benzyl alcohol.
[021] The application can be carried out on static structures such as metallic substrates, concrete and wood, manually or by airless equipment. Iron, steel, other metals, wood, masonry and other clean materials can be coated with the composition as described after mixing with a curing agent or hardener. It is preferable to clean the surface before applying the coating, by means of a brush, sandblasting and similar methods, so that dust and oil are removed from the surface. The coating, which may also contain pigments, can be applied with a brush or paint roller, or in other ways.
[022] The main technical effect obtained by the invention was the greater adhesion of the coating composition to the substrate. As will be demonstrated below, the greater micron count in terms of wet thickness generates less runoff when compared with conventional products.
[023] A second beneficial effect provided by the claimed composition is the elimination of surface defects. The resulting layer is able to correct the Petition 870250034949, dated 04 / 30 / 2025, page 10 / 18 7 / 9 surface imperfections and also surface leveling, in comparison with state-of-the-art products. EXAMPLE 1
[024] In a preferred embodiment, the composition was prepared for a pilot batch of 52.5 kg. 21.0 kg of bisphenol A epoxy resin was weighed and added to a mixer. Then, 2.7 kg of quartz was weighed and gradually added to the mixer under stirring for about 5 minutes. Next, 15.8 kg of silica carbide was weighed and gradually added under stirring for about 5 minutes. After that, 2.6 kg of 3-glycidoxypropyltrimethosilane was added. Under the same conditions (gradual addition under stirring), 5.25 kg of calcium carbonate was added to the mixer and finally 5.25 kg of glass microspheres.
[025] Finally, 840 grams of the composition were separated and mixed with 160 grams of a curing agent = a mixture of 3-aminoethyl-3,5,5-trimethylcyclohexylamine, 5-amino-1,3,3-trimethylcyclohexanomethanamine and benzyl alcohol. EXAMPLE 2
[026] This is a comparative example in which epoxy-amine resin systems were prepared from conventional products. To illustrate the differences between the invention and the results obtained from it and a conventional coating system, the amine-curing systems were mixed. Petition 870250034949, dated 04 / 30 / 2025, page 11 / 18 8 / 9 with 840 grams of a state-of-the-art composition selected from Belzona 1341® and 1321®, ARC 855®, ARC 821®, ITWDevcon 11765® and 11767®, Henkel PC7333® and 7255®, Silibonde 8 liquid®, Silibonde 71 Brushable®, Plasteel Paintable Ceramic Blue®, APLIPOX 1102® and ADBOND-X 1102®. Measuring the thickness of the ceramic coating layer on iron.
[027] As described in Example 1, 840 grams of the coating composition of the invention were mixed with 160 grams of curing agent. After about 3 to 4 minutes, the coating was applied with a brush to the surface of an iron part. The micron thickness performance was tested by the wet comb thickness measurement method.
[028] The measuring comb was positioned next to the coating of Example 1. After contact was observed, the device was removed from the vicinity of the coating and the tooth of the comb where the coating contacts the disc was recorded. Measurements were taken and calculated to an accurate final thickness value. The coating composition yielded a thickness of 600.00 microns on an iron surface.
[029] This procedure was repeated with the products mentioned in Example 2 on the surface of a piece of iron. Similarly, the micron rating was tested using a comb for wet thickness measurement. The average of the observed results was 180.0 microns. This result Petition 870250034949, dated 04 / 30 / 2025, page 12 / 18 9 / 9 reflects the greater number of coats required for these coating systems to prevent unwanted product runoff.
[030] On the other hand, the coating system of the present invention provides greater wet layer thickness, consistently reducing the number of applications and consequently requiring fewer man-hours employed.
[031] Those skilled in the art will appreciate the knowledge presented and may reproduce the invention in other variants, covered within the scope of the appended claims. Petition 870250034949, dated 04 / 30 / 2025, page 13 / 18
Claims
1 / 2 CLAIMS 1. CERAMIC COATING COMPOSITION AND RELATED USE, said composition characterized by comprising: - an epoxy resin; - at least one reinforcing agent, selected from the group consisting of quartz, silica carbide; - at least one filler; - an adhesion agent.
2. Composition, according to claim 1, characterized in that the epoxy resin is bisphenol A in proportions ranging from 30 to 70% by weight.
3. Composition according to claim 1, characterized in that at least one reinforcing agent comprises 2 to 10% by weight of quartz and / or 25 to 40% by weight of silicon carbide.
4. Composition according to claim 1 characterized in that at least one filler comprises 5 to 20% by weight of precipitated calcium carbonate and / or 3 to 15% of glass microspheres.
5. Composition according to claim 1 characterized in that the adhesive agent comprises 2 to 7% by weight of 3-glycidoxypropyltrimethosilane.
6. Composition, according to claim 1, characterized in that it comprises 42% by weight of bisphenol A epoxy resin; 5% quartz; 31.6% silicon carbide; 5% 3-glycidoxypropyltrimethosilane; 10% by weight of precipitated calcium carbonate and 10% by weight of glass microspheres. Petition 870250034949, dated 04 / 30 / 2025, page 14 / 18 2 / 2 7. Use of a composition as defined in any one of claims 1 to 6, characterized in that the composition is mixed with a curing agent and applied to a static structure, using a brush or airless sprayer.
8. Use, according to claim 7, characterized in that said structure is selected from the group consisting of metallic, concrete and wood substrates.
9. Use, according to claim 7 or 8, characterized in that the curing agent is a mixture of 3-aminoethyl-3,5,5-trimethylcyclohexylamine, 5-amino-1,3,3-trimethylcyclohexanemethanamine and benzyl alcohol.
10. Use, according to any one of claims 7 to 9, characterized by providing 600-micron layers on the substrate, measured by a wet thickness gauge. Petition 870250034949, dated 04 / 30 / 2025, pp. 15 / 18