Method for forming an article

The method achieves a thin-walled, recyclable, and leak-proof foamed plastic article with precise geometric shape and thermal insulation by controlling expansion and stretching of a molten plastic composition between solid films, addressing the limitations of existing technologies.

BR112022016658B1Active Publication Date: 2026-11-17BOCKATECH LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
BR112022016658
Authority / Receiving Office
BR · BR
Patent Type
Patents
Current Assignee / Owner
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing methods for producing foamed plastic articles, such as cups or containers, struggle to achieve a thin wall thickness, low mass, and precise geometric shape with high wall strength and thermal insulation, while using a single recyclable material, and often result in non-uniform expansion leading to leakage issues.

Method used

A method involving controlled expansion of a molten plastic composition between opposing solid films with precise thickness tolerances and controlled stretching to form a uniform expanded cellular foam core, ensuring a single-layer, recyclable material with integral construction and no seams.

Benefits of technology

The method produces articles with a highly smooth surface, precise geometric shape, high rigidity, and good thermal insulation, while being easily recyclable and leak-proof, using a single material with reduced wall thickness and mass.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000036_0000
    Figure 00000036_0000
  • Figure 00000036_0001
    Figure 00000036_0001
  • Figure 00000037_0000
    Figure 00000037_0000
Patent Text Reader

Abstract

METHOD FOR FORMING AN ARTICLE. A method for forming an article, the method comprising: (a) providing a mold having a first mold part and a second mold part, the first and second mold parts having their respective first and second cavity-forming surfaces; (b) closing the mold thereby defining a cavity between the first and second cavity-forming surfaces;(c) injecting a molten plastic composition comprising a polymer and a physical blowing agent into the cavity, wherein during or after the injection step (c), the injected plastic composition in contact with the first and second cavity-forming surfaces is cooled to form the first and second solid films, respectively adjacent to and in contact with the first and second cavity-forming surfaces, wherein at least one region of the cavity is located respectively containing at least a portion of the plastic composition, wherein at least part of the plastic composition between the first and second solid films remains molten, wherein the thickness of the respective portion is constant within a tolerance of + / - 0.5%, preferably + / - 0.2%, based on a nominal thickness of the respective portion;(d) opening the mold before the molten plastic composition between the first and second solid films has solidified in at least one portion, so as to expose the molten plastic composition of the respective portion to an external pressure lower than the injection pressure, thereby allowing the molten plastic composition between the first and second solid films of the respective portion to expand by foaming to form an expanded cellular foam as a result of the molten plastic composition below the first solid film expanding outward from the second solid film stretching the first solid film in the respective portion, wherein the opening step comprises removing the first part of the mold so that the first solid film is no longer in contact with the first cavity-forming surface;and (e) cooling the expanded cellular foam to cause the molten plastic composition between the first and second solid films of the respective portion to solidify and form in the article at least a first part comprising a layer of the cellular foam core between the first and second solid films, wherein after the cooling step (e) the length of the first solid film in the respective portion has stretched, compared to the first solid film present before the opening step (d), by a stretching ratio of between 0.5 and 3%, wherein the stretching ratio is the ratio of the increase in the length of the first solid film after the cooling step (e) based on the length of the first solid film before the opening step (d).
Need to check novelty before this filing date? Find Prior Art

Description

/ 27 METHOD FOR WRITING AN ARTICLE

[001] The present invention relates to the formation of foamed plastic articles, for example cups or containers for liquids and / or food.

[002] In the packaging industry, a type of disposable cup commonly used (e.g., takeaway coffee cups) is a paper cup with an inner lining of a plastic material, for example, low-density polyethylene (LDPE). Because these cups are made of two different materials that can be difficult and / or expensive to separate, their recycling can be a challenge. Additionally, because there is a seam on one side of the cup where the paper material is joined, liquid can leak from the seam area at the rim of the cup when the cup is tilted to consume the beverage inside (particularly when the cup is used in conjunction with a lid with a spout through which the beverage passes for consumption).

[003] Efforts have been made in the industry to provide disposable polypropylene cups. In conventional injection molding, a thick wall is needed to create some thermal insulation in a cup. Typically, a cellular structure provides the thermal insulation, and a blowing agent is added to the thermoplastic polymer to create a foamed structure to further improve thermal insulation and reduce the density of the foamed wall.

[004] Document WO-A-2017 / 134181 describes an article and a method for forming the article, wherein the article is a polypropylene cup having an expanded region comprising a cellular foam. The production method requires that a corrugated surface be provided on at least one molding surface defining a mold cavity in order to control the expansion of a central molten polypropylene between opposing solid films after the removal of an outer mold part that molded an outer solid film. The corrugated surface effectively divides a Petition 870220075197, dated 08 / 22 / 2022, page 10 / 56 / 27: annular pre-mold injected in a series of arc-shaped zones that expand individually in order to prevent uncontrolled circumferential expansion around the pre-mold, so that the resulting article has a controlled shape and dimensions. However, a reinforced structure is formed that is not homogeneous and does not have a uniformly circular cross-section in a side wall, since the outer surface of the side wall tends to exhibit some residual waviness and therefore the outer surface is not highly smooth or a precise geometric shape. This known method provides a hollow article with high wall strength and low mass, but not a cup with the desired highly smooth surface and precise geometric shape.

[005] However, despite this description of the previous technique, there is still a need to produce foamed plastic articles, for example cups or containers for liquids and / or food, with even smaller wall thickness and even smaller mass, and a highly smooth surface corresponding to a desired precise geometric shape, but still with high wall strength and, preferably, walls that exhibit good thermal insulation properties, and are composed of a single recyclable material.

[006] The present invention aims, at least partially, to overcome the problem of obtaining an even smaller wall thickness and an even smaller mass, and a completely smooth surface corresponding to a desired precise geometric shape, but still with high wall strength and, preferably, walls that exhibit good thermal insulation properties, in articles composed of a single recyclable material.

[007] The present invention provides a method for forming an article according to claim 1.

[008] The preferred features of the method are defined in the dependent claims. Petition 870220075197, dated 08 / 22 / 2022, p. 11 / 56 / 27

[009] The method of the present invention forms an article with a wall that can have any shape, morphology or function. However, the present invention has particular application in the manufacture of hollow articles, such as a cup, or any other container or reservoir for holding a liquid or food.

[0010] The present invention provides the technical effects and advantages that the article formed by the method is easily recyclable and reusable, has a high level of rigidity provided by the expanded wall part(s), and also has good thermal insulation properties provided by the expanded wall part(s), but is very thin and, consequently, uses a low mass of the plastic composition to produce an article of a given size, for example, a cup with a desired volume capacity and a highly smooth surface corresponding to a desired precise geometric shape. The article may incorporate unexpanded, or less expanded, areas that may impart structural and / or aesthetic properties to the article; for example, the unexpanded, or less expanded, areas may be transparent or visually clear, while the expanded wall part(s) may be translucent or opaque.

[0011] The present invention is based, at least in part, on the present inventor's finding that by controlling the thickness of a portion of the plastic composition comprising a layer of molten plastic composition between the first and second opposing solid films, such that the thickness is constant with a very low tolerance of + / - 0.5%, preferably + / - 0.2%, when the portion is subsequently exposed to reduced pressure to cause expansion of the molten plastic composition layer to form an expanded cellular foam core layer between the first and second solid films, and controlling the stretching of the first solid film to be Petition 870220075197, dated 08 / 22 / 2022, page 12 / 56 / 27 within the range of 0.5 to 3%, the expansion of the plastic composition can be controlled in a highly uniform manner in the expanded wall portions. This means that there is no uncontrolled expansion, which in turn means that the expanded wall portions can provide a lower, thinner, and more uniform wall mass of the article than in the prior art.

[0012] The present inventor has also found that articles produced by the method of the present invention also have the level of rigidity required for such articles, despite the reduction in the amount of material used in them. It has been found that, as the cellular foamed plastic composition, typically a thermoplastic polymer such as a polyolefin, typically polypropylene, cools slowly, due to its thermal insulation qualities, the crystallinity of the plastic composition can increase, which in turn can increase the rigidity of the cellular foamed plastic composition. The expansion of the molten plastic composition between the first and second films by foaming also provides the articles with good thermal insulation properties.

[0013] Furthermore, since the entire container can be made from a single layer of recyclable material (i.e., without layers of different materials that need to be separated), the container is easier to recycle than the commonly used plastic-coated paper cups.

[0014] Additionally, since the articles are injection molded using the methods of the present invention, there is no joint present in the article through which leakage of a liquid contained therein could occur. For example, the side wall and base of a hollow container can be molded integrally.

[0015] The embodiments of the present invention will now be described by way of example with reference only to the accompanying drawings, in which: Figure 1 is a side view of a cup formed by the method of a first embodiment of the present invention; Petition 870220075197, dated 08 / 22 / 2022, page 13 / 56 / 27 Figure 2 is a cross-section along line AA of a first part of the cup of Figure 1 illustrating the appearance of an expanded translucent region of the cup; and Figures 3a and 3b are each a cross-section along line AA of a mold for forming the expanded cellular foam region of the cup of Figure 1 at different respective stages in the method of the present invention, Figure 3a showing an injection step and Figure 3b showing a cooling step; Figures 4a and 4b are each a cross-section along line BB of a mold to form a second part of the cup from Figure 1, illustrating the appearance of an unexpanded transparent region of the cup, with Figure 4a showing the injection stage and Figure 4b showing the cooling stage; Figure 5 is a bottom view of a base and side wall of a food tray formed by the method of a second embodiment of the present invention; Figure 6 is a cross-section of part of a region to form the base and / or side wall of the food tray in Figure 5 before expansion in the opening step; Figure 7 is a cross-section of part of a region of the base and / or side wall of the food tray formed from the part shown in Figure 6 after expansion in the opening step; Figure 8 is a cross-section of a mold for forming a hollow article using in-mold labeling according to a method of a third embodiment of the present invention; Figure 9 is a side view of a hollow article with a label inserted inside the mold cavity (in-mold label) produced by the mold in Figure 8; Figure 10 is a side view, partially in section. Petition 870220075197, dated 08 / 22 / 2022, page 14 / 56 / 27 phantom cross-section of a third part of a mold, in combination with a second part of the mold as used in the first embodiment, to form a hollow article according to a method of a fourth embodiment of the present invention; Figures 11a and 11b are schematic lateral cross-sections of a wall of an injection-molded portion at different respective stages in a fifth embodiment of the method of the present invention, Figure 11a showing the shape and configuration of the first solid film before mold opening and Figure 11b showing the shape and configuration of the first solid film after mold opening and cooling of the expanded cellular foam; Figure 12 is a schematic perspective view of a wall of an article formed from the injection-molded portion of Figure 11a, showing the shape and configuration of the first solid film after the mold is opened and the expanded cellular foam has cooled; Figure 13 is a cross-section of a mold for forming a hollow article according to a sixth embodiment of the present invention; and Figure 14 is a cross-section of a hollow article made by the mold of Figure 13.

[0016] With reference to Figure 1, a side view of an article is shown, for example, a hollow container, such as a cup, or, for example, a coffee cup, formed by the method of the present invention.

[0017] Cup 2 has an annular side wall 4 having an annular expanded foam region 6 and an annular non-expanded region 8. In this descriptive report, the term “annular” means “generally ring-shaped”, is not limited to geometrically circular shapes and encompasses shapes that may be circular or non-circular, for example elliptical, polygonal, etc. The expanded foam region 6 typically has a Petition 870220075197, dated 08 / 22 / 2022, page 15 / 56 / 27 thickness between 1 and 2 mm, optionally between 1 and 1.5 mm. The unexpanded region 8 normally has a thickness between 0.25 and 0.75 mm, optionally between 0.25 and 0.5 mm.

[0018] The expanded foam region 6 normally appears translucent to the naked eye because the expanded cellular foam includes cells that have cell walls that reflect visible light. However, if a pigment is incorporated into the thermoplastic polymer at a high concentration, the expanded region 6 may normally appear opaque, with a solid color.

[0019] In contrast, the unexpanded region 8 has no cells, or if any cells are present, for example in a low concentration, they have a cell size typically less than 0.5 microns and are therefore not visible to the naked eye and, consequently, the unexpanded cells in region 8 appear transparent to the naked eye. The unexpanded region 8 appears transparent to the naked eye because the blowing agent, in this embodiment CO2 gas, remained in solution in the polymer, in this embodiment polypropylene, during the manufacture of the article. After the solidification of the molten polymer, the formation of cells as a result of any action of the blowing agent is not possible.

[0020] The present invention relates to the reliable manufacture of such an article comprising an expanded foam region 6 and optionally a non-expanded region 8. In some embodiments, substantially the entire area of ​​the article may consist of an expanded foam region 6.

[0021] With reference to Figure 2, a cross-section along line AA is shown illustrating the structure of a segment of the expanded region 6 in the article of Figure 1, wherein the dimensions are exaggerated for clarity of illustration. The expanded foam region 6 is a part of the wall 10 comprising a core layer 12 of cellular foam, comprising hollow cells 11 in a matrix 9, between the first and the Petition 870220075197, dated 08 / 22 / 2022, page 16 / 56 / 27 second solid films 14, 16.

[0022] The hollow container also has an integral base 13. At least one region of at least one, or both, of the annular side wall 4 and the base 13 is comprised respectively by part of the wall 10. Different parts of the wall 10 of different expanded foam configurations may be provided, for example, only on the side wall 4, either on the entire side wall 4 or only on parts of the side wall 4, and / or on the base 13, either on the entire base 13 or only on parts of the base 13.

[0023] The method of the present invention for making article 2 will now be described with reference to Figures 3a and 3b.

[0024] With reference to Figure 3a, which shows an injection step, the article is formed using a mold 20 having a first outer mold part 22 and a second inner mold part 24. The first and second mold parts 22, 24 have the first and second cavity-forming surfaces 26, 28, which are annular in the illustrated embodiment. The first cavity-forming surface 26 of the outer mold part 22 and the second cavity-forming surface 28 are macroscopically smooth and without any undulations in a circumferential direction and, in the illustrated embodiment, each of the surfaces 26, 28 defines a precise geometric surface that is circular in horizontal cross-section. Since a cup must be formed, the surfaces 26, 28 are also frustoconical in vertical cross-section.

[0025] The mold 20 is closed, thus defining a region 30 of a cavity 32 between the first and second cavity-forming surfaces 26, 28. When the first and second cavity-forming surfaces 26, 28 are circular and annular, the region 30 of the cavity 32 is correspondingly circular and annular.

[0026] In the illustrated embodiment, region 30 is in a side wall forming portion 31 of mold 20 and extends to a portion of Petition 870220075197, dated 08 / 22 / 2022, page 17 / 56 / 27 base formation (not shown) of mold 20. Region 30 defines the largest portion of the side wall formation 31. However, region 30 may be located in any location(s) in the cavity 32 to define parts of the wall in the final article that must comprise expanded cellular foam, as further described below.

[0027] According to the present invention, the first and second cavity-forming surfaces 26, 28 are molded and dimensioned with high precision, and also any unwanted movement of the first and second parts of the mold 22, 24 during the molding operation as described below is substantially avoided, so that during the molding operation the width of the cavity region 30 between the first and second cavity-forming surfaces 26, 28 is constant within a tolerance of + / - 0.5%, preferably + / - 0.2%, based on a nominal, i.e., designed width.

[0028] A molten plastic composition 40, comprising a polymer and a physical blowing agent, is injected into cavity 32. The physical blowing agent is a gas dissolved in the polymer.

[0029] In the embodiment of the present invention, the polymer of the plastic composition may comprise a polyolefin or a mixture of a plurality of polyolefins, optionally polyethylene or polypropylene; or a polyester, optionally polyethylene terephthalate or polybutylene terephthalate; or polylactic acid. In the preferred embodiment, the polymer comprises polypropylene. Polypropylenes with a melt melt index (MFI) of 10 to 120 are particularly preferred. The Hot Melt Index of a polymer may be measured in accordance with ASTM D1238.

[0030] The blowing agents that can be used in the embodiment of the present invention include physical blowing agents in the form of a gas dissolved in the molten plastic composition. Such gas can Petition 870220075197, dated 22 / 08 / 2022, page 18 / 56 / 27, may include, for example, carbon dioxide. The gas may optionally include a perfume composition (i.e., an aroma) that remains present in the polymeric material after expansion, to enhance the consumer experience.

[0031] When using carbon dioxide as a blowing agent, CO2 gas is produced by the blowing agent in the extruder of the injection molding machine and the CO2 gas goes into solution during the injection phase (typically 30000 to 50000 kPa (300 to 500 bar) inside the mold cavity) because the relatively high pressure exerted on the material is greater than the pressure required (typically greater than 8000 kPa (80 bar)) to force the CO2 into solution within the molten thermoplastic resin, such as polypropylene.

[0032] The molten plastic composition is injected at an injection pressure Pjection. Typically, the injection pressure Pjection is at least 15000 kPa (150 bar). At the end of the injection step, optionally, a packing pressure, Ppacking, is applied to cavity 32. Typically, the packing pressure Ppacking is at least 15000 kPa (150 bar).

[0033] During or after the injection stage, the injected plastic composition 40 in contact with the first and second cavity-forming surfaces 26, 28 is cooled to form the first and second solid films 14, 16 respectively adjacent to and in contact with the first and second cavity-forming surfaces 26, 28.

[0034] In region 30 of cavity 32, a respective portion 52 of the plastic composition 40 is located. In portion 52 of the plastic composition 40, at least part of the plastic composition, in a central layer 54 between the first and second solid films 14, 16 remains fused.

[0035] Once the first and second parts of the mold 22, 24 Petition 870220075197, dated 08 / 22 / 2022, page 19 / 56 / 27 provides that during the molding operation the width of region 30 of cavity 32 between the first and second cavity forming surfaces 26, 28 is constant within a tolerance of + / - 0.5%, preferably + / - 0.2%, based on a nominal, i.e., projected width, correspondingly in portion 52 of the plastic composition 40 the thickness of portion 52 is constant within a tolerance of + / - 0.5%, preferably + / - 0.2%, based on a nominal, i.e., projected thickness of portion 52.

[0036] Normally, before opening mold 20 as further described below, portion 52 has a thickness of more than 0.5 mm up to 1 mm.

[0037] During the injection stage, and any packing, the injection pressure Pinjection and any packing pressure Ppacking, respectively, are above a minimum pressure limit, Plimit, in region 30 of cavity 32. Typically, the minimum pressure limit Plimit is 8000 kPa (80 bar). This prevents the physical blowing agent from partially escaping from the solution in the polymer in region 30, so that no cellular gas bubbles form in region 30 during the injection stage and any packing.

[0038] Region 30 of the mold cavity 32 has sufficient thickness and / or the processing time is so short that the molten polymer resin in the central layer 54 does not solidify during the injection stage and any subsequent packaging. Furthermore, region 30 can be additionally heated by an external heater to maintain the plastic composition 40 in the central layer 54 in a molten liquid phase. The first part of the mold 22 can be cooled by a cooling system, for example, by a flow of cooling fluid through it, to maintain the first part of the mold 22 at a lower temperature than the second part of the mold 24. Such temperature control can control the absolute thickness and Petition 870220075197, dated 08 / 22 / 2022, page 20 / 56 / 27 relating to the central layer 54 and the first and second solid films 14, 16, so that, as described below, the desired expansion of the central layer 54 and the stretching of the first solid film 14 are achieved.

[0039] With reference to Figure 3b, after that, the mold 20 is opened before the molten plastic composition 40 in the central layer 54 between the first and second solid films 14, 16 has solidified in the region 30 of the cavity 32.

[0040] During the opening stage, at least part of the molten plastic composition 40 in the central layer 54 is exposed to an external pressure below the minimum pressure limit, for example, atmospheric pressure, to allow the blowing agent to come out of solution and form gas bubbles within the molten plastic composition 40 in the central layer 54. This action forms in article 2 the expanded foam region 6 comprising the expanded cellular foam core layer 12, between the first and second solid films 14, 16, formed from the plastic composition 40.

[0041] The opening step comprises removing the first part of the mold 22 so that the first solid film 14 is no longer in contact with the first cavity-forming surface 26, while keeping the second solid film 16 in contact with the second cavity-forming surface 28. In the illustrated embodiment, this opening is achieved by removing the outer part of the mold 22, exposing the first solid film 14 to atmospheric pressure and leaving the second film 16 on the inner part 24.

[0042] However, any other configuration for opening the mold may be used. In particular, in an alternative embodiment, at least one or more portions of the inner part of the mold 24 may be removed from the second solid film 16 so that the second solid film 16, or any part thereof, is additionally or alternatively exposed to atmospheric pressure. Petition 870220075197, dated 08 / 22 / 2022, page 21 / 56 / 27

[0043] This opening step thus allows the molten plastic composition 40 in the central layer 54 between the first and second solid films 14, 16 to expand by foaming to form the expanded cellular foam core layer 12 21. The expanded cellular foam 21 is formed as a result of the molten plastic composition 40 in the central layer 54 below the first solid film 14 expanding outward from the second solid film 16. This action is controlled to stretch the first solid film 14 in the portion 52 by a desired stretching ratio.

[0044] After that, in a cooling step, the expanded cellular foam 21 is cooled to cause the molten plastic composition 40 in the central layer 54 between the first and second solid films 14, 16 of portion 52 to solidify and form in article 2 the expanded layer cellular foam region 6 comprising the core layer 12 of cellular foam 21 between the first and second solid films 14, 16. Cooling can be carried out passively in the ambient atmosphere or by active cooling, for example, by blowing cold air over article 2.

[0045] After the cooling stage, wall part 10 typically has a thickness of 1 to 2 mm. Typically, portion 52 increased in thickness by 1 to 1.5 mm to form wall part 10 from the opening stage to the cooling stage.

[0046] Before the opening stage, in portion 52, the first and second solid films 14, 16 are curved and parallel, and after the cooling stage, in the wall part 10, the first and second solid films 14, 16 are also curved and parallel.

[0047] After the cooling step, the length of the first solid film 14 in portion 52 stretched, compared to the first solid film 14 present before the opening step, by a stretching ratio of between 0.5 and up to 3%. The stretching ratio is the rate of increase Petition 870220075197, dated 08 / 22 / 2022, page 22 / 56 / 27, regarding the length of the first solid film 14 after the cooling stage, based on the length of the first solid film before the opening stage. For example, an increase in the length of the first solid film from an initial value of 100 mm to a final value of 102.5 mm would represent a stretch ratio of 2.5%. Preferably, the stretch ratio is between 2 and 3%, more preferably between 2.25 and 2.75%, even more preferably between 2.4 and 2.6%, for example, around 2.5%.

[0048] According to the present invention, the solid film 14 is stretched as a result of the expansion of the molten plastic composition 40 in the central layer 54 between the first and second solid films 14, 16 to form the final solidified core layer 12 of cellular foam, comprising hollow cells 11 in a solid matrix 9, between the first and second solid films 14, 16. This stretching is controlled, together with the highly uniform thickness of the portion 52 before the opening of the mold 20, so that the stretching is measurable, but small and uniform around the circumference of the expanded cellular foam region 6.

[0049] The degree of stretching can be controlled by a series of parameters that can be readily determined by the skilled, for example, to control the thickness of the first and second solid films 14, 16 before opening the mold 20, since thicker films would have a reduced tendency to stretch as a result of the expansion pressure applied to the films by the expanding molten plastic composition and to control the expansion pressure applied to the films by the expanding molten plastic composition by varying the concentration of the expanding agent in the molten plastic composition.

[0050] Fundamentally, the present inventor has surprisingly found that by controlling the uniformity of the shape and dimensions of the portion(s) to be expanded and by controlling the degree of stretching of the film(s) that are subjected to stretching as Petition 870220075197, dated 08 / 22 / 2022, page 23 / 56 / 27 result of the expansion of the molten plastic composition, in the resulting article the corresponding wall part(s) may exhibit a highly precise shape, for example, a highly precise concentricity of an annular cross-section, combined with small thickness and low mass. The wall part(s) may also exhibit high strength and thermal insulation properties resulting from the presence of the expanded cellular foam core layer.

[0051] In contrast, in document WO-A-2017 / 134181, the corrugated surface on at least one molding surface effectively divides an annular injection pre-mold into a series of arc-shaped zones that expand individually. The corrugated surface of the outer solid film has “peaks” and “grooves,” and during expansion the grooves are circumferentially “exploded” so that the shape of the outer film is modified to become more circular, but the length of the outer solid film is not increased. The length is not increased because before the mold opens the outer film is sufficiently thick and / or the concentration of the blowing agent is sufficiently low, so that at the opening there is insufficient blow pressure to stretch the outer film.However, when providing the wavy surface, the end wall is not uniformly circular, but has a slightly wavy outer surface as a result of the formation of vertical longitudinal ribs in the end wall, and the end wall may also be excessively thick.

[0052] The present invention solves these problems in document WO-A-2017 / 134181 by stretching the outer film in a controlled manner and providing a constant and uniform thickness of the portion to be expanded. The constant and uniform thickness of the portion to be expanded ensures that a uniform expansion pressure is applied to the entire area of ​​the respective wall or part of the wall. By providing a uniform expansion pressure to a portion that has a constant thickness and Petition 870220075197, dated 08 / 22 / 2022, page 24 / 56 / 27 uniform, this ensures that the expansion is also constant and uniform, so that the final wall or part of the wall has a highly uniform shape, dimensions and configuration. For example, in cup 2 of Figure 1, the outer surface of the side wall is, in a horizontal cross-section, geometrically circular with high precision, and the side wall has a highly constant wall thickness.

[0053] As a result of this improvement, the thickness and mass of the article's wall can be reduced while maintaining the properties of the cellular foam layer necessary to provide rigidity and thermal insulation to the wall. The present invention can provide a finished article with a side wall thickness that is substantially constant around the circumference, so that the resulting article has a controlled shape and dimensions, for example, a uniformly circular cross-section in a side wall and a hollow article with high wall strength and low mass, which has improved properties compared to the articles described in document WO-A-2017 / 134181.

[0054] With reference to Figures 4a and 4b, for the unexpanded region 8, the mold 20 is molded and dimensioned so that a narrow cavity region 35 is formed between the first and second cavity-forming surfaces 26, 28. During the injection and optional packing stage, the injection pressure and optional packing pressure are maintained above the minimum pressure limit in the narrow cavity region 35 to maintain the physical blowing agent as a dissolved gas in the molten plastic composition 40 so that substantially no gas bubbles are formed in the narrow cavity region 35. Before the opening stage, the plastic composition 40 in the narrow cavity region 35 is cooled to be fully solidified, to form in Article 2 at least one unexpanded region 8 comprising a solid-phase unexpanded plastic composition. Petition 870220075197, dated 08 / 22 / 2022, page 25 / 56 / 27 substantially homogeneous 37.

[0055] This narrow region 35 of the mold cavity 32 is thin and therefore the molten polymer resin requires a relatively short time period, shorter than the injection stage and optional packing, to cool and solidify. Furthermore, this narrow region 35 can be additionally cooled by an external chiller to facilitate the transition of the polymer resin from the molten liquid phase to a solid phase. After the opening stage, the solid plastic composition cannot expand further by foaming and cannot form an expanded cellular foam. Therefore, the unexpanded region 8 appears transparent to the naked eye.

[0056] With reference to Figures 5 to 7, Figure 5 is a bottom view of a base 70 of a food tray 72 formed by the method of a second embodiment of the present invention. The base 70 and the adjacent parts 78a, 78b, 78c, 78d of a side wall 80 comprise four different regular matrices 74a, 74b, 74c, 74d of a plurality of expanded wall parts 76a, 76b, 76c, 76d.

[0057] Four different dies 74a, 74b, 74c, 74d are shown on a common base 70 and side wall 80, mainly to illustrate different configurations for the respective dies 74a, 74b, 74c, 74d according to different embodiments of the present invention.

[0058] Normally, however, only one of these matrices 74a, 74b, 74c, 74d is present in the base 70 and the side wall 80, and one of the illustrated matrices 74a, 74b, 74c, 74d extends substantially over the entire area of ​​the base 70, and at least a central area of ​​the respective adjacent part 78a, 78b, 78c, 78d of the side wall 80.

[0059] In the illustrated embodiment, the matrices 74a, 74b, 74c, 74d are present in the base 70 and the side wall 80. However, in alternative embodiments, a matrix 74a, 74b, 74c, 74d can be understood in Petition 870220075197, dated 08 / 22 / 2022, p. 26 / 56 / 27 either one, or both, of the annular side wall 80 and the integral base 70.

[0060] Each of the expanded wall parts 76a, 76b, 76c, 76d is spaced from one or more adjacent expanded wall parts 76a, 76b, 76c, 76d by an area 82a, 82b, 82c, 82d of the plastic composition. The area 82a, 82b, 82c, 82d comprises, between the inner and outer solid films, a layer of the expanded cellular foam core with an expansion less than the expanded wall parts 76a, 76b, 76c, 76d or comprises the plastic composition that is not expanded throughout its thickness.

[0061] Figure 6 is a cross-section of portion 152 of a region to form the base or side wall of the food tray of Figure 5 before expansion in the opening step. Portion 152 shown in Figure 6 is within the mold cavity 132, defined by mold parts 122, 124, before mold opening 120. Portion 152 comprises the first outer solid film and the second inner film 114, 116 on opposite sides of a central layer 154 of a molten plastic composition 140.

[0062] Before the opening stage, in portion 152, the first outer solid film and the second inner film 114, 116 are flat and parallel. Between adjacent portions 152, the plastic composition 140 is in the form of a thin layer 190 that is fully solidified or has a thinner central layer of a molten plastic composition.

[0063] Figure 7 is a cross-section of part of the wall 110 of a region of the base 70 of the food tray 72 formed from the part shown in Figure 6 after expansion in the opening step. Part of the wall 110 comprises the first outer solid film and the second inner film 114, 116 on opposite sides of a core layer 112 of an expanded cellular foam composed of the plastic composition. After the opening step, in part of the wall 110, the second inner solid film 116 remained flat, but the first outer solid film 114 was stretched. Petition 870220075197, dated 08 / 22 / 2022, page 27 / 56 / 27 so that it is curved and not parallel to the second internal solid film 116.

[0064] Between adjacent wall parts 110, in areas 82 the thin layer 190 remains, or the thinnest central layer of the molten plastic composition has expanded only slightly, so that areas 82 function as a series of anchor points 115 to prevent excessive or uncontrolled stretching of the first outer solid film 114.

[0065] Figure 8 is a cross-section of a mold for forming a hollow article using in-mould labeling according to a third embodiment of the present invention. Figure 9 is a side view of a hollow article with an in-mould label produced by the mold of Figure 8. Again, some dimensions are exaggerated for clarity of illustration.

[0066] With reference to Figures 8 and 9, the first and second parts of the mold 222, 224 are, respectively, the outer and inner parts of the mold 222, 224 forming outer and inner surfaces 278, 280 of article 202. The method is modified compared to the method described in relation to the first embodiment by additionally comprising the step, before the injection step from an injection nozzle 221, of providing a label inserted inside the mold cavity 290 that at least partially surrounds the cavity 232. The label inserted inside the mold cavity 290 is located adjacent to the first cavity-forming surface 246 and is radially outward from the second cavity-forming surface 248. Typically, the label inserted inside the mold cavity 290 is annular and completely surrounds the cavity 232.Preferably, the label inserted inside the mold cavity 290 is composed of a length of a polymer layer 292 that has opposite ends 294, 296 that are joined at a seam 298 to form an annular shape. Petition 870220075197, dated 08 / 22 / 2022, page 28 / 56 / 27 as shown in Figure 9.

[0067] In the third embodiment, the injection and opening steps are performed as in the first embodiment. However, after the opening step, the label inserted inside the mold cavity 290 restricts the stretching of the first solid film formed adjacent to it. The label inserted inside the mold cavity 290 is placed under tension as a result of the expansion of the molten central layer to form the solidified core layer of expanded cellular foam and as a result of the stretching of the first outer solid film.

[0068] The mechanical properties and dimensions of the label inserted inside the mold cavity 290 can be selected to control the stretch ratio of the first outer solid film of the hollow article 202. In this way, the label inserted inside the mold cavity 290 functions to control the shape, dimensions and properties of the wall part 210 of the hollow article 202.

[0069] Figure 10 is a side view, partially in phantom cross-section, of a third part of a mold, in combination with a second part of the mold as used in the first embodiment, to form a hollow article according to a method of a fourth embodiment of the present invention.

[0070] In the fourth embodiment, the injection and opening steps are performed as in the first embodiment. The intermediate molded article 302 with a wall portion 310 having the first outer solid film 314 is in the second mold part 324 after the first mold part (not shown) has been removed. However, after the opening step and before the cooling step, the molded article is placed in a second mold 320 with a third mold part 322. The third mold part 322 has a molding surface 324. The first outer solid film 314 is placed in contact with the molding surface 324. Petition 870220075197, dated 08 / 22 / 2022, page 29 / 56 / 27

[0071] Therefore, the molding surface 324 restricts the stretching of the first outer solid film 314 in contact with it after the opening step, but before cooling to solidify the molten plastic composition in the central layer to form the solidified core layer of expanded cellular foam.

[0072] Normally, during the disposition stage, the molding surface 324 compresses the wall part 310 to reduce the thickness of the central layer of the molten plastic composition and thus reduce the thickness of the radially inward cellular foam core layer of the first solid film 314. Consequently, the molding surface 324 can function to control and optionally shrink the length of the first outer solid film 314 in the wall part 310.

[0073] In the preferred embodiment, the third part of the mold 322 is hollow and the molding surface 324 defines a hollow cavity 380 with a tapered surface 382. During the disposition step, the molding surface 324 is progressively pressed against the first outer solid film 314. This causes compression as described above.

[0074] Normally, the third part of the mold 322 is at a lower temperature than the first part of the mold that has been removed so that the first solid film 314 is cooled in contact with the third part of the mold 322. The third part of the mold 322 can be cooled by a cooling system, for example, by a flow of cooling fluid through it, to keep the third part of the mold 322 at a lower temperature than the second part of the mold 324 in which the hollow article 302 is supported during the arrangement of the hollow article 302 in contact with the third part of the mold 322.

[0075] In some embodiments of the present invention, the method may further comprise the step, prior to solidification of the molten plastic composition between the first and second solid films Petition 870220075197, dated 08 / 22 / 2022, page 30 / 56 / 27 in the cooling stage, pressing an embossing tool against the first solid film to press an inward-oriented image onto the first solid film, stretching the first solid film inward against the expanded cellular foam. In the embodiment where the third part of the mold 322 is pressed against the first solid film 314, the third part of the mold 322 can function as the embossing tool. The embossed image can be a pattern, logo, name, etc.

[0076] Figures 11a and 11b are schematic side sections of a wall of an injection-molded portion at different respective stages in a further embodiment of the method of the present invention. Figure 11a shows the shape and configuration of the first solid film before mold opening and Figure 11b shows the shape and configuration of the first solid film after mold opening and cooling of the expanded cellular foam.

[0077] After the injection step (c), but before the opening step (d), a regular matrix 400 is formed from a plurality of wall portions 402 of an intermediate article 404. Each of the wall portions 402 comprises a central layer 406 of the molten plastic composition between the first and second solid films 408, 410 opposite each other. A three-dimensional part 412 of the first solid film 408 defines an outward-extending convex surface 414 formed by the first cavity-forming surface 416 and a substantially smooth part 418 of the second solid film 410 formed by the second cavity-forming surface 420.

[0078] Before the opening step (d), each wall portion 402 of the regular matrix 400 comprises a central convex peak 422. Furthermore, before the opening step (d), the outward-extending convex surfaces 414 of the wall portions 402 are spaced from the adjacent outward-extending convex surfaces 414 of the wall portions 402 Petition 870220075197, dated 08 / 22 / 2022, page 31 / 56 / 27 for an area 424 of the plastic composition that is a solid layer 426 of the plastic composition extending between, and in contact with, the first and second cavity-forming surfaces 416, 420.

[0079] Figure 12 is a schematic perspective view of a wall 430 of an article formed from the injection-molded portion of Figure 11 showing the shape and configuration of the first solid film 408 after mold opening and cooling of the expanded cellular foam.

[0080] During the opening step (d), each wall portion 402 of the regular matrix 400 of the plurality of wall portions 402 expands to stretch the first solid film 408 by which after the cooling step (e) a regular matrix 432 of a plurality of wall parts 434 is formed, each wall part 434 being formed from a respective wall portion 402. The regular matrix 432 of the plurality of wall parts 434 comprises a matrix of substantially pyramidal, conical or partially spherical convex wall parts 434. Each of the convex wall parts 434 comprises a core layer 436 of expanded cellular foam between opposing film layers 438, 440 consisting of a three-dimensional shaped first solid film part 438 defining the convex surface 442 of the convex wall part 434 and a substantially smooth part of second solid film 444.The convex wall parts 434 are spaced from the adjacent convex wall parts 434 by an area 446 of the plastic composition that is not expanded. In this embodiment, the plan view of the unexpanded area 446 comprises an individual point, normally in the form of a circle, although in other embodiments the unexpanded area 446 may have other shapes and dimensions and a plurality of unexpanded areas 446 may be interconnected.

[0081] Figure 13 is a cross-section of a mold for forming a hollow article according to a sixth embodiment of the present invention. Figure 14 is a cross-section of a hollow article made Petition 870220075197, dated 08 / 22 / 2022, page 32 / 56 / 27, for the mold of Figure 13. The hollow article is a cup in the form of an expanded and molded end article 550, shown in Figure 14, which has an open upper end 552 and a closed lower end 554 and a side wall 556.

[0082] With reference to Figures 13 and 14, after the injection step (c) and before the opening step (d), the plastic composition 500 forms a molded intermediate article 502 within the cavity 504. In an initial phase of the opening step (d), as shown by the arrow in Figure 13, the first part of the mold 506 is removed so that the first solid film 508 is no longer in contact with the first cavity-forming surface 510. The initial removal of the first part of the mold 506 exposes a first end part 512 of the intermediate article 502 while a second opposite end part 514 of the intermediate article 502 remains in contact with the first and second cavity-forming surfaces 510, 516.Subsequently, the first part of the mold 506 is completely removed so that the first solid film 508 is fully exposed, extending from the first end part 512 to the opposite second end part 514, as described above for the previous embodiments.

[0083] After the start of the initial phase, the first solid film 508 in the first end part 512 of the intermediate article 502 is exposed and, therefore, for the entire opening step (d) the first solid film 508 in the first end part 512 of the intermediate article 502 is exposed for a longer period of time than the first solid film 508 in the second end part 514 of the intermediate article 502. Furthermore, the plastic composition in the first end part 512 is warmer than in the second end part 514 because the plastic composition in the first end part 512 has been in contact with the relatively cooler first mold part 506 for a shorter period than the Petition 870220075197, dated 08 / 22 / 2022, page 33 / 56 / 27 plastic composition in the second end part 514 as a result of the first end part 512 being exposed before the second end part 514.

[0084] Consequently, after the cooling step (e), the length of the first solid film 508 in the first end part 512 of the expanded and molded final article 550, shown in Figure 14, stretched at a greater stretching rate than the length of the first solid film 508 in the second end part 514 of the expanded and molded final article 550. This is because the time to reach stretching before cooling is longer for the first end part 512 than for the second end part 514.

[0085] The first end portion 512 of the intermediate article 502 is injection molded to have a smaller wall thickness than the second end portion 514 of the intermediate article 512, and this thickness difference is highly exaggerated in Figure 13. Typically, the wall thickness of the intermediate article 502 progressively tapers in increasing thickness in one direction from the first end portion 512 of the intermediate article 502 to the second end portion 514 of the intermediate article 502. This thickness difference at least partially compensates for the greater stretch-to-length ratio of the first solid film 508 in the first end portion 512 of the intermediate article 502 compared to the second end portion 514 of the intermediate article 502.Typically, the wall thickness of the first end portion 512 of the intermediate article 502 is between 5 and 15% less than the wall thickness of the second end portion 514 of the intermediate article 502. This reduced wall thickness at the upper end of the intermediate article 502 reduces excessive film stretching at the upper end of the resulting article. As an example, for a typical container with a side wall, for example with a height of 135 mm, that is... Petition 870220075197, dated 08 / 22 / 2022, page 34 / 56 / 27 inclined in relation to the longitudinal geometric axis of the container by an angle of 6 degrees, having a thickness of the second end part 514 of 0.7 mm, the thickness of the first end part 512 would be approximately 0.05 mm thinner than the second end part to avoid excessive stretching at the upper end of the container.

[0086] The first and second end portions 512, 514 of the intermediate article 502 form the respective first and second wall portions 520, 522 of the expanded and molded end article 550 shown in Figure 14. The first and second wall portions 520, 522 normally have the same thickness within a tolerance of + / - 0.5% based on a nominal thickness of the respective wall portions 520, 522.

[0087] In this embodiment of the present invention, the initial removal of the first part of the mold 506 exposes the first end part 512 of the intermediate article 502, normally to the atmosphere. This exposure causes the first solid film in the first end part 512 to stretch as a result of the expansion of the molten plastic composition in the central layer. In contrast, the opposite second end part 514 of the intermediate article 502 remains in contact with the first and second cavity-forming surfaces 510, 516 and, therefore, in the initial phase, cannot expand or stretch. After the opposite second end part 514 has been subsequently exposed, which takes a finite period of time, after the complete removal of the first part of the mold 506, the first solid film 508 in the second end part 514 can subsequently stretch.Since the first solid film 508 in the first end part 512 has a longer time to stretch than in the second end part 514, if it is desired to maintain a substantially constant wall thickness in the expanded and molded end article 550, the cavity thickness in the first end part 512 is made smaller than in the second end part 514, to compensate for the increased stretching ratio. Petition 870220075197, dated 08 / 22 / 2022, page 35 / 56 / 27 associated with the increased stretch time, in the first end part 512 compared to the second end part 514. This allows, for example, a constant wall thickness to be formed despite there being a higher film stretch ratio in the upper open end 552 of the hollow article compared to the lower closed end 554 of the hollow article.

[0088] In the illustrated embodiments of the present invention, the annular side wall is linear in a longitudinal cross-section and, therefore, the annular side wall can be truncated conical or truncated pyramidal. In other embodiments of the present invention, the annular side wall has an upper annular end away from the base and a lower annular end adjacent to the base, the upper end has a larger circumference than the lower end, and the side wall is curved in a transverse longitudinal direction, and, for example, the article may have the shape of a bowl with a large diameter opening. In such embodiments, the stretch ratio in the first outer solid film is greater at the upper annular end than at the lower annular end, as a result of the significantly larger circumference causing greater stretch of the first outer solid film during the formation of the expanded cellular foam core layer.In preferred embodiments of the present invention, the article may be a cup, mug, bottle, basin, bowl, tray, container, or reservoir for holding a liquid or food, for example, a coffee cup or a food tray. The container may be heat-resistant and suitable for heating a beverage or food in a microwave oven. The items may be disposable or reusable and, in both cases, are recyclable, as the item is composed of a single polymer, for example, polypropylene.

[0089] Several modifications to the illustrated embodiments will be apparent to those skilled in the art and are intended to be included within the scope of the present invention, as defined by the appended claims. Petition 870220075197, dated 08 / 22 / 2022, pp. 36 / 56

Claims

1 / 8 CLAIMS 1. Method for forming an article, wherein the article is a hollow container (2), characterized in that the method comprises: (a) providing a mold (20) having a first mold part (22) and a second mold part (24), the first and second mold parts (22, 24) having respective first and second cavity-forming surfaces (26, 28); (b) closing the mold (20), thereby defining an annular cavity (32) between the first and second cavity-forming surfaces (26, 28); (c) injecting a molten plastic composition (40) comprising a polymer and a physical blowing agent into the cavity (32), wherein the physical blowing agent is a gas dissolved in the polymer, the molten plastic composition (40) being injected at an injection pressure, wherein during or after injection step (c), the injected plastic composition in contact with the first and second cavity-forming surfaces (26,28) is cooled to form first and second solid films (14, 16) respectively adjacent to and in contact with the first and second cavity-forming surfaces (26, 28), wherein in at least one annular region (30) of the annular cavity (32) is respectively located at least one annular portion (52) of the plastic composition in which portion (52) at least part of the plastic composition between the first and second solid films (14, 16) remains molten, wherein the thickness of the respective portion (52) is constant within a tolerance of + / - 0.5% based on a nominal thickness of the respective portion (52), and wherein in that at least one portion (52) the first and second solid films (14, 16) are curved and parallel; (d) open the mold (20) before the molten plastic composition (40) between the first and second solid films (14, 16) has solidified in that at least one portion (52), so as to expose Petition 870260103268, dated 06 / 10 / 2026,pg. 12 / 46 2 / 8 molten plastic composition (40) of the respective portion (52) at an external pressure lower than the injection pressure, thus allowing the molten plastic composition (40) between the first and second solid films (14, 16) of the respective portion (52) to expand by foaming to form an expanded cellular foam (21) as a result of the molten plastic composition (40) below the first solid film (14) having expanded out of the second solid film (16) stretching the first solid film (14) in the respective portion (52), wherein the opening step (d) comprises removing the first mold part (22) so that the first solid film (14) is no longer in contact with the first cavity-forming surface (26); and (e) cooling the expanded cellular foam (21) to cause the molten plastic composition (40) between the first and second solid films (14,16) of the respective portion (52) solidify and form in article (2) at least a first wall part (10) comprising a core layer (12) of cellular foam between the first and second solid films (14, 16), wherein the hollow container (2) has an annular side wall (4), and the wall part (10) is comprised in the annular side wall (4) and is both continuous and annular, wherein after cooling step (e) the length of the first solid film (14) in the respective portion (52) has stretched, compared with the first solid film (14) present before opening step (d), by a stretching ratio of 0.5 to 3%, wherein the stretching ratio is the ratio of the increase in the length of the first solid film (14) after cooling step (e) based on the length of the first solid film (14) before opening step (d).

2. Method according to claim 1, characterized in that the thickness of the respective portion (52) is constant within a tolerance of + / - 0.2% based on a nominal thickness of the respective portion Petition 870260103268, dated 06 / 10 / 2026, page 13 / 46 3 / 8 (52).

3. Method according to claim 2, characterized in that after the cooling step (e) the length of the first solid film (14) in the respective portion (52) stretched, compared with the first solid film (14) present before the opening step (d), by a stretching ratio of 2 to 3%, optionally 2.25 to 2.75%, also optionally 2.4 to 2.6%, yet more optionally 2.5%.

4. Method according to any one of claims 1 to 3, characterized in that before the opening step (d), at least one portion (52) has a thickness of more than 0.5 mm up to 1 mm.

5. Method according to any one of claims 1 to 4, characterized in that after the cooling step (e), at least one part of the wall (10) has a thickness of 1 to 2 mm.

6. Method according to any one of claims 1 to 5, characterized in that from the opening step (d) to the cooling step (e), that at least one first portion (52) increased in thickness from 1 to 1.5 mm to form that at least one wall part (10).

7. Method according to any one of claims 1 to 6, characterized in that the first and second mold parts (22, 24) are, respectively, outer and inner mold parts (22, 24) forming outer and inner surfaces of the hollow container (2).

8. Method according to any one of claims 1 to 7, characterized in that after the cooling step (e), in that at least one part of the wall (10) the first and second solid films (14, 16) are curved and parallel.

9. Method according to any one of claims 1 to 8, characterized in that the article is a hollow container (2) having an annular side wall (4) and an integral base (13), wherein at least one region of at least one, or both, of the annular side wall (4) and of the base (13) is, respectively, comprised by that at least one part of the wall (10).

10. Method according to claim 9, characterized in that the annular side wall (4) has an upper annular end distant from the base (13) and a lower annular end adjacent to the base (13), the upper end has a larger circumference than the lower end, and the side wall (4) is curved in a longitudinal cross-section, wherein the stretch ratio is greater at the upper annular end than at the lower annular end.

11. Method according to any one of claims 1 to 10, characterized in that after injection step (c) and before opening step (d), the plastic composition forms a molded intermediate article (502) within the cavity (504), and at an early stage of opening step (d) the removal of the first mold part (506) so that the first solid film (508) is no longer in contact with the first cavity-forming surface (510) exposes a first end part (512) of the intermediate article (502) while a second opposite end part (514) of the intermediate article (502) remains in contact with the first and second cavity-forming surfaces (510, 516).

12. Method according to claim 11, characterized in that after the start of the initial phase, the first solid film (508) on the first end part (512) of the intermediate article (502) is exposed for a longer period of time than the first solid film (508) on the second end part (514) of the intermediate article (502), whereby after the cooling step (e) the length of the first solid film (509) on the first end part (512) of the final expanded and molded article (550) has stretched by a greater stretching ratio than the length of the first solid film (508) on the second end part (514) of the final expanded and molded article (550).

13. Method according to claim 12, characterized in that the first end part (512) of the intermediate article (502) has a smaller wall thickness than the second end part (514) of the intermediate article (502) to compensate at least partially for the greater stretch-to-length ratio of the first solid film (508) in the first end part (512) of the intermediate article (502) compared with the second end part (514) of the intermediate article (502).

14. Method according to claim 13, characterized in that the wall thickness of the first end part (512) of the intermediate article (502) is 5 to 15% less than the wall thickness of the second end part (514) of the intermediate article (502).

15. Method according to claim 13 or 14, characterized in that the first and second end portions (512, 514) of the intermediate article (502) form respective first and second wall portions (520, 522) of the expanded and molded final article (520) and in that the first and second wall portions (520, 522) have the same thickness within a tolerance of + / - 0.5% based on a nominal thickness of the respective wall portions (520, 522).

16. Method according to any one of claims 13 to 15, characterized in that the wall thickness of the intermediate article (502) progressively tapers in increasing thickness in one direction from the first end part (512) of the intermediate article (502) to the second end part (514) of the intermediate article (502).

17. Method according to any one of claims 1 to 16, characterized in that the polymer is polypropylene.

18. Method according to any one of claims 1 to 17, characterized in that the blowing agent is carbon dioxide. Petition 870260103268, dated 06 / 10 / 2026, page 16 / 46 6 / 8 19. Method according to any one of claims 1 to 18, characterized in that during injection step (c) the injection pressure is at least 15000 kPa (150 bar).

20. Method according to any one of claims 1 to 19, characterized in that at the end of injection step (c) a packing pressure of at least 15000 kPa (150 bar) is applied to the plastic composition in the cavity (32).

21. Method according to any one of claims 1 to 20, characterized in that during the opening step (d) the first solid film (14) is exposed to the atmosphere and the external pressure is atmospheric pressure.

22. Method according to any one of claims 1 to 21, characterized in that the first and second mold parts (222, 224) are, respectively, external and internal mold parts (222, 224) forming external and internal surfaces (278, 280) of the article (202), and further comprising the step, before injection step (b), of providing an in-mold label (290) inserted inside the mold cavity (“in-mold label”) at least partially enclosing the cavity (232), the in-mold label (290) being located adjacent to that first cavity-forming surface (246), and wherein after opening step (d) the in-mold label (290) restricts stretching of the first solid film formed adjacent to it.

23. Method according to claim 22, characterized in that the label (290) inserted inside the mold cavity is annular and completely encloses the cavity (232).

24. Method according to claim 23, characterized in that the label (290) inserted inside the mold cavity is composed of a length of a polymer layer (292) having Petition 870260103268, dated 06 / 10 / 2026, page 17 / 46 7 / 8 opposite ends (294, 296) that are joined together in a seam (298) to form an annular shape.

25. Method according to any one of claims 1 to 24, characterized in that it further comprises the step, between the opening step (d) and the cooling step (e), of disposing the molded article in a second mold (320) having a third mold part (322), the third mold part (322) having a molding surface (324), wherein the first solid film (314) is in contact with the molding surface (324), and wherein after the opening step (d) the molding surface (324) restricts stretching of the first solid film (314) in contact with it.

26. Method according to claim 25, characterized in that during the disposition step the molding surface (324) compresses at least one wall portion (310) to reduce the thickness of the cellular foam core layer between the first and second solid films and shrink the length of the first solid film (314) in at least one wall portion (310).

27. Method according to claim 25 or 26, characterized in that the third mold part (322) is hollow and the molding surface (324) defines a hollow cavity (380) with a tapered surface (382), and during the disposition step the molding surface (324) is progressively pressed against the first solid film (314).

28. Method according to any one of claims 25 to 27, characterized in that the third mold part (322) is at a lower temperature than the first mold part, so that the first solid film (314) is cooled when in contact with the third mold part (322).

29. Method according to any of claims 1 Petition 870260103268, dated 06 / 10 / 2026, p. 18 / 46 8 / 8 to 28, characterized in that the first mold part (22) is at a lower temperature than the second mold part (24).

30. Method according to any one of claims 1 to 29, characterized in that it further comprises the step, before solidification of the molten plastic composition (40) foamed between the first and second solid films (14, 16, 314) in the cooling step (e), of pressing an embossing tool against the first solid film (14, 314) to press an inwardly oriented image into the first solid film (14, 314) stretching the first solid film (14, 314) inward against the expanded cellular foam.

31. A method according to any one of claims 1 to 30, characterized in that the article is a cup, mug, bottle, basin, bowl, tray, container or reservoir for holding a liquid or food. Petition 870260103268, dated 06 / 10 / 2026, p. 19 / 46