Process control method for a 3d-printing process
Patent Information
- Application Number
- CA3128833
- Authority / Receiving Office
- CA · CA
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-10-15
- Filing Date
- 2021-08-20
- Publication Date
- 2026-10-20
- Estimated Expiration
- 2041-08-20
AI Technical Summary
Current 3D-printing processes, particularly stereolithography and digital light processing, face challenges in efficiently tracking progress and determining optimal curing time, leading to inefficiencies and increased costs due to complex and costly monitoring systems, especially in dental technology where biocompatibility and oral compatibility are critical.
A process control method using a thermal imaging camera attached to a 3D printer to monitor temperature changes during the polymerization process, allowing for spatially and temporally resolved temperature tracking, which determines the optimal illumination duration and prevents overexposure, thereby ensuring efficient printing with minimal time and resource expenditure.
This method enables the production of high-quality 3D-printed items with reduced production time and costs by accurately controlling the polymerization process, extending the service life of light sources and transparent films, and preventing damage from overexposure or incomplete curing.
Abstract
Description
PROCESS CONTROL METHOD FOR A 3D-PRINTING PROCESS The invention relates to a process control method for a 3D-printing process and to a 3D printer comprising a building platform. According to current prior art, in a 3D-printing process of this type, stereolithography and / or a DLP process (digital light processing process), the components are produced from special print- able plastics material, which is in liquid form and is treated with light and cured by selective illu- mination in layers, generally of a low thickness such as 0.1 or 0.05 mm. Typically, the light is passed through a transparent film and, after the relevant layer is finished, the film is detached from the component or the component from the film. Recently, it has become known to use stereolithography devices and / or DLP processes (digital light processing process) for dental technology, in particular for producing dental restoration parts. It will be appreciated both that components of this type have to be biocompatible and that high requirements are and have to be placed on oral compatibility. To make a 3D-printing process of this type as efficient as possible, the progress of the process has to be tracked. This makes possible a minimal printing duration with optimum curing and thus the best cost- / outlay-to-use ratio. Monitoring the surface in fine metal powder sintering processes by temperature measurement using a thermal imaging camera is known from "Layerwise Monitoring of the Selective Laser Melting Process by Thermography" by Krauss et al., Physics Procedia, 56 (2014) 64 – 71. A stereolithography process or digital light processing process in which a photosensitive mate- rial is cured by radiation, and the measurement radiation is fed into a reference layer and mostly remains within the reference layer as a result of internal reflection, and the measurement radia- tion is detected in a spatially and temporally resolved manner by a sensor, is known from WO 2017 / 106895 A1. In this context, the radiation is spatially and temporally resolved using a com- plicated construction. This construction is highly cost-intensive and thus ill-suited to dental tech- nology. Moreover, in this solution it is not possible to establish when the optimal time is to end the illumination. The object of the invention is therefore to create a simple process control method for a 3D-print- ing process, and a 3D printer comprising a building platform, which make it possible to obtain the best possible printing result with minimum time expenditure. In the process control method according to the invention for a 3D-printing process, a thermal im- aging camera is attached to a 3D printer or connected to the control device of the 3D printer. The output signal thereof is transmitted to the control device. According to the invention, the 3D printer consists of a building platform, a light source, a receiv- ing device for printing material, a thermal imaging camera and a control device. A preferred ap- plication option comprises stereolithography processes and digital light processing processes. The receiving device consists of a trough which may be upwardly open or is at least open to the building platform. For example, a monomer or monomer mix and a photoinitiator are placed in this receiving de- vice for printing material. Other starting solutions such as a photosensitive monomer / monomer mix or a diluted monomer solution are possible. The receiving device has a glass plate as a base and a transparent layer, for example a film, thereon. An inhibitor layer, which prevents adhesion of the printing material upon curing or polymerisation, may be applied to this film. According to the invention, a building platform is introduced into the printing material, so as to dip into the printing material and reach almost as far as the transparent film of the receiving de- vice. So as to achieve a defined spacing between the base film and the building platform, the building platform can be lowered into contact with the base film and subsequently raised by the desired defined value. Between the base film and the building platform, there is thus a monomer layer of a defined thickness, which can subsequently be illuminated positionally selectively. This layer may for example be between 50 and 100 µm thick. A typical cycle of a printing process of this type lasts approximately 10 s, the illumination by the light source making up 2 s thereof. In a preferred embodiment of the invention, the item is produced in layers. This means that after a layer is illuminated the building platform is raised, in such a way that printing material can flow into the resulting gap, and subsequently this material is illuminated. For larger printed items, the building platform is initially raised by more than one layer thickness, preferably by approximately 1 cm, in such a way that the illuminated layer can detach from the film better and printed material can flow into the resulting gap. Subsequently, the building platform is lowered to the desired height again, in such a way that the desired layer thickness is achieved between the building platform and the film. Thus, in each illumination step, the item to be printed is enlarged by one further layer of the cured printing material. It is particularly advantageous if the building platform is raised asymmetrically. For example, the raising may start at one side or one corner. This makes it possible for the building material to detach from the film better. The shear forces are lower, and so there is only a low probability of the film tearing. In addition, the service life of the film is increased, since weaker forces act on it than if the building platform were raised vertically upwards. In layer-wise production of the item, it is possible to print at a building rate of approximately 0.5 mm / min. To reduce the shear forces, it is also conceivable for the device to be embodied in such a way that, during the detachment process of the layer which has been built, the building platform is displaced vertically and the trough moves horizontally. Alternatively, they may also move at an angle at a slight inclination to the horizontal. In a further advantageous embodiment, the item may also be produced continuously. In this context, the transparent layer of the trough of the 3D printer which comes into contact with the printing material is protected against adhesion of the curing printing material by an inhibitor layer. An advantage of this embodiment is that formed layers do not have to be detached from a film individually, but instead the building platform is raised continuously at a defined speed, for example 10 mm / min, during the illumination. However, this requires a higher power of the light source than layer-wise production. Thus, an end product is achieved which does not allow individual layers to be perceived but rather has a homogeneously smooth surface. Moreover, this method makes it possible to accelerate the printing process and thus to reduce the production time, with an accompanying minimisation of the production costs. The light source, which is attached for example centrally below the transparent layer of the receiving device, may for example be a high-precision laser, which emits the optimum wavelength as appropriate to the relevant photoinitiator, or else preferably an LED light source. This is directed onto the transparent base of the trough, and thus onto the base film of the receiving device, and can thus illuminate the printing material from below / outside through the transparent film. Said material preferably cures between the building platform, or the layer already solidified or partially solidified in the previous illumination process, and the transparent film, and adheres to the building platform or the preceding layer, but not to the transparent film. In this step, the layer is illuminated positionally selectively. This may take place either along the entire surface of the layer or only in selected parts of the layer, such as a two- dimensional pattern. As a result of the photoinitiator or photosensitive polymer, the light energy of the light source starts up the positionally selective, exothermic polymerisation at the illuminated points only. According to the invention, during the illumination process and thus during the polymerisation at the illuminated points, the temperature of the entire layer, in other words the thermal radiation of the layer, is tracked in a spatially resolved manner using a thermal imaging camera. The thermal imaging camera is preferably located to the side, below the receiving device, and is directed onto the transparent base film. For this purpose, the thermal imaging camera is directed onto the lower surface of the transparent film, in particular the illuminated region of this film, which is approximately a few square centimetres (1-10 cm<com:Sup>2< / com:Sup>) for dental technology applications for example. Thermal imaging camera of this type detect the heat emission over the entire surface at a spatial resolution of a few hundredths of a square millimetre, in a temporally resolved manner, during (for a few seconds) and between (for approximately 1 minute) the illuminations. The data acquired from a temporally resolved temperature measurement of this type over an illuminated surface correspond to a three-dimensional Gauss distribution of the measured temperature curves. The control device can thus compute a temporally resolved 2-dimensional temperature distribution over the entire surface of the film from the values measured by the thermal imaging camera, while taking into account the thermal conductivity and heat capacity of the materials used (printing material and printer construction materials). On the one hand, the part of the light energy which leads to the heating of the surface is captured by the thermal imaging camera. However, this is approximately constant throughout the illumination process and is subtracted by the control device. Further, the thermal imaging camera detects the energy arising during the exothermic polymerisation of the material. The measured temperature at the surface thus corresponds to the emission of particular wavelengths and wavelength ranges of the illuminated surface. This is detected by the thermal image camera in a temporally resolved manner. The change in temperature dT / dt thus corresponds to the first derivative of the temperature curve. A positive change in temperature <com:Math><semantics>(dT / dt>0)<annotation encoding="application / x-tex">(dT / dt > 0)< / annotation>< / semantics>< / com:Math> represents heating (heat of emission) and a negative change in temperature (dT / dt < 0) represents cooling (coldness of emission) of the surface. A constant temperature, in other words no change in temperature <com:Math><semantics>(dT / dt=0)<annotation encoding="application / x-tex">(dT / dt = 0)< / annotation>< / semantics>< / com:Math>, means a constant surface temperature or a maximum / minimum of the temperature curve (<com:Math><semantics>Tmax<annotation encoding="application / x-tex">T_{max}< / annotation>< / semantics>< / com:Math> or <com:Math><semantics>Tmin<annotation encoding="application / x-tex">T_{min}< / annotation>< / semantics>< / com:Math>). The change in temperature over the film surface is detected in a spatially resolved manner by the thermal imaging camera and passed to the control device. In an advantageous embodiment, the integral of the temperature curve, in other words the amount of heat, is detected in a spatially resolved manner. The time of the end of the illumination is established by a predefined temperature <com:Math><semantics>Tmax<annotation encoding="application / x-tex">T_{max}< / annotation>< / semantics>< / com:Math> or a predefined change in temperature dT / dt being reached. If this temperature or change in temperature is measured by the thermal imaging camera and detected by the control device, the control device emits a signal. The control device subsequently ends the building process of this layer by ending the illumination. Further, it is possible that, as a result of an undesired, inhomogeneous temperature distribution being measured, particular regions of the layer may continue to be illuminated while other parts are no longer illuminated, since the curing has already taken place satisfactorily at these points. The desired polymerisation rate can thus be achieved in all regions. The predefined temperature <com:Math><semantics>Tmax<annotation encoding="application / x-tex">T_{max}< / annotation>< / semantics>< / com:Math> is established as the maximally desired heating temperature detected at the surface of the polymerising layer by the thermal imaging camera. The change in temperature dT / dt at this time converges towards zero or in particular has a zero value. Since it is difficult to track the change in temperature as far as the zero value in a finite time period, it is also possible to work with a defined threshold (for example <com:Math><semantics>dT / dt=2<annotation encoding="application / x-tex">dT / dt = 2< / annotation>< / semantics>< / com:Math> to 5 K / s). This monitoring of the spatially resolved temperature progression can prevent damage to or undesired polymerisation of the surrounding material due to overexposure. Preferably, the illumination is ended as soon as a desired predefined degree of curing is achieved, since in the event of excessive or even complete polymerisation of the monomers the adhesion of the next layer would be reduced. Moreover, the LEDs and LED-DMDs or other light sources used as a light source each have a limited, specific burn time. Thus, as a result of the monitoring of the spatially resolved temperature progression, the optimum illumination duration can be determined and unnecessarily long illumination can be prevented, which would otherwise reduce the service life of the light source unnecessarily. After the illumination ends, the layer has to be released from the film. This takes place in that for example the building platform is raised from the film by a particular amount. This amount has to be at least for example the layer thickness of a printing process. However, it is preferred initially to raise the building platform by a larger amount so as to facilitate complete detachment, and subsequently to lower it to the desired layer thickness (for example 50 to 100 mm). It is further conceivable to lower the film down. For this purpose, it is advantageous to lower the film diagonally with the trough, in other words starting at one side, in such a way that the film is in effect detached from the cured printing material. In a continuous printing process, the inhibitor layer prevents adhesion of the cured printing material to the transparent film. This makes a detachment process of this type superfluous. Overexposure in a 3D stereolithography process or a digital light processing process also leads to excessively strong adhesion between the material and the film and an unnecessarily drawn-out printing process. This can be avoided using the method according to the invention, since the optimum illumination duration is determined using the temperature tracking by the thermal imaging camera. Aside from the aforementioned conservation of the light source, this also makes an increased service life of the transparent film and a time saving possible. The excess adhesion can lead to damage to, scratches on, or detachment of the inhibitor layer and / or to scratches on, damage to or even tearing of the film, or both. Once damage of this type has occurred, it can only be eliminated by interrupting the printing process, or said process may even have to be aborted entirely, since otherwise building errors will be left in the final product. Upon detachment, new material to be polymerised enters the resulting gap. This can be detected by the thermal imaging camera as a large fall in the measured heat emission, in other words a fall in the temperature (change in temperature dT / dt << 0). After the detachment and after the first downward jump in temperature when printing material flows in for the first time, any further material flow with or without gas bubbles between the building platform and the film can be detected by the thermal imaging camera as a change in temperature in each case <com:Math><semantics>(dT / dt>0)<annotation encoding="application / x-tex">(dT / dt > 0)< / annotation>< / semantics>< / com:Math> or <com:Math><semantics>dT / dt<0)<annotation encoding="application / x-tex">dT / dt < 0)< / annotation>< / semantics>< / com:Math> and recognised in the control device. Further, it is favourable that impurities on the film with or without an inhibitor layer – for example due to sedimentation, contamination, adhesion of residues from any erroneous building process or of foreign particles – can be detected. Cases of this type can be detected in that, for example during a movement of the building platform, an excessively small change in temperature is detected by the thermal imaging camera and recognised in the control device. This applies not only in the event of an excessively small change in temperature over the entire film surface, but also on sub-areas, in other words if it the thermal imaging camera records that the temperature distribution / change is not plausible over the entire film surface. The control device subsequently emits a warning signal. This is particularly important if gas bubbles or small impurities are left behind on the film or on the inhibitor layer, in particular between the item and the film or inhibitor layer. This is detected because the temperature is lower at the location of a gas bubble than in the environment. The thermal imaging camera detects the temperature in a spatially resolved, high-precision manner, in such a way that the control device can detect temperature differences of this type and thus output an error signal or warning signal. The spatial resolution of the thermal imaging camera is preferably in the region of the layer thickness of the building process, in other words approximately 0.1 mm <com:Math><semantics>×<annotation encoding="application / x-tex">\times< / annotation>< / semantics>< / com:Math> 0.1 mm, but may also be much greater, for example ten times greater, in other words 1 mm <com:Math><semantics>×<annotation encoding="application / x-tex">\times< / annotation>< / semantics>< / com:Math> 1 mm, or much smaller, for example <com:Math><semantics>0.025×0.025<annotation encoding="application / x-tex">0.025 \times 0.025< / annotation>< / semantics>< / com:Math> mm. The control device only triggers the illumination process of a following step when these faults have been eliminated or the user triggers the illumination manually. The faults are recognised as eliminated when the thermal imaging camera records and the control device detects that there are no gas bubble(s) or no impurities left on the film. This can be detected from the thermal imaging camera measuring a homogeneous change in temperature over the entire surface during a material flow. In this case, the control device detects no irregularities in the change in temperature, and thus detects that there are no impurities or gas bubbles adhering to the surface of the film. Once the inward flow of new printing material is ended, in other words once the material flow is ended, the thermal imaging camera measures a constant temperature over the entire surface of the film. The control device thus verifies its results during a material flow, and can check whether there are really no impurities or gas bubbles left on the surface of the film. A further embodiment provides that if disruptive factors are detected the entire printing process is aborted. Moreover, the control device only triggers the illumination process of the next step once the thermal imaging camera has recorded and the control device has recognised that, after a change in temperature exceeding a predetermined threshold – corresponding to a material flow –, no further significant change in temperature (dT / dt converges towards 0) is measurable. This means that the entirety of the cured material has to have detached from the film surface and the material flow is approaching a standstill. In an advantageous development, the control device outputs a warning signal or error signal when the thermal imaging camera records and the control device detects that the heat emission at the start of the illumination does not change within a predefined time, preferably 2 seconds. This would mean that the light source has failed, that the illuminated layer is already fully cured, or that the polymerisation has not been started up as a result of another source of error. It is also possible for example that the layer might not have detached completely from the film, the film might have torn, or the printing material might have run out. Thus, by monitoring the temperature progression during the polymerisation process and also between the illumination of different layers, most errors during the 3D-printing process, for example soiling of the foil, deposition of foreign bodies, incomplete detachment of the item from the film or ageing of the film, LED or LED-DMD, are recognised early. As a result, when a warning signal is outputted, the illumination process is delayed, in particular paused, or aborted by the control device. The building process of the next layers can be adapted for example automatically by the control device or by user intervention to minimise damage. When a warning output is outputted during an illumination process, it is also possible to start the current illumination of the layer afresh, in such a way that, for example, if the light source fails the illumination process can be continued after said source is checked and repaired, without obtaining an erroneous layer in the end product. In an advantageous embodiment, the dimensions of the illuminated layer of the 3D-printed item during polymerisation may be tracked using multi-dimensionally, in particular two- dimensionally spatially resolved temperature measurement. For this purpose, during the printing process, in particular both during the illumination and between the illuminations, the heat emission of the surface of the transparent film is tracked and displayed using a thermal imaging camera. The illuminated points emit more heat than the remaining regions. This is caused both by the incoming light energy of the light source and by the heat occurring during the exothermic polymerisation process. Thus, the control device can calculate the actual dimensions of the illuminated layer from the determined data of the thermal imaging camera and compare them with the theoretical values, in other words the raw data before the illumination, which have been passed to the light source. For monitoring and checking the printing process, during each illumination process the dimensions of the illuminated parts of the film are determined using the thermal imaging camera and stored by the control device. These data may subsequently be compared with one another and with the raw data. If the dimensions of an illuminated layer decrease by comparison with the previous layer, it can be assumed that the illuminated region is being reduced. Otherwise, if the dimensions of the illuminated layer increase, said region is being enlarged. This is important in particular in the event of very large differences between the layers. The large difference indicates an error in the building process. If an unexpectedly large change of this type in the illuminated area is measured between two or more layers, the control device outputs a warning signal, in particular an error signal. Thus far, in 3D-printing methods, it has been necessary to carry out distortion correction so as to compensate the shift in the individual layers with respect to one another during the printing process. According to the invention, this distortion correction is now superfluous as a result of the monitoring of the increase or decrease in area of the printed layer of a 3D item to be produced, since the size of the item is tracked during the polymerisation and the building process can be adapted accordingly. When a warning signal of the control device is outputted, it can be decided by the user – or optionally automatically by the control device – whether or not the large increase or decrease in area was intended. If it was not intended, the source of error can be eliminated. If a layer is too small, the desired region of this erroneous layer can subsequently be illuminated afresh so as to achieve optimum curing of the desired area. In the event of unintended excessive illumination, the error is more difficult to eliminate. In this context, after the source of error is removed, the next layer can be printed without error, and after the end of the printing process the remaining undesired parts can be removed by the user by hand. This may take place for example using a conventional hand sander. The 3D printer according to the invention consists of a building platform, a light source, a receiving device for the printing material, a control device and an attached thermal imaging camera. The thermal imaging camera transfers the output signal thereof to the control device. The control device may for example be a computer comprising a special software which actuates the 3D-printing unit in such a way that an item made from the printing material can be produced layer-wise or continuously, as described above. In a further embodiment according to the invention, a DMD unit is attached to the 3D printer. If the thermal imaging camera and the control device now recognise that a layer is curing non-uniformly, the radiation can be deflected from the already cured regions by the DMD unit. Thus, the regions which are not yet fully cured continue to be illuminated, and at the same time overexposure of the already fully cured regions is prevented. This process is based on the projection technology of digital light processing (DLP). In this context, images, or in this case light rays having a defined light energy, are produced by modulating a digital image, or wavelengths of defined energies, onto a light ray. The light ray is decomposed by an arrangement of movable micromirrors into individual image points or pixels, and subsequently individually reflected either into or out of the projection path. This makes possible fine, high-precision control of the light rays onto the desired regions of the lower surface of the transparent film, in such a way that overexposure of individual regions can be prevented. This arrangement of movable micromirrors, including the actuation technology thereof, is referred to as a DMD (digital micromirror device) unit. Preferably, the individual micromirrors of a DMD unit are arranged in the form of a square matrix, and can be controlled or tilted by the control device individually as required. Tilting of this type between an on and an off position, which can be controlled autonomously for each individual micromirror, is brought about by applying electrostatic fields. This makes surprisingly fine and precise control of the light radiation or laser radiation possible. Preferably, for each individual micromirror, two stable end states are defined, here an on and an off position, between which the micromirror can switch frequently within one second, in particular up to 5000 times. The on position describes the state in which the light energy is passed to the region for illumination, whilst the off position describes the state in which the light energy is deflected away from the illumination surface. The edge length of these individual micromirrors of a DMD unit is preferably a few micrometres, in particular approximately 16 µm. The number of mirrors within a DMD unit corresponds to the resolution of the projected image, in other words in this case the desired resolution of the illuminated region, it preferably also being possible for a plurality of pixels to be represented by one micromirror. In a preferred embodiment, the individual pixels may also be actuated at any desired different brightness levels. This is achieved in that the individual micromirrors are controlled by binary pulse-width-modulated actuation, in other words pulse-density modulation. The brightness level of a pixel is thus dependent on how long a micromirror is switched on. In a preferred embodiment, a colour filter can be arranged in front of the DMD unit, in other words in the projection path of the light radiation. It can for example filter out a wavelength from the deflected light or restrict the deflected light ray to one wavelength. It is also possible to use a monochromator, for spectral isolation of a particular wavelength from the incident beam, instead of a colour filter. A major advantage of this DLP technology comprising a DMD unit is the increased precision. The light energy, in other words the light radiation, can be guided away very precisely from the regions of the lower surface of the transparent film in which the material to be polymerised already has a desired curing level, in such a way that overexposure is avoided. Further advantages, details and features will be apparent from the following description of a plurality of embodiments of the invention with reference to the drawings, in which: Fig. 1 is a schematic drawing of the lateral cross section of a 3D printer according to the invention in a first embodiment; Fig. 2 is a schematic drawing of the lateral cross section of a further embodiment of a 3D printer according to the invention; Fig. 3 is a schematic drawing of the light output, the temperature progression and the z-position of the building platform during the 3D-printing process; Fig. 4 is a further schematic drawing of the light output, the temperature progression and the z-position of the building platform during the 3D-printing process; and Fig. 5 is a schematic drawing of an optical construction of a further embodiment of a 3D printer according to the invention. Fig. 1 is a schematic drawing of the lateral cross section of a 3D printer 2 according to the invention for a stereolithography process or digital light processing process, comprising a building platform 4, a receiving device 10 for printing material 8, a thermal imaging camera 12 and a control device 14. In this embodiment, printing material 6 cured on the lower face of the building platform 4 is represented schematically. The cured printing material 6 can take on a different embodiment depending on the printed item, and is represented here by columns of different thickness. Further, an arrow indicates the movement direction of the building platform 4, which can be displaced vertically up and down. Below the building platform 4, there is a receiving device 10 for printing material 8, the fill level of the printing material 8 being represented by a dashed line. The lower boundary 11 of the receiving device 10 consists of a transparent material, preferably a transparent film. A thermal imaging camera 12 is directed onto the outer and lower surface 9 of this film 11, and is in turn connected to a control device 14. Using this thermal imaging camera 12, the temperature of the part to be checked of the surface 9 of the film 11 can be measured. For this purpose, the thermal imaging camera is directed onto the lower surface 9 of the very thin film 11, and the heat emission during and between illuminations is recorded. In this case, a dental restoration part is involved, and the region of the film 11 to be monitored is approximately 5 cm <com:Math><semantics>×<annotation encoding="application / x-tex">\times< / annotation>< / semantics>< / com:Math> 5 cm. From the data received from the thermal imaging camera 12, the control device 14 can create a 2-dimensional temperature distribution over the part to be checked of the surface 9 of the film 11, while taking into account the thermal conductivity and heat capacity of the materials used – the transparent film 11 and the printing material 8. In the event of abnormalities in the 2-dimensional temperature distribution between two or more layers and / or other unexpected changes in temperature, the control device 14 emits a signal to warn of errors. Possible errors are for example the absence of an upward jump in heat emission at the start of the illumination or the absence of a downward jump in temperature when the cured printing material is detached from the film. It is also possible that upon comparison of the 2-dimensional temperature tracking – and thus the illuminated and cured areas – of two or more layers, an excessive area increase or decrease in the cured layer is recorded. In the event that errors are recorded in the printing process, it may optionally be adapted automatically by the control device 14. However, it is more common that if a warning signal is outputted the control device 14 pauses the printing process until all errors have been eliminated by the user and the user triggers the printing process again. Fig. 2 is a schematic drawing of the lateral cross section of a further embodiment of a 3D printer 2. This shows an active printing process – in other words occurring illumination of a layer – by a 3D printer according to Fig. 2. The columns shown herein of the cured printing material 6, which are intended to represent schematically the already printed item, now dip into the printing material 8. Centrally below the receiving device 10, a light source 18 having a conical illumination region 20 is schematically shown. A light source of this type may be a high-precision laser which emits the optimum wavelength as appropriate to the relevant photoinitiator, or else preferably an LED light source. For simplicity, the entire possible detection region is shown here, although the capture may take place in a spatially resolved manner using a focus mark of for example 0.5 mm <com:Math><semantics>×<annotation encoding="application / x-tex">\times< / annotation>< / semantics>< / com:Math> 0.5 mm. Between the already cured printing material 6 and the transparent film 11, newly cured material 16 is schematically shown. For simplicity, conical illumination 20 is shown. However, it would also be possible to illuminate only the desired regions (1 pixel for example <com:Math><semantics>20×20μm<annotation encoding="application / x-tex">20 \times 20 \mu m< / annotation>< / semantics>< / com:Math>) between the already cured material 6 and the transparent film 11 using a plurality of light source which illuminate smaller regions or appropriate deflection mirrors, optionally with a slight increase or decrease in area. In this embodiment, the thermal imaging camera 12 is only directed onto the illuminated region of the film surface 9, even if this is not shown in detail in the drawings, and is focused and therefore only receives the heat emission of this small region. By way of illustration, this is shown using dot-dash lines. As a result of this concentration on the important region, in other words the exact region of the 3D-printing process, it is possible to avoid unnecessarily large datasets and thus slow processing by the control device 14. Fig. 3 graphically displays the light output, the temperature progression and the z-position of the building platform <com:Math><semantics>4−in<annotation encoding="application / x-tex">4 - in< / annotation>< / semantics>< / com:Math> other words the internal vertical displacement of the building platform 4 with respect to the transparent film 11 – during the 3D-printing process. Line a) gives information about the light output of the light source 18 in [mW / cm<com:Sup>2< / com:Sup>]. When the light source 18 is switched on, the light output increases linearly with a steep gradient, optimally jumping up. During the illumination, the light output is kept constant and subsequently switched off, bringing about a downward jump in the light output. Line b) shows the progression of the room temperature during the 3D-printing process. This should optimally be kept constant so as to avoid incorrect measurement of the temperature progression at the film surface 9. Line c) shows an optimum temperature progression at the surface 9 of the transparent film 11 during the printing process. This temperature progression is received by the thermal imaging camera 12 and evaluated by the control device 14. The temperature increases at the time when the light source 18 is switched on. This is caused by the incoming light output of the light source 18 and the onset of the exothermic polymerisation of the printing material 8. When the change in temperature dT / dt approaches a particular value as close as possible to zero, in particular a zero value, the maximum of the temperature during the polymerisation process <com:Math><semantics>Tmax<annotation encoding="application / x-tex">T_{max}< / annotation>< / semantics>< / com:Math> is approximately reached. The value <com:Math><semantics>dT / dt=0<annotation encoding="application / x-tex">dT / dt = 0< / annotation>< / semantics>< / com:Math> cannot be reached within a finite time, and therefore a value close to zero is resorted to so as to keep the illumination duration as short as possible and nevertheless to achieve appropriate curing of the printing material 8. At this time, the light source 18 is switched off and the temperature of the surface 9 of the transparent film 11 slowly takes on the initial value thereof again. Line d) gives information about the z-position of the building platform <com:Math><semantics>4−in<annotation encoding="application / x-tex">4 - in< / annotation>< / semantics>< / com:Math> other words the internal vertical displacement of the building platform 4 with respect to the transparent film 11 – during the progression of a 3D-printing process. The building platform 4 is displaced close to the transparent film 11 before the illumination so as to achieve a defined gap of x mm (where x may be adapted depending on the requirements). After the end of the illumination process, the building platform 4 is moved away from the film 11 again so as to achieve detachment of the cured material 6 from the transparent film 11. Moreover, time periods 1 to 5 are marked in Fig. 3. These denote the individual portions of the 3D-printing process. Region 1 is the initial value, and represents the initial position and the temperature without illumination. This point is optimally reached again after the printing process for all of curves a) to d). Region 2 shows the approach of the building platform 4 towards the transparent film 11. At this time, the light source 18 is switched off and the temperatures correspond to the starting value. At the end of the region 2, in other words if the building platform 4 approaches the film 11 optimally, the light source 18 is switched on and the polymerisation starts up. This can be seen from the initial temperature increase of line c). In region 3, the maximum heating temperature <com:Math><semantics>Tmax<annotation encoding="application / x-tex">T_{max}< / annotation>< / semantics>< / com:Math> of the film surface 9 during the illumination is reached. Here, the change in temperature dT / dt approaches a particular value, in particular a zero value. When this value is reached, the light source 18 is switched off and the temperature of the surface 9 of the transparent film 11 starts to fall again. Region 4 denotes the cooling process of the film surface 9, after the illumination has ended and the polymerisation is thus ended. When the starting temperature of the film surface 9 is reached, time period 5 starts, at which the building platform 4 travels back into the starting position thereof and the polymerised printing material 6 is thus detached from the transparent film 11. At the end of region 5, the starting values (region 1) of all parameters are reached again. Fig. 4 shows an embodiment modified from that of Fig. 3. In this context, the light output, the temperature progression and the Z-position of the building platform <com:Math><semantics>4−in<annotation encoding="application / x-tex">4 - in< / annotation>< / semantics>< / com:Math> other words the internal vertical displacement of the building platform 4 with respect to the transparent film 11 – during the 3D-printing process are again shown. The Z-position of the building platform 4 is different from in Fig. 3. Line a) shows the Z- position of the building platform 4 – in other words the internal vertical displacement of the building platform 4 with respect to the transparent film 11 – during the progression of a 3D-printing process. The building platform 4 is moved away after the curing (illumination) of the transparent film 11 and subsequently approaches again, so as to achieve a defined gap of x mm (where x may be adapted depending on the requirements). Line b) shows the progression of the light output 18 in [mW / cm<com:Sup>2< / com:Sup>]. When the light source 18 is switched on, the light output jumps up. While the building platform 4 is moving, the light source is switched off and thus has an output of 0 mW / cm<com:Sup>2< / com:Sup>. During the illumination, the light power is kept constant. Line c) shows, similarly to in Fig. 3, an optimum temperature progression at the surface 9 of the transparent film 11 during the printing process. The temperature increases at the time when the light source 18 is switched on and the building platform 4 is displaced in the Z-direction, and remains constant when a particular value is reached, in particular the temperature of the liquid printing material 8. If the light source is switched on again, the temperature increases again. This is caused by the incoming light output of the light source 18 and the onset of the exothermic polymerisation of the printing material 8. After the curing has ended, the temperature remains constant again (change in temperature dT / dt approaches a zero value). This corresponds to the maximum of the temperature during the polymerisation process <com:Math><semantics>Tmax<annotation encoding="application / x-tex">T_{max}< / annotation>< / semantics>< / com:Math>. The room temperature (in this case line d)) during the 3D-printing process should be kept as constant as possible in this case too so as to avoid erroneous measurement of the temperature progression at the film surface 9. Moreover, Fig. 4 shows time periods I to III. These denote the individual portions of the 3D-printing process. Region I shows the Z-position of the building platform 4 during the illumination process. In this context, the light source 18 is switched on and the film surface 9 shows the maximum heating temperature <com:Math><semantics>Tmax<annotation encoding="application / x-tex">T_{max}< / annotation>< / semantics>< / com:Math> reached during the illumination. The change in temperature dT / dt approaches a zero value here. Region II shows the change in the Z-position of the building platform 4 between two illumination processes. The building platform 4 is raised. At the start of the movement of the building platform 4, the light source 18 is switched off, causing the temperature at the surface 9 of the transparent film 11 to decrease greatly and to remain constant until the end of this region II once a particular temperature is reached, in particular the temperature of the liquid printing material 8. Region III again shows the lowering of the Z-position of the building platform 4 at the start of an illumination progress. The light source is switched on again, in such a way that the temperature at the surface 9 of the transparent film 11 increases again. This is caused by the incoming light output of the light source 18 and the onset of the exothermic polymerisation of the printing material 8. After the curing is complete, the temperature again takes on the constant value <com:Math><semantics>Tmax<annotation encoding="application / x-tex">T_{max}< / annotation>< / semantics>< / com:Math> in accordance with region I (change in temperature dT / dt approaches a zero value). This indicates the end of the polymerisation process, and so the cycle can start afresh. Fig. 5 is a schematic drawing of a further embodiment of a 3D printer 2 according to the invention. The peculiarity here is the optics used for guiding the light radiation towards the printed item or printing material 6, in other words towards the surface 9 of the transparent film 11, and the thermal or IR radiation from the printed item / printing material 6 towards the thermal imaging camera 12. The light source 18 is next to the item to be printed in this embodiment, and is shown above said item in Fig. 5. Radiation 19 exiting the light source 18 and used for illumination is deflected via a mirror 30 to a converging lens 28. In an advantageous embodiment, the mirror 30 is formed with an edge filter, in such a way that the radiation 19 is reliably reflected but natural light can pass freely through the mirror. The lens 28 is suitable for converging and parallelising the individual light rays of the illumination radiation 19, and optionally also the additional natural light radiation. The now parallel rays of the illumination radiation 19 are passed on from the (converging) lens 28 to two laminated prisms 25 and 26 and a DMD unit 24. In this embodiment, the two prisms 25 and 26 together form a "total internal reflection" prism" (TIR prism) 27 Total internal reflection is a physical phenomenon occurring in waves, such as light rays, and occurs when the light is shallowly incident on a boundary surface with another transparent medium in which the propagation speed of the light is greater than in the starting medium. If the angle of incidence is varied continuously, this effect occurs relatively abruptly at a particular value of the angle of incidence. This specific angle of incidence is known as the critical angle for total internal reflection. The light mostly no longer passes over into the other medium, but instead is (more or less) totally reflected back into the starting medium from this angle onwards. The TIR prism, in other words the optical element, which is composed of the two laminated prisms 25 and 26, can thus be used as a mirror. If the refractive index of the TIR prism 27 is high enough, total internal reflection (TIR) is achieved, and the TIR prism 27 acts like a mirror with 100% reflection. As a combination of two laminated prisms 25 and 26, the TIR prism 27 deflects the incident light onto the DMD unit 24, and the image to be produced is projected using the light ray reflected from the DMD unit 24. The use of a TIR prism 27 thus makes considerable saving of space possible, since the same effect could only be achieved with a highly complex combination of mirrors. Moreover, this greatly increases the contrast achieved by the system. The radiation exiting the TIR prism extends onwards to a projection lens 22, which again splits the parallel rays of the illumination radiation 19 into a conical illumination region 20. For simplicity, a possible illumination region 20 is shown here, but the illumination may be spatially resolved using a focus mark of for example 0.5 mm <com:Math><semantics>×<annotation encoding="application / x-tex">\times< / annotation>< / semantics>< / com:Math> 0.5 mm. The radiation of the conical illumination region 20 is subsequently passed to a semi- transparent mirror 32, known as a splitter mirror, which the illumination radiation 19 can pass through. Subsequently, the illumination radiation 19 is incident on a transparent film 11, and illuminates a desired region between said film and the already cured material 6. The resulting thermal radiation 13, in other words the IR radiation, is emitted by the material 6 and back through the transparent film 11 to the semi-transparent mirror 32. In an advantageous embodiment, the mirror 32 is formed as a splitter mirror, in other words in such a way that the thermal radiation 13, in other words the IR radiation, is reflected towards the thermal imaging camera 12, but the illumination radiation 19, for example UV radiation, can pass through the mirror unchanged. For simplicity, a conical illumination region 20 is shown. However, by using a plurality of light sources which illuminate smaller regions, it is also possible to illuminate only the desired region (1 pixel for example <com:Math><semantics>20×20μm<annotation encoding="application / x-tex">20 \times 20 \mu m< / annotation>< / semantics>< / com:Math>) between the already cured material 6 and the transparent film 11 – optionally with a slight increase or decrease in area. In an advantageous embodiment, the DMD unit 24 can further switch individual pixels of the illumination region on or off depending on completeness of curing. This makes it possible to prevent overexposure of already cured regions.
Claims
1. Process control method for a 3D-printing process using a 3D printer which has a building platform, a light source, a receiving device for printing material and a control device by means of which an item is produced layer-wise or continuously from the printing material, wherein a thermal imaging camera, the output signal of which is transmitted to the control de- vice, is attached to the 3D printer, and the method comprising the following steps: illuminating a layer or parts of said layer positionally selectively, detecting the temperature of the layer during polymerisation using the thermal imaging camera, ending a building process of a layer by ending the illumination, the time of the end of the illumination being established by a predefined temperature T m a x T_{max} or a predefined change in temperature dT / dt being reached.
2. Method according to claim 1, wherein the 3D-printing process comprises a stereo- lithography process and / or a digital light processing process.
3. Method according to claim 1 or claim 2, wherein the predefined temperature T m a x T_{max} is established as the maximum heating temperature detected at the surface of the polymerising layer by the thermal imaging camera, the change in temperature dT / dt at this time converging towards zero.
4. Method according to any one of claims 1 to 3, wherein the change in temperature dT / dt takes on a zero value.
5. Method according to any one of claims 1 to 4, wherein the thermal radiation of the layer is detected by the thermal imaging camera, the change in temperature dT / dt correspond- ing to a first derivative of the temperature curve, a positive change in temperature dT / dt > 0 indi- cating heating of the surface, a negative change in temperature dT / dt < 0 indicating cooling of the surface, and no change in temperature dT / dt = 0 indicating a constant temperature or the maximum / minimum of a temperature curve T m a x T_{max} or T m i n T_{min} .
6. Method according to any one of claims 1 to 5, wherein the change in temperature over a film surface is detected in a spatially resolved manner by the thermal imaging camera and passed to the control device.
7. Method according to any one of claims 1 to 6, wherein after the illumination ends the layer is detached from a film and the building platform is raised, new material to be polymerised arriving in a resulting gap, and the detachment of the item from the film being recognised by the thermal imaging camera as a decrease in temperature dT / dt << 0.
8. Method according to claim 7, wherein during the illumination the building platform is raised continuously at a defined speed, new material to be polymerised arriving in the resulting gap, and wherein an inhibitor layer prevents adhesion to the film.
9. Method according to claim 8, wherein the defined speed is 0.5 mm / min.
10. Method according to any one of claims 1 to 6, wherein the building platform is raised incrementally between the illumination times with a defined step height, and subsequently low- ered to a desired layer thickness, new material to be polymerised arriving in a resulting gap and being cured in the next illumination step.
11. Method according to claim 10, wherein the defined step height is about 0.3 to about 3 cm.
12. Method according to claim 10 or claim 11, wherein the building platform is raised di- agonally, to a height of 1 cm between the illumination times, and wherein the building platform is subsequently orientated substantially horizontally and subsequently lowered to the desired layer thickness.
13. Method according to claim 12, wherein the building platform is raised starting from one side or edge.
14. Method according to any one of claims 7-9, wherein the material flow with or without gas bubbles between the building platform and the film is detected by the thermal imaging cam- era as a change in temperature dT / dt > 0 or dT / dt < 0 in each case and recognised in the con- trol device.
15. Method according to any one of claims 7-9, or 14, wherein impurities on the film or an inhibitor layer are detected by the thermal imaging camera and are recognised in the control de- vice on the basis of a detected change in temperature.
16. Method according to claim 15, wherein the impurities are due to sedimentation, con- tamination, adhesion of residues from any erroneous building process or of foreign particles.
17. Method according to claim 15 or claim 16, wherein the impurities on the film or inhibi- tor layer are detected during movement of the building platform.
18. Method according to any one of claims 7-9, or 14-17, wherein an illumination process of a next step only starts when the thermal imaging camera records and the control device rec- ognises that no gas bubbles or no impurities have been left behind on the film.
19. Method according to any one of claims 1 to 17, wherein an illumination process of a next step only starts when the thermal imaging camera records and the control device recog- nises that after a change in temperature exceeding a predetermined threshold no further change in temperature is measurable.
20. Method according to any one of claims 1 to 19, wherein the control device outputs an error signal or warning signal when the thermal imaging camera records that a temperature dis- tribution is not plausible over an entire film surface.
21. Method according to claim 20, wherein the temperature distribution is not plausible over the entire film surface because gas bubbles or small impurities have been left behind on the film or inhibitor layer.
22. Method according to claim 20 or claim 21, wherein the temperature distribution is not plausible over the entire film surface because gas bubbles or small impurities have been left be- hind between the item and the film or inhibitor layer.
23. Method according to any one of claims 1 to 22, wherein the control device outputs an error signal or warning signal when the thermal imaging camera records and the control device detects that a thermal emission does not change within a predefined time at the start of the illu- mination.
24. Method according to claim 23, wherein the predefined time is approximately 2 sec- onds.
25. Method according to any one of claims 1 to 24, wherein an illumination process is de- layed, or aborted by the control device if the control device outputs a warning signal and subse- quently the building process of a next layer is adapted or a previous illumination process is re- peated.
26. Method according to claim 25, wherein the illumination process is delayed comprises the illumination process is paused.
27. Method according to any one of claims 1 to 26, wherein the dimensions of each printed layer are tracked during polymerisation using multi-dimensional spatially resolved tem- perature measurement, the dimensions of the illuminated layer being compared against the real dimensions of a preceding layer and against the theoretical dimensions of the item, the next layer being reduced if the size of the illuminated area decreases and enlarged if it increases.
28. Method according to claim 27, wherein the multi-dimensional spatially resolved tem- perature measurement is 2-dimensional.
29. 3D printer comprising a building platform, a light source, a receiving device for print- ing material and a control device by means of which an item is produced layer-wise or continu- ously from the printing material, wherein a thermal imaging camera, the output signal of which is transmitted to the control device, is attached to the 3D printer, and the control device is config- ured to perform the following steps: illuminating a layer, • detecting the temperature of the layer during polymerisation using the thermal imaging camera, • ending a building process of a layer by ending the illumination, the exact time of the end of the illumination being established by a predefined temperature or a predefined change in temperature being reached.
30. The 3D printer of claim 29, wherein the item is produced layer-wise or continuously from the printing material for stereolithography processes and / or digital light processing pro- cesses.