Process to conduct a steam cracking reaction in a fluidized bed reactor

CA3184993CActive Publication Date: 2026-10-13TOTALENERGIES ONE TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CA3184993
Authority / Receiving Office
CA · CA
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-07-27
Filing Date
2021-07-27
Publication Date
2026-10-13
Estimated Expiration
2041-07-27

AI Technical Summary

Technical Problem

Current steam cracking processes in fluidized bed reactors rely on fossil carbon-based fuels for heating, which are environmentally unfriendly and inefficient, and there is a need for a scalable solution to transition away from these fuels.

Method used

A process using a fluidized bed reactor with at least two electrodes and a bed comprising electrically conductive particles, where the bed is heated by passing an electric current through it, eliminating the need for external heating devices and achieving temperatures of 500 C to 1200 C for steam cracking reactions.

Benefits of technology

This approach allows for efficient and environmentally friendly steam cracking of hydrocarbons into valuable chemicals like hydrogen, ethylene, and propylene without external heating, minimizing energy loss and reducing carbon footprint.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The disclosure relates to a process to perform a steam cracking reaction, said process comprising the steps of providing a fluidized bed reactor comprising at least two electrodes; and a bed comprising particles, wherein the particles are put in a fluidized state by passing upwardly through the said bed a fluid stream, to obtain a fluidized bed; heating the fluidized bed to a temperature ranging from 500°C to 1200°C to conduct the endothermic chemical reaction; wherein at least 10 wt.% of the particles based on the total weight of the particles of the bed are electrically conductive particles and have a resistivity ranging from 0.001 Ohm.cm to 500 Ohm.cm at 800°C and in that the step of heating the fluidized bed is performed by passing an electric current through the fluidized bed.
Need to check novelty before this filing date? Find Prior Art

Description

<DP=1>²WO 2022 / 023346 1 ²PCT / EP2021 / 071011²Process to conduct a steam cracking reaction in a fluidized bed reactor ²Field of the disclosure²The present disclosure relates to a process for performing a steam cracking ²reaction in a ²fluidized bed reactor wherein the reaction is performed without the need of an ²external heating²device in the said fluidized bed reactor. The present disclosure aims to ²contribute to the²replacement of the use of fossil carbon-based fuels heating devices. The ²present disclosure ²relates to the electrification of the chemical industry.²Background²Climate change and ongoing energy transition make it mandatory to replace ²fossil carbon-²based fuels in chemical production and recycled processes with a more ²environmentally²friendly decarbonized source of energy. Transforming natural gas into valuable ²chemicals ²requires elevated temperature, often higher than 800 C and even up to 1000 C ²and are often ²endothermic. The energy needed is, therefore, high and not often ²environmentally friendly, as ²is demonstrated by the common use of fired heated reactors. Several studies ²have been² undertaken to reduce the burden imposed by these (harsh) reaction conditions.²The study of Asensio J. M. et al., entitled "Hydrodeoxygenation using magnetic ²induction: high-²temperature heterogeneous catalysis in solution" (Angew. Chem. Int. Ed., 2019, ²58, 1-6) ²describes the use of magnetic nanoparticles as heating agents to improve the ²energy ²efficiency of reactions performed at high temperature, as the heat can be then ²directly and²homogeneously transferred to the medium without the need for heating the ²reactor walls. This²was applied in the hydrodeoxygenation of ketones. However, in such a system, ²relatively low ²temperatures up to 280 C were reached and the reaction is exothermic.²In the study of Wsmann S.T. et al., entitled "Electrified methane reforming: A ²compact ²approach to greener industrial hydrogen production" (Science, 2019, 364, 756-²759), a²conventional fired reactor was replaced by an electric-resistance-heated ²reactor. A laboratory-²scale reactor based on FeCrAl alloy tube having a diameter of 6 mm and coated ²with a 130-²pm-nickel-impregnated washcoat was used to carry out steam methane reforming. ²As the heat ²source and the wall of the tube are one, it is possible to minimize the loss ²of heat and then to ²render more efficient and more economical the process of steam methane ²reforming.² Temperatures with a maximum of 800 C were reached with this kind of reactor.²In the study of Malerod-Fjeld H. et al., entitled "Thermo-electrochemical ²production of ²compressed hydrogen from methane with near-zero energy loss" (Nat. Energy, ²2017, 2, 923-²CA 03184993 2023- 1-4²<DP=2>²WO 2022 / 023346 2 ²PCT / EP2021 / 071011²931), a ceramic tube, having an outer diameter of 1 cm and made of a ²perovskite derivative, ²is used as the electrolyte. By applying a voltage and hence a current across ²the electrolyte, ²hydrogen can be selectively extracted from methane and steam. The perovskite ²derivative is ²supplemented with nickel nanoparticles to provide the catalyst necessary for ²the reaction.²In the study of Varsano F. et al., entitled "Diy reforming of methane powered ²by magnetic²induction" (mt. J. of Hydrogen Energy, 2019, 44, 21037-21044), electromagnetic ²induction ²heating of catalytic heterogeneous processes was used and has been ²demonstrated as ²bringing several advantages in terms of process intensification, energy ²efficiency, reactor ²setup simplification and safety issues coming from the use of radiofrequency. ²Temperatures²ranging between 850 C and 900 C in reactors having 1 cm of inner diameter can ²be reached²using Ni6oCo60 pellets as heat mediators in a continuous-flow fixed-bed ²reactor.²US 2,982,622 describes a method for producing hydrogen and high quality coke ²which ²comprises passing inert solid particles as a relatively dense mass downwardly ²through an ²elongated reaction zone, applying an electrical voltage of 0.1 to 1000 volts ²per inch across at²least a portion of said solids mass in said reaction zone, said voltage being ²sufficient to raise²the temperature of said solids to 1800 to 3000 F due to their resistance to ²the flow of electricity ²without causing substantial electrical spark discharges through said solids ²mass, downwardly ²withdrawing thus heated solids from said reaction zone, preheating a ²hydrocarbon feed by ²heat exchange with said withdrawn solids and introducing said preheated feed ²into and²upwardly through said reaction zone in the form of an upwardly moving gasiform ²stream, said²feed contacting said heated solids and being converted to light vapors ²including a substantial ²portion of hydrogen and carbon which deposits on said solids, heat exchanging ²hot vapors ²withdrawn from said reaction zone with inert solids in a heating zone, ²circulating at least a ²portion of the solids withdrawn from the reaction zone and previously heat ²exchanged with²said feed to said heating zone, passing solids from said heating zone to said ²reaction zone as²solids feed thereto, and recovering at least a portion of the solids withdrawn ²from the reaction ²zone as product and recovering hydrogen gas and light vapors from the upper ²portion of said ²reaction zone.²US3259565 describes a process for converting hydrocarbons to produce lower ²boiling²hydrocarbons and solid coke particles of a size larger than fluidizable size ²which comprises²passing coke agglomerates down through a hot fluidized bed of coke particles, ²introducing ²hydrocarbon oil feed into said fluidized bed to crack the hydrocarbon oil, ²passing cracked ²vaporous products overhead, removing coke agglomerates from said fluid bed and ²passing ²them down through a heat exchanger zone in counter-current contact with said ²withdrawn²cracked vaporous products to cool said cracked vaporous products and to heat ²said coke²CA 03184993 2023- 1-4²<DP=3>²WO 2022 / 023346 3 ²PCT / EP2021 / 071011²agglomerates while condensing and depositing higher boiling hydrocarbons from ²said cracked ²vaporous products on said coke agglomerates, withdrawing resulting cracked ²vaporous ²products as product, recirculating the so treated coke agglomerates a number ²of times through ²said heat exchange zone to deposit hydrocarbons and through said hot fluidized ²coke bed to²coke the deposited high boiling hydrocarbons and to increase the size of the ²coke²agglomerates, withdrawing coke agglomerates of increased size as product from ²the system.²GB1262166 describes a process for the production of ethylene by cracking heavy ²²hydrocarbons in a fluidized bed with indirect heating, in which the bed is ²heated via heat ²transfer from a heated gas.²US3948645 describes a method for carrying out heat-requiring processes in a ²reactor²containing a fluidized bed in which the bed comprises mainly coke and in which ²at least a part ²of the energy is electro inductively generated.²These examples show that progress exists in the field of transforming fossils ²sources into ²valuable chemicals with the perspective to diminish the impact on the climate. ²However, this²progress has not been developed to a large scale as it is rather limited to ²the laboratory²envi ronment_²With regards to this matter, the Shawinigan process, described in CA 573348, ²relates to a ²process to prepare hydrocyanic acid from ammonia using in a fluidized bed ²reactor made of ²high temperature-resistant silica glass and comprising conductive carbon ²particles, such as²coke and / or petroleum coke. The principle resides in that the electricity is ²used to heat the²conductive carbon particles which can maintain the fluidized bed at a ²temperature sufficient to ²transform ammonia into hydrocyanic acid, which is then recovered from the ²outgoing gas ²coming off the fluidized bed. The inner diameter of the reactor tube was 3.4 ²cm. A temperature ²ranging between 1300 C and 1600 C, sufficient to perform the requested ²reaction, can be² reached by using such conductive carbon particles.²The disclosure of US 2017 / 0158516 described a fluidized-bed reactor made of ²silicon carbide ²for preparing granular polycrystalline silicon at the industrial level. The ²fluidized-bed reactor is ²heated using a heating device which is placed in an intermediate jacket ²between the outer ²wall of the reactor tube and the inner wall of the reactor vessel. Such ²intermediate jacket²comprises an insulation material and is filled or flushed with an inert gas. ²It was found that the²use of sintered silicon carbide (SSiC) having a SiC content of 98% by weight ²as the main ²element of the reactor tube with a high purity SiC coating deposited by ²chemical vapour ²deposition allowed reaching high temperature up to 1200 C without the tube ²being corroded.²CA 03184993 2023- 1-4²<DP=4>²WO 2022 / 023346 4 ²PCT / EP2021 / 071011²It was also found that using siliconized silicon carbide (SiSiC) as the main ²element of the ²reactor tube without any surface treatment, such as the deposition of a ²coating layer, led to ²the tube being corroded.²On the other hand, the disclosure of Goldberger W. M. et al., entitled "The ²electrothermal²fluidized bed' (Chem. Eng. Progress, 1965, 61 (2), 63-67, relates to fluidized-²bed reactor²made in graphite and susceptible to perform reactions such as the ²hydrocracking of ²hydrocarbons, the pyrolysis of organics, the production of elemental ²phosphorus or the ²chlorination of zirconium oxide. Operation at temperatures up to about 4400 C ²appears ²possible. However, it is not certain that from the long-term perspective, the ²graphite material²used to design the fluidized-bed reactor can resist such harsh reaction ²conditions. Indeed, in²the study of Uda T. et a / ., entitled "Experiments on high temperature graphite ²and steam ²reactions under loss of coolant accident conditions", (Fusion Engineering and ²Design, 1995, ²29, 238-246), it has been shown that graphite corrodes under conditions ²involving steam and ²elevated temperature, for instance between 1000 C and 1600 C. Also, as shown ²in the study²of Qiao M-X. et a / ., entitled "Corrosion of graphite electrode in ²electrochemical advanced²oxidation processes: degradation protocol and environmental application", ²(Chem. Eng. J., ²2018, 344, 410-418), the graphite is susceptible to carbon oxidation reaction, ²which impacts ²its activity as an electrode by restricting notably the voltage that can be ²applied to it.²The present disclosure aims to provide a large-scale solution to one or more ²of the problems²encountered in the prior art that is suitable for application in the industry, ²such as the chemical²industry. The present disclosure aims to contribute to the replacement of the ²use of fossil ²carbon-based fuels heating devices in fluidized bed reactors. The present ²disclosure provides ²a solution to conduct endothermic steam cracking of hydrocarbons into ²hydrogen, ethylene, ²propylene, butadiene and single ring aromatics.² Summary of the disclosure²According to a first aspect, the disclosure provides for a process to perform ²steam cracking ²reaction of hydrocarbons having at least two carbons, said process comprising ²the steps of:²a) providing at least one fluidized bed reactor comprising at least two ²electrodes and a²bed comprising particles;²b) putting the particles of the bed in a fluidized state by passing upwardly ²through the said ²bed a fluid stream, to obtain a fluidized bed; and²c) heating the fluidized bed to a temperature ranging from 500 C to 1200 C to ²conduct ²the steam cracking reaction on a hydrocarbon feedstock;²CA 03184993 2023-1-4²<DP=5>²WO 2022 / 023346 5 ²PCT / EP2021 / 071011²the process is remarkable in that at least 10 wt. (:) / 0 of the particles based ²on the total weight of ²the particles of the bed are electrically conductive particles and have a ²resistivity ranging from ²0.001 Ohm.cm to 500 Ohm.cm at 800 C; in that the step c) of heating the ²fluidized bed is ²performed by passing an electric current through the fluidized bed; and in ²that the electrically²conductive particles of the bed are or comprise one or more selected from ²graphite, carbon²black, one or more metallic alloys, one or more non-metallic resistors, one or ²more metallic ²carbides, one or more transition metal nitrides, one or more metallic ²phosphides, one or more ²superionic conductors, one or more phosphate electrolytes, one or more mixed ²oxides being ²doped with one or more lower-valent cations, one or more mixed sulphides being ²doped with² one or more lower-valent cations, and any mixture thereof.²Surprisingly, it has been found that the use of electrically conductive ²particles, such as silicon ²carbide, mixed oxides and / or mixed sulphides, said mixed oxides and / or said ²mixed sulphides ²being an ionic or mixed conductor, namely being doped with one or more lower-²valent cations, ²in one or more fluidized bed reactors which are electrified, allows ²maintaining a temperature²sufficient to carry out a steam cracking reaction of hydrocarbons requesting ²high-temperature²conditions such as temperature reaction ranging from 500 C to 1200 C without ²the need of ²any external heating device. The use of at least 10 wt.% of electrically ²conductive particles ²within the particles of the bed allows minimizing the loss of heat when a ²voltage is applied. ²Thanks to the Joule effect, most, if not all, the electrical energy is ²transformed into heat that is²used for the heating of the reactor medium.²The fluid stream may be a gaseous stream and / or a vaporized stream.²Advantageously, said process further comprises a step d) of recovering the ²cracking products ²of the reaction. Step d) is performed after step c).²In a preferred embodiment, the volumetric heat generation rate is greater than ²0.1 MW / m3 of²fluidized bed, more preferably greater than 1 MW / m3, in particular, greater ²than 3 MW / m3.²In a preferred embodiment, the at least one fluidized bed reactor is devoid of ²heating means. ²For example, the at least one fluidized bed reactor comprises a vessel and is ²devoid of heating ²means located around or inside the vessel. For example, at least one fluidized ²bed reactor is ²devoid of heating means selected from ovens, gas burners, hot plates, or any ²combination²thereof. For example, all the fluidized bed reactors are devoid of heating ²means selected from²ovens, gas burners, hot plates, or any combination thereof²For example, the content of electrically conductive particles is ranging from ²10 wt.% to ²100 wt.% based on the total weight of the particles of the bed; preferably, ²from 15 wt.% to 95²CA 03184993 2023- 1-4²<DP=6>²WO 2022 / 023346 6 ²PCT / EP2021 / 071011²wt.%, more preferably from 20 wt.% to 90 wt.%, even more preferably from 25 ²wt.% to 80 wt.% ²and most preferably from 30 wt.% to 75 wt.%.²For example, the content of electrically conductive particles based on the ²total weight of the ²bed is at least 12 wt.% based on the total weight of the particles of the bed; ²preferably, at least²15 wt.%, more preferably, at least 20 wt.%; even more preferably at least 25 ²wt.%, and most²preferably at least 30 wt.% or at least 40 wt.% or at least 50 wt.% or at ²least 60 wt.%.²For example, the electrically conductive particles have a resistivity ranging ²from 0.005 to 400 ²Ohm.cm at 800 C, preferably ranging from 0.01 to 300 Ohm.cm at 800 C; more ²preferably ²ranging from 0.05 to 150 Ohm.cm at 800 C and most preferably ranging from 0.1 ²to 100² Ohm.cm at 800 C²For example, the electrically conductive particles have a resistivity of at ²least 0.005 Ohm.cm ²at 800 C; preferably of at least 0.01 Ohm.cm at 800 C, more preferably of at ²least 0.05 ²Ohm.cm at 800 C; even more preferably of at least 0.1 Ohm.cm at 800 C, and ²most preferably ²of at least 0.5 Ohm.cm at 800 C.²For example, the electrically conductive particles have a resistivity of at ²most 400 Ohm.cm at²800 C; preferably of at most 300 Ohm.cm at 800 C, more preferably of at most ²200 Ohm.cm ²at 800 C; even more preferably of at most 150 Ohm.cm at 800 C, and most ²preferably of at ²most 100 Ohm.cm at 800 C.The selection of the content of electrically ²conductive particles ²based on the total weight of the particles of the bed and of the electrically ²conductive particles²of a given resistivity influence the temperature reached by the fluidized bed. ²Thus, in case the²targeted temperature is not attained, the person skilled in the art may ²increase the density of ²the bed of particles, the content of electrically conductive particles based ²on the total weight ²of the particles of the bed and / or select electrically conductive particles ²with a lower resistivity ²to increase the temperature reach by the fluidized bed.²For example, the density of the bed of particles is expressed as the void ²fraction. Void fraction²or bed porosity is the volume of voids between the particles divided by the ²total volume of the ²bed. At the incipient fluidisation velocity, the void fraction is typically ²between 0.4 and 0.5. The ²void fraction can increase up to 0.98 in fast fluidised beds with lower values ²at the bottom of ²about 0.5 and higher than 0.9 at the top of the bed. The void fraction can be ²controlled by the²linear velocity of the fluidising gas and can be decreased by recycling solid ²particles that are²recovered at the top and send back to the bottom of the fluidized bed, which ²compensates for ²the entrainment of solid particles out of the bed.²The void fraction VF is defined as the volume fraction of voids in a bed of ²particles and is ²determined according to the following equation:²CA 03184993 2023- 1-4²<DP=7>²WO 2022 / 023346 7 ²PCT / EP2021 / 071011²Vt¨Vp²VF = _______________________________________________ (1)²Vt²wherein Vt is the total volume of the bed and is determined by²Vt = AH (2)²wherein A is the cross-sectional area of the fluidized bed and H is the height ²of the fluidized² bed; and²wherein Vp is the total volume of particles within the fluidized bed.²For example, the void fraction of the bed is ranging from 0.5 to 0.8; ²preferably ranging from ²0.5 to 0.7, more preferably from 0.5 to 0.6. To increase the density of the ²bed of particles, the ²void fraction is to be reduced.²For example, the particles of the bed have an average particle size ranging ²from 5 to 300 pm²as determined by sieving according to ASTM D4513-11, preferably ranging from ²10 to 200 pm ²and more preferably ranging from 20 to 200 pm or from 30 to 150 pm.²Determination by sieving according to ASTM D4513-11 is preferred. In case the ²particles have ²an average size of below 20 pm the determination of the average size can also ²be done by² Laser Light Scattering according to ASTM D4464-15.²For example, the electrically conductive particles of the bed have an average ²particle size ²ranging from 5 to 300 pm as determined by sieving according to ASTM D4513-11, ²preferably ²ranging from 10 to 200 pm and more preferably ranging from 30 to 150 pm.²In an embodiment, from 50 wt.% to 100 wt.% of the electrically conductive ²particles of the bed²based on the total weight of the electrically conductive particles of the bed ²are one or more²selected from graphite, carbon black, one or more metallic alloys, one or more ²non-metallic ²resistors, one or more metallic carbides, one or more transition metal ²nitrides, one or more ²metallic phosphides, one or more superionic conductors, one or more phosphate ²electrolytes, ²one or more mixed oxides being doped with one or more lower-valent cations, ²one or more²mixed sulphides being doped with one or more lower-valent cations, and any ²mixture thereof;²preferably, from 60 wt.% to 100 wt.%; more preferably from 70 wt.% to 100 ²wt.%; even more ²preferably from 80 wt.% to 100 wt.% and most preferably from 90 wt.% to 100 ²wt.%.²With preference, the electrically conductive particles of the bed are or ²comprise one or more ²selected from graphite, carbon black, one or more metallic alloys, one or more ²non-metallic²resistors, one or more metallic carbides, one or more transition metal ²nitrides, one or more²metallic phosphides, one or more superionic conductors, one or more phosphate ²electrolytes, ²one or more mixed oxides being doped with one or more lower-valent cations, ²one or more²CA 03184993 2023- 1-4²<DP=8>²WO 2022 / 023346 8 ²PCT / EP2021 / 071011²mixed sulphides being doped with one or more lower-valent cations, and any ²mixture thereof; ²with preference in a content of from 50 wt.% to 100 wt.% based on the total ²weight of the ²electrically conductive particles of the bed; preferably, from 60 wt.% to 100 ²wt.%; more ²preferably from 70 wt.% to 100 wt.%; even more preferably from 80 wt.% to 100 ²wt.% and² most preferably from 90 wt.% to 100 wt.%.²With preference, the electrically conductive particles of the bed are or ²comprise one or more ²selected from graphite, carbon black, one or more non-metallic resistors, one ²or more metallic ²carbides, one or more transition metal nitrides, one or more metallic ²phosphides, one or more ²superionic conductors, one or more phosphate electrolytes, one or more mixed ²oxides being²doped with one or more lower-valent cations, one or more mixed sulphides being ²doped with²one or more lower-valent cations, and any mixture thereof; with preference in ²a content of from ²50 wt.% to 100 wt.% based on the total weight of the electrically conductive ²particles of the ²bed; preferably, from 60 wt.% to 100 wt.%; more preferably from 70 wt.% to 100 ²wt.%; even ²more preferably from 80 wt.% to 100 wt.% and most preferably from 90 wt.% to ²100 wt.%.²With preference, the electrically conductive particles of the bed are or ²comprise one or more²selected from one or more non-metallic resistors, one or more metallic ²carbides, one or more ²transition metal nitrides, one or more metallic phosphides, one or more ²superionic conductors, ²one or more phosphate electrolytes, one or more mixed oxides being doped with ²one or more ²lower-valent cations, one or more mixed sulphides being doped with one or more ²lower-valent²cations, and any mixture thereof; with preference in a content of from 50 wt.% ²to 100 wt.%²based on the total weight of the electrically conductive particles of the bed; ²preferably, from ²60 wt.% to 100 wt.%; more preferably from 70 wt.% to 100 wt.%; even more ²preferably from ²80 wt.% to 100 wt.% and most preferably from 90 wt.% to 100 wt.%.²For example, the electrically conductive particles of the bed are devoid of ²one or more carbon-²containing particles selected from petroleum coke, carbon black, coke or a ²mixture thereof.²In an embodiment, the electrically conductive particles of the bed are devoid ²of one or more ²carbon-containing particles selected from graphite, petroleum coke, carbon ²black, coke or a ²mixture thereof. For example, the electrically conductive particles of the bed ²are devoid of ²graphite and / or carbon black. For example, the electrically conductive ²particles of the bed are²devoid of petroleum coke and / or coke.²Alternatively, the electrically conductive particles of the bed are or ²comprise graphite and one ²or more selected from one or more metallic alloys, one or more non-metallic ²resistors, one or ²more metallic carbides, one or more transition metal nitrides, one or more ²metallic phosphides, ²one or more superionic conductors, one or more phosphate electrolytes, one or ²more mixed²oxides being doped with one or more lower-valent cations, one or more mixed ²sulphides being²CA 03184993 2023- 1-4²<DP=9>²WO 2022 / 023346 9 ²PCT / EP2021 / 071011²doped with one or more lower-valent cations, and any mixture thereof; with ²preference in a ²content of from 50 wt.% to 100 wt.% based on the total weight of the ²electrically conductive ²particles of the bed; preferably, from 60 wt.% to 100 wt.%; more preferably ²from 70 wt.% to ²100 wt.%; even more preferably from 80 wt.% to 100 wt.% and most preferably ²from 90 wt.%² to 100 wt.%.²As an alternative, the electrically conductive particles of the bed are one or ²more particles ²selected from one or more metallic alloys, one or more non-metallic resistors ²provided that the ²non-metallic resistor is not silicon carbide, one or more metallic carbides, ²one or more ²transition metal nitrides, one or more metallic phosphides, graphite, carbon ²black, one or more²superionic conductors, one or more phosphate electrolytes, one or more mixed ²oxides being²doped with one or more lower-valent cations and / or one or more and / or mixed ²sulphides being ²doped with one or more lower-valent cations and any mixture thereof; with ²preference in a ²content of from 50 wt.% to 100 wt.% based on the total weight of the ²electrically conductive ²particles of the bed; preferably, from 60 wt.% to 100 wt.%; more preferably ²from 70 wt.% to²100 wt.%; even more preferably from 80 wt.% to 100 wt.% and most preferably ²from 90 wt.%²to 100 wt.%.²For example, the electrically conductive particles of the bed are or comprise ²one or more ²selected from one or more metallic alloys, one or more non-metallic resistors, ²graphite, carbon ²black, one or more mixed oxides being doped with one or more lower-valent ²cations, one or²more mixed sulphides being doped with one or more lower-valent cations, and ²any mixture²thereof with preference in a content of from 50 wt.% to 100 wt.% based on the ²total weight of ²the electrically conductive particles of the bed; preferably, from 60 wt.% to ²100 wt.%; more ²preferably from 70 wt.% to 100 wt.%; even more preferably from 80 wt.% to 100 ²wt.% and ²most preferably from 90 wt.% to 100 wt.%.²For example, the electrically conductive particles of the bed are or comprise ²graphite and one²or more selected from one or more metallic alloys, one or more non-metallic ²resistors, one or ²more mixed oxides being doped with one or more lower-valent cations, one or ²more mixed ²sulphides being doped with one or more lower-valent cations, and any mixture ²thereof; with ²preference in a content of from 50 wt.% to 100 wt.% based on the total weight ²of the electrically²conductive particles of the bed; preferably, from 60 wt.% to 100 wt.%; more ²preferably from²70 wt.% to 100 wt.%; even more preferably from 80 wt.% to 100 wt.% and most ²preferably ²from 90 wt.% to 100 wt.%.²For example, the electrically conductive particles of the bed are or comprise ²one or more ²selected from one or more metallic alloys, one or more non-metallic resistors, ²one or more²mixed oxides being doped with one or more lower-valent cations, one or more ²mixed sulphides²CA 03184993 2023- 1-4²<DP=10>²WO 2022 / 023346 10 ²PCT / EP2021 / 071011²being doped with one or more lower-valent cations, and any mixture thereof; ²with preference ²in a content of from 50 wt.% to 100 wt.% based on the total weight of the ²electrically conductive ²particles of the bed; preferably, from 60 wt.% to 100 wt.%; more preferably ²from 70 wt.% to ²100 wt.%; even more preferably from 80 wt.% to 100 wt.% and most preferably ²from 90 wt.%² tO 1 00 Wt.%.²For example, the electrically conductive particles of the bed are or comprise ²one or more ²selected from one or more non-metallic resistors, one or more mixed oxides ²being doped with ²one or more lower-valent cations, one or more mixed sulphides being doped with ²one or more ²lower-valent cations, and any mixture thereof; with preference in a content of ²from 50 wt.% to²100 wt.% based on the total weight of the electrically conductive particles of ²the bed;²preferably, from 60 wt.% to 100 wt.%; more preferably from 70 wt.% to 100 ²wt.%; even more ²preferably from 80 wt.% to 100 wt.% and most preferably from 90 wt.% to 100 ²wt.%.²For example, said one or more metallic alloys are selected from Ni-Cr, Fe-Ni-²Cr, Fe-Ni-Al or ²a mixture thereof. With preference, when said metallic alloy comprises at ²least chromium, the²chromium content is at least 15 mol.% of the total molar content of said ²metallic alloy²comprising at least chromium, more preferably at least 20 mol.%, even more ²preferably at ²least 25 mol.%, most preferably at least 30 mol.%. Advantageously yet, the ²iron content in the ²metallic alloys is at most 2.0% based on the total molar content of the said ²metallic alloy, ²preferably at most 1.5 mol.%, more preferably at most 1.0 mol.%, even more ²preferably at²most 0.5 mol.%.²For example, a non-metallic resistor is silicon carbide (SiC), molybdenum ²disilicide (MoSi2), ²nickel silicide (NiSi), sodium silicide (Na2Si), magnesium silicide (Mg2Si), ²platinum silicide ²(PtSi), titanium silicide (TiSi2), tungsten silicide (WSi2) or a mixture ²thereof, preferably silicon ²carbide.²For example, said one or more metallic carbides are selected from iron carbide ²(Fe3C),²molybdenum carbide (such as a mixture of MoC and Mo2C).²For example, said one or more transition metal nitrides are selected from ²zirconium nitride ²(ZrN), tungsten nitride (such as a mixture of W2N, WN, and VVN2), vanadium ²nitride (VN), ²tantalum nitride (TaN), and / or niobium nitride (NbN).²For example, said one or more metallic phosphides are selected from copper ²phosphide²(Cu3P), indium phosphide (InP), gallium phosphide (GaP), sodium phosphide ²Na3P), ²aluminium phosphide (AIP), zinc phosphide (Zn3P2) and / or calcium phosphide ²(Ca3P2).²For example, said one or more superionic conductors are selected from ²LiAlSiO4, ²LiloGeP2S12, 1_,3.6Si0.6P0.404, sodium superionic conductors (NaSICON), such ²as²CA 03184993 2023- 1-4²<DP=11>²WO 2022 / 023346 1J_ ²PCT / EP2021 / 071011²Na3Zr2PSi2012, or sodium beta alumina, such as NaA111017, Na1.6A111017.3, ²and / or ²Na1.76Li0.38A110.62017.²For example, said one or more phosphate electrolytes are selected from LiPO4 ²or LaPO4.²For example, said one or more mixed oxides are ionic or mixed conductors being ²doped with²one or more lower-valent cations. Advantageously, said mixed oxides are doped ²with one or²more lower-valent cations, and are selected from oxides having a cubic ²fluorite structure, ²perovskite, pyrochlore.²For example, said one or more mixed sulphides are ionic or mixed conductors ²being doped ²with one or more lower-valent cations.²For example, the electrically conductive particles of the bed are or comprise ²a non-metallic²resistor being silicon carbide.²For example, the electrically conductive particles of the bed are or comprise ²a mixture of a ²non-metallic resistor being silicon carbide and electrically conductive ²particles different from ²silicon carbide. The presence of electrically conductive particles different ²from silicon carbide²in the bed is optional. It can be present as a starting material for heating ²the bed since it was²found that the resistivity of silicon carbide at room temperature is too high ²to start heating the ²bed. Alternatively to the presence of electrically conductive particles ²different from silicon ²carbide, it is possible to provide heat to the reactor for a defined time to ²start the reaction.²For example, the silicon carbide is selected from sintered silicon carbide, ²nitride-bounded²silicon carbide, recrystallised silicon carbide, reaction bonded silicon ²carbide and any mixture²thereof. The type of silicon carbide material is selected according to the ²required heating ²power necessary for supplying the reaction heat of the steam cracking.²For example, the electrically conductive particles of the bed are or comprise ²a mixture of a ²non-metallic resistor being silicon carbide and electrically conductive ²particles different from²silicon carbide and the electrically conductive particles of the bed comprises ²from 10 wt.% to²99 wt.% of silicon carbide based on the total weight of the electrically ²conductive of the bed; ²preferably, from 15 wt.% to 95 wt.%, more preferably from 20 wt.% to 90 wt.%, ²even more ²preferably from 25 wt.% to 80 wt.% and most preferably from 30 wt.% to 75 ²wt.%.²For example, the electrically conductive particles of the bed are or comprise ²a mixture of a²non-metallic resistor being silicon carbide and electrically conductive ²particles different from²silicon carbide and the said electrically conductive particles different from ²silicon carbide are ²graphite and / or one or more mixed oxides being doped with one or more lower-²valent cations ²and / or one or more mixed sulphides being doped with one or more lower-valent ²cations.²CA 03184993 2023-1-4²<DP=12>²WO 2022 / 023346 12 ²PCT / EP2021 / 071011²For example, the electrically conductive particles of the bed are or comprise ²one or more ²mixed oxides being ionic conductor, namely being doped with one or more lower-²valent ²cations; with preference, the mixed oxides are selected from:²- one or more oxides having a cubic fluorite structure being at least ²partially substituted²with one or more lower-valent cations, preferentially selected from Sm, Gd, Y, ²Sc, Yb,²Mg, Ca, La, Dy, Er, Eu; and / or²- one or more AB03-perovskites with A and B tri-valent cations, being at ²least partially ²substituted in A position with one or more lower-valent cations, ²preferentially selected ²from Ca, Sr, or Mg, and comprising at least one of Ni, Ga, Co, Cr, Mn, Sc, Fe ²and / or a² mixture thereof in B position; and / or²- one or more AB03-perovskites with A bivalent cation and B tetra-valent ²cation, being ²at least partially substituted with one or more lower-valent cations, ²preferentially ²selected from magnesium (Mg), scandium (Sc), yttrium (Y), neodymium (Nd) or ²ytterbium (Yb) in the B position or with a mixture of different B elements in ²the B²position; and / or.²- one or more A2B207-pyrochlores with A trivalent cation and B tetra-valent ²cation being ²at least partially substituted in A position with one or more lower-valent ²cations, ²preferentially selected from Ca or Mg, and comprising at least one of Sn, Zr ²and Ti in ²B position.² Examples of one or more mixed sulphides are²- one or more sulphides having a cubic fluorite structure being at least ²partially ²substituted with one or more lower-valent cations, preferentially selected ²from Sm, Gd, ²Y, Sc, Yb, Mg, Ca, La, Dy, Er, Eu; and / or²- one or more ABS3 structures with A and B tri-valent cations being at ²least partially²substituted in A position with one or more lower-valent cations, preferably ²selected²from Ca, Sr, or Mg and comprising at least one of Ni, Ga, Co, Cr, Mn, Sc, Fe ²and / or a ²mixture thereof in B position; and / or²- one or more ABS3 structures with A bi-valent cation and B tetra-valent ²cation, being ²at least partially substituted with one or more lower-valent cations, ²preferably²selected from Mg, Sc, Y, Nd or Yb in the B position or with a mixture of ²different B²elements in the B position; and / or²- one or more A2B2S7 structures with A tri-valent cation and B tetra-valent ²cation, ²being at least partially substituted in A position with one or more lower-²valent cations, ²preferably selected from Ca or Mg, and comprising at least one of Sn, Zr and ²Ti in B² position.²CA 03184993 2023- 1-4²<DP=13>²WO 2022 / 023346 13 ²PCT / EP2021 / 071011²With preference, the degree of substitution in the one or more mixed oxides ²doped with one ²or more lower-valent cations and having a cubic fluorite structure is between ²1 and 15 atom% ²based on the total number of atoms present in the one or more oxides having a ²cubic fluorite ²structure, preferably between 3 and 12 atom%, more preferably between 5 and 10 ²atom%.²With preference, the degree of substitution in the one or more mixed oxides ²doped with one²or more lower-valent cations is between 1 and 50 atom% based on the total ²number of atoms ²present in the one or more AB03-perovskites with A and B tri-valent cations, ²in the one or ²more AB03-perovskites with A bivalent cation and B tetra-valent cation or in ²the one or more ²A2B207-pyrochlores with A trivalent cation and B tetra-valent cation ²respectively, preferably² between 3 and 20 atom%, more preferably between 5 and 15 atom%.²With preference, the degree of substitution in the one or more mixed sulphides ²doped with one ²or more lower-valent cations and having a cubic fluorite structure is between ²1 and 15 atom% ²based on the total number of atoms present in the one or more oxides having a ²cubic fluorite ²structure, preferably between 3 and 12 atom%, more preferably between 5 and 10 ²atom%.²With preference, the degree of substitution in the one or more mixed sulphides ²doped with²one or more lower-valent cations is between 1 and 50 atom% based on the total ²number of ²atoms present in the one or more ABS3 structures with A and B tri-valent ²cations, in the one ²or more ABS3 structures with A bivalent cation and B tetra-valent cation or in ²the one or more ²A2B2S7 structures with A trivalent cation and B tetra-valent cation ²respectively, preferably²between 3 and 20 atom%, more preferably between 5 and 15 atom%.²For example, the electrically conductive particles of the bed are or comprise ²one or more ²metallic alloys; with preference, one or more metallic alloys are selected ²from Ni-Cr, Fe-Ni-Cr, ²Fe-Ni-Al or a mixture thereof.²With preference, when said metallic alloy comprises at least chromium, the ²chromium content²is at least 15 mol.% of the total molar content of said metallic alloy ²comprising at least²chromium, more preferably at least 20 mol.%, even more preferably at least 25 ²mol.%, most ²preferably at least 30 mol.%. Advantageously yet, the iron content in the ²metallic alloys is at ²most 2.0% based on the total molar content of said metallic alloy, preferably ²at most 1.5 mol.%, ²more preferably at most 1.0 mol.%, even more preferably at most 0.5 mol.%.²For example, the electrically conductive particles of the bed are or comprise ²a mixture of a²non-metallic resistor being silicon carbide and particles different from ²silicon carbide wherein ²the particles different from silicon carbide are or comprise graphite; with ²preference, said ²graphite is graphite particles having an average particle size ranging from 5 ²to 300 pm as²CA 03184993 2023- 1-4²<DP=14>²WO 2022 / 023346 14 ²PCT / EP2021 / 071011²determined by sieving according to ASTM D4513-11, more preferably ranging from ²10 to 200 ²pm and most preferably ranging from 30 to 150 pm.²For example, the said steam cracking reaction is conducted at a temperature ²ranging from²55000 to 1200 C, preferably from 600 C to 1100 C, more preferably from 650 C ²to 1050 C²and most preferably from 700 C to 1000 C.²For example, the said steam cracking reaction is performed at a pressure ²ranging between ²0.01 MPa and 1_0 MPa, preferably between 0.1 MPa and 0_5 MPa.²In an embodiment, said process comprises a step of pre-heating with a gaseous ²stream said²fluidized bed reactor before conducting said steam cracking reaction in the ²fluidized bed²reactor; with preference, said gaseous stream is a stream of inert gas and / or ²has a ²temperature comprised between 500 C and 1200 C. The said embodiment is of ²interest when ²the particles of the bed such as graphite and / or the electro-resistive ²material have too high ²resistivity at room temperature to start the electro-heating of the bed.²For example, the said steam cracking of a hydrocarbon stream is conducted in ²presence of a²dilution stream and is performed at a weight hourly space velocity of said ²reaction stream ²comprised between 0.1 h-1 and 100 h-1, preferably comprised between 1.0 h-1 ²and 50 h-1, more ²preferably comprised between 1.5 h-1 and 10 h-1, even more preferably ²comprised between ²2.0 h-1 and 6.0 h-1. The weight hourly space velocity is defined as the ratio ²of mass flow of the²reaction stream to the mass of solid particulate material in the fluidized ²bed.²The hydrocarbon feedstock for the present process is selected from ethane, ²liquefied ²petroleum gas, naphtha, gasoils and / or whole crude oil.²For example, the fluid stream provided in step b) comprises a hydrocarbon ²feedstock.²Liquefied petroleum gas (LPG) comprises mainly propane and butanes. Petroleum ²naphtha²or naphtha is defined as the hydrocarbons fraction of petroleum having a ²boiling point from²15 C up to 200 C. It is a complex mixture of linear and branched paraffins ²(single and multi-²branched), cyclic paraffins and aromatics having carbons numbers ranging from ²5 to about 11 ²carbons atoms. Light naphtha has a boiling range from 15 to 90 C and comprises ²C5 to 06 ²hydrocarbons, while heavy naphtha has a boiling range from 90 to 200 C and ²comprises C7²to about C11 hydrocarbons. Gasoils have a boiling range from about 200 to 350 ²C, and²comprise C10 to 022 hydrocarbons, including essentially linear and branched ²paraffins, cyclic ²paraffins and aromatics (including mono-, naphtho- and poly-aromatic). Heavier ²gasoils (like ²atmospheric gasoil, vacuum gasoil, atmospheric residua and vacuum residua), ²having boiling²CA 03184993 2023-1-4²<DP=15>²WO 2022 / 023346 15 ²PCT / EP2021 / 071011²ranges above 300 C and C20+ hydrocarbons including essentially linear and ²branched ²paraffins, cyclic paraffins and aromatics (including mono-, naphtho- and poly-²aromatic) are ²available from atmospheric or vacuum distillations units.²In particular, the cracking products obtained in the present process may ²include one or more²of ethylene, propylene and benzene, and optionally hydrogen, toluene, xylenes, ²and 1,3-²butadiene.²In a preferred embodiment, the outlet temperature of the reactor may range ²from 800 to ²1200 C, preferably from 820 to 1100 C, more preferably from 830 to 950 C, more ²preferably ²from 840 C to 900 C.²In a preferred embodiment, the residence time of the hydrocarbon feedstock in ²the fluidised²bed section of the reactor where the temperature is between 500 and 1200 C, ²may range from ²0.005 to 0.5 seconds, preferably from 0.01 to 0.4 seconds.²In a preferred embodiment, the steam cracking reaction performed on the ²hydrocarbon ²feedstock is done in presence of dilution steam in a ratio of 0.1 to 1.0 kg ²steam per kg of²hydrocarbon feedstock, preferably from 0.25 to 0.7 kg steam per kg of ²hydrocarbon feedstock,²more preferably in a ratio from 0.35 to 0.6 kg steam per kg of hydrocarbon ²feedstock, to obtain ²cracking products as defined above.²In a preferred embodiment, the reactor outlet pressure may range from 0.050 to ²0.250 MPa,²preferably from 0.070 to 0200. MPa, more preferably may be about 0.15 MPa. ²Lower operating²pressure results in more light olefins yield and reduced coke formation. The ²lowest pressure²possible is accomplished by (i) maintaining the output pressure of the reactor ²as close as ²possible to atmospheric pressure at the suction of the cracked gas compressor ²(ii) reducing ²the partial pressure of the hydrocarbons by dilution with steam (which has a ²substantial ²influence on slowing down coke formation).²Effluent from the pyrolysis furnaces contains unreacted feedstock, desired ²olefins (mainly²ethylene and propylene), hydrogen, methane, a mixture of C4's (primarily ²isobutylene and ²butadiene), pyrolysis gasoline (aromatics in the C6 to C8 range), ethane, ²propane, di-olefins ²(acetylene, methyl acetylene, propadiene), and heavier hydrocarbons that boil ²in the ²temperature range of fuel oil (pyrolysis fuel oil). This cracked gas is ²rapidly quenched to 330-²520 C to stop the pyrolysis reactions, minimize consecutive reactions and ²recover the sensible²heat in the gas by generating high-pressure steam in parallel transfer-line ²heat exchangers ²(TLE's). In gaseous feedstock-based plants, the TLE-quenched gas stream flows ²forward to ²a direct water quench tower, where the gas is cooled further with ²recirculating cold water. In²CA 03184993 2023- 1-4²<DP=16>²WO 2022 / 023346 16 ²PCT / EP2021 / 071011²liquid feedstock-based plants, a pre-fractionator precedes the water quench ²tower to ²condense and separate the fuel oil fraction from the cracked gas. In both ²types of plants, the ²major portions of the dilution steam and heavy gasoline in the cracked gas are ²condensed in ²the water quench tower at 35-40 C. The water-quench gas is subsequently ²compressed to²about 2.5 MPa-3.5 MPa in 4 or 5 stages. Between compression stages, the ²condensed water²and light gasoline are removed, and the cracked gas is washed with a caustic ²solution or with ²a regenerative amine solution, followed by a caustic solution, to remove acid ²gases (002, H2S ²and SO2). The compressed cracked gas is dried with a desiccant and cooled with ²propylene ²and ethylene refrigerants to cryogenic temperatures for the subsequent product ²fractionation:²front-end de-methanization, front-end de-propanization or front-end de-²ethanization.²For example, the step of heating the fluidized bed is performed by passing an ²electric current ²at a voltage of at most 300 V through the fluidized bed, preferably at most ²200 V, more ²preferably at most 150 V, even more preferably at most 120 V, most preferably ²at most 100 ²V, even most preferably at most 90 V.²For example, said process comprises a step of pre-heating with a gaseous ²stream said²fluidized bed reactor before conducting said steam cracking reaction in the ²fluidized bed ²reactor; with preference, said gaseous stream is a stream of inert gas and / or ²has a ²temperature comprised between 500 C and 1200 C.²For example, wherein the at least one fluidized bed reactor provided in step ²a) comprises a²heating zone and a reaction zone and wherein the fluid stream provided in step ²b) is provided²to the heating zone and comprises diluent gases, the step c) of heating the ²fluidized bed to a ²temperature ranging from 500 C to 1200 C to conduct the steam cracking ²reaction of a ²hydrocarbon feedstock comprises the following sub-steps:²- heating the fluidized bed to a temperature ranging from 500 C to 1200 C ²by passing²an electric current through the heating zone of the at least one fluidized ²bed,²- transporting the heated particles from the heating zone to the reaction ²zone,²- in the reaction zone, putting the heated particles in a fluidized state ²by passing ²upwardly through the said bed of the reaction zone a fluid stream comprising a ²²hydrocarbon feedstock and optional diluent gases to obtain a fluidized bed and ²to² conduct the steam cracking reaction on the hydrocarbon feedstock,²- optionally, recovering the particles from the reaction zone and recycling ²them to the ²heating zone.²The fluid stream may be a gaseous stream and / or a vaporized stream.²CA 03184993 2023-1-4²<DP=17>²WO 2022 / 023346 17 ²PCT / EP2021 / 071011²Step c) provides that the steam cracking reaction is performed on a ²hydrocarbon feedstock ²which implies that a hydrocarbon feedstock is provided.²For example, wherein the heating zone and the reaction zone are mixed (i.e. ²the same zone); ²the fluid stream provided in step b) comprises a hydrocarbon feedstock.²For example, wherein the heating zone and the reaction zone are separated ²zones, the fluid²stream provided in step b) to the heating zone is devoid of a hydrocarbon ²feedstock. For ²example, wherein the process comprises providing at least one fluidized bed ²reactor being a ²heating zone and at least one fluidized bed reactor being a reaction zone, the ²fluid stream ²provided in step b) to the heating zone is devoid of a hydrocarbon feedstock ²and the fluid²stream provided in step b) to the reaction zone comprises a hydrocarbon ²feedstock.²It is understood that the hydrocarbon feedstock is provided to the reaction ²zone and that when ²the heating zone is separated from the reaction zone, no hydrocarbon feedstock ²is provided ²to the heating zone. It is understood that in addition to the hydrocarbon ²feedstock provided to ²the reaction zone, steam can be provided to the reaction zone to reach the ²recommended² steam to hydrocarbon ratio in the reaction zone as described above.²According to a second aspect, the disclosure provides an installation to ²perform a steam ²cracking reaction, according to the first aspect, said installation comprises ²at least one ²fluidized bed reactor comprising:²- at least two electrodes; with preference, one electrode is a submerged ²central electrode²or two electrodes are submerged electrodes,²- a reactor vessel;²- one or more fluid nozzles for the introduction of a fluidizing gas and / or ²of a hydrocarbon ²feedstock within at least one fluidized bed reactor; and²- a bed comprising particles;²the installation is remarkable in that at least 10 wt.% of the particles of ²the bed based on the²total weight of the particle of the bed are electrically conductive, have a ²resistivity ranging from ²0.001 Ohm.cm to 500 Ohm.cm at a temperature of 800 C and are or comprise one ²or more ²selected from one or more metallic alloys, one or more non-metallic resistors, ²one or more ²metallic carbides, one or more transition metal nitrides, one or more metallic ²phosphides,²graphite, carbon black, one or more superionic conductors, one or more ²phosphate²electrolytes, one or more mixed oxides being doped with one or more lower-²valent cations, ²one or more mixed sulphides being doped with one or more lower-valent cations, ²and any ²mixture thereof.²CA 03184993 2023- 1-4²<DP=18>²WO 2022 / 023346 18 ²PCT / EP2021 / 071011²Advantageously, at least one fluidized bed reactor is devoid of heating means. ²For example, ²at least one fluidized bed reactor is devoid of heating means located around ²or inside the ²reactor vessel. For example, all the fluidized bed reactors are devoid of ²heating means. When ²stating that at least one of the fluidized bed reactors is devoid of "heating ²means", it refers to²"classical' heating means, such as ovens, gas burners, hot plates and the ²like. There are no²other heating means than the at least two electrodes of the fluidized bed ²reactor itself. For ²example, at least one fluidized bed reactor is devoid of heating means ²selected from ovens, ²gas burners, hot plates, or any combination thereof. For example, all the ²fluidized bed reactors ²are devoid of heating means selected from ovens, gas burners, hot plates, or ²any combination² thereof.²In a preferred embodiment, the at least one fluidized bed reactor comprising ²at least two ²electrodes and a bed comprising particles is devoid of packing.²For example, the fluidizing gas is one or more diluent gases.²For example, the at least one reactor vessel has an inner diameter of at least ²100 cm,² preferably at least 200 cm, more preferably at least 300 cm.²With preference, the reactor vessel comprises a reactor wall made of materials ²that are ²corrosion-resistant materials and advantageously said reactor wall materials ²comprise nickel ²(Ni), SiAION ceramics, yttria-stabilized zirconia (YSZ), tetragonal ²polycrystalline zirconia ²(TZP) and / or tetragonal zirconia polycrystal (TPZ).²With preference, one of the electrodes is the reactor vessel or the gas ²distributor and / or said²at least two electrodes are made in stainless steel material or nickel-²chromium alloys or nickel-²chromium-iron alloys.²For example, the at least one fluidized bed reactor comprises a heating zone ²and a reaction ²zone, one or more fluid nozzles to provide a hydrocarbon feedstock to the ²reaction zone, and²optional means to transport the particles of the bed from the reaction zone ²back to the heating²zone.²For example, the installation comprises at least two fluidized bed reactors ²connected one to ²each other wherein at least one reactor of said at least two fluidized bed ²reactors is the heating ²zone and at least another reactor of said at least two fluidized bed reactors ²is the reaction²zone. With preference, the installation comprises one or more fluid nozzles ²arranged to inject²a hydrocarbon feedstock to the at least one fluidized bed reactor being the ²reaction zone, ²means to transport the particles of the bed from the heating zone to the ²reaction zone when ²necessary and optional means to transport the particles from the reaction zone ²back to the²CA 03184993 2023- 1-4²<DP=19>²WO 2022 / 023346 19 ²PCT / EP2021 / 071011²heating zone. This configuration is remarkable in that a given particle bed is ²common to at ²least two fluidized bed reactors.²For example, the at least one fluidized bed reactor is a single fluidized bed ²reactor wherein ²the heating zone is the bottom part of the fluidized bed reactor while the ²reaction zone is the²top part of the fluidised bed reactor. With preference, the installation ²comprises one or more²fluid nozzles to inject a hydrocarbon feedstock between the two zones. The ²diameter of the ²heating zone and reaction zone can be different to accomplish optimum ²conditions for heating ²in the bottom zone and optimum conditions for methane conversion in the top ²zone. Particles ²can move from the heating zone to the reaction zone by entrainment and the ²other way around²from the reaction zone back to the heating zone by gravity. Optionally, ²particles can be²collected from the upper heating zone and transferred by a separate transfer ²line back to the ²bottom heating zone.²For example, the at least one fluidized bed comprises at least two lateral ²zones being an outer ²zone and an inner zone wherein the outer zone is surrounding the inner zone, ²with the outer²zone being the heating zone and the inner zone being the reaction zone. In a ²less preferred²configuration, the outer zone is the reaction zone and the inner zone is the ²heating zone. With ²preference, the installation comprises one or more fluid nozzles to inject a ²hydrocarbon ²feedstock in the reaction zone.²In an embodiment, from 50 wt.% to 100 wt.% of the electrically conductive ²particles of the bed²based on the total weight of the electrically conductive particles of the bed ²are one or more²selected from graphite, carbon black, one or more metallic alloys, one or more ²non-metallic ²resistors, one or more metallic carbides, one or more transition metal ²nitrides, one or more ²metallic phosphides, one or more superionic conductors, one or more phosphate ²electrolytes, ²one or more mixed oxides being doped with one or more lower-valent cations, ²one or more²mixed sulphides being doped with one or more lower-valent cations, and any ²mixture thereof;²preferably, from 60 wt.% to 100 wt.%; more preferably from 70 wt.% to 100 ²wt.%; even more ²preferably from 80 wt.% to 100 wt.% and most preferably from 90 wt.% to 100 ²wt.%.According ²to a third aspect, the disclosure provides the use of a bed comprising ²particles in at least one ²fluidized bed reactor to perform a process of steam cracking of hydrocarbons ²having at least²two carbons according to the first aspect, the use is remarkable in that at ²least 10 wt.% of the²particles of the bed based on the total weight of the particles of the bed are ²electrically ²conductive, have a resistivity ranging from 0.001 Ohm.cm to 500 Ohm cm at a ²temperature of ²800 C and are or comprise one or more selected from one or more metallic ²alloys, one or ²more non-metallic resistors, one or more metallic carbides, one or more ²transition metal²nitrides, one or more metallic phosphides, graphite, carbon black, one or more ²superionic²CA 03184993 2023- 1-4²<DP=20>²WO 2022 / 023346 20 ²PCT / EP2021 / 071011²conductors, one or more phosphate electrolytes, one or more mixed oxides being ²doped with ²one or more lower-valent cations, one or more mixed sulphides being doped with ²one or more ²lower-valent cations, and any mixture thereof.²For example, the use comprises heating the bed comprising particles to a ²temperature ranging²from 500 C to 1200 C in a first reactor, transporting the heated particle bed ²from the first²reactor to a second reactor and providing a hydrocarbon feedstock to the ²second reactor; with ²preference, at least the second reactor is a fluidized bed reactor and / or at ²least the second ²reactor is devoid of heating means; more preferably, the first reactor and the ²second reactor ²are fluidized bed reactors and / or the first and the second reactor are devoid ²of heating means.² For example, the second reactor is devoid of electrodes.²In an embodiment, from 50 wt.% to 100 wt.% of the electrically conductive ²particles of the bed ²based on the total weight of the electrically conductive particles of the bed ²are one or more ²selected from graphite, carbon black, one or more metallic alloys, one or more ²non-metallic ²resistors, one or more metallic carbides, one or more transition metal ²nitrides, one or more²metallic phosphides, one or more superionic conductors, one or more phosphate ²electrolytes,²one or more mixed oxides being doped with one or more lower-valent cations, ²one or more ²mixed sulphides being doped with one or more lower-valent cations, and any ²mixture thereof; ²preferably, from 60 wt.% to 100 wt.%; more preferably from 70 wt.% to 100 ²wt.%; even more ²preferably from 80 wt.% to 100 wt.% and most preferably from 90 wt.% to 100 ²wt.%.²According to a fourth aspect, the disclosure provides the use of an ²installation comprising at²least one fluidized bed reactor to perform a steam cracking reaction, ²remarkable in that the ²installation is according to the second aspect. With preference, the use of an ²installation at ²least one fluidized bed reactor to perform a steam cracking reaction in a ²process according to ²the first aspect.²The particular features, structures, characteristics or embodiments may be ²combined in any²suitable manner, as would be apparent to a person skilled in the art from this ²disclosure, in ²one or more embodiments.²Description of the figures²- Figure 1 illustrates an installation according to the prior art.²- Figure 2 illustrates an installation according to the disclosure with one ²reactor wherein²the heating zone and reaction zone are the same.²- Figure 3 illustrates an installation according to the disclosure with one ²reactor wherein ²the heating zone and reaction zone are arranged one above the other.²CA 03184993 2023- 1-4²<DP=21>²WO 2022 / 023346 21 ²PCT / EP2021 / 071011²- Figure 4 illustrates an installation according to the disclosure with one ²reactor wherein ²the heating zone and reaction zone are arranged one lateral to the other.²- Figure 5 illustrates an installation according to the disclosure with two ²reactors.²Detailed description² For the disclosure, the following definitions are given:²The terms "comprising", "comprises" and "comprised of" as used herein are ²synonymous with ²"including", "includes" or "containing", "contains", and are inclusive or open-²ended and do not ²exclude additional, non-recited members, elements or method steps. The terms ²"comprising", ²"comprises" and "comprised of" also include the term "consisting of".²The recitation of numerical ranges by endpoints includes all integer numbers ²and, where²appropriate, fractions subsumed within that range (e.g. 1 to 5 can include 1, ²2, 3, 4, 5 when ²referring to, for example, a number of elements, and can also include 1.5, 2, ²2.75 and 3.80, ²when referring to, for example, measurements). The recitation of endpoints ²also includes the ²recited endpoint values themselves (e.g. from 1.0 to 5.0 includes both 1.0 and ²5.0). Any²numerical range recited herein is intended to include all sub-ranges subsumed ²therein.²Conventional steam crackers are complex industrial facilities that can be ²divided into three ²main zones, each of which has several types of equipment with very specific ²functions:²(i) the hot zone including cracking furnaces, quench exchanger and quench ²loop, the ²columns of the hot separation train;²(ii) the compression zone including a cracked gas compressor, purification and²separation columns, dryers and²(iii) the cold zone including the cold box, de-methaniser, fractionating ²columns of the ²cold separation train, the 02 and 03 converters, the gasoline ²hydrostabilization reactor.²Conventional steam cracking is carried out in tubular reactors in direct-fired ²heaters (furnaces).²Various vessel sizes and configurations can be used, such as a coiled tube, U-²tube, or straight²tube layouts. Tube diameters range from 2.5 cm to 25 cm. Each furnace ²comprises a ²convection zone in which the waste heat is recovered and a radiant zone in ²which cracking ²takes place.²The present disclosure provides a process to perform a steam cracking reaction ²of²hydrocarbons having at least two carbons, said process comprising the steps ²of:²a) providing at least one fluidized bed reactor comprising at least two ²electrodes and a²bed comprising particles;²CA 03184993 2023- 1-4²<DP=22>²WO 2022 / 023346 22 ²PCT / EP2021 / 071011²b) putting the particles of the bed in a fluidized state by passing upwardly ²through the said ²bed a fluid stream, to obtain a fluidized bed;²C) heating the fluidized bed to a temperature ranging from 500 C to 1200 C to ²conduct ²the steam cracking reaction on a hydrocarbon feedstock; and² d) optionally, recovering the cracking products of the reaction²the process is remarkable in that at least 10 wt.% of the particles based on ²the total weight of ²the particles of the bed are electrically conductive and have a resistivity ²ranging from 0.001 ²Ohm.cm to 500 Ohm.cm at of 800 C; in that the step c) of heating the fluidized ²bed is ²performed by passing an electric current through the fluidized bed; and in ²that the electrically²conductive particles of the bed are or comprise one or more selected from ²graphite, carbon²black, one or more metallic alloys, one or more non-metallic resistors, one or ²more metallic ²carbides, one or more transition metal nitrides, one or more metallic ²phosphides, one or more ²superionic conductors, one or more phosphate electrolytes, one or more mixed ²oxides being ²doped with one or more lower-valent cations, one or more mixed sulphides being ²doped with²one or more lower-valent cations, and any mixture thereof.²In an embodiment, from 50 wt.% to 100 wt.% of the electrically conductive ²particles of the ²bed based on the total weight of the electrically conductive particles of the ²bed are one or ²more selected from graphite, carbon black, one or more metallic alloys, one or ²more non-²metallic resistors, one or more metallic carbides, one or more transition ²metal nitrides, one or²more metallic phosphides, one or more superionic conductors, one or more ²phosphate ²electrolytes, one or more mixed oxides being doped with one or more lower-²valent cations, ²one or more mixed sulphides being doped with one or more lower-valent cations, ²and any ²mixture thereof; preferably, from 60 wt.% to 100 wt.%; more preferably from 70 ²wt.% to 100²wt.%; even more preferably from 80 wt.% to 100 wt.% and most preferably from ²90 wt.% to²100 wt.%.²The fluid stream may be a gaseous stream and / or a vaporized stream.²For example, the step of heating the fluidized bed is performed by passing an ²electric current ²at a voltage of at most 300 V through the fluidized bed, preferably at most ²200 V, more²preferably at most 150 V, even more preferably at most 120 V, most preferably ²at most 100 V,²even most preferably at most 90 V.²The solid particulate material in the fluidized bed reactor is typically ²supported by a porous ²plate, a perforated plate, a plate with nozzles or chimneys, known as a ²distributor. The fluid ²is then forced through the distributor up and travelling through the voids ²between the solid²particulate material. At lower fluid velocities, the solids remain settled as ²the fluid passes²CA 03184993 2023-1-4²<DP=23>² WO 2022 / 023346 23 PCT / EP2021 / 071011²through the voids in the material, known as a packed bed reactor. As the fluid ²velocity is ²increased, the particulate solids will reach a stage where the force of the ²fluid on the solids is ²enough to counterbalance the weight of the solid particulate material. This ²stage is known as ²incipient fluidization and occurs at this minimum fluidization velocity. Once ²this minimum²velocity is surpassed, the contents of the reactor bed begin to expand and ²become fluidized.²Depending on the operating conditions and properties of the solid phase ²various flow regimes ²can be observed in such reactors. The minimum fluidization velocity needed to ²achieve bed ²expansion depends upon the size, shape, porosity and density of the particles ²and the density ²and viscosity of the upflowing fluid.²P.R. Gunjal, V.V. Ranade, in Industrial Catalytic Processes for Fine and ²Specialty Chemicals,²(2016) reads that four different categories of fluidization based on the mean ²particle have ²been differentiated by Geldart that determine the fluidization regimes:²- type A, aeratable fluidization (medium size, medium-density particles ²which are easier²to fluidize; Particles of typically 30-100 pm, density - 1500 kg / m3);²- type ²B, sand-like fluidization (heavier particles which are difficult to fluidize; ²Particles²of typically 100-800 urn, density between 1500 and 4000 kg / m3);²- type C, cohesive fluidization (typical powder-like solid particle ²fluidization; Fine-size ²particles (- 20 pm) with a dominance of intraparticle or cohesive forces); and²- type D, spoutable fluidization (large density and larger particle - 1-4 ²mm, dense and²spoutable).²Fluidization may be broadly classified into two regimes (Fluid Bed Technology ²in Materials ²Processing, 1999 by CRC Press): homogeneous fluidization and heterogeneous ²fluidization. ²In homogeneous or particulate fluidization, particles are fluidized uniformly ²without any ²distinct voids. In heterogeneous or bubbling fluidization, gas bubbles devoid ²of solids are²distinctly observable. These voids behave like bubbles in gas-liquid flows and ²exchange gas²with the surrounding homogeneous medium with a change in size and shape while ²rising in ²the medium. In particulate fluidization, the bed expands smoothly with ²substantial particle ²movement and the bed surface is well defined. Particulate fluidization is ²observed only for ²Geldart-A type particles. A bubbling fluidization regime is observed at much ²higher velocities²than homogeneous fluidization, in which distinguishable gas bubbles grow from ²the²distributor, may coalesce with other bubbles and eventually burst at the ²surface of the bed. ²These bubbles intensify the mixing of solids and gases and bubble sizes tend ²to increase ²further with a rise in fluidization velocity. A slugging regime is observed ²when the bubble ²diameter increases up to the reactor diameter. In a turbulent regime, bubbles ²grow and start²breaking up with the expansion of the bed. Under these conditions, the top ²surface of the bed²is no longer distinguishable. In fast fluidization or pneumatic fluidization, ²particles are²CA 03184993 2023- 1-4²<DP=24>²WO 2022 / 023346 24 ²PCT / EP2021 / 071011²transported out of the bed and need to be recycled back into the reactor. No ²distinct bed ²surface is observed.²Fluidized bed reactors have the following advantages:²Uniform Particle Mixing: Due to the intrinsic fluid-like behaviour of the ²solid particulate²material, fluidized beds do not experience poor mixing as in packed beds. The ²elimination of²radial and axial concentration gradients also allows for better fluid-solid ²contact, which is ²essential for reaction efficiency and quality.²Uniform Temperature Gradients: Many chemical reactions require the addition or ²removal of ²heat. Local hot or cold spots within the reaction bed are avoided in a ²fluidized situation.²Ability to Operate the Reactor Continuously: The fluidized bed nature of these ²reactors allows²for the ability to continuously withdraw products and introduce new reactants ²into the reaction ²vessel. On top of continuous operation of the chemical reactions, the ²fluidized bed allows also ²to continuously or at given frequency withdraw solid material or add ²continuously or at given ²frequency new fresh solid material thanks to the flowable solid particulate ²material.²Heat can be produced by passing an electrical current through a conducting ²material that has²sufficiently high resistivity (the resistor) to transform electricity into ²heat. Electrical resistivity ²(also called specific electrical resistance or volume resistivity, is an ²intrinsic property ²independent of shape and size) and its inverse, electrical conductivity, is a ²fundamental ²property of a material that quantifies how strongly it resists or conducts ²electric current (SI²unit of electrical resistivity is the ohm-meter (Q-m) and for conductivity ²Siemens per meter²(S / m)).²When electricity is passed through a fixed bed of electrically conducting ²particulate solids, ²having a sufficient resistivity, the bed offers resistance to the flow of ²current; this resistance ²depends on many parameters, including the nature of the solid, the nature of ²the linkages²among the particles within the bed, the bed voidage, the bed height, the ²electrode geometry,²etc. If the same fixed bed is fluidized by passing gas, the resistance of the ²bed increases; the ²resistance offered by the conducting particles generates heat within the bed ²and can maintain ²the bed in isothermal conditions (termed an electrothermal fluidized bed or ²electrofluid ²reactor). In many high-temperature reactions, electrofluid reactors offer in ²situ heating during²the reaction and are particularly useful for operating endothermic reactions ²and hence save²energy because no external heating or transfer of heat is required. It is a ²prerequisite that at ²least part of the solid particulate material is electrically conducting but ²non-conducting solid ²particulates can be mixed and still result in enough heat generation. Such non-²conducting or ²very high resistivity solids can play a catalytic role in the chemical ²conversion. The²CA 03184993 2023- 1-4²<DP=25>²WO 2022 / 023346 25 ²PCT / EP2021 / 071011²characteristics of the bed material determine the resistance of an ²electrothermal fluidized bed ²furnace; as this is a charge resistor type of heat generation, the specific ²resistivity of the ²particles affects the bed resistance. The size, shape, composition, and size ²distribution of the ²particles also influence the magnitude of the bed resistance. Also, when the ²bed is fluidized,²the voids generated between the particles increases the bed resistance. The ²total resistance²of the bed is the sum of two components, e.g. the electrode contact-resistance ²(i.e., the ²resistance between the electrode and the bed) and the bed resistance. A large ²contact-²resistance will cause extensive local heating in the vicinity of the electrode ²while the rest of ²the bed stays rather cool. The following factors determine the contact-²resistance: current²density, fluidization velocity, type of bed material, electrode size and the ²type of material used²for the electrodes. The electrode compositions can be advantageously metallic ²like iron, cast ²iron or other steel alloys, copper or a copper-based alloy, nickel or a nickel-²based alloy or ²refractory like metal, intermetallics or an alloy of Zr, Hf, V, Nb, Ta, Cr, ²Mo, W or ceramic-like ²carbides, nitrides or carbon-based like graphite. The area of contact between ²the bed material²and the electrodes can be adjusted, depending on the electrode submergence and ²the²amount of particulate material in the fluidized bed. Hence, the electrical ²resistance and the ²power level can be manipulated by adjusting these variables. Advantageously, ²to prevent ²overheating of the electrodes compared to the fluidised bed, the resistivity ²of the electrode ²should be lower (and hence the joule heating) than of the particulate material ²of the fluidized²bed. In a preferred embodiment, the electrodes can be cooled by passing a ²colder fluid inside²or outside the electrodes. Such fluids can be any liquid that vaporises upon a ²heating, gas ²stream or can be a part of the colder feedstock that first cools the electrode ²before entering ²the fluidised bed.²Bed resistance can be predicted by the ohmic law. The mechanism of current ²transfer in²fluidized beds is believed to occur through current flow along continuous ²chains of conducting²particles at low operating voltages. At high voltages, a current transfer ²occurs through a ²combination of chains of conducting particles and arcing between the electrode ²and the bed ²as well as particle-to-particle arcing that might ionize the gas, thereby ²bringing down the bed ²resistance. Arcing inside the bed, in principle, is not desirable as it would ²lower the electrical²and thermal efficiency. The gas velocity impacts strongly the bed resistance, ²a sharp increase²in resistance from the settled bed onward when the gas flow rate is increased; ²a maximum ²occurred close to the incipient fluidization velocity, followed by a decrease ²at higher velocities. ²At gas flow rates sufficient to initiate slugging, the resistance again ²increased. Average ²particle size and shape impact resistance as they influence the contacts ²points between²particles. In general, the bed resistivity increases 2 to 5 times from a ²settled bed (e.g. 20²Ohm.cm for graphite) to the incipient fluidisation (60 Ohm.cm for graphite) ²and 10 to 40 times²CA 03184993 2023- 1-4²<DP=26>²WO 2022 / 023346 26 ²PCT / EP2021 / 071011²from a settled bed to twice (300 Ohm.cm for graphite) the incipient ²fluidisation velocity. Non ²or less-conducting particles can be added to conducting particles. If the ²conducting solid ²fraction is small, the resistivity of the bed would increase due to the ²breaking of the linkages ²in the chain of conducting solids between the electrodes. If the non-²conducting solid fraction²is finer in size, it would fill up the interstitial gaps or voidage of the ²larger conducting solids²and hence increase the resistance of the bed.²In general, for a desired high heating power, a high current at a low voltage ²is preferred. The ²power source can be either AC or DC. Voltages applied in an electrothermal ²fluidized bed are ²typically below 100 V to reach enough heating power. The electrothermal ²fluidized bed can² be controlled in the following three ways:²1. Adjusting the gas flow: Because the conductivity of the bed depends on the ²extent of ²voidage or gas bubbles inside the bed, any variation in the gas flow rate ²would change the ²power level; hence the temperature can be controlled by adjusting the ²fluidizing gas flow rate. ²The flow rate required for optimum performance corresponds to a velocity which ²equals or²slightly exceeds the minimum fluidization velocity.²2. Adjusting the electrode submergence: The power level can also be controlled ²by varying ²the electrode immersion level inside the bed because the conductivity of the ²bed is dependent ²on the area of contact between the conducting particles and the electrode: the ²surface area ²of the electrode available for current flow increases with electrode ²submergence, leading to²a reduction in overall resistance.²3. Adjusting the applied voltage: although changing the power level by using ²the first two ²methods is often more affordable or economical than increasing the applied ²voltage, however ²in electrothermal fluidized beds three variables are available to control the ²produced heating ²power.²The wall of the reactor is generally made of graphite, ceramics (like SiC), ²high-melting metals²or alloys as it is versatile and compatible with many high-temperature ²reactions of industrial ²interest. The atmosphere for the reaction is often restricted to the neutral ²or the reducing type ²as an oxidising atmosphere can combust carbon materials or create a non-²conducting metal ²oxide layer on top of metals or alloys. The wall and / or the distribution plate ²itself can act as²an electrode for the reactor. The fluidized solids can be graphite or any ²other high-melting-²point, electrically conducting particles. The other electrodes, which is ²usually immersed in the²bed, can also be graphite or a high-melting-point metal, intermetallics or ²alloys.²It may be advantaged to generate the required reaction heat by heating the ²conductive ²particles and / or catalyst particles in a separate zone of the reactor where ²little or substantially²CA 03184993 2023- 1-4²<DP=27>²WO 2022 / 023346 27 ²PCT / EP2021 / 071011²no feedstock hydrocarbons are present, but only diluent gases. The benefit is ²that the ²appropriate conditions of fluidization to generate heat by passing an ²electrical current through ²a bed of conductive particles can be optimized whereas the optimal reaction ²conditions during ²hydrocarbon transformation can be selected for the other zone of the reactor. ²Such conditions²of optimal void fraction and linear velocity might be different for heating ²purposes and²chemical transformation purposes.²In an embodiment of the present disclosure, the installation comprises of two ²zones arranged ²in series namely a first zone being a heating zone and a second zone being a ²reaction zone,²where the conductive particles and catalyst particles are continuously moved ²or transported²from the first zone to the second zone and vice versa. The first and second ²zones can be ²different parts of a fluidized bed or can be located in separate fluidized ²beds reactors ²connected one to each other.²In the said embodiment, the process to perform steam cracking reaction of ²hydrocarbons²having at least two carbons said process comprising the steps of:²a) providing at least one fluidized bed reactor comprising at least two ²electrodes and a ²bed comprising particles;²b) putting the particles in a fluidized state by passing upwardly through the ²said bed a fluid² stream, to obtain a fluidized bed;²c) heating the fluidized bed to a temperature ranging from 500 C to 1200 C to ²conduct ²the steam cracking reaction of a hydrocarbon feedstock; and²d) optionally, recovering the cracking products of the reaction;²wherein at least 10 wt.% of the particles based on the total weight of the ²particles of the bed²are electrically conductive particles, have a resistivity ranging from 0.001 ²Ohm.cm to 500²Ohm.cm at 800 C and are or comprise one or more selected from one or more ²metallic alloys, ²one or more non-metallic resistors, one or more metallic carbides, one or more ²transition metal ²nitrides, one or more metallic phosphides, graphite, carbon black, one or more ²superionic ²conductors, one or more phosphate electrolytes, one or more mixed oxides being ²doped with²one or more lower-valent cations, one or more mixed sulphides being doped with ²one or more²lower-valent cations, and / or any mixture thereof, wherein the at least one ²fluidized bed reactor ²provided in step a) comprises a heating zone and a reaction zone and wherein ²the fluid stream ²provided in step b) is provided to the heating zone and comprises diluent ²gases and the step ²c) of heating the fluidized bed to a temperature ranging from 500 C to 1200 C ²to conduct the²steam cracking reaction of a hydrocarbon feedstock comprises the following sub-²steps:²- heating the fluidized bed to a temperature ranging from 500 C to 1200 C by ²passing²an electric current through the heating zone of the at least one fluidized ²bed,²CA 03184993 2023- 1-4²<DP=28>²WO 2022 / 023346 28 ²PCT / EP2021 / 071011²- transporting the heated particles from the heating zone to the reaction ²zone,²- in the reaction zone, putting the heated particles in a fluidized state ²by passing ²upwardly through the said bed of the reaction zone a fluid stream comprising a ²²hydrocarbon feedstock and optional diluent gases to obtain a fluidized bed and ²to² conduct the endothermic steam cracking reaction on the hydrocarbon feedstock,²- optionally, recovering the particles from the reaction zone and recycling ²them to the ²heating zone.²For example, the diluent gases can be one or more selected from steam, ²hydrogen, carbon²dioxide, argon, helium, nitrogen and methane.²The fluid stream may be a gaseous stream and / or a vaporized stream.²For example, the at least one fluidized bed reactor is at least two fluidized ²bed reactors²connected one to each other wherein at least one of said at least two ²fluidized bed reactors²is the heating zone and at least another of said at least two fluidized bed ²reactors is the ²reaction zone. With preference, the at least one fluidized bed reactor being ²the heating zone ²comprises gravitational or pneumatic transport means to transport the ²particles from the ²heating zone to the reaction zone and / or the installation comprises means ²arranged to inject²a hydrocarbon feedstock to the at least one fluidized bed reactor being the ²reaction zone. The²installation is devoid of means to inject a hydrocarbon feedstock to the at ²least one fluidized ²bed reactor being the heating zone.²For example, the at least one fluidized bed reactor is a single fluidized bed ²reactor wherein²the heating zone is the bottom part of the fluidized bed reactor while the ²reaction zone is the²top part of the fluidised bed reactor. With preference, the installation ²comprises means to ²inject a hydrocarbon feedstock and / or diluent between the two zones. The ²diameter of the ²heating zone and reaction zone can be different in order to accomplish optimum ²conditions ²for heating in the bottom zone and optimum conditions for hydrocarbon ²conversion in the top²zone. Particles can move from the heating zone to the reaction zone by ²entrainment and the²other way around from the reaction zone back to the heating zone by gravity. ²Optionally, ²particles can be collected from the upper heating zone and transferred by a ²separate transfer ²line back to the bottom heating zone.²Step c) provides that the steam cracking reaction is performed on a ²hydrocarbon feedstock²which implies that a hydrocarbon feedstock is provided. It is understood that ²the hydrocarbon²feedstock is provided to the reaction zone and that when the heating zone is ²separated from²CA 03184993 2023- 1-4²<DP=29>²WO 2022 / 023346 29 ²PCT / EP2021 / 071011²the reaction zone then, with preference, no hydrocarbon feedstock with at ²least two carbons ²is provided to the heating zone. It is understood that in addition to the ²hydrocarbon feedstock ²provided to the reaction zone, steam can be provided to the reaction zone to ²reach the ²recommended steam to methane ratio in the reaction zone. When the heating zone ²and the²reaction zone are mixed (i.e. the same zone); the fluid stream provided in ²step b) comprises²a hydrocarbon feedstock.²It is a specific embodiment of the present disclosure that the distance ²between the heat ²sources, being the hot particulate material and the feedstock is significantly ²reduced because ²of the small size of the particulates and the mixing of the particulates in ²the vaporous fluidising²stream, compared to steam crackers coils having typically 2.5 to 25 cm ²internal diameter²requiring large temperature gradients to concur the large distance that heat ²has to travel.²The bed comprisind particles ²To achieve the required temperature necessary to carry out the steam cracking ²reaction, at ²least 10 wt.% of the particles based on the total weight of the particles of ²the bed are²electrically conductive, have a resistivity ranging from 0.001 Ohm.cm to 500 ²Ohm.cm at 800 C²and are or comprise one or more selected from one or more metallic alloys, one ²or more non-²metallic resistors, one or more metallic carbides, one or more transition ²metal nitrides, one or ²more metallic phosphides, graphite, carbon black, one or more superionic ²conductors, one or ²more phosphate electrolytes, one or more mixed oxides being doped with one or ²more lower-²valent cations, one or more mixed sulphides being doped with one or more lower-²valent²cations, and any mixture thereof.²For example, from 50 wt.% to 100 wt.% of the electrically conductive particles ²of the bed based ²on the total weight of the electrically conductive particles of the bed are ²one or more selected ²from graphite, carbon black, one or more metallic alloys, one or more non-²metallic resistors,²one or more metallic carbides, one or more transition metal nitrides, one or ²more metallic²phosphides, one or more superionic conductors, one or more phosphate ²electrolytes, one or ²more mixed oxides being doped with one or more lower-valent cations, one or ²more mixed ²sulphides being doped with one or more lower-valent cations, and any mixture ²thereof; ²preferably, from 60 wt.% to 100 wt.%; more preferably from 70 wt.% to 100 ²wt.%; even more²preferably from 80 wt.% to 100 wt.% and most preferably from 90 wt.% to 100 ²wt.%.²In an embodiment, from 50 wt.% to 100 wt.% of the electrically conductive ²particles of the bed ²based on the total weight of the electrically conductive particles of the bed ²are devoid of ²graphite and / or carbon black; preferably, from 60 wt.% to 95 wt.%; more ²preferably from 70 ²wt.% to 90 wt.%; and even more preferably from 75 wt.% to 85 wt.%.²CA 03184993 2023- 1-4²<DP=30>²WO 2022 / 023346 30 ²PCT / EP2021 / 071011²For example, the content of electrically conductive particles is ranging from ²10 wt.% to ²100 wt.% based on the total weight of the particles of the bed; preferably, ²from 15 wt.% to 95 ²wt.%, more preferably from 20 wt.% to 90 wt.%, even more preferably from 25 ²wt.% to 80 wt.% ²and most preferably from 30 wt.% to 75 wt.%.²For example, the content of electrically conductive particles based on the ²total weight of the²bed is at least 12 wt.% based on the total weight of the particles of the bed; ²preferably, at least ²wt.%, more preferably, at least 20 wt.%; even more preferably at least 25 ²wt.%, and most ²preferably at least 30 wt.% or at least 40 wt.% or at least 50 wt.% or at ²least 60 wt.%.²For example, the electrically conductive particles have a resistivity ranging ²from 0.005 to 400²10 Ohm.cm at 800 C, preferably ranging from 0.01 to 300 Ohm.cm at 800 C; ²more preferably²ranging from 0.05 to 150 Ohm.cm at 800 C and most preferably ranging from 0.1 ²to 100 ²Ohm.cm at 800 C.²For example, the electrically conductive particles have a resistivity of at ²least 0.005 Ohm.cm ²at 800 C; preferably of at least 0.01 Ohm.cm at 800 C, more preferably of at ²least 0.05²15 Ohm.cm at 800 C; even more preferably of at least 0.1 Ohm.cm at 800 C, ²and most preferably²of at least 0.5 Ohm.cm at 800 C.²For example, the electrically conductive particles have a resistivity of at ²most 400 Ohm.cm at ²800 C; preferably of at most 300 Ohm.cm at 800 C, more preferably of at most ²200 Ohm.cm ²at 800 C; even more preferably of at most 150 Ohm.cm at 800 C, and most ²preferably of at² Most 100 Ohm.cm at 800 C.²For example, the particles of the bed have an average particle size ranging ²from 5 to 300 pm ²as determined by sieving according to ASTM D4513-11, preferably ranging from ²10 to 200 pm ²and more preferably ranging from 30 to 150 pm.²For example, the electrically conductive particles of the bed have an average ²particle size²ranging from 5 to 300 pm as determined by sieving according to ASTM D4513-11, ²preferably²ranging from 10 to 200 pm and more preferably ranging from 30 to 150 pm.²The electrical resistance is measured by a four-probe DC method using an ²ohmmeter. A ²densified power sample is shaped in a cylindrical pellet that is placed ²between the probe ²electrodes. Resistivity is determined from the measured resistance value, R, ²by applying the²known expression p= RxA / L, where L is the distance between the probe ²electrodes typically²a few millimetres and A the electrode area.²The electrically conductive particles of the bed can exhibit electronic, ionic ²or mixed electronic-²ionic conductivity. The ionic bonding of many refractory compounds allows for ²ionic diffusion²CA 03184993 2023-1-4²<DP=31>²WO 2022 / 023346 31 ²PCT / EP2021 / 071011²and correspondingly, under the influence of an electric field and appropriate ²temperature ²conditions, ionic conduction.²The electrical conductivity, a, the proportionality constant between the ²current density j and ²the electric field E, is given by² cs=j / E=ECiXZiqX ;²where ci is the carrier density (number / cm3), la; the mobility (cm2 / Vs), and ²Z'q the charge (q=1.6 ²x 10-19 C) of the ith charge carrier. The many orders of magnitude differences ²in a between ²metals, semiconductors and insulators generally result from differences in c ²rather than t. On ²the other hand, the higher conductivities of electronic versus ionic ²conductors are generally²due to the much higher mobilities of electronic versus ionic species.²The most common materials that can be used for resistive heating is subdivided ²into nine ²groups:²(1) Metallic alloys for temperatures up to 1200-1400 C,²(2) non-metallic resistors like silicon carbide (SiC), molybdenum disilicide ²(MoSi2), nickel²silicide (NiSi), sodium silicide (Na2S0, magnesium silicide (Mg2Si), platinum ²silicide²(PtSi), titanium silicide (TiSi2) and tungsten silicide (WSi2) up to 1600-1900 ²C,²(3) several mixed oxides and / or mixed sulphides being doped with one or more ²lower-²valent cations with variable temperature optima,²(4) graphite up to 2000 C,²(5) metallic carbides,²(6) transition metal nitrides,²(7) metallic phosphides,²(8) superionic conductors, and²(9) phosphate electrolytes.²A first group of metallic alloys, for temperatures up to 1150-1250 C, can be ²constituted by Ni¨²²Cr alloys with low Fe content (0.5-2.0 %), preferably alloy Ni¨Cr (80 % Ni, 20 ²% Cr) and (70 ²% Ni, 30 `K. Cr). Increasing the content of Cr increases the material ²resistance to oxidation at ²high temperatures. A second group of metallic alloys having three components ²are Fe¨Ni¨Cr ²alloys, with maximum operating temperature in an oxidizing atmosphere to 1050-²1150 C but²which can be conveniently used in reducing atmospheres or Fe¨Cr¨Al (chemical ²composition²15-30 % Cr, 2-6 % Al and Fe balance) protecting against corrosion by a surface ²layer of ²oxides of Cr and Al, in oxidizing atmospheres can be used up to 1300-1400 C. ²Silicon carbide ²as non-metallic resistor can exhibit wide ranges of resistivity that can be ²controlled by the way ²they are synthesized and the presence of impurities like aluminium, iron, ²oxide, nitrogen or²extra carbon or silicon resulting in non-stoichionnetric silicon carbide. In ²general silicon carbide²CA 03184993 2023-1-4²<DP=32>²WO 2022 / 023346 32 ²PCT / EP2021 / 071011²has a high resistivity at low temperature but has good resistivity in the ²range of 500 to 1200 C. ²In an alternative embodiment, the non-metallic resistor can be devoid of ²silicon carbide, and / or ²can comprise molybdenum disilicide (MoSi2), nickel silicide (NiSi), sodium ²silicide (Na2Si), ²magnesium silicide (Mg2S0, platinum silicide (PtSi), titanium silicide ²(TiSi2), tungsten silicide² (WSi2) or a mixture thereof.²Graphite has rather low resistivity values, with a negative temperature ²coefficient up to about ²600 C after which the resistivity starts to increase.²Many mixed oxides and / or mixed sulphides being doped with one or more lower-²valent ²cations, having in general too high resistivity at low temperature, become ²ionic or mixed²conductors at high temperature. The following circumstances can make oxides or ²sulphides²sufficient conductors for heating purposes: ionic conduction in solids is ²described in terms of ²the creation and motion of atomic defects, notably vacancies and interstitials ²of which its ²creation and mobility is very positively dependent on temperature. Such mixed ²oxides or ²sulphides are ionic or mixed conductors, namely being doped with one or more ²lower-valent²cations. Three mechanisms for ionic defect formation in oxides are known: (1) ²Thermally²induced intrinsic ionic disorder (such as Schottky and Frenkel defect pairs ²resulting in non-²stoichiometry), (2). Redox-induced defects and (3) Impurity-induced defects. ²The first two ²categories of defects are predicted from statistical thermodynamics and the ²latter form to ²satisfy electroneutrality. In the latter case, high charge carrier densities ²can be induced by²substituting lower valent cations for the host cations. Mixed oxides and / or ²mixed sulphides²with fluorite, pyrochlore or perovskite structure are very suitable for ²substitution by one or more ²lower-valent cations.²Several sublattice disordered oxides or sulphides have high ion transport ²ability at increasing ²temperature. These are superionic conductors, such as LiAlSiO4, Li1oGeP2S12, ²Li3.6Sio.6P0.404,²NaSICON (sodium (Na) Super Ionic CONductor) with the general formula Nai-²ExZr2P3_xSix012²with 0 <x < 3, for example Na3Zr2PSi2012 (x = 2), or sodium beta alumina, such ²as NaA111017, ²Nai .6,8,111017.3, and / or Na1.76Lio.38A113.62017.²High concentrations of ionic carriers can be induced in intrinsically ²insulating solids and ²creating high defective solids. Thus, the electrically conductive particles of ²the bed are or²comprise one or more mixed oxides being ionic or mixed conductor, namely being ²doped with²one or more lower-valent cations, and / or one or more mixed sulphides being ²ionic or mixed ²conductor, namely being doped with one or more lower-valent cations. With ²preference, the ²mixed oxides are selected from one or more oxides having a cubic fluorite ²structure being at ²least partially substituted with one or more lower-valent cations, ²preferentially selected from²Sm, Gd, Y, Sc, Yb, Mg, Ca, La, Dy, Er, Eu; and / or from one or more AB03-²perovskites with A²CA 03184993 2023-1-4²<DP=33>²WO 2022 / 023346 33 ²PCT / EP2021 / 071011²and B tri-valent cations, being at least partially substituted in A position ²with one or more lower-²valent cations, preferentially selected from Ca, Sr, or Mg, and comprising at ²least one of Ni, ²Ga, Co, Cr, Mn, Sc, Fe and / or a mixture thereof in B position; and / or from one ²or more AB03-²perovskites with A bivalent cation and B tetra-valent cation, being at least ²partially substituted²with one or more lower-valent cations, preferentially selected from Mg, Sc, Y, ²Nd or Yb in the²B position or with a mixture of different B elements in the B position; and / or ²from one or more ²A2B207-pyrochlores with A trivalent cation and B tetra-valent cation being at ²least partially ²substituted in A position with one or more lower-valent cations, ²preferentially selected from Ca ²or Mg, and comprising at least one of Sn, Zr and Ti in B position.²With preference, the one or more mixed sulphides are selected from one or more ²sulphides ²having a cubic fluorite structure being at least partially substituted with ²one or more lower-²valent cations, preferentially selected from Sm, Gd, Y, Sc, Yb, Mg, Ca, La, ²Dy, Er, Eu; and / or ²from one or more ABS3 structures with A and B tri-valent cations, being at ²least partially²substituted in A position with one or more lower-valent cations, ²preferentially selected from²Ca, Sr, or Mg, and comprising at least one of Ni, Ga, Co, Cr, Mn, Sc, Fe ²and / or a mixture ²thereof in B position; and / or from one or more ABS3 structures with A bivalent ²cation and B ²tetra-valent cation, being at least partially substituted with one or more ²lower-valent cations, ²preferentially selected from Mg, Sc, Y, Nd or Yb in the B position or with a ²mixture of different²B elements in the B position; and / or from one or more A2B257 structures with A ²trivalent cation²and B tetra-valent cation being at least partially substituted in A position ²with one or more ²lower-valent cations, preferentially selected from Ca or Mg, and comprising at ²least one of Sn, ²Zr and Ti in B position.²With preference, the degree of substitution in the one or more mixed oxides ²doped with one²or more lower-valent cations and having a cubic fluorite structure is between ²1 and 15 atom²% based on the total number of atoms present in the one or more oxides or ²sulphides having ²a cubic fluorite structure, in the one or more AB03-perovskites with A and B ²tri-valent cations, ²in the one or more AB03-perovskites with A bivalent cation and B tetra-valent ²cation or in the ²one or more A2B207-pyrochlores with A trivalent cation and B tetra-valent ²cation respectively,² preferably between 3 and 12 atom %, more preferably between 5 and 10 atom%.²With preference, the degree of substitution in the one or more mixed oxides ²doped with one ²or more lower-valent cations is between 1 and 50 atom% based on the total ²number of atoms ²present in the one or more AB03-perovskites with A and B tri-valent cations, ²in the one or ²more AB03-perovskites with A bivalent cation and B tetra-valent cation or in ²the one or more²A2B207-pyrochlores with A trivalent cation and B tetra-valent cation ²respectively, preferably²between 3 and 20 atom%, more preferably between 5 and 15 atom%.²CA 03184993 2023-1-4²<DP=34>²WO 2022 / 023346 34 ²PCT / EP2021 / 071011²With preference, the degree of substitution in the one or more mixed sulphides ²doped with ²one or more lower-valent cations and having a cubic fluorite structure is ²between 1 and 15 ²atom % based on the total number of atoms present in the one or more ABS3 ²structures with²A and B tri-valent cations, in the one or more ABS3 structures with A bivalent ²cation and B²tetra-valent cation or in the one or more A2B2S7 structures with A trivalent ²cation and B tetra-²valent cation respectively, preferably between 3 and 12 atom %, more ²preferably between 5 ²and 10 atom%.²With preference, the degree of substitution in the one or more mixed sulphides ²doped with ²one or more lower-valent cations is between 1 and 50 atom% based on the total ²number of²atoms present in the one or more ABS3 structures with A and B tri-valent ²cations, in the one²or more ABS3 structures with A bivalent cation and B tetra-valent cation or in ²the one or more ²A2B257 structures with A trivalent cation and B tetra-valent cation ²respectively, preferably ²between 3 and 20 atom%, more preferably between 5 and 15 atom%.²Said one or more oxides having a cubic fluorite structure, said one or more ²AB03-perovskites²with A and B tri-valent cations, said one or more AB03-perovskites with A ²bivalent cation and²B tetra-valent cation or said one or more A2B207-pyrochlores with A trivalent ²cation and B ²tetra-valent cation being at least partially substituted with lower valent ²cations, said one or ²more sulphides having a cubic fluorite structure, said one or more ABS3 ²structures with A and ²B tri-valent cations, said one or more ABS3 structures with A bivalent cation ²and B tetra-valent²cation, said one or more A2B2S7 structures with A trivalent cation and B tetra-²valent cation²being at least partially substituted with lower valent cations also means that ²the same element, ²being a high-valent cation, can be reduced in the lower-valent equivalent, for ²example, Ti(IV) ²can be reduced in Ti(III) and / or Co(III) can be reduced in Co(II) and / or Fe(' ²II) can be reduced ²in Fe(' I) and / or Cu(' I) can be reduced in Cu(I).²Phosphate electrolytes such as LiPO4 or LaPO4 can also be used as electrically ²conductive²particles.²Metallic carbides, transition metal nitrides and metallic phosphides can also ²be selected as ²electrically conductive particles. For example, metallic carbides are selected ²from iron carbide ²(Fe3C), molybdenum carbide (such as a mixture of MoC and Mo2C). For example, ²said one or²more transition metal nitrides are selected from zirconium nitride (ZrN), ²tungsten nitride (such²as a mixture of W2N, WN, and WN2), vanadium nitride (VN), tantalum nitride ²(TaN), and / or ²niobium nitride (NbN). For example, said one or more metallic phosphides are ²selected from ²copper phosphide (Cu3P), indium phosphide (InP), gallium phosphide (GaP), ²sodium ²phosphide Na3P), aluminium phosphide (AIP), zinc phosphide (Zn3P2) and / or ²calcium² phosphide (Ca3P2).²CA 03184993 2023- 1-4²<DP=35>²WO 2022 / 023346 35 ²PCT / EP2021 / 071011²It is a preferred embodiment of the present disclosure, the electrically ²conductive particles that ²exhibit only sufficiently low resistivity at a high temperature can be heated ²by external means ²before reaching the high enough temperature where resistive heating with ²electricity overtakes ²or can be mixed with a sufficiently low resistivity solid at a low temperature ²so that the resulting²resistivity of the mixture allows to heat the fluidized bed to the desired ²reaction temperature.²For example, the electrically conductive particles of the bed are or comprise ²silicon carbide. ²For example, at least 10 wt.% of the electrically conductive particles based ²on the total weight ²of the electrically conductive particles of the bed are silicon carbide ²particles and have a ²resistivity ranging from 0.001 Ohm.cm to 500 Ohm.cm at of 800 C.²In the embodiment wherein the electrically conductive particles of the bed are ²or comprise²silicon carbide, the person skilled in the art will have the advantage to ²conduct a step of pre-²heating with a gaseous stream said fluidized bed reactor before conduct said ²endothermic ²reaction in the fluidized bed reactor. Advantageously, the gaseous stream is a ²stream of inert ²gas, i.e., nitrogen, argon, helium, methane, carbon dioxide, hydrogen or ²steam. The²temperature of the gaseous stream can be at least 500 C, or at least 550 C, or ²at least 600 C,²or at least 650 C, or at least 700 C, or at least 750 C, or at least 800 C, or ²at least 850 C, or ²at least 900 C. Advantageously, the temperature of the gaseous stream can be ²comprised ²between 500 C and 900 C, for example between 600 C and 800 C or between 650 C ²and ²750 C. Said gaseous stream of inert gas can also be used as the fluidification ²gas. The pre-²heating of the said gaseous stream of inert gas is performed thanks to ²conventional means,²including using electrical energy. The temperature of the gaseous stream used ²for the ²preheating of the bed doesn't need to reach the temperature reaction.²Indeed, the resistivity of silicon carbide at ambient temperature is high, to ²ease the starting of ²the reaction, it may be useful to heat the fluidized bed by external means, as ²with preference²the fluidized bed reactor is devoid of heating means. Once the bed is heated ²at the desired²temperature, the use of a hot gaseous stream may not be necessary.²However, in an embodiment, the electrically conductive particles of the bed ²are or comprise a ²mixture of silicon carbide particles and electrically conductive particles ²different from silicon ²carbide particles.²The pre-heating step may be also used in the case wherein electrically ²conductive particles²different from silicon carbide particles are present in the bed. For example, ²it may be used ²when the content of silicon carbide in the electrically conductive particles ²of the bed is more ²than 80 wt.% based on the total weight of the particles of the bed, for ²example, more than 85 ²wt.%, for example, more than 90 wt.%, for example, more than 95 wt.%, for ²example, more²CA 03184993 2023-1-4²<DP=36>²WO 2022 / 023346 36 ²PCT / EP2021 / 071011²than 98 wt.%, for example, more than 99 wt.%. However, a pre-heating step may ²be used ²whatever is the content of silicon carbide particles in the bed.²In the embodiment wherein the electrically conductive particles of the bed are ²or comprise a ²mixture of silicon carbide particles and electrically conductive particles ²different from silicon²carbide particles, the electrically conductive particles of the bed may ²comprise from 10 wt.%²to 99 wt.% of silicon carbide particles based on the total weight of the ²electrically conductive ²particles of the bed; preferably, from 15 wt.% to 95 wt.%, more preferably ²from 20 wt.% to 90 ²wt.%, even more preferably from 25 wt.cY0 to 80 wt.% and most preferably from ²30 wt.% to 75 ²wt.%.²For example, the electrically conductive particles of the bed are or comprise ²a mixture of silicon²carbide particles and electrically conductive particles different from silicon ²carbide particles ²and the electrically conductive particles of the bed comprises at least 40 ²wt.% of silicon carbide ²particles based on the total weight of the electrically conductive particles ²of the bed; preferably ²at least 50 wt.%, more preferably at least 60 wt.%, even more preferably at ²least 70 wt.% and² most preferably at least 80 wt.%.²In an embodiment, the electrically conductive particles of the bed may ²comprise from 10 wt.% ²to 90 wt.% of electrically conductive particles different from silicon carbide ²particles based on ²the total weight of the electrically conductive particles of the bed; ²preferably, from 15 wt.% to ²95 wt.%, more preferably from 20 wt.% to 90 wt.%, even more preferably from 25 ²wt.% to 80²wt.% and most preferably from 30 wt.% to 75 wt.%.²However, it may be interesting to keep the content of electrically conductive ²particles different ²from silicon carbide particles quite low in the mixture. Thus, in an ²embodiment, the electrically ²conductive particles of the bed are or comprise a mixture of silicon carbide ²particles and ²electrically conductive particles different from silicon carbide particles and ²electrically²conductive particles of the bed comprises from 1 wt.% to 20 wt.% of ²electrically conductive²particles different from silicon carbide based on the total weight of the ²electrically conductive ²particles of the bed; preferably, from 2 wt.% to 15 wt.%, more preferably, ²from 3 wt.% to 10 ²wt.%, and even more preferably, from 4 wt.% to 8 wt.%.²For example, the electrically conductive particles of the bed are or comprise ²a mixture of silicon²carbide particles and particles different from silicon carbide particles and ²the said particles²different from silicon carbide particles are or comprise graphite particles.²Thus, in an embodiment, the electrically conductive particles are a ²combination of silicon ²carbide particles and graphite particles. Such electrically conductive ²particles, upon the ²electrification of the fluidized bed reactor, will heat up and because of ²their fluidification, will²CA 03184993 2023-1-4²<DP=37>²WO 2022 / 023346 37 ²PCT / EP2021 / 071011²contribute to the raise and / or to the maintaining of the temperature within ²the reactor. The ²Joule heating of graphite allows accelerating the heating of the reactant ²and / or of the other ²particles that are present within the fluidized bed reactor.²For example, graphite can be flake graphite. It is also preferable that the ²graphite has an²average particle size ranging from 1 to 400 pm as determined by sieving ²according to ASTM²D4513-11, preferably from 5 to 300 pm, more preferably ranging from 10 to 200 ²pm and most ²preferably ranging from 30 to 150 pm.²The presence of graphite particles in the bed allows applying the process ²according to the ²disclosure with or without the pre-heating step, preferably without the pre-²heating step. Indeed,²the graphite particles, upon the electrification of the fluidized bed reactor, ²will heat up and²because of their fluidification, will contribute to raising and / or maintaining ²the desired ²temperature within the reactor.²The silicon carbide particles ²For example, the silicon carbide is selected from sintered silicon carbide, ²nitride-bounded²silicon carbide, recrystallised silicon carbide, reaction bonded silicon ²carbide and any mixture²thereof.²Sintered SIC (SSiC) is a self-bonded material containing a sintering aid ²(typically boron) of ²less than 1% by weight.²Recrystallized silicon carbide (RSiC), a high purity SiC material sintered by ²the process of² evaporation - condensation without any additives.²Nitride-bonded silicon carbide (NBSC) is made by adding fine silicon powder ²with silicon ²carbide particles or eventually in the presence of a mineral additive and ²sintering in a nitrogen ²furnace. The silicon carbide is bonded by the silicon nitride phase (Si3N4) ²formed during ²nitriding.²Reaction bonded silicon carbide (RBSC), also known as siliconized silicon ²carbide or SiSiC,²is a type of silicon carbide that is manufactured by a chemical reaction ²between porous carbon ²or graphite with molten silicon. The silicon reacts with the carbon forming ²silicon carbide and ²bonds the silicon carbide particles. Any excess silicon fills the remaining ²pores in the body and ²produces a dense SiC-Si composite. Due to the left-over traces of silicon, ²reaction bonded²silicon carbide is often referred to as siliconized silicon carbide. The ²process is known²variously as reaction bonding, reaction sintering, self-bonding, or melt ²infiltration.²CA 03184993 2023-1-4²<DP=38>²WO 2022 / 023346 38 ²PCT / EP2021 / 071011²In general, high purity SiC particles have resistivity above 1000 Ohm.cm, ²whereas sintered, ²reaction bonded and nitride-bonded can exhibit resistivities of about 100 to ²1000 depending ²on the impurities in the SiC phase. Electrical resistivity of bulk ²polycrystalline SiC ceramics ²shows a wide range of resistivity depending on the sintering additive and heat-²treatment²conditions (Journal of the European Ceramic Society, Volume 35, Issue 15, ²December 2015,²Pages 4137; Ceramics International, Volume 46, Issue 4, March 2020, Pages ²5454). SiC ²polytypes with high purity possess high electrical resistivity (>106 ficm) ²because of their large ²bandgap energies. However, the electrical resistivity of SiC is affected by ²doping impurities. N ²and P act as n-type dopants and decrease the resistivity of SiC, whereas Al, ²B, Ga, and Sc²act as p-type dopants. SiC doped with Be, 0, and V are highly insulating. N is ²considered the²most efficient dopant for improving the electrical conductivity of SiC. For N ²doping of SiC (to ²decrease resistivity) Y203 and Y203-REM203 (REM, rare earth metal = Sm, Gd, ²Lu) have been ²used as sintering additives for efficient growth of conductive SiC grains ²containing N donors. ²N-doping in SiC grains was promoted by the addition of nitrides (AIN, BN, ²Si3N4, TIN, and ZrN)²or combinations of nitrides and Re203 (AIN¨REM203 (REM = Sc, Nd, Eu, Gd, Ho, ²and Er) or²TiN¨Y203).²The installation ²The terms "bottom" and "top" are to be understood in relation to the general ²orientation of the ²installation or the fluidized bed reactor. Thus, "bottom" will mean greater ²ground proximity²than "top" along the vertical axis. In the different figures, the same ²references designate²identical or similar elements.²Figure 1 illustrates a prior art fluidized bed reactor 1 comprising a reactor ²vessel 3, a bottom ²fluid nozzle 5 for the introduction of a fluidizing gas and a hydrocarbon ²feedstock, an optional²inlet 7 for the material loading, an optional outlet 9 for the material ²discharge and a gas outlet²11 and a bed 15. In the fluidized bed reactor 1 of figure 1 the heat is ²provided by preheating ²the feedstock by combustion of fossil fuels using heating means 17 arranged ²for example at ²the level of the line that provides the reactor with the fluidizing gas and ²the hydrocarbon ²feedstock.²The installation of the present disclosure is now described with reference to ²figures 2 to 5. ²For sake of simplicity, internal devices are known by the person in the art ²that are used in ²fluidized bed reactors, like bubble breakers, deflectors, particle termination ²devices, cyclones, ²ceramic wall coatings, thermocouples, etc... are not shown in the ²illustrations.² CA 03184993 2023-1-4²<DP=39>²WO 2022 / 023346 39 ²PCT / EP2021 / 071011²Figure 2 illustrates a first installation with a fluidized bed reactor 19 ²where the heating and ²reaction zone are the same. The fluidized bed reactor 19 comprises a reactor ²vessel 3, a ²bottom fluid nozzle 21 for the introduction of a fluidizing gas and a ²hydrocarbon feedstock, an ²optional inlet 7 for the material loading, an optional outlet 9 for the ²material discharge and a²gas outlet 11. The fluidized bed reactor 1 of figure 19 shows two electrodes ²13 submerged in²bed 25.²Figure 3 illustrates an embodiment wherein at least one fluidized bed reactor ²19 comprises a ²heating zone 27 and a reaction zone 29 with the heating zone 27 is the bottom ²zone and the²reaction zone 29 is on top of the heating zone 27. One or more fluid nozzles ²23 to provide a²hydrocarbon feedstock to the reaction zone from a distributor 33. As it can be ²seen in figure ²3, the one or more fluid nozzles 23 can be connected to a distributor 33 to ²distribute the ²hydrocarbon feedstock inside the bed 25.²Figure 4 illustrates an installation wherein at least one fluidized bed ²reactor 18 comprises at²least two lateral zones with the outer zone being the heating zone 27 and the ²inner zone ²being the reaction zone 29. The heated particles of the bed 25 from the outer ²zone are ²transferred to the inner zone by one or more openings 41 and mixed with the ²hydrocarbon ²feedstock and / or steam. At the end of the reaction zone the particles are ²separated from the²reaction product and transferred to the heating zone.²Figure 5 illustrates the installation that comprises at least two fluidized ²bed reactors (37, 39) ²connected one to each other wherein at least one fluidized bed reactor is the ²heating zone ²27 and one at least one fluidized bed reactor is the reaction zone 29.²The present disclosure provides for an installation to be used in a process to ²perform a steam ²cracking reaction, said installation comprises at least one fluidized bed ²reactor (18, 19, 37, ²39) comprising:²- at least two electrodes 13,²- a reactor vessel 3;²- one or more fluid nozzles (21, 23) for the introduction of a fluidizing ²gas and / or of a ²hydrocarbon feedstock within at least one fluidized bed reactor (18, 19, 37, ²39); and²- a bed 25 comprising particles;²wherein at least 10 wt.% of the particles of the bed based on the total weight ²of the particles²of the bed 25 are electrically conductive, have a resistivity ranging from ²0.001 Ohm.cm to 500²Ohm.cm at 800 C and are or comprise one or more selected from one or more ²metallic alloys, ²one or more non-metallic resistors, one or more metallic carbides, one or more ²transition²CA 03184993 2023-1-4²<DP=40>²WO 2022 / 023346 40 ²PCT / EP2021 / 071011²metal nitrides, one or more metallic phosphides, graphite, carbon black, one ²or more ²superionic conductors, one or more phosphate electrolytes, one or more mixed ²oxides being ²doped with one or more lower-valent cations, one or more mixed sulphides being ²doped with ²one or more lower-valent cations, and any mixture thereof.²In an embodiment, from 50 wt.% to 100 wt.% of the electrically conductive ²particles of the bed²based on the total weight of the electrically conductive particles of the bed ²are one or more ²selected from graphite, carbon black, one or more metallic alloys, one or more ²non-metallic ²resistors, one or more metallic carbides, one or more transition metal ²nitrides, one or more ²metallic phosphides, one or more superionic conductors, one or more phosphate ²electrolytes,²one or more mixed oxides being doped with one or more lower-valent cations, ²one or more²mixed sulphides being doped with one or more lower-valent cations, and any ²mixture thereof; ²preferably, from 60 wt.% to 100 wt.%; more preferably from 70 wt.% to 100 ²wt.%; even more ²preferably from 80 wt.% to 100 wt.% and most preferably from 90 wt.% to 100 ²wt.%.²For example, one electrode is a submerged central electrode or two electrodes ²13 are² submerged within the reactor vessel 3 of at least one reactor (18, 19, 37).²For example, the fluidizing gas is one or more diluent gases.²In a preferred embodiment, the at least one fluidized bed reactor (18, 19, 37, ²39) is devoid of ²heating means. For example, at least one fluidized bed reactor is devoid of ²heating means ²selected from ovens, gas burners, hot plates, or any combination thereof. For ²example, all the²fluidized bed reactors are devoid of heating means selected from ovens, gas ²burners, hot²plates, or any combination thereof. In a preferred embodiment, the at least ²one fluidized bed ²reactor comprising at least two electrodes and a bed comprising particles is ²devoid of packing.²For example, the reactor vessel 3 has an inner diameter of at least 100 cm, or ²at least 200 ²cm; or at least 400 cm. Such a large diameter allows to carry out the chemical ²reaction at an²industrial scale, for example at a weight hourly space velocity of said ²reaction stream²comprised between 0.1 h-1 and 100 h-1, preferably comprised between 1.0 h-1 ²and 50 h-1, more ²preferably comprised between 1.5 h-1 and 10 h-1, even more preferably ²comprised between ²2.0 h-1 and 6.0 h-1. The weight hourly space velocity is defined as the ratio ²of mass flow of the ²reaction stream to the mass of solid particulate material in the fluidized ²bed.²The at least one fluidized bed reactor (18, 19, 37) comprises at least two ²electrodes 13. For²example, one electrode is in electrical connection with the outer wall of the ²fluidized bed ²reactor, while one additional electrode is submerged into the fluidized bed ²25, or both ²electrodes 13 are submerged into the fluidized bed 25. Said at least two ²electrodes 13 are ²electrically connected and can be connected to a power supply (not shown). It ²is advantageous²CA 03184993 2023-1-4²<DP=41>²WO 2022 / 023346 41 ²PCT / EP2021 / 071011²that said at least two electrodes 13 are made of graphite. The person skilled ²in the art will have ²an advantage that the electrodes 13 are more conductive than the particle bed ²25.²For example, at least one electrode 13 is made of or comprises graphite; ²preferably, all or the ²two electrodes 13 are made of graphite. For example, one of the electrodes is ²the reactor²vessel, so that the reactor comprises two electrodes, one being the submerged ²central²electrode and one being the reactor vessel 3.²For example, the at least one fluidized bed reactor comprises at least one ²cooling device ²arranged to cool at least one electrode.²During use of the fluidized bed reactor, an electric potential of at most 300 ²V is applied,²preferably at most 250 V, more preferably at most 200 V, even more preferably ²at most 150²V, most preferably at most 100 V, even most preferably at most 90 V, or at ²most 80 V.²Thanks to the fact that the power of the electric current can be tuned, it is ²easy to adjust the ²temperature within the reactor bed.²The reactor vessel 3 can be made of graphite. In an embodiment, it can be made ²of electro-²resistive material that is silicon carbide or a mixture of silicon carbide and ²graphite.²With preference, the reactor vessel 3 comprises a reactor wall made of ²materials that are ²corrosion-resistant materials and advantageously said reactor wall materials ²comprise nickel ²(Ni), SiAION ceramics, yttria-stabilized zirconia (YSZ), tetragonal ²polycrystalline zirconia ²(TZP) and / or tetragonal zirconia polycrystal (TPZ). SiAION ceramics are ²ceramics based on²the elements silicon (Si), aluminium (Al), oxygen (0) and nitrogen (N). They ²are solid solutions²of silicon nitride (Si3N4), where Si¨N bonds are partly replaced with Al¨N and ²Al-0 bonds.²For example, the reactor vessel 3 is made of an electro-resistive material ²that is a mixture of ²silicon carbide and graphite; and the electro-resistive material of the ²reactor vessel 3 ²comprises from 10 wt.% to 99 wt.% of silicon carbide based on the total weight ²of the electro-²resistive material; preferably, from 15 wt.% to 95 wt.%, more preferably from ²20 wt.% to 90²wt.%, even more preferably from 25 wt.% to 80 wt.% and most preferably from 30 ²wt.% to 75 ²wt.%.²For example, the reactor vessel 3 is made of an electro-resistive material ²that is a mixture of ²silicon carbide and graphite.²For example, the reactor vessel 3 is not conductive. For example, the reactor ²vessel 3 is made²of ceramic.²CA 03184993 2023- 1-4²<DP=42>²WO 2022 / 023346 42 ²PCT / EP2021 / 071011²For example, the at least one fluidized bed reactor (18, 19, 37, 39) comprises ²a heating zone ²27 and a reaction zone 29, one or more fluid nozzles 21 to provide a ²fluidizing gas to at least ²the heating zone from a distributor 31, one or more fluid nozzles 23 to ²provide a hydrocarbon ²feedstock to the reaction zone from a distributor 33, and means 41 to ²transport the particles²from the heating zone 27 to the reaction zone 29 when necessary, and optional ²means 35 to²transport the particles from the reaction zone 29 back to the heating zone 27.²For example, as illustrated in figure 3, the at least one fluidized bed ²reactor is a single one ²fluidized bed reactor 19 wherein the heating zone 27 is the bottom part of the ²fluidized bed ²reactor 19 while the reaction zone 29 is the top part of the fluidised bed ²reactor 19; with²preference, the installation comprises one or more fluid nozzles 23 to inject ²a hydrocarbon²feedstock between the two zones (27, 29) or in the reaction zone 29. The ²fluidized bed reactor ²19 further comprises optionally an inlet 7 for the material loading, ²optionally an outlet 9 for the ²material discharge and a gas outlet 11. With preference, the fluidized bed ²reactor 19 is devoid ²of heating means. For example, the electrodes 13 are arranged at the bottom ²part of the²fluidized bed reactor 19, i.e. in the heating zone 27. For example, the top ²part of the fluidised²bed reactor 19, i.e. the reaction zone 29, is devoid of electrodes. ²Optionally, the fluidized bed ²reactor 19 comprises means 35 to transport the particles from the reaction ²zone 29 back to ²the heating zone 27; such as by means of a line arranged between the top part ²and the bottom ²part of the fluidized bed reactor 19.²For example, as illustrated in figure 4, the installation comprises at least ²two lateral fluidized²bed zones (27, 29) connected one to each other wherein at least one fluidized ²bed zone 27 is ²the heating zone and at least one fluidized bed zone 29 is the reaction zone. ²For example, the ²heating zone 27 is surrounding the reaction zone 29. With preference, the ²installation ²comprises one or more fluid nozzles 23 arranged to inject a hydrocarbon ²feedstock and / or²steam to the at least one reaction zone 29 by means of a distributor 33. The ²fluidized bed²zones (27, 29) further comprise optionally an inlet 7 for the material loading ²and a gas outlet ²11. With preference, the at least one fluidized bed zone being the heating ²zone 27 and / or the ²at least one fluidized bed zone being the reaction zone 29 is devoid of ²heating means. For ²example, the at least one fluidized bed zone being the reaction zone 29 shows ²optionally an²outlet 9 for the material discharge. One or more fluid nozzles 21 provide a ²fluidizing gas to at²least the heating zone from a distributor 31. With one or more inlet devices ²41, heated particles ²are transported from the heating zone 27 to the reaction zone 29, and with one ²or more means ²comprising downcomers, the separated particles are transported from the ²reaction zone ²29 back to the heating zone 27. The fluidization gas for the heating zone 27 ²can be an inert²35 diluent, like one or more selected from steam, hydrogen, carbon dioxide, ²methane, argon,²CA 03184993 2023-1-4²<DP=43>²WO 2022 / 023346 43 ²PCT / EP2021 / 071011²helium and nitrogen. In such a configuration the fluidization gas for the ²heating zone can also ²comprise air or oxygen to burn deposited coke from the particles.²For example, as illustrated in figure 5, the installation comprises at least ²two fluidized bed ²reactors (37, 39) connected one to each other wherein at least one fluidized ²bed reactor 37 is²the heating zone 27 and at least one fluidized bed reactor 39 is the reaction ²zone 29. With²preference, the installation comprises one or more fluid nozzles 23 arranged ²to inject a ²hydrocarbon feedstock and / or steam to the at least one fluidized bed reactor ²39 being the ²reaction zone 29. The fluidized bed reactors (37, 39) further comprise ²optionally an inlet 7 for ²the material loading and a gas outlet 11. With preference, the at least one ²fluidized bed reactor²37 being the heating zone 27 and / or the at least one fluidized bed reactor 39 ²being the reaction²zone 29 is devoid of heating means. For example, the at least one fluidized ²bed reactor 39 ²being the reaction zone 29 shows optionally an outlet 9 for the material ²discharge. By means ²of the inlet device 41, heated particles are transported from the heating zone ²27 to the reaction ²zone 29 when necessary, and by means of device 35, the separated particles ²after the reaction²zone are transported from the reaction zone back to the heating zone. The ²fluidization gas for²the heating zone can be an inert diluent, like one or more selected from ²steam, hydrogen, ²carbon dioxide, methane, argon, helium, and nitrogen. In such a configuration ²the fluidization ²gas for the heating zone can also comprise air or oxygen to burn deposited ²coke from the ²particles.²For example, the at least one fluidized bed reactor 37 being the heating zone ²27 comprises at²least two electrodes 13 whereas the at least one fluidized bed reactor 39 ²being the reaction ²zone 29 is devoid of electrodes.²For example, the at least two fluidized bed reactors (37, 39) are connected ²one to each other ²by means 41 suitable to transport the particles from the heating zone 27 to ²the reaction zone² 29, such as one or more lines_²For example, the at least two fluidized bed reactors (37, 39) are connected ²one to each other ²by means 35 suitable to transport the particles from the reaction zone 29 back ²to the heating ²zone 27, such as one or more lines.² The steam cracking reaction ²In one embodiment, the steam cracking reaction does not require any catalytic ²composition. ²For example, the said steam cracking reaction is conducted at a temperature ²ranging between ²500 C and 1200 C, preferably between 700 C and 1000 C.²CA 03184993 2023- 1-4²<DP=44>²WO 2022 / 023346 44 ²PCT / EP2021 / 071011²For example, the said steam cracking reaction is performed at a pressure ²ranging between ²0.1 MPa and 1.0 MPa, preferably between 0.1 MPa and 0.5 MPa.²For example, the said steam cracking reaction is conducted in presence of a ²reaction stream ²and is performed at a weight hourly space velocity of said reaction stream ²comprised between²0.1 h-1 and 100 h-1, preferably comprised between 1.0 h-1 and 50 h-1, more ²preferably²comprised between 1.5 h-1 and 10 h-1, even more preferably comprised between ²2.0 h-1 and ²6.0 h-1.²The residence time of the hydrocarbon feedstock in the fluidised bed section ²of the reactor ²where the temperature is between 500 and 1200 C, may advantageously range from ²0.005 to²1.0 seconds, preferably from 0.01 to 0.6 seconds, more preferably from 0.1 to ²0.3 seconds.²Such low residence time is advantageous to avoid secondary reactions and thus ²to prevent ²the formation and deposition of coke.²CA 03184993 2023- 1-4²

Claims

<DP=1>²WO 2022 / 023346 45 ²PCT / EP2021 / 071011²Claims²1. A process to perform steam cracking reaction of hydrocarbons having at ²least two ²carbons, said process comprising the steps of:²a) providing at least one fluidized bed reactor comprising at least two ²electrodes²and a bed comprising particles;²b) putting the particles of the bed in a fluidized state by passing upwardly ²through²the said bed a fluid stream, to obtain a fluidized bed; and²c) heating the fluidized bed to a temperature ranging from 500 C to 1200 C to² conduct the steam cracking reaction of a hydrocarbon feedstock;²characterized in that at least 10 wt.% of the particles based on the total ²weight of the ²particles of the bed are electrically conductive particles and have a ²resistivity ranging ²from 0.001 Ohm.cm to 500 Ohm.cm at 800 C; in that the step c) of heating the ²fluidized bed is performed by passing an electric current through the ²fluidized bed; and²in that the electrically conductive particles of the bed comprise one or more ²selected²from graphite, carbon black, one or more metallic alloys, one or more non-²metallic ²resistors, one or more metallic carbides, one or more transition metal ²nitrides, one or ²more metallic phosphides, one or more superionic conductors, one or more ²phosphate ²electrolytes, one or more mixed oxides being doped with one or more lower-²valent²cations, one or more mixed sulphides being doped with one or more lower-valent²cations, and any mixture thereof.²2. The process of claim 1, characterized in that from 50 wt.% to 100 wt.% of ²the ²electrically conductive particles of the bed based on the total weight of the ²electrically ²conductive particles of the bed are one or more selected from graphite, carbon ²black,²one or more metallic alloys, one or more non-metallic resistors, one or more ²metallic²carbides, one or more transition metal nitrides, one or more metallic ²phosphides, one ²or more superionic conductors, one or more phosphate electrolytes, one or more ²mixed ²oxides being doped with one or more lower-valent cations, one or more mixed ²sulphides being doped with one or more lower-valent cations, and any mixture ²thereof.²3. The process of claim 1 or 2, characterized in that said process further ²comprises a ²step d) of recovering the cracking products of the reaction.²4. The process according to any one of claims 1 to 3, characterized in that ²the electrically²conductive particles of the bed are or comprise one or more selected from one ²or more²metallic alloys, one or more non-metallic resistors, one or more metallic ²carbides, one²CA 03184993 2023- 1- 4²<DP=2>²WO 2022 / 023346 46 ²PCT / EP2021 / 071011²or more transition metal nitrides, one or more metallic phosphides, one or ²more ²superionic conductors, one or more phosphate electrolytes, one or more mixed ²oxides ²being doped with one or more lower-valent cations, one or more mixed sulphides ²being ²doped with one or more lower-valent cations, and any mixture thereof.²5. The process according to any one of claims 1 to 4, characterized in that ²the electrically ²conductive particles of the bed are or comprise one or more non-metallic ²resistors ²selected from silicon carbide, molybdenum disilicide or a mixture thereof.²6. The process according to any one of claims 1 to 5, characterized in that ²the electrically²conductive particles of the bed are or comprise a mixture of a non-metallic ²resistor ²being silicon carbide and electrically conductive particles different from ²silicon carbide.²7. The process according to claim 6, characterized in that the electrically ²conductive²particles of the bed comprise from 10 wt.% to 99 wt.% of silicon carbide based ²on the²total weight of the electrically conductive particles of the bed.²8. The process according to claim 6 or 7, characterized in that the said ²electrically ²conductive particles different from silicon carbide are or comprise graphite ²and / or² carbon black.²9. The process according to any one of claims 6 to 8, characterized in that ²the said ²electrically conductive particles different from silicon carbide are or ²comprise one or ²more mixed oxides being doped with one or more lower-valent cations.²10. The process according to any one of claims 6 to 9, characterized in that ²the said ²electrically conductive particles different from silicon carbide are or ²comprise one or ²more mixed sulphides being doped with one or more lower-valent cations.²11. The process according to any one of claims 1 to 10, characterized in that ²the²electrically conductive particles of the bed are or comprise one or more mixed ²oxides ²being doped with one or more lower-valent cations.²12. The process according to claim 11, characterized in that the mixed oxides ²are selected²from one or more oxides having a cubic fluorite structure being at least ²partially²substituted with one or more lower-valent cations.²CA 03184993 2023- 1- 4²<DP=3>²WO 2022 / 023346 47 ²PCT / EP2021 / 071011²13. The process according to claim 12, characterized in that said one or more ²lower-valent ²cations are selected from Sm, Gd, Y, Sc, Yb, Mg, Ca, La, Dy, Er, Eu.²14. The process according to any one of claims 11 to 13, characterized in that ²the mixed²oxides are selected from one or more AB03-perovskites with A and B tri-valent ²cations,²being at least partially substituted in A position with one or more lower-²valent cations, ²and comprising at least one of Ni, Ga, Co, Cr, Mn, Sc, Fe and / or a mixture ²thereof in ²B position.²15. The process according to claim 14, characterized in that said one or more ²lower-valent²cations are selected from Ca, Sr or Mg.²16. The process according to any one of claims 11 to 15, characterized in that ²the mixed ²oxides are selected from one or more AB03-perovskites with A bivalent cation ²and B²tetra-valent cation, being at least partially substituted with one or more ²lower-valent²cations in the B position or with a mixture of different B elements in the B ²position.²17. The process according to claim 16, characterized in that said one or more ²lower-valent ²cations are selected from Mg, Sc, Y, Nd or Yb.²18. The process according to any one of claims 11 to 17, characterized in that ²the mixed ²oxides are selected from one or more A2B207-pyrochlores with A trivalent ²cation and ²B tetra-valent cation being at least partially substituted in A position with ²one or more ²lower-valent cations and comprising at least one of Sn, Zr and Ti in B ²position.²19. The process according to claim 18, characterized in that said one or more ²lower-valent ²cations are selected from Ca or Mg.²20. The process according to any one of claims 1 to 19, characterized in that ²the²electrically conductive particles of the bed are or comprise one or more ²metallic alloys.²21. The process according to any one of claims 1 to 20, characterized in that ²the ²electrically conductive particles of the bed are or comprise one or more ²superionic ²conductors.² CA 03184993 2023- 1- 4²<DP=4>²WO 2022 / 023346 48 ²PCT / EP2021 / 071011²22. The process according to claim 21, characterized in that the one or more ²superionic ²conductors are selected frorn LiAlSiO4, LiloGeP2S12, 1_13.6Sio.6Po.404, sodium ²superionic ²conductors, or sodiurn beta alumina.²23. The process according to any one of claims 1 to 22, characterized in that ²hydrocarbon ²feedstock is selected from ethane, liquefied petroleum gas, naphtha, gasoils ²and / or ²whole crude oil.²24. The process according to any one of claims 1 to 23, characterized in that ²the cracking²products include one or more of ethylene, propylene and benzene.²25. The process according to claim 24, characterized in that the cracking ²products further ²include one or more of hydrogen, toluene, xylenes, and 1,3-butadiene.²26. The process according to any one of clairns 1 to 25, characterized in that ²the fluid²strearn provided in step b) comprises a hydrocarbon feedstock.²27. The process according to any one of claims 1 to 26, characterized in that ²said process ²comprises a step of pre-heating with a gaseous stream said fluidized bed ²reactor²before conducting said steam cracking reaction in the fluidized bed reactor.²28. The process according to claim 27, characterized in that said gaseous ²stream is a ²stream of inert gas.²29. The process according to claim 27 or 28, characterized in that said ²gaseous stream²has a temperature comprised between 500 C and 1200 C.²30. The process according to any one of claims 1 to 29, characterized in that, ²the at least ²one fluidized bed reactor provided in step a) comprises a heating zone and a ²reaction²zone, the fluid stream provided in step b) is provided to the heating zone and ²comprises²diluent gases, and the step c) of heating the fluidized bed to a temperature ²ranging ²from 500 C to 1200 C to conduct the steam cracking reaction of a hydrocarbon ²feedstock comprises the following sub-steps:²- heating the fluidized bed to a temperature ranging from 500 C to 1200 C ²by²passing an electric current through the heating zone of the at least one ²fluidized²bed,²- transporting the heated particles from the heating zone to the reaction ²zone,²CA 03184993 2023- 1- 4²<DP=5>²WO 2022 / 023346 49 ²PCT / EP2021 / 071011²- ² in the reaction zone, putting the heated particles in a fluidized state ²by passing²upwardly through the said bed of the reaction zone a fluid stream comprising a ²²hydrocarbon feedstock and optional diluent gases to obtain a fluidized bed and ²²to conduct the steam cracking reaction on the hydrocarbon feedstock.²31. The process according to claim 30, characterized in that the step c) of ²heating the ²fluidized bed to a temperature ranging from 500 C to 1200 C to conduct the ²steam ²cracking reaction of a hydrocarbon feedstock further comprises the sub-step of ²²recovering the particles from the reaction zone and recycling them to the ²heating zone.²32. An installation to perform steam cracking reaction in a process according ²to any one ²of claims 1 to 31, said installation comprises at least one fluidized bed ²reactor (18, 19, ²37, 39) comprising²- at least two electrodes (13);² - a reactor vessel (3);²- one or more fluid nozzles (21; 23) for the introduction of a fluidizing ²gas and / or of ²a hydrocarbon feedstock within at least one fluidized bed reactor (18, 19, 37, ²39); ²and²- a bed (25) comprising particles;²the installation is characterized in that at least 10 wt.% of the particles of ²the bed (25)²based on the total weight of the particles of the bed are electrically ²conductive, have a ²resistivity ranging from 0.001 Ohm.cm to 500 Ohm.cm at 800 C and are one or ²more ²selected from graphite, carbon black, one or more metallic alloys, one or more ²non-²rnetallic resistors, one or more metallic carbides, one or more transition ²metal nitrides,²one or more metallic phosphides, one or more superionic conductors, one or ²more²phosphate electrolytes, one or more mixed oxides being doped with one or more ²lower-²valent cations, one or more mixed sulphides being doped with one or more lower-²²valent cations, and / or any mixture thereof.²33. The installation according to claim 32, characterized in that at least one ²fluidized bed²reactor (18, 19, 37, 39) is devoid of heating means.²34. The installation according to claim 32 or 33 to perform steam cracking ²reaction in a ²process according to claim 28 or 29, characterized in that the at least one ²fluidized bed²reactor (18, 19, 37, 39) comprises a heating zone (27) and a reaction zone ²(29), one²or more fluid nozzles (23) to provide a hydrocarbon feedstock to the reaction ²zone ²(29).²CA 03184993 2023-1-4²<DP=6>²WO 2022 / 023346 50 ²PCT / EP2021 / 071011²35. The installation according to claim 34, characterized in that the at least ²one fluidized ²bed reactor (18, 19, 37, 39) further comprises means (35) to transport the ²particles of ²the bed (25) frorn the reaction zone (29) back to the heating zone (27).²36. The installation according to claim 34 or 35, characterized in that it ²comprises at least ²two fluidized bed reactors (37, 39) connected one to each other wherein at ²least one ²reactor (37) is the heating zone (27) and at least another reactor (39) is the ²reaction ²zone (29).²37. The installation according to claim 36, characterized in that the ²installation comprises ²means (23) arranged to inject a hydrocarbon feedstock to the at least one ²fluidized bed ²reactor (39) being the reaction zone (29).²38. The installation according to claim 36 or 37, characterized in that the ²installation²comprises means (41) to transport the particles of the bed (25) from the ²heating zone ²(27) to the reaction zone (29).²39. The installation according to claim 34 or 35, characterized in that the at ²least one²fluidized bed reactor (19) is a single one fluidized bed reactor wherein the ²heating zone²(27) is the bottom part of the fluidized bed reactor (19) while the reaction ²zone (29) is ²the top part of the fluidised bed reactor (19).²40. The installation according to claim 34 or 35, characterized in that the at ²least one²fluidized bed (18) comprises at least two lateral zones being an outer zone ²and an²inner zone wherein the outer zone is surrounding the inner zone, with the ²outer zone ²being the heating zone (27) and the inner zone being the reaction zone (29).²41. Use of a bed (25) comprising particles to perform a process in at least ²one fluidized²bed reactor (18, 19, 37, 39) of steam cracking of hydrocarbons having at least ²two²carbons according to any one of claims 1 to 31, the use is characterized in ²that at least ²10 wt.% of the particles of the bed (25) based on the total weight of the ²particles of the ²bed are electrically conductive, have a resistivity ranging from 0.001 Ohm.cm ²to 500 ²Ohm.cm at 800 C and are one or more selected from graphite, carbon black, one ²or²more metallic alloys, one or more non-metallic resistors, one or more metallic ²carbides,²one or more transition metal nitrides, one or more metallic phosphides, one or ²more ²superionic conductors, one or more phosphate electrolytes, one or more mixed ²oxides²CA 03184993 2023-1-4²<DP=7>²WO 2022 / 023346 51 ²PCT / EP2021 / 071011²being doped with one or more lower-valent cations, one or more mixed sulphides ²being ²doped with one or more lower-valent cations, and any mixture thereof.²42. The use of an installation comprising at least one fluidized bed reactor ²(18, 19, 37, 39)²to perform a steam cracking reaction, characterized in that the installation ²is according ²to any one of claims 32 to 40.²CA 03184993 2023- 1- 4²