A manufacturing process for a free reflective mirror applied to a HUD

By optimizing parameters such as temperature and pressure, and combining the coating process of SiO2 and Al layers, the problem of insufficient quality inspection of the reflector was solved, and high-precision image display effect was achieved.

CN112848425BActive Publication Date: 2026-11-20NINGBO JINHUI OPTICAL TECHNOLOGY CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202011632622.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-12-31
Publication Date
2026-11-20
Estimated Expiration
2040-12-31

AI Technical Summary

Technical Problem

In existing HUD display technologies, insufficient quality testing of reflectors leads to poor image accuracy and quality, especially since indicators such as the reflector's dimensions, surface, PV (photovoltaic particle size), color reflectance, and adhesion have not been effectively controlled.

Method used

A manufacturing process is employed, including steps such as base material drying, injection molding, edge trimming of semi-finished products, coating, and inspection. By controlling the combination of temperature, pressure, and coating layers, the forming quality of the reflector and the stability of the coating layer are improved, thereby ensuring image quality.

Benefits of technology

It improves the surface adhesion and coating stability of the reflector, increases the reflector's wear resistance and service life, ensures image clarity and distortion-free image, and improves the product qualification rate.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112848425B_ABST
    Figure CN112848425B_ABST
Patent Text Reader

Abstract

The application discloses a manufacturing process of a free reflecting mirror applied to a HUD, and comprises the following steps: S1, providing a base material; S2, baking the base material; S3, forming injection molding; S4, removing edges of a semi-finished base body; S5, coating the semi-finished base body; and S6, detecting the finished base body.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of head-up display technology, and more specifically to a manufacturing process for a free-reflecting mirror used in HUDs. Background Technology

[0002] A HUD (Heads-Up Display) is a head-up display system that uses optical reflection to project important driving information onto the windshield, such as vehicle speed, mileage, navigation information, and driver assistance information.

[0003] One existing HUD display technology projects an image onto the windshield directly from a projection device. To prevent the image from distorting on the windshield, a reflector array is needed between the windshield and the projection device to correct the image. To ensure image accuracy and quality, the quality of the reflector is particularly important, especially the need to test the product's dimensions, surface, face shape, PV, color reflectance, adhesion, and RMS. Summary of the Invention

[0004] In view of the shortcomings of the existing technology, the purpose of this invention is to provide a manufacturing process for a free-form reflector for use in HUD, thereby improving the quality of reflector molding and ensuring the image quality of the vehicle head-up display.

[0005] The above-mentioned technical objective of the present invention is achieved through the following technical solution: a manufacturing process for a free-reflecting mirror applied to a HUD, the manufacturing process comprising the following steps:

[0006] S1: Provide base material, control the ambient temperature and dust-free level of base material storage, and clean the packaging surface;

[0007] S2: Base material drying. The base material is placed in a drying equipment and continuously dried to remove the surface moisture of the base material. The drying temperature and drying time are controlled and multiple base materials are circulated for drying.

[0008] S3: Molding injection molding, pre-set the pressure inside the mold cavity, and control the injection temperature of the upper mold and the lower mold respectively. The molten base material is input into the mold cavity, and after the semi-finished product is formed, it is squeezed out of the mold core and cooled. After demolding, the semi-finished product is taken out.

[0009] S4: Remove the edges of the semi-finished substrate. Set up tooling fixtures and control the milling cutter feed rate and speed to remove the glue edges after demolding the semi-finished product.

[0010] S5: Semi-finished product substrate coating, setting up coating fixtures to form a coating layer on the effective mirror surface of the semi-finished product, performing resist coating treatment on the outside of the effective mirror surface of the finished product, and taking out the finished product after coating is completed. The coating layer includes a SiO2 layer, an Al layer, and a SiO2 layer that are sequentially covered from the inside to the outside.

[0011] S6: Finished product substrate inspection, including dimensional data inspection, surface inspection, surface PV inspection, color reversibility inspection, adhesion and RMS inspection. If the inspection is qualified, protective treatment will be carried out.

[0012] Furthermore, in step S2, the drying time of the base material is controlled to be greater than 4 hours and the drying temperature is 125°C. The drying is carried out in a cycle within 24 hours to ensure that each base material is dry and free of moisture, avoid the formation of bubbles in the semi-finished base material, increase the surface area of ​​the base material, and ensure the water absorption rate and external cleanliness of the base material.

[0013] Furthermore, in step S2, the positive and negative deviation of the drying temperature of the base material is controlled within 0.5℃.

[0014] Furthermore, in step S3, an optical screw is used for feeding between the upper and lower molds. The optical screw includes a feeding section, at least one compression section, and a homogenization section. The temperature of the feeding section is controlled at 50°C, the temperature of the compression section is controlled at 290°C, and the temperature of the homogenization section is controlled at 280°C, so that the base material is released more fully, so that the surface shape of the semi-finished substrate meets the requirement of PV < 50μm.

[0015] Furthermore, the compression section includes a first compression section, a second compression section, and a third compression section, and the material feeding ratios of the first compression section, the second compression section, and the third compression section increase sequentially. Preferably, the material feeding ratio of the first compression section is 10%, the material feeding ratio of the second compression section is 11.8%, the material feeding ratio of the third compression section is 14.4%, and the material feeding ratio of the homogenization section is 16.2%.

[0016] Furthermore, between steps S3 and S4, the process includes: transferring the semi-finished substrate. A production line and a robotic arm are installed between the injection molding station and the semi-finished product trimming station. The robotic arm picks up the semi-finished substrate and places it onto the production line. The production line is equipped with an anti-static device, and a protective film is applied to the surface of the semi-finished substrate after passing through the anti-static device. These improvements prevent dust from adhering to the surface of the semi-finished product, improve surface accuracy, and reduce static electricity on the surface of the semi-finished substrate.

[0017] Furthermore, step S4 also includes a semi-finished product dust removal process. An air blowing device and a dust suction device are set on one side of the tooling fixture and facing the milling cutter. The air blowing device and the dust suction device are arranged opposite each other on both sides of the milling cutter and operate simultaneously. The air blowing device continuously blows air during the process of the milling cutter removing burrs, thereby effectively reducing the temperature of the milling cutter and preventing burrs from sticking to the tool, so that the surface cut of the semi-finished product substrate is smooth. At the same time, the dust suction device is on the other side of the milling cutter relative to the air blowing device, thereby effectively cleaning the burrs removed by the milling cutter, keeping the product surface clean, and thus controlling the surface shape PV accuracy of the mirror.

[0018] Furthermore, the semi-finished product station is provided with a Y-axis slide rail and an X-axis slide rail located above the Y-axis slide rail. The X-axis slide rail is provided with a Z-axis slide rail, and a vertical milling cutter head is provided on the Z-axis slide rail. The tooling fixture is located on the Y-axis slide rail.

[0019] The semi-finished product substrate is provided with a plurality of limb ends, and the tooling fixture includes a lower template and an upper template for forming the semi-finished product mold cavity, and the connection position between the limb ends corresponding to the lower template and the semi-finished product substrate is provided with an opening for inserting a milling cutter.

[0020] The Y-axis slide rail is also provided with positioning cylinders on both sides, and the output end of the positioning cylinder is provided with a pressure plate for pressing the tooling fixture.

[0021] The coating fixture includes a coating base plate and four coating pressure plates. The coating base plate is adapted to the contour of the semi-finished substrate, and the coating pressure plates are pressed onto the outer contour of the semi-finished substrate and expose an effective mirror surface for coating.

[0022] Furthermore, step S5 also includes a coating pretreatment. Before loading the coating fixture, the surface of the protective film is cleaned with a dust-free ion air gun, the protective film is removed, and the surface of the semi-finished product is baked to eliminate internal stress, improve the surface properties of the substrate, and increase the bonding and adhesion between the coating layer and the surface of the semi-finished product substrate.

[0023] In step S5, the SiO2 layer is sputtered onto the semi-finished product substrate by positive and negative electrode electro-ionization vacuum sputtering, and the Al layer is sputtered onto the product surface by current-excited molecularization vacuum sputtering. Preferably, the surface of the semi-finished product substrate is activated before coating. Optionally, oxygen is introduced and activated for 80-100 seconds.

[0024] Furthermore, in step S6, the protective treatment refers to packaging the finished product into an anti-static blister box.

[0025] Compared with the prior art, the present invention has the following advantages and beneficial effects: baking the material before injection molding of the semi-finished substrate improves the adhesion of the semi-finished substrate surface, improves the coating quality and coating layer stability of the reflector surface, and effectively increases the wear resistance and service life of the reflector.

[0026] By controlling the upper and lower molds of the molding machine with two sets of high-temperature mold temperature controllers, the surface shape change of the semi-finished substrate can be controlled, thereby controlling the curvature and fullness of the finished mirror surface.

[0027] In the coating station, a SiO2 layer is deposited on the substrate surface to increase reflectivity. Another SiO2 layer is deposited on the outermost layer of the substrate to increase surface adhesion. This ensures that both the inner and outer surfaces of the intermediate Al layer are coated with SiO2, making the layers more robust, reducing the internal stress of the reflector, and increasing the bonding and adhesion between the coating layer and the surface of the semi-finished substrate.

[0028] The optical screw adopts multi-segment heating, using different heating temperatures for different segments, which saves costs, improves product quality, and results in a stable and high-precision semi-finished substrate. This ensures the surface accuracy and reflectivity of the mirror, which helps improve the quality and clarity of the generated image, ensuring that the image is free from distortion, black and white spots, fog, and other appearance defects, thereby increasing the product qualification rate. Attached Figure Description

[0029] Figure 1 This is a schematic diagram of the process flow of the present invention;

[0030] Figure 2 This is a schematic diagram of the coating process of the present invention;

[0031] Figure 3 This is a schematic diagram showing the fit between the coating tooling and the semi-finished substrate of the present invention;

[0032] Figure 4 This is a schematic diagram of the structure of the coating layer and the substrate of the present invention;

[0033] Figure 5 This is a schematic diagram of the optical screw structure of the present invention;

[0034] Figure 6 This is a schematic diagram of the semi-finished product edge removal station of the present invention;

[0035] Figure 7 This is a schematic diagram of the tooling fixture of the present invention;

[0036] Figure 8 This is a schematic diagram illustrating the fit between the lower template and the semi-finished substrate of the present invention;

[0037] In the diagram: 1. Semi-finished substrate; 1.1. Limb; 2. Tooling fixture; 2.1. Upper template; 2.2. Lower template; 2.3. Opening; 3. Milling cutter; 4. Coating fixture; 4.1. Coating pressure plate; 4.2. Coating base plate; 5. SiO2 layer; 6. Al layer; 7. Optical screw; 7.1. Feeding section; 7.2. First compression section; 7.3. Second compression section; 7.4. Third compression section; 7.5. Homogenization section; 8. Static eliminator; 9. Air blowing device; 10. Dust collection device; 11. X-axis slide rail; 12. Y-axis slide rail; 13. Z-axis slide rail; 14. Positioning cylinder; 15. Pressure plate; Detailed Implementation

[0038] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0039] It should be understood that although the terms upper, middle, lower, top, one end, etc., appear in this document to describe various elements, these elements are not limited by these terms. These terms are only used to distinguish the elements from each other for ease of understanding, and are not used to define any directional or sequential restrictions.

[0040] like Figure 1-8 As shown, a manufacturing process for a free-floating mirror used in a HUD includes the following steps:

[0041] S1: Provide base material, control the ambient temperature and dust-free level of base material storage, and clean the packaging surface;

[0042] S2: Base material drying. The base material is placed in a drying equipment and continuously dried to remove the surface moisture of the base material. The drying temperature and drying time are controlled and multiple base materials are circulated for drying.

[0043] S3: Molding injection, pre-set the pressure inside the mold cavity, and control the injection temperature of the upper mold and the lower mold respectively. The molten base material is input into the mold cavity. After the semi-finished product is formed, the mold core is squeezed and cooled. After demolding, the semi-finished product is taken out. Optionally, the injection temperature of the upper mold is controlled at 290℃, and the injection temperature of the lower mold is controlled at 250 to 280℃.

[0044] S4: Remove the edges of the semi-finished substrate 1, set up the tooling fixture 2 and control the feed rate and speed of the milling cutter 3 to remove the glue edge after demolding the semi-finished product;

[0045] S5: The semi-finished substrate 1 is coated. A coating fixture 4 is set up to form a coating layer on the effective mirror surface of the semi-finished product. A resist coating treatment is performed on the outside of the effective mirror surface of the finished product. After the coating is completed, the finished product is taken out. The coating layer includes SiO2 layer 5, Al layer 6 and SiO2 layer 5 covered from the inside to the outside. The film formation time is controlled at 22s.

[0046] S6: Finished product substrate inspection, including dimensional data inspection, surface inspection, surface PV inspection, color reversibility inspection, adhesion and RMS inspection. If the inspection is qualified, protective treatment will be carried out. The inspection can be carried out by a mirror surface inspection device, a mirror size inspection device, a surface PV inspection device, a color reversibility inspection device, an adhesion inspection device and an RMS inspection device.

[0047] Specifically, in step S2, the drying time of the base material is controlled to be greater than 4 hours and the drying temperature is 125°C. The drying is carried out in a cycle within 24 hours to ensure that each base material is dry and free of moisture, avoid the appearance of bubbles in the semi-finished base 1, increase the surface area of ​​the base, and ensure the water absorption rate and external cleanliness of the base.

[0048] Specifically, in step S2, the positive or negative deviation of the drying temperature of the base material is controlled within 0.5℃.

[0049] Specifically, in step S3, an optical screw 7 is used for feeding between the upper and lower molds. The optical screw 7 includes a feeding section 7.1, at least one compression section, and a homogenization section 7.5. The temperature of the feeding section 7.1 is controlled at 50°C, the temperature of the compression section is controlled at 290°C, and the temperature of the homogenization section 7.5 is controlled at 280°C, so that the base material is released more fully, so that the surface shape of the semi-finished substrate 1 meets the requirement of PV < 50μm.

[0050] Specifically, the compression section includes a first compression section 7.2, a second compression section 7.3, and a third compression section 7.4, and the material feeding ratios of the first compression section 7.2, the second compression section 7.3, and the third compression section 7.4 increase sequentially. Preferably, the material feeding ratio of the first compression section 7.2 is 10%, the material feeding ratio of the second compression section 7.3 is 11.8%, the material feeding ratio of the third compression section 7.4 is 14.4%, and the material feeding ratio of the homogenization section 7.5 is 16.2%. The maximum injection pressure of the optical screw 7 is controlled at 1300 kgf / cm2, and the maximum injection time is 30 s. Before injection molding, the temperature of the compression section and the homogenization section 7.5 is maintained at 200°C.

[0051] Specifically, between steps S3 and S4, the process also includes: transferring the semi-finished substrate 1. A production line and a robot are set up between the injection molding station and the semi-finished edge trimming station. The robot grabs the semi-finished substrate 1 onto the production line. The production line is equipped with an anti-static device 8. After passing through the anti-static device 8, a protective film is applied to the surface of the semi-finished substrate 1 to prevent dust from adsorbing on the surface of the semi-finished product, improve the surface accuracy, and reduce the static electricity on the surface of the semi-finished substrate 1.

[0052] Specifically, step S4 also includes a semi-finished product dust removal process. An air blowing device 9 and a dust suction device 10 are set on one side of the tooling fixture 2, facing the milling cutter 3. The air blowing device 9 and the dust suction device 10 are arranged opposite each other on both sides of the milling cutter 3 and operate simultaneously. The air blowing device 9 continuously blows air during the process of the milling cutter 3 removing burrs, thereby effectively reducing the temperature of the milling cutter 3 and preventing burrs from sticking to the tool, so that the surface cut of the semi-finished product substrate 1 is smooth. At the same time, the dust suction device 10 is on the other side of the milling cutter 3 relative to the air blowing device 9, thereby effectively cleaning the burrs removed by the milling cutter 3, keeping the product surface clean, and thus controlling the surface shape PV accuracy of the mirror.

[0053] Specifically, the semi-finished product station is provided with a Y-axis slide rail 12 and an X-axis slide rail 11 located above the Y-axis slide rail 12. The X-axis slide rail 11 is provided with a Z-axis slide rail 13, and a vertical milling cutter 3 is provided on the Z-axis slide rail 13. The tooling fixture 2 is located on the Y-axis slide rail 12.

[0054] The semi-finished product base 1 is provided with a plurality of limb ends 1.1. The tooling fixture 2 includes a lower template 2.2 and an upper template 2.1 for forming the semi-finished product mold cavity. The connection position between the limb end 1.1 corresponding to the upper template 2.1 and the semi-finished product base 1 is provided with an opening 2.3 for inserting a milling cutter 3.

[0055] The Y-axis slide rail 12 is also provided with positioning cylinders 14 on both sides, and the output end of the positioning cylinder 14 is provided with a pressure plate 15 for pressing the tooling fixture 2.

[0056] The coating fixture 4 includes a coating base plate 4.2 and four coating pressure plates 4.1. The coating base plate 4.2 is adapted to the contour of the semi-finished substrate 1. The coating pressure plates 4.1 are pressed on the outer contour of the semi-finished substrate 1 and expose an effective mirror surface for coating.

[0057] Specifically, step S5 also includes a coating pretreatment. Before loading the coating fixture 4, the surface of the protective film is cleaned with a dust-free ion air gun, the protective film is removed, and the surface of the semi-finished product is baked to eliminate internal stress, improve the surface properties of the substrate, and increase the bonding and adhesion between the coating layer and the surface of the semi-finished product substrate 1.

[0058] In step S5, the SiO2 layer 5 is sputtered onto the semi-finished product substrate by positive and negative electrode electro-ionization vacuum sputtering, and the Al layer 6 is sputtered onto the product surface by current-excited molecularization vacuum sputtering. Preferably, the surface of the semi-finished product substrate 1 is activated before coating. Optionally, oxygen is introduced and activated for 80-100 seconds.

[0059] Specifically, in step S6, the protective treatment refers to packaging the finished product into an anti-static blister box.

[0060] Compared with the prior art, the present invention has the following advantages and beneficial effects: the material is baked before the semi-finished substrate 1 is injection molded, which improves the adhesion of the surface of the semi-finished substrate 1, improves the coating quality and coating layer stability of the reflector surface, and effectively increases the wear resistance and service life of the reflector.

[0061] By controlling the upper and lower molds of the molding machine with two sets of high-temperature mold temperature controllers, the surface shape change of the semi-finished substrate 1 can be controlled, thereby controlling the curvature and fullness of the finished mirror surface.

[0062] In the coating station, a SiO2 layer 5 is deposited on the substrate surface to increase reflectivity. Another SiO2 layer 5 is deposited on the outermost layer of the substrate to increase surface adhesion. This ensures that the inner and outer surfaces of the Al layer 6 in the middle are coated with SiO2 layer 5, making the layers more firmly bonded, reducing the internal stress of the reflector, and increasing the bonding and adhesion between the coating layer and the surface of the semi-finished substrate 1.

[0063] The optical screw 7 adopts multi-segment heating, using different heating temperatures for different segments, which saves costs and improves product quality. The resulting semi-finished substrate 1 is stable and highly accurate, ensuring the surface accuracy and reflectivity of the mirror surface. This helps improve the quality and clarity of the generated image, ensuring that the image is free from distortion, black and white spots, fog, and other appearance defects, thereby increasing the product qualification rate.

[0064] This specific embodiment is merely an explanation of the present invention and is not intended to limit the invention. After reading this specification, those skilled in the art can make modifications to this embodiment without contributing any inventive step, but such modifications are protected by patent law as long as they are within the scope of the claims of the present invention.

Claims

1. A manufacturing process for a free-reflecting mirror used in a HUD, characterized in that, The manufacturing process includes the following steps: S1: Provide base material, control the ambient temperature and dust-free level of base material storage, and clean the packaging surface; S2: Base material drying. The base material is placed in a drying equipment and continuously dried to remove the surface moisture of the base material. The drying temperature and drying time are controlled and multiple base materials are circulated for drying. S3: Molding injection molding, pre-set the pressure inside the mold cavity, and control the injection temperature of the upper mold and the lower mold respectively. The molten base material is input into the mold cavity, and after the semi-finished product is formed, it is squeezed out of the mold core and cooled. After demolding, the semi-finished product is taken out. The upper and lower molds are fed by an optical screw (7). The optical screw (7) includes a feeding section (7.1), at least one compression section and a homogenization section (7.5). The feeding section (7.1) is controlled at a temperature of 50°C, the compression section is controlled at a temperature of 290°C, and the homogenization section (7.5) is controlled at a temperature of 280°C, so that the surface profile of the semi-finished substrate (1) satisfies: PV < 50 μm. The compression section includes a first compression section (7.2), a second compression section (7.3), and a third compression section (7.4), and the material feeding ratios of the first compression section (7.2), the second compression section (7.3), and the third compression section (7.4) increase sequentially. The material feeding ratio of the first compression section (7.2) is 10%, the material feeding ratio of the second compression section (7.3) is 11.8%, the material feeding ratio of the third compression section (7.4) is 14.4%, and the material feeding ratio of the homogenization section (7.5) is 16.2%. The maximum injection pressure of the optical screw (7) is controlled at 1300 kgf / cm², and the maximum injection time is 30s. Before injection molding, the compression section and the homogenization section (7.5) are kept at 200°C. S4: Remove the edges of the semi-finished product base (1), set up a tooling fixture (2) and control the feed rate and speed of the milling cutter (3) to remove the glue edge after demolding of the semi-finished product. The semi-finished product base (1) is provided with several limbs. The tooling fixture (2) includes a lower template (2.2) and an upper template (2.1) for forming the mold cavity of the semi-finished product. The lower template (2.2) is provided with an opening (2.3) for the connection position between the limbs corresponding to the semi-finished product base (1) and the semi-finished product base (1). It also includes dust removal treatment for semi-finished products. The tooling fixture (2) is provided with an air blowing device (9) and a dust suction device (10) facing the milling cutter (3). The air blowing device (9) and the dust suction device (10) are arranged opposite to each other on both sides of the milling cutter (3) and operate simultaneously. S5: Coating of the semi-finished substrate (1), setting up a coating fixture (4) to form a coating layer on the effective mirror surface of the semi-finished product, and performing a resist coating treatment on the outside of the effective mirror surface of the semi-finished product. After the coating is completed, the finished product is taken out. The coating layer includes a SiO2 layer (5), an Al layer (6), and a SiO2 layer (5) sequentially covering from the inside to the outside. Before coating, the surface of the semi-finished substrate (1) is activated by introducing oxygen and activating for 80-100 seconds. The coating fixture (4) includes a coating base plate (4.2) and four coating pressure plates (4.1). The coating base plate (4.2) is adapted to the contour of the semi-finished substrate (1). The coating pressure plates (4.1) are pressed on the outer contour of the semi-finished substrate (1) and expose an effective mirror surface for coating. S6: Finished product substrate inspection, including dimensional data inspection, surface inspection, surface PV inspection, reflectivity inspection, adhesion and RMS inspection. If the inspection is qualified, protective treatment will be carried out. In step S2, the drying time of the base material is controlled to be greater than 4 hours and the drying temperature is 125°C. Multiple base materials are cyclically dried within 24 hours. In step S2, the positive and negative deviation of the drying temperature of the base material is controlled within 0.5℃; Between steps S3 and S4, the process also includes: transfer of semi-finished substrate (1), setting up a production line and a robot between the injection molding station and the semi-finished edge removal station, the robot grabbing the semi-finished substrate (1) to the production line, the production line being equipped with an anti-static device (8), and after passing through the anti-static device (8), a protective film is applied to the surface of the semi-finished substrate (1). Step S5 also includes a coating pretreatment. Before loading the coating fixture (4), the protective film surface is cleaned and then removed, and the surface of the semi-finished product is baked to eliminate internal stress. In step S5, the SiO2 layer (5) is sputtered onto the surface of the semi-finished product by positive and negative electrode ion attraction vacuum sputtering, and the Al layer (6) is sputtered onto the product surface by current-excited molecularization vacuum sputtering. In step S6, the protective treatment refers to packing the finished product into an anti-static blister box. The semi-finished product trimming station is provided with a Y-axis slide rail (12) and an X-axis slide rail (11) located above the Y-axis slide rail (12). The X-axis slide rail (11) is provided with a Z-axis slide rail (13), and a vertical milling cutter (3) is provided on the Z-axis slide rail (13). The tooling fixture (2) is located on the Y-axis slide rail (12). The Y-axis slide rail (12) is provided with positioning cylinders (14) on both sides. The output end of the positioning cylinder (14) is provided with a pressure plate (15) for pressing the tooling fixture (2). In step S4, the air blowing device (9) blows air continuously during the process of the milling cutter (3) removing the burrs, thereby effectively reducing the temperature of the milling cutter (3) and preventing the burrs from sticking to the tool, so that the surface cut of the semi-finished substrate (1) is smooth. At the same time, the dust suction device (10) is on the other side of the milling cutter (3) relative to the air blowing device (9), thereby effectively cleaning the burrs removed by the milling cutter (3), keeping the product surface clean, and thus controlling the surface shape PV accuracy of the mirror.

Citation Information

Patent Citations

  • Head-up display device

    CN107250892A

  • Head-up display reflective mirror and support part, production method thereof

    WO2016189361A1

  • High-durability silver mirror

    CN106062590A

  • Production technology of one-time-molded radian of glass high-light cover plate

    CN109747132A