Control system for micro-adjusting polymer melt forming slot dies

By adjusting the gap of the slit mold in real time using a pressure sensor and actuator system, the problem of uneven melt outlet in the prior art is solved, enabling rapid and uniform molding of polymer mesh and reducing waste during the start-up process.

CN113580529BActive Publication Date: 2026-11-24DAVIS STANDARD LLC
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202110481876.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2020-04-30
Filing Date
2021-04-30
Publication Date
2026-11-24
Estimated Expiration
2041-04-30

AI Technical Summary

Technical Problem

Existing technologies cannot precisely adjust the melt outlet of the slit mold during the polymer mesh molding process, resulting in waste and uneven thickness of the polymer mesh during startup.

Method used

Employing a pressure sensor and actuator system, the gap of the slit mold is automatically adjusted through a control unit and algorithm. The profile of the melt outlet is adjusted in real time according to the melt pressure and flow rate to ensure uniformity.

Benefits of technology

This technology enables real-time adjustment of the melt outlet during startup, reducing polymer waste and improving the uniformity and production efficiency of the formed polymer mesh.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113580529B_ABST
    Figure CN113580529B_ABST
Patent Text Reader

Abstract

This invention discloses a control system for micro-adjusting a slit mold for polymer melt molding. The system is used to adjust the gap in a slit mold for producing polymer meshes. The slit mold includes a polymer reservoir extending between a polymer inlet and a melt outlet. The melt outlet has a first edge extending longitudinally along the melt outlet and a second edge opposite to the first edge. Multiple actuators move the second edge at multiple positions along its length. The first edge is spaced from the second edge by a gap with an adjustable profile. A pressure sensor communicates with the reservoir and measures the pressure of the polymer in the reservoir. A control unit with an algorithm correlates the profile of the gap with the pressure in the reservoir. The algorithm generates a control signal to make the profile of the gap uniform.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Cross-references to related applications

[0002] This application claims the benefit of U.S. Provisional Patent Application Serial No. 63 / 018,082, filed April 30, 2020, the entire contents of which are incorporated herein by reference. Technical Field

[0003] The present invention relates to a system for adjusting the gap in a slit mold used in the production of polymer meshes. Background Technology

[0004] In polymer film or sheet forming, extrusion coating, or lamination applications, the polymer melt exiting the melt profile forming die lip of a slit die must be uniform or flat in a direction perpendicular to the material flow direction. As the flow rate of the polymer melt through the melt profile forming die lip increases, the resulting increase in die internal pressure causes the melt profile forming die lip forming the die to expand or "clamshell" (from the...). Figure 2A The cross section shown becomes Figure 2B (See the cross-section shown). The shape of this expansion is typically parabolic, with greater expansion at the center than at the ends. The thickness of the polymer melt is directly related to this expansion effect due to the increased flow rate of the polymer material and the resulting increased pressure within the slit mold and across the melt profile forming lip. The expansion or shelling of the melt profile forming lip, caused by deformation of the mold body and melt profile forming lip due to increased internal mold pressure, makes the melt heavier or thicker at the center than at the ends.

[0005] Typically, adjusting the melt profile forming die lip of a slit mold requires repeated and iterative measurements of the formed polymer mesh (e.g., thickness measurement), mold adjustments, and remeasurement of the formed polymer mesh. Cross-mesh scanning devices require time to traverse the formed polymer mesh, and the formed polymer mesh itself requires even more time to determine accurate mesh profile measurements. Existing melt forming processes cannot precisely adjust the melt outlet of the slit mold during startup. Therefore, existing scanning equipment can only determine a suitable cross-mesh profile for automated control after the film production line or system has reached steady-state operation. Consequently, existing polymer mesh forming processes result in significant waste of polymer mesh during the startup-to-steady-state operation period.

[0006] Therefore, there is a need in the art for systems that can function automatically to achieve a flatter polymer mesh profile before the system reaches steady-state operation. Summary of the Invention

[0007] This document discloses a system for adjusting the gap in a slit mold for producing polymer meshes. The system includes a slit mold having a polymer inlet (i.e., an inlet for receiving polymer) and a melt outlet (i.e., an outlet for discharging molten polymer). A polymer reservoir (i.e., a reservoir in the slit mold containing polymer flowing through the mold) extends between the polymer inlet and the melt outlet. The melt outlet has a first edge extending longitudinally along the melt outlet and a second edge extending longitudinally along the melt outlet. The second edge is opposite to the first edge. The polymer melt within the polymer reservoir begins to solidify into a partially shaped polymer melt as it exits the melt outlet. The second edge is selectively movable at multiple locations along its length. The first edge is spaced from the second edge by a gap having an adjustable profile extending between a first end and a second end of the slit mold. A plurality of actuators are fixed to the slit mold at an anchoring frame. Each actuator includes an extendable member and a drive unit communicating with the extendable member. The extendable member, in response to a force generated by the drive unit, moves a portion of its second edge relative to the first edge to adjust the profile of the gap. A pressure sensor is in communication with the reservoir. The pressure sensor measures the pressure of the polymer melt in the reservoir or just before the reservoir. A control unit receives the pressure value measured by the pressure sensor. The control unit has a first algorithm and an automatic profile control algorithm. The first algorithm includes software having a set of empirical polymer pressure-flow data (i.e., information obtained from observations or experiments relating to how pressure affects the flow rate of polymer materials and presented in the form of recorded data) that correlates the profile of the gap with the pressure in the reservoir. The first algorithm generates a control signal that is sent to the automatic profile control algorithm. The automatic profile control algorithm generates actuator control signals and sends them to each of the plurality of actuators, causing the drive unit to move the extendable member and causing the profile of the gap to be uniform between the first and second ends of the slit mold.

[0008] In one embodiment, before pressurizing the reservoir, the profile of the gap has a uniform size between the first and second ends of the slit mold. When the reservoir is initially pressurized, the profile of the gap has a parabolic profile, which has a maximum value at the midpoint between the first and second ends of the slit mold and a minimum value adjacent to the first and second ends of the slit mold.

[0009] In one embodiment, the system further includes a hopper having one or more load sensors, each load sensor measuring the weight loss of material contained in the hopper over time. The control unit communicates with each of the load sensors. The load sensors generate a flow rate signal based on the weight loss of material contained in the hopper over time. The first algorithm includes software having a set of empirical polymer weight-flow rate data (i.e., information obtained from observations or experiments relating to how the weight of the polymer material affects the flow rate of the polymer material and presented in the form of recorded data) that correlates the pressure signal and the flow rate signal based on the hopper weight with the profile of the gap. The first algorithm generates a control signal that is sent to the automatic profile control algorithm. The automatic profile control algorithm generates an actuator control signal and sends the signal to each of the plurality of actuators, causing the drive unit to move the extendable member and causing the profile of the gap to be uniform between the first and second ends of the slit mold.

[0010] In one embodiment, the system further includes a speed measurement system comprising a tachometer that measures the rotational speed (e.g., revolutions per minute) of the motor rotating the extruder screw and / or the rotational speed of the extruder screw. The speed measurement system generates a flow rate signal based on the extruder screw rotational speed based on the correlation between the extruder screw rotational speed and the amount of polymer material leaving the extruder. The first algorithm includes software having a set of empirical polymer extrusion flow rate data (i.e., information obtained from observations or experiments relating to how the extruder screw rotational speed affects the flow rate of the polymer material and presented in the form of recorded data) that correlates the pressure signal and the flow rate signal based on the extruder screw rotational speed with the profile of the gap. The first algorithm generates control signals that are sent to an automatic profile control algorithm. The automatic profile control algorithm generates actuator control signals and sends these signals to each of the plurality of actuators, causing the drive unit to move the extendable member and causing the profile of the gap to be uniform between the first and second ends of the slit die.

[0011] In one embodiment, the system further includes a speed measurement system that measures the rotational speed (e.g., revolutions per minute) of one or more gears in the gear set of the geared melt pump. The speed measurement system generates a flow rate signal based on the gear set rotational speed, relating the rotational speed of one or more gears in the melt pump to the amount of polymer material leaving the melt pump. The first algorithm includes software having a set of empirical polymer pump flow rate data (i.e., information obtained from observations or experiments relating to how the rotational speed of one or more gears in the gear set of the geared melt pump affects the flow rate of the polymer material and presented in the form of recorded data) that correlates the pressure signal and the flow rate signal based on the gear set rotational speed with the profile of the gap. The first algorithm generates a control signal that is sent to the automatic profile control algorithm. The automatic profile control algorithm generates an actuator control signal and sends the signal to each of the plurality of actuators, causing the drive unit to move the extendable member and causing the profile of the gap to be uniform between the first and second ends of the slit mold.

[0012] In one embodiment, the system further includes a setpoint rate for adjusting the control of the control unit based on historical data to achieve a predetermined profile of the gap. The setpoint rate generates a profile flow signal based on the profile of the gap. The first algorithm includes software having a set of historical polymer flow experience data (i.e., information obtained through observation or experimentation related to historical flow rates that result in a profile of the polymer material) that correlates the pressure signal and the profile flow signal with the profile of the gap. The first algorithm generates a control signal that is sent to the automatic profile control algorithm. The automatic profile control algorithm generates an actuator control signal and sends the signal to each of the plurality of actuators, causing the drive unit to move the extendable member and causing the profile of the gap to be uniform between the first and second ends of the slit mold.

[0013] In one embodiment, the system further includes a measuring device that measures the thickness and / or mass of the portion of the molded polymer melt exiting the slit mold near the melt outlet. The automatic contour control algorithm adjusts the contour of the gap in response to the thickness and / or mass of the molded polymer melt measured by the measuring device.

[0014] In one embodiment, the control unit utilizes the first algorithm before and during system startup. However, in some embodiments, the control unit utilizes the first algorithm and / or the automatic contour control algorithm during steady-state operation of the system.

[0015] This document also discloses a system for adjusting the gap in a slit mold for producing polymer meshes. The system includes a slit mold having a polymer inlet (i.e., an inlet for receiving polymer) and a melt outlet (i.e., an outlet for discharging molten polymer), and a polymer reservoir (i.e., a reservoir in the slit mold containing polymer flowing through the mold) extending between the polymer inlet and the melt outlet. The polymer melt within the polymer reservoir begins to solidify into a partially shaped polymer melt as it exits the melt outlet. The melt outlet has a first edge extending longitudinally along the melt outlet and a second edge extending longitudinally along the melt outlet opposite the first edge. The second edge is selectively movable at multiple locations along its length. The first edge is spaced apart from the second edge by a gap having an adjustable profile extending between a first end and a second end of the slit mold. A plurality of actuators are fixed to the slit mold at an anchoring frame. The plurality of actuators move a portion of the second edge relative to the first edge to adjust the profile of the gap. A pressure sensor measures the pressure of the polymer melt in the reservoir or just before the reservoir. A measuring device measures the thickness and / or mass of the partially formed polymer melt exiting the slit mold near the melt outlet. The control unit communicates with the pressure sensor and the measuring device. The control unit has a first algorithm and an automatic profile control algorithm. The first algorithm includes software having a set of empirical polymer pressure-flow data (i.e., information obtained from observations or experiments relating to how pressure affects the flow rate of the polymer material and presented in the form of recorded data) that correlates the profile of the gap with the pressure in the reservoir. The first algorithm generates a control signal in response to the pressure measured by the pressure sensor and sends it to the automatic profile control algorithm. The automatic profile control algorithm includes software that generates an actuator control signal in response to the thickness and / or mass per unit area of ​​the partially formed polymer melt measured by the measuring device and sends the signal to each of the plurality of actuators to adjust the profile of the gap. The control unit uses the first algorithm before the operation of the system and during the startup of the system. The control unit uses the first algorithm and / or the automatic contour control algorithm during stable operation of the system.

[0016] In one embodiment, during steady-state operation of the system, the control unit utilizes the automatic contour control algorithm to generate a coarse adjustment actuator control signal that provides coarse adjustment of the profile of the gap, and the control unit utilizes the first algorithm to generate a fine adjustment actuator control signal that provides fine adjustment of the profile of the gap. Attached Figure Description

[0017] Figure 1A This is a schematic diagram of the system of the present invention for adjusting the gap in a slit mold for producing polymer mesh.

[0018] Figure 1B yes Figure 1A A magnified view of detail 1B, which shows an exemplary pressure sensor used in the system.

[0019] Figure 2A It is shown in steady state and is cut along section 2-2. Figure 1A A bottom view of the slit mold.

[0020] Figure 2B It is shown under pressure and is cut along section 2-2. Figure 1A A bottom view of the slit mold.

[0021] Figure 2C yes Figure 1A The cross-sectional view of the slit mold taken along section 2C-2C.

[0022] Figure 3A It is under pressure and after adjusting the mold gap. Figure 2B A schematic diagram of a slit mold, showing the actuator.

[0023] Figure 3B yes Figure 3A Enlarged views of several actuators, showing various clearance adjustments.

[0024] Figure 4 yes Figure 3B A front view of one of the actuators, showing the adjustment range.

[0025] Figure 5 This is a schematic diagram of a system for adjusting the gap in a slit mold for producing polymer mesh according to the present invention. The system includes a hopper, an extruder, and a melt pump. Detailed Implementation

[0026] like Figure 1AAs shown, a system (e.g., a linear slit mold) for adjusting the gap GC in a slit mold 10 for polymer melt production is generally indicated by the numeral 100. The slit mold 10 is essentially a metallic structure comprising an inlet referred herein as a polymer inlet 10A and an outlet referred herein as a melt outlet 10B. The slit mold includes a reservoir referred herein as a polymer reservoir 10C extending between the polymer inlet 10A and the melt outlet 10B. The melt outlet 10B has a first edge 12A extending longitudinally along the melt outlet 10B and a second edge 12B extending longitudinally along the melt outlet 10B. The second edge 12B is opposite to the first edge 12A. As described herein, the second edge 12B is selectively movable along its length at multiple locations. The first edge 12A is spaced apart from the second edge 12B by the gap GC. Figure 2A and Figure 2B As shown, the gap GC is defined by a profile extending between the first end 10X and the second end 10Y of the slit mold 10.

[0027] like Figure 3A As best shown, multiple actuators 20 (e.g., fifteen actuators 20A, 20B, 20C, 20D, 20E, 20F, 20G, 20H, 20I, 20J, 20K, 20L, 20M, 20N, and 20P are shown) are fixed to the slot mold 10 at various locations on the anchoring frame 10F. (Refer to...) Figure 3B and Figure 4 Each of the plurality of actuators 20 is a die lip forming actuator, and each actuator includes an extendable member 21E (e.g., a rod, shaft, etc.) and a drive unit 21D (e.g., a servo motor) in communication with the extendable member 21E. The extendable member 21E is configured to move a portion of the second edge 12B relative to the first edge 12A in response to a force applied to the extendable member 21E by the drive unit 21D.

[0028] like Figure 1A As shown, in one embodiment, the slit mold 10 comprises a first mold portion 10M and a second mold portion 10N. A first edge 12A extends along the exit surface 10E of the first mold portion 10M, and a second edge 12B extends along the exit surface 10E' of the second mold portion 10N. The second mold portion 10N includes a recess 10P (e.g., a concave portion) formed between the second edge 12B and the anchoring frame 10F. The recess 10P gives the second mold portion 10N flexibility, which allows the tail end 10T of the second mold portion 10N to deflect when a force is applied to an abutment surface 10K extending from the recess 10P.

[0029] like Figure 1AAs shown, a pressure sensor 30 (e.g., a pressure transducer) is configured to communicate with the reservoir 10C via a pressure transmission line 30A (e.g., a tube, channel, or conduit) integrated on the pressure sensor 30. The pressure sensor 30 is configured to measure the pressure of the polymer in or near the reservoir 10C. The pressure transmission line 30A is arranged along a reference line RL1 in an opening 10W (e.g., a cylindrical hole) in the first mold portion 10M, wherein the reference line RL1 is parallel to a reference line RL2 extending along the outlet faces 10E, 10E' of the slit mold 10. The pressure transmission line 30A is positioned in the direction of polymer melt flow from the polymer inlet 10A of the reservoir 10C to the melt outlet 10B (see [reference]). Figure 1A The arrow F1 in the figure is perpendicular. In one embodiment, the pressure transmission line 30A is positioned to prevent flow lines in the melt from leaving the gap GC at the melt outlet 10B.

[0030] like Figure 1B As shown, the pressure sensor 30 is positioned such that the pressure transmission line 30A is located in the first mold portion 10M of the slit mold 10. The pressure sensor 30 includes a pressure-sensing diaphragm 30D connected to and in communication with the pressure transmission line 30A. The pressure-sensing diaphragm 30D has a flat tip flush with the flat inner surface 10F1 of the reservoir 10C of the slit mold 10 to prevent flow lines in the melt from leaving the gap GC at the melt outlet 10B. In some embodiments, the pressure transmission line 30A has a threaded portion 30M (e.g., a male thread) at one end adjacent to the pressure-sensing diaphragm 30D. The threaded portion 30M is screwed into a complementary threaded portion 10W1 (e.g., a female thread) formed in an opening 10W in the first mold portion 10M. The pressure sensor 30 includes a pressure transducer 30T connected to and in communication with the pressure transmission line 30A. The pressure transducer 30T is located outside the slit mold 10. The pressure transducer 30T is connected to the signal line 30S via connector 30C.

[0031] like Figure 2C As shown, in one embodiment, the pressure transmission line 30A is located between the first side 10Q1 and the second side 10Q2 of the reservoir 10C of the sewing mold 10. In another embodiment, the pressure transmission line 30A is located at an intermediate position between the first side 10Q1 and the second side 10Q2 of the reservoir 10C of the sewing mold 10. In yet another embodiment, the pressure transmission line 30A is placed perpendicular to the reservoir 10C of the sewing mold 10, wherein the reservoir 10C is considered as a reservoir between the first side 10Q1 and the second side 10Q2.

[0032] like Figure 1AAs shown, system 100 includes a control unit 60 that communicates with pressure sensor 30 via signal line 30S. As will be detailed below, control unit 60 includes a first algorithm 60A or “macro” control algorithm having software configured to correlate the profile of the gap GC with the pressure in the reservoir 10C with one or more sets of empirical data (i.e., information obtained from observation or experimentation and presented in the form of recorded data). The first algorithm 60A generates a control signal 62 sent to an automatic profile control algorithm 60B, which further generates an actuator control signal 64 sent to each of the plurality of actuators 20 to move the extension member 21E with drive unit 21D and thus homogenize the gap GC between the first edge 12A and the second edge 12B of the slit mold 10 (see [link to documentation]). Figure 3A In some embodiments, a first algorithm 60A is used to generate a control signal 62, which is sent directly to each of the plurality of actuators 20 to cause the drive unit 21D to move the extendable member 21E and thus to homogenize the gap GC between the first edge 12A and the second edge 12B of the slit mold 10 (see [link]). Figure 3A ).

[0033] like Figure 2A As shown, before pressurizing the reservoir 10C, the gap GC has a uniform size G in the profile between the first edge 12A and the second edge 12B of the slit mold 10. In one embodiment, before pressurizing the reservoir 10C, the profile of the gap GC has a uniform size G of 0.025 inches to 0.030 inches (0.635 mm to 0.762 mm).

[0034] like Figure 2B As shown, when the reservoir 10C is initially pressurized, the gap GC has a parabolic profile G', which has a maximum value at the midpoint between the first end 10X and the second end 10Y of the slit mold 10, and a minimum value adjacent to the first end 10X and the second end 10Y of the slit mold 10. In one embodiment, the gap GC has a maximum value of 0.045 inches to 0.050 inches (0.885 mm to 1.263 mm) at the midpoint MP of the slit mold 10. In one embodiment, the gap GC has a minimum value of 0.035 inches to 0.040 inches (0.89 mm to 1.016 mm) at the end point EP of the slit mold 10. Figure 2B In the middle, the first edge 12A' is shown as moving away from Figure 2A The orientation of the static position of the first edge 12A shown (in) Figure 2BThe middle edge (indicated by dashed line 12A") is bent (e.g., elastic deformation). The second edge 12B' is shown as moving away from... Figure 2A The orientation of the static position of the second edge 12B shown (in) Figure 2B (represented by dashed line "12B") bending (e.g., elastic deformation).

[0035] refer to Figure 3A System 100 compensates for expansion or clamshelling of the gap GC of the slit mold 10 caused by the polymer melt flowing through the melt outlet 10B (e.g., in the form of a slit opening) by employing a brake to automatically adjust the gap GC to be proportional to the production rate (i.e., flow rate) and / or production pressure (i.e., pressure of the polymer melt). Specifically, system 100 controls the melt outlet 10B of the slit mold 10 to achieve a flat polymer melt profile both in a static state and during accelerated operation. During accelerated operation and / or before reaching steady-state operation, system 100 compensates for dynamic input pressure (e.g., pressure rise) at or near the melt outlet 10B of the slit mold 10 by automatically adjusting and controlling the gap GC. In some embodiments, once steady-state operation is achieved, the automatic profile control algorithm 60B takes over control of the gap GC. (See reference...) Figure 1A The control unit 60 includes an internal first algorithm 60A and an internal automatic contour control algorithm 60B. Although the internal automatic contour control algorithm 60B has been shown and described, the invention is not limited thereto, and other configurations, including but not limited to those incorporating an external automatic contour control algorithm, are also conceivable.

[0036] As discussed in detail below, system 100 is employed prior to the actuation of the measuring device 50 traversing the solidified polymer melt. Therefore, system 100 controls the thickness of the molded polymer melt at a “microscale” (i.e., the automatic contour control algorithm 60B can be activated earlier to achieve a flat polymer melt thickness and contour more quickly compared to using the automatic contour control algorithm 60B only in response to the measuring device 50). In one embodiment, system 100 is linked to the automatic contour control algorithm 60B, and because the actuator 20 has already been adjusted during steady-state operation, the speed at which the molded polymer melt is adjusted to a flat contour is accelerated. As a result, system 100 according to this disclosure achieves faster control of the flat contour of the polymer melt in less time compared to using only the automatic contour control algorithm 60B, because system 100 precisely adjusts the gap GC prior to steady-state operation. The faster control achieved by this invention also reduces waste in the production process and improves the quality of the final product.

[0037] In operation, the automatic control position of each actuator 20 is related to the point rate in the first algorithm 60A, which drives each actuator (e.g., actuators 20A, 20B, 20C, 20D, 20E, 20F, 20G, 20H, 20I, 20J, 20K, 20L, 20M, 20N, and 20P as shown in Figure 3) to its micro-position (i.e., adjusting the profile of the gap GC before steady-state operation) to accelerate the control response during production line acceleration or before the control measurement device 50 (a specific mesh measurement system traversing the molded polymer melt) is activated via the automatic profile control algorithm 60B. Figure 1A In the illustrated embodiment, when the system 100 is stationary and during startup, the first algorithm 60A adjusts the actuator 20 to adjust the profile of the gap GC based on the pressure of the polymer melt in the reservoir 10C (e.g., measured by pressure sensor 30). After startup (where the system maintains control over the gap GC), once the slit mold 10 reaches steady-state operation, the measuring device 50 measures the molded polymer melt exiting the slit mold 10 (i.e., measures thickness, mass, thickness and mass, or thickness and weight, etc.) and initiates control of the actuator 20. In one embodiment, an automatic profile control algorithm 60B is employed during steady-state operation to coarsely adjust the profile of the molded polymer melt. In one embodiment, the first algorithm 60A is employed during steady-state operation to further finely adjust the profile of the molded polymer melt. System 100 allows the automatic contour control algorithm 60B to control the slit mold 10 earlier than in prior art methods. For example, system 100 allows control of the slit mold 10 in an accelerated state prior to steady-state control of the thickness of the molded polymer melt (i.e., automatic contour control algorithm 60B). System 100 is used during startup and can be shut down during steady-state operation, or it can be used in conjunction with steady-state control (i.e., automatic contour control algorithm 60B) during steady-state operation to reduce the time required to achieve a uniform mesh profile (i.e., consistent thickness of the molded polymer melt) and reduce polymer waste.

[0038] The polymer material within the slit die 10 generates pressure between its flow surface and the melt outlet 10B due to its viscosity and based on its flow through a pressure compensation manifold spanning the machine. This pressure increases with increasing production rate and consequently, with an increase in the deflection of the gap GC. The pressure sensor 30 provides real-time operating pressure values ​​to a first algorithm 60A to also determine the required actuator 20 correction amount to compensate for the deflection of the gap GC at the melt outlet 10B of the slit die 10.

[0039] The polymer melt and the pressure formed by its obstruction as it flows through the slit mold 10 due to its viscosity cause swelling or shelling at the first edge 12A and the second edge 12B of the melt outlet 10B, respectively. A first algorithm 60A uses pressure measured within the slit mold 10 or prior to the slit mold 10 in the melt capillary delivery system to accelerate control over the contour of a flat or even transverse melt film or coating. Figure 2B An example of the clam shell effect is shown, and Figure 2A The automatic compensation position is shown.

[0040] Figure 3A and 3B Actuator 20 is shown in the figure. Each individual actuator (e.g., such as...) Figure 3A The actuators shown (20A, 20B, 20C, 20D, 20E, 20F, 20G, 20H, 20I, 20J, 20K, 20L, 20M, 20N, and 20P) can be manually adjusted to suit various needs. Figure 3A and 3B The outline of the gap GC is shown. Figure 4 The screw-type thread is shown in detail as an adjustment method, but other adjustment methods may be used without departing from the invention disclosed herein.

[0041] Figure 3A , Figure 3B and Figure 4 The manual adjustment of the actuator shown includes an automatic adjustment method, which includes a manual adjustment device shown for illustrative purposes, wherein the length or stroke of the actuator automatically changes within a set control stroke range to affect the change of the melt outlet 10B of the first edge 12A and the second edge 12B, respectively. Within the control stroke range, the stroke is infinitely adjustable.

[0042] Furthermore, the shelling of the melt outlet 10B is primarily affected by pressure, which is caused by, but not limited to, the profile G of the gap GC with a uniform profile G, the final forming section length of the die lip gap, the metal temperature of the die, the polymer temperature, the surface material of the polymer structure flowing close to the die wall, and the viscosity of the polymer material. For this reason, the first algorithm 60A includes implementing a decremental or incremental adjustment as an adjustment input, which in turn increases or decreases the required die expansion or the shape of the shell parameters to adjust the profile of the gap GC for any particular situation.

[0043] The combined use of the control unit 60 and the pressure sensor 30 allows for rapid adjustment of the profile dimensions of the gap GC before the slit mold 10 reaches a steady-state production of the melt, and allows for rapid control of the melt thickness via the melt thickness measuring device, thereby reducing melt waste and shortening the time required to obtain a consistent and constant melt thickness.

[0044] like Figure 1A and Figure 5 System 100 includes a flow signal 70 that transmits flow rate information of the polymer material to control unit 60. The flow signal 70 includes a pressure signal 70A received from pressure sensor 30. As described above, pressure sensor 30 is used to measure the pressure of the polymer in or near reservoir 10C. Pressure sensor 30 generates pressure signal 70A based on the measured polymer pressure and transmits pressure signal 70A to control unit 60.

[0045] In some implementations, such as Figure 1A and Figure 5 The flow signal 70 includes a flow signal 70B based on the weight of the hopper 90, received from a system (e.g., a weighing sensor or load sensor) for measuring the weight 92 of the polymer material in the hopper 90. The load sensor measures the weight of the polymer material in the hopper 90 and transmits the flow signal 70B based on the hopper weight to the control unit 60. The outflow rate is determined by the weight loss over time measured by the load sensor 92. When the hopper 90 is being filled, the weight loss over time measured by the load sensor 92 cannot determine the outflow rate (i.e., when the load sensor 92 detects an increase in weight, the calculation of the outflow rate is stopped until the load sensor 92 detects a decrease in weight again).

[0046] In some embodiments, the flow signal 70 includes a flow signal 70C received by the self-measuring system based on the extruder screw speed. In some embodiments, such as Figure 1A and Figure 5 As shown, the speed measurement system includes a tachometer 110, which measures the rotational speed (e.g., revolutions per minute) of the electric motor that rotates the extruder screw 105X and / or the rotational speed of the extruder screw 105X set to rotate in the extruder. The speed measurement system generates a flow rate signal 70C based on the extruder screw rotational speed, which is transmitted to the control unit 60. Figure 5 In the illustrated embodiment, tachometer 110 measures the revolutions per minute (RPM) of the motor 112 driving the extruder screw 105X, but tachometer 110 directly measuring the RPM of the extruder screw 105X of the extruder 105 does not depart from the invention disclosed herein. A flow signal 70C based on the extruder screw speed is determined according to the known weight of the material leaving the extruder 105 per revolution and the screw speed of the extruder 105.

[0047] In some embodiments, the flow signal 70 includes a flow signal 70D based on the gear set rotational speed received from a speed measurement system. In some embodiments, such as Figure 1A and Figure 5As shown, the speed measuring system includes a tachometer 125 that measures the rotational speed (e.g., revolutions per minute) of one or more gears in the gear set 122 of the gear-type melt pump 120. The speed measuring system generates a flow rate signal 70D based on the gear set rotational speed, which is transmitted to the control unit 60. The output rate of material from the melt pump 120 to the slit mold 10 is determined by measuring the rotational speed of the gear set 122 of the melt pump 120 and the known material output rate per rotational speed.

[0048] In some implementations, such as Figure 1A and Figure 5 As shown, the flow signal 70 includes a profile flow signal 70E received from the setpoint rate 55. The setpoint rate 55 generates the profile flow signal 70E based on historical data of the adjusted and / or calibrated melt forming process, and transmits the profile flow signal 70E to the control unit 60. The setpoint rate 55 allows the slit mold 10 to be formed before the operation of the system 100, and allows pre-forming of the first edge 12A and the second edge 12B respectively before steady-state operation.

[0049] In some embodiments, the flow signal 70 includes a pressure signal 70A, a flow signal 70B based on hopper weight, a flow signal 70C based on extruder screw speed, a flow signal 70D based on gear set speed, and a profile flow signal 70E. As described in detail below, this combined flow signal 70 is transmitted to the control unit 60 to generate control signals 62, 64 for each of the plurality of actuators 20.

[0050] In some embodiments, the first algorithm 60A includes software configured with a set of polymer pressure-flow empirical data (i.e., information obtained from observations or experiments relating to how pressure affects the flow rate of a polymer material and presented in the form of recorded data) that correlates the flow rate of the polymer with the future pressure in the reservoir 10C (i.e., pressure expected or calculated via empirical data). The first algorithm 60A generates a control signal 62, which is sent to an automatic contour control algorithm 60B. The automatic contour control algorithm 60B then generates an actuator control signal 64, which is sent to each of the plurality of actuators 20 to move the extendable member 21E of the drive unit 21D, thereby uniformly positioning the gap GC between the first edge 12A and the second edge 12B of the slit mold 10 before the future pressure in the reservoir 10C is achieved (see [link to relevant documentation]). Figure 3A ).

[0051] In some embodiments, the first algorithm 60A includes software configured with a set of empirical polymer weight-flow rate data (i.e., information obtained from observations or experiments relating to how polymer weight affects the flow rate of the polymer material and presented in the form of recorded data) that correlates the pressure signal 70A and the flow rate signal 70B based on hopper weight with the profile of the gap GC. The first algorithm 60A is used to generate a control signal 62, which is sent to an automatic profile control algorithm 60B. The automatic profile control algorithm 60B is further used to generate an actuator control signal 64, which is sent to each of the plurality of actuators 20 to move the extendable member 21E of the drive unit 21D, thereby uniformly positioning the profile of the gap GC between the first edge 12A and the second edge 12B of the slot die 10.

[0052] In some embodiments, the first algorithm 60A includes software configured with a set of empirical polymer extrusion flow data (i.e., information obtained from observations or experiments relating to how the extruder screw speed affects the flow rate of the polymer material and presented in the form of recorded data) that correlates a pressure sensor signal 70A and a flow rate signal 70C based on the extruder screw speed with the profile of the gap GC. The first algorithm 60A is used to generate a control signal 62, which is sent to an automatic profile control algorithm 60B, which is further used to generate an actuator control signal 64, which is sent to each of a plurality of actuators 20 to move the extendable member 21E of the drive unit 21D, thereby making the profile of the gap GC uniform between the first edge 12A and the second edge 12B of the slit die 10.

[0053] In some embodiments, the first algorithm 60A includes software configured with a set of empirical polymer pump flow data (i.e., information obtained from observations or experiments relating to how the rotational speed of one or more gears in the gear set of the geared melt pump affects the flow rate of the polymer material) that correlates the pressure signal 70A and the flow rate signal 70D based on the gear set rotational speed with the profile of the gap GC. The first algorithm 60A is used to generate a control signal 62, which is sent to an automatic profile control algorithm 60B, which is further used to generate an actuator control signal 64, which is sent to each of the plurality of actuators 20 to move the extendable member 21E of the drive unit 21D, thereby uniformly positioning the profile of the gap GC between the first edge 12A and the second edge 12B of the slot die 10.

[0054] In some embodiments, the first algorithm 60A includes software configured with a set of historical polymer flow experience data (i.e., information obtained through observation or experimentation related to historical flow rates that result in the profile of the polymer material) that correlates the pressure signal 70A and the profile flow rate signal 70E with the profile of the gap GC. The first algorithm 60A is used to generate a control signal 62, which is sent to an automatic profile control algorithm 60B, which is further used to generate an actuator control signal 64, which is sent to each of a plurality of actuators 20 to move the extendable member 21E of the drive unit 21D, thereby making the profile of the gap GC uniform between the first edge 12A and the second edge 12B of the slot die 10.

[0055] like Figure 3A As shown, multiple actuators 20 move the second edge 12B”’ towards the deformed state of the first edge 12A’, thereby making the gap GC uniform. Each of the multiple actuators 20 moves the second edge 12B”’ a different distance depending on its position relative to the midpoint MP and the first end 10X and the second end 10Y of the gap mold 10. For example, in Figure 3B In the diagram, the drive units 21D of actuators 20A and 20P, adjacent to the first end 10X and the second end 10Y, are shown to move their respective extendable members 21E from the reference line RL by a distance D1, respectively; the drive units 21D of actuator 20D (located between the first end 10X and the midpoint MP) and actuator 20L (located between the second end 10Y and the midpoint MP) are shown to move their respective extendable members 21E from the reference line RL by a distance D2, respectively; the drive unit 21D of actuator 20H (located at the midpoint MP) is shown to move its respective extendable member 21E from the reference line RL by a distance D3. Distance D3 is greater than distance D2, and distance D2 is greater than distance D1. The other actuators 20B, 20C, 20E, 20F, 20G, 20I, 20J, 20K, 20M, and 20N move their respective distances relative to the midpoint MP of the slit mold 10 and the positions of the first end 10X and the second end 10Y.

[0056] exist Figure 1A and Figure 5 In the illustrated embodiment, the pressure signal 70A based on the pressure measured by the pressure sensor 30 is the most accurate method for controlling the thickness of the molded polymer melt, while the flow signal 70B based on the weight of the feed hopper, the flow signal 70C based on the speed of the extruder screw, the flow signal 70D based on the speed of the gear set and / or the profile flow signal 70E are less accurate in controlling the profile of the molded polymer melt.

[0057] While the invention has been disclosed with reference to various exemplary embodiments, those skilled in the art will understand that various changes and substitutions of elements with equivalents can be made without departing from the scope of the invention. Furthermore, many modifications can be made to adapt particular situations or materials to the teachings of the invention without departing from the essential scope of the invention. Therefore, the invention is not intended to be limited to the specific embodiments disclosed as the best mode for carrying out the invention, but includes all embodiments falling within the scope of the appended claims.

Claims

1. A system (100) for adjusting the gap in a slit mold for producing polymer mesh, characterized in that, The system includes: A slit mold (10) includes a polymer inlet (10A) and a melt outlet (10B), a polymer reservoir (10C) extending between the polymer inlet (10A) and the melt outlet (10B), wherein polymer melt within the polymer reservoir (10C) begins to solidify into a partially shaped polymer melt as it exits the melt outlet (10B), the melt outlet (10B) having a first edge (12A) extending longitudinally along the melt outlet (10B) and a second edge (12B) extending longitudinally along the melt outlet (10B) and opposite to the first edge (12A), the second edge (12B) being selectively movable at multiple positions along the length direction of the second edge (12B), the first edge (12A) being spaced apart from the second edge (12B) by a gap (GC) having an adjustable profile extending between a first end (10X) and a second end (10Y) of the slit mold (10); A plurality of actuators (20) are fixed to the slit mold (10) at an anchoring frame (10F). Each of the plurality of actuators (20) includes an extendable member (21E) and a drive unit (21D) in communication with the extendable member (21E). The extendable member (21E) is configured to move a portion of the second edge (12B) relative to the first edge (12A) in response to a force generated by the drive unit (21D) to adjust the profile of the gap (GC). A pressure sensor (30) is connected to the reservoir (10C) and is used to measure the pressure of the polymer melt in the reservoir (10C) and generate a pressure signal (70A). A control unit (60) having a first algorithm (60A) and an automatic contour control algorithm (60B), the control unit (60) receiving a pressure signal (70A) from the pressure sensor (30), the first algorithm (60A) including software configured to correlate the contour of the gap (GC) with the pressure in the reservoir (10C) based on a set of empirical polymer pressure-flow data, and the first algorithm (60A) generating a control signal (62) for the automatic contour control algorithm (60B), the automatic contour control algorithm (60B) generating an actuator control signal (64) for each of the plurality of actuators (20) such that the drive unit (21D) moves the extendable member (21E) such that the contour of the gap (GC) is uniform between the first end (10X) and the second end (10Y) of the slit mold (10); and at least one of the following: a) A hopper (90) having at least one load sensor (92) for measuring the weight loss of material contained in the hopper (90) over time, a control unit (60) communicating with the at least one load sensor (92) for generating a flow rate signal (70B) based on the weight loss of material contained in the hopper over time, the first algorithm (60A) including software configured to correlate the pressure signal (70A) and the flow rate signal (70B) based on the hopper weight with the profile of the gap (GC); b) A first speed measurement system comprising a first tachometer (110) measuring revolutions per minute of at least one of an electric motor (112) and an extruder screw (105X) of an extruder (105), the first tachometer (110) generating a flow rate signal (70C) based on the extruder screw speed based on the correlation between the number of revolutions of the extruder screw (105X) and the amount of polymer material leaving the extruder (105), the first algorithm (60A) comprising software configured to correlate the pressure signal (70A) and the flow rate signal (70C) based on the extruder screw speed with the profile of the gap (GC); c) A second speed measurement system comprising a second tachometer (125) measuring the revolutions per minute of the gear set (122) of the melt pump (120), the second tachometer (125) generating a flow rate signal (70D) based on the gear set rotational speed based on the correlation between the rotational speed of the gear set (122) of the melt pump (120) and the amount of polymer material leaving the melt pump (120), the first algorithm (60A) comprising software configured to correlate the pressure signal (70A) and the flow rate signal (70D) based on the gear set rotational speed with the profile of the gap (GC).

2. The system (100) according to claim 1, characterized in that, Before the reservoir (10C) is pressurized, the profile of the gap (GC) has a uniform size (G) between the first end (10X) and the second end (10Y) of the slit mold (10). When the reservoir (10C) is initially pressurized, the profile of the gap (GC) has a parabolic profile (G') with a maximum value at the midpoint (MP) between the first end (10X) and the second end (10Y) of the slit mold (10) and a minimum value adjacent to the first end (10X) and the second end (10Y) of the slit mold (10).

3. The system (100) according to claim 1, characterized in that, It also includes a setpoint rate (55) for determining control changes of the control unit (60) based on historical data to obtain the profile of the gap (GC), the setpoint rate (55) generating a profile flow signal (70E) based on the profile of the gap (GC), and the first algorithm (60A) including software configured to associate the pressure signal (70A) and the profile flow signal (70E) with the profile of the gap (GC).

4. The system (100) according to claim 1, characterized in that, It also includes a measuring device (50) that measures at least one of the thickness and mass of the partially formed polymer melt exiting the slit mold (10) near the melt outlet (10B). The automatic contour control algorithm (60B) adjusts the contour of the gap (GC) in response to at least one of the thickness and mass of the partially formed polymer melt measured by the measuring device (50).

5. The system (100) according to claim 4, characterized in that, The control unit (60) uses the first algorithm (60A) before and during the startup of the system (100), and the control unit (60) uses at least one of the first algorithm (60A) and the automatic contour control algorithm (60B) during the steady-state operation of the system (100).

Citation Information

Patent Citations

  • Apparatus and method for controlling mass flow in an extrusion die

    US5770129A