Method of producing a thermal infrared sensor array in a vacuum-filled wafer-level housing

By thinning the central and bottom wafers in wafer-level packaging, combined with vacuum sealing and CMOS signal processing, the space constraints and signal processing problems of high-resolution infrared sensor arrays in small devices have been solved, enabling the production of high-density, small-size, and low-loss sensor arrays.

CN114097086BActive Publication Date: 2026-11-24HEIMANN SENSOR GMBH
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202080050185.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2019-07-09
Filing Date
2020-07-09
Publication Date
2026-11-24
Estimated Expiration
2040-07-09

AI Technical Summary

Technical Problem

Existing technologies struggle to achieve high-resolution infrared sensor arrays in miniaturized devices, especially in mobile devices such as smartphones. The sensor modules are too large in overall size and pixel size, have insufficient signal processing space, and are difficult to vacuum seal, leading to signal loss and mechanical stress problems.

Method used

Using monolithic silicon micromachining technology, thermal infrared sensor arrays are fabricated in wafer-level packaging by thinning the central and bottom wafers and combining them with vacuum sealing technology. Anti-reflective layers and filter layers are used to improve transmittance, reduce pixel edges and via sizes, and integrate CMOS signal processing to achieve high-density packaging.

Benefits of technology

It achieves a high fill factor and small total thickness for high-resolution infrared sensor arrays in small devices, reduces pixel size and via size, improves signal processing capabilities, reduces mechanical stress and signal loss, and is suitable for economical production compatible with standard CMOS processes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114097086B_ABST
    Figure CN114097086B_ABST
Patent Text Reader

Abstract

A method for producing a thermal infrared sensor array in a vacuum-filled wafer-level housing, the wafer-level housing having a particularly small size, the wafer-level housing comprising at least two wafers, the two wafers being a cover wafer (1) and a central wafer (3), the central wafer (3) having a plurality of sensitive infrared-sensitive sensor pixels (5) respectively located on a slit-film thin film (5”) above an adiabatic cavity (11). The present invention provides a method for producing a high-resolution monolithic silicon micromechanical thermopile array sensor using wafer-level packaging technology, wherein the sensor achieves particularly high spatial resolution and a very high fill factor in a very small housing size, particularly a very small total thickness, and can be economically produced by compatibility with standard CMOS processes. This is achieved by the following: the cover wafer (1) is first rigidly mechanically bonded to the provided central wafer (3) including sensor pixels (5) with infrared-sensitive pixels by wafer bonding, and then the central wafer (3) is thinned from the back of the wafer to achieve a specified thickness.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to a method for producing thermal infrared sensor arrays in a vacuum-filled wafer-level housing using monolithic silicon micromachining technology in wafer-level packaging. Background Technology

[0002] For the application of infrared sensor arrays in small, cost-effective thermal imaging cameras, high spatial and thermal resolution, as well as the minimum housing size of the sensor module, are all important.

[0003] This is especially true for so-called mobile applications, such as smartphones.

[0004] These applications must achieve high thermal resolution with good measurement accuracy within a minimal space, while simultaneously maintaining a minimal overall sensor module size. For example, in order to accommodate a miniaturized thermal imaging camera built from an infrared array sensor module within the casing of a smartphone itself, a very small overall height of the infrared array sensor module is particularly important. To accommodate a miniature thermal imaging camera on a circuit board next to a small CMOS camera with the same viewing direction, the overall height of the sensor array (including all optics) must be less than 2.5–3 mm.

[0005] Therefore, the only thermal (uncooled) sensors that can be conceived are infrared sensor arrays. This group of thermal sensors includes so-called microbolometers, thermoelectric arrays, and thermopile arrays (TP arrays).

[0006] To achieve the required measurement accuracy, thermopile arrays require continuously modulated mechanical choppers, and microbolometers require so-called mechanical shutters. In addition to the sensor array and infrared optics, these components also need to be mounted in the beam path. The additional mechanical dimensions of the controlled chopper or shutter module increase the housing height and make installation in smartphone housings difficult. Only thermopile sensor arrays (TP arrays) can achieve the required measurement accuracy without the need for additional mechanical choppers or mechanical shutters in the beam path.

[0007] For miniaturized, high-resolution thermopile arrays, pixel size must be very small, which is necessary for the hermetically sealed packaging of sensitive array chips under vacuum. Since traditional housings (such as metal housings, like the TO series) are also too large, wafer-level packaging (WLP) remains the most promising improvement. This is a particularly economical form of vacuum sealing for thermopile array chips, where the wafer assembly is hermetically sealed, and the active components in between are under high vacuum.

[0008] WLP also has a further advantage: all silicon-based wafers have the same coefficient of thermal expansion. This means that if the sensor temperature changes during packaging or use, no additional stress will occur between the cover / sensor and / or the bottom wafer, as they all have the same coefficient of thermal expansion.

[0009] Because a single sensor pixel in a sensor array provides only a very small voltage signal (typically in the µV range), local amplification of the signal is necessary, if possible, within the sensor package itself. Furthermore, due to the large number of pixels on the same sensor chip in a high-resolution array sensor, a large number of preamplifiers (operating in parallel) are also required.

[0010] Infrared thermopile sensor arrays have long been known in various forms and designs. Thermopile sensors, fabricated using silicon micromachining, typically consist of a thin film containing thermocouples manufactured using thin-film technology. Beneath the thin film, a cavity exists in the substrate.

[0011] The "hot" contact of the thermocouple is located in the center of the thin film, while the "cold" contact is located at the silicon edge, which serves as a heat sink. Between the center of the thin film and the heat sink, there are, for example, as long as possible narrow beams (bars) that connect the central portion of the thin film (absorption region) to the heat sink (the silicon edge of the pixel) and contain one or more thermocouples.

[0012] On both sides of the long beam, slits separate the beam from the central portion or silicon heat sink (support). Most of the absorption of IR radiation occurs in the central region of the thin film. This is especially true in arrays with high spatial resolution, where pixels are small and apertures (slits) are very narrow. To increase the sensor's fill factor, infrared shielding (umbrella-like structures) can be applied to the thin film or pixels to allow for the reception of more infrared radiation over a larger area.

[0013] The thermocouple (on the beam) is located relatively close to the silicon heat sink, so a significant proportion of the heat can escape through the gas located between the heat sinks. This can cause signal loss. To eliminate this, a vacuum seal is required.

[0014] The slits in the thin film are used to create cavities beneath it. Wafers bonded to the thin film are used to create hermetically sealed closures. However, the isotropic etching of the substrate beneath the thin film needs to protect nearby electronics from potential damage.

[0015] US 2008 / 0128620 A1 describes a wafer-level package for multiple thermopiles on a thin film, having a cavity for thermal insulation below or above the film, which is typically etched anisotropically (KOH) but may optionally be etched by DRIE.

[0016] To provide a high-resolution TP array with many small pixels, many channels are needed for the necessary parallel signal processing, which is not feasible due to space constraints.

[0017] EP 2889 909 proposes a solution that incorporates multiple slits in the absorber region of a pixel to better guide the silicon sacrificial layer beneath the thin film outward from the groove. However, this approach results in a loss of effective absorber area, and consequently, a loss of signal and measurement accuracy.

[0018] WO 2015004166 A1 describes a hermetically sealed method for reducing stress in electronic devices. Similarly, fine processing is required to expose the pixels, and applying a reflective metal layer to the bottom of the cavity beneath the pixels is difficult or very expensive.

[0019] No solution can produce particularly small and highly sensitive pixels and accommodate the necessary signal processing channels in a particularly small area.

[0020] DE 10 2006 122 850 proposed a high-resolution thermopile array in WLP. The array has three interconnected wafers (cap, sensor chip, and bottom).

[0021] However, the three interconnected wafers are approximately the same thickness; that is, the cavity of the central sensor wafer is etched using bulk micromechanical etching, and the vertical holes of the cavity pass through the entire wafer. Due to tolerance requirements, this limits the achievable pixel size. Furthermore, because there is not enough space for the required parallel signal processing channels, not many pixels can be accommodated on the sensor wafer.

[0022] US 8519336 B2 discloses a configuration in which an IR detection device is located above a reflective layer. Furthermore, algorithm evaluation circuitry is located on a circuit board below. Here, three silicon substrates (wafers) are combined together. The receiver unit consists of a thermopile and a depressurized sealing recess in the silicon substrate. The reflective layer forms a notch below the receiver unit. The surface of the notch is composed of a reflective material, such as gold or aluminum. With this arrangement, IR radiation initially undetected in the receiver unit is reflected and refocused back onto the receiver unit, thus regaining the possibility of detection.

[0023] The "notch" with a reflective structure has a configuration similar to a parabolic reflector, thus reflecting as much infrared radiation as possible back to the receiver unit.

[0024] The necessary electrical contacts extend from the back side of the upper wafer to the front side of the central wafer via so-called through-silicon vias (TSVs) (i.e., through-contacts) (which are known in themselves), through the central wafer in the "three-wafer sandwich" all the way to the back side of the wafer and the signal processing unit, and finally further through vias to the back side of the bottom wafer and the solder contacts. This thermopile array in WLP thus has SMD functionality.

[0025] Therefore, signal lines can, in principle, be routed outside the pixel area or between pixels. In this case, the signal processing operation for each pixel can be performed on the bottom chip below the pixel.

[0026] A typical TSV produced using current technology requires a lateral dimension on the wafer that is approximately one-tenth of the wafer thickness. Therefore, for a wafer thickness of 400-500 µm, a typical via size is approximately 40-50 µm.

[0027] Therefore, it is not possible to produce arrays with particularly small pixels and particularly high spatial resolution, because the size of the vias in the pixel regions alone increases the lateral pixel size.

[0028] However, this is difficult to be compatible with arrays of small camera chips in smartphones, because the lens optics with the corresponding focal length still need to be mounted on the sensor array chip.

[0029] Existing technological solutions cannot produce high-resolution infrared sensor arrays with a large number of very small pixels and a particularly small overall height (e.g., suitable for smartphones), and these infrared sensor arrays cannot be directly manufactured using standard CMOS processes.

[0030] The sensitivity of an infrared sensor also depends on heat dissipation through the gas surrounding the sensor, and this can be increased through vacuum-sealed encapsulation. In a vacuum-sealed housing, signal loss due to heat conduction through the gas is nonexistent or minimal. However, conventional vacuum housings in construction and assembly techniques are expensive in terms of materials and cost to achieve the necessary vacuum seal. In such cases, even ordinary chip adhesives become cost and problem factors due to degassing and leakage. Since the various materials of the housing typically differ (bottom, cap, optical window), they also have different coefficients of thermal expansion, which can lead to mechanical stress and leakage.

[0031] Wafer-level packaging and vacuum sealing are economical and can be mass-produced. The necessary vacuum sealing is achieved by encapsulating the thermopile sensor wafer with a cover wafer and a bottom wafer underneath.

[0032] One drawback of known wafer-level packaging (WLP) for thermopile arrays is the very large overall height resulting from assembling multiple individual wafers. This is because each individual wafer must be processed and has cavities, metal sputtering, filter layers, etc. For the dimensions of modern semiconductor wafers (200 mm and 300 mm in diameter), this necessitates a certain minimum wafer thickness. If it is too thin (e.g., only 100-200 µm), it will break during processing in most systems encountered during manufacturing.

[0033] Currently, wafer thicknesses of approximately 400-500 µm are typical and can be mass-produced at reasonable yields. Two-wafer assemblies already exist with thicknesses of approximately 0.8-1 mm, two-wafer composite assemblies, and three-wafer assemblies (a particularly preferred bulk micromachining variant among known solutions) with thicknesses of approximately 1.2-1.5 mm. This prevents the achievement of very small overall heights (e.g., for smartphones).

[0034] A second drawback of existing technologies is the low spatial resolution due to the excessively large size of the thermopile pixels. To date, the smallest known thermopile array has a pixel size of 90 µm.

[0035] A third drawback of known thermal infrared array solutions (e.g., thermopile arrays) is their large overall lateral size, which also makes them difficult to fit into small mobile devices such as smartphones. Sensor array chips are typically mounted in metal TO housings or metal-sealed housings, whose external dimensions are much larger than the sensor chip itself. Summary of the Invention

[0036] The purpose of this invention is to provide a method for producing thermal infrared sensor arrays in a vacuum-filled wafer-level housing using monolithic silicon micromachining technology in wafer-level packaging. This method achieves exceptionally high spatial resolution (due to very small pixels) and a very high fill factor with minimal housing size, particularly very small overall thickness, and can be economically produced by compatibility with standard CMOS processes.

[0037] According to the invention, this objective is achieved through the following steps: first, at least two, preferably three or more, semiconductor wafers, such as silicon or infrared-transmitting glass for covering the wafers, are processed separately, and then mounted, wherein the wafers are thinned in stages in this process.

[0038] - Preferably, the cover wafer has a cavity ranging in size from tens to hundreds of micrometers on its underside, and then so-called anti-reflective layers or filter layers are disposed on both sides of the wafer. On the one hand, these filter layers are designed to allow the cover wafer to have particularly high transmittance in the infrared range, and are designed to be able to additionally block certain spectral ranges in which there would be transmission loss, for example, in the atmosphere, which leads to distance dependence in the measurement of distant objects.

[0039] These filter layers may also consist of special subwavelength structures.

[0040] For example, the cavity depth can reach approximately half the total thickness of the cover wafer, as this also increases the wafer's transmission of IR radiation. However, the remaining thickness should not become too small so that the wafer assembly remains mechanically stable.

[0041] The central wafer or the wafer with sensor pixels has functional layers known in themselves. These include, for example, multiple polycrystalline or amorphous silicon layers with different conductivity, an absorber structure (preferably a so-called umbrella structure), and a CMOS structure for signal processing. All steps on the surface side (e.g., introducing slits in the thin film for thermal insulation from the silicon substrate) need to be performed before bonding.

[0042] According to the present invention, the central sensor wafer, after thinning, has a small remaining thickness of less than 200-300 μm, preferably less than 50-100 μm. This has two advantages compared to previously known solutions for thermopile arrays.

[0043] On the one hand, it can handle much smaller thermopile pixels than previously known, because the silicon edge of the pixel retained after the DRIE etching process (used for thermal separation and as a heat sink for cold contacts) can be reduced to a few micrometers.

[0044] On the other hand, compared to using a standard wafer thickness of, for example, approximately 400-500 µm, electrical through-contacts from the front to the back of the thermopile wafer (or bottom wafer) can also produce smaller lateral dimensions.

[0045] In current prior art, the achievable lateral dimension of a TSV is typically about one-tenth of the wafer thickness. Therefore, for a wafer thickness of 400 µm, a typical via size is about 40 µm. However, if the wafer is thinned to 30 µm, the via size will, for example, be only about 3 µm. In a further embodiment, even with particularly small thermopile pixel sizes, each pixel can still be connected to the back side.

[0046] Fabricating electrical contacts for further external processing of sensor signals from array pixels includes:

[0047] The central chip, containing sensor pixels and some signal processing electronics, is led directly to the outside via pads prepared in the central chip and subsequent line bridges, or...

[0048] Signal processing, for example, is fed to the bottom wafer through very small vias (so-called through-silicon vias, TSVs). Further signal processing (ROIC) can be housed on the bottom wafer. The space there is larger than the space next to the thermopile array on the central wafer.

[0049] In the largest cases, even each pixel is individually connected to the bottom chip. This is made possible by the extremely thin central chip, which allows for the formation of very small and extremely precise plated vias in the corners of the pixels, thus further increasing the array's packaging density.

[0050] Apart from signal processing such as preamplifiers and analog-to-digital converters, most digital signal processing, including image evaluation, can be housed as processors on the bottom layer wafer (ROIC).

[0051] To further transmit signals down to the carrier substrate, there may be more vias / through contacts in the bottom wafer so that signals can be fed directly down to appropriate contacts (e.g., solder bumps).

[0052] Aligning with the thermal pads of a quad flat no-lead (QFN) package can also be useful to dissipate heat unintentionally generated in the ASIC.

[0053] In the cover wafer, there are recesses created by appropriate methods (e.g., wet etching or DRIE) for mechanical stability reasons. The depth of the recesses should not exceed 50% of the cover wafer thickness.

[0054] In one variant, the bottom wafer (ROIC) can also be significantly thinned to less than 0.2-0.3 mm, making the overall stack of the three wafers as thin as possible to accommodate mobile devices such as smartphones. Attached Figure Description

[0055] The invention will now be explained in more detail with reference to exemplary embodiments. In the relevant figures of the accompanying drawings:

[0056] Figure 1 A cross-sectional view of the basic structure of a very thin infrared sensor array according to the present invention in a vacuum wafer-level package is shown.

[0057] Figure 2 This illustrates the fabrication of the cover wafer, sensor wafer, and bottom wafer as separate wafers prior to assembly into wafer-level packaging.

[0058] Figure 3The illustration shows various assembly steps for forming individual wafers of a thin wafer assembly according to the invention in a wafer-level package, wherein cavities are etched out from the back side below the pixels in the sensor wafer;

[0059] Figure 4 This illustrates one configuration of a very thin thermal array chip in WLP, where the chip does not require through-contacts (TSVs).

[0060] Figure 5 This illustrates one configuration of a very thin thermal array chip in WLP, where cavities are etched into the front side of the sensor wafer;

[0061] Figure 6 This illustrates a particularly simplified configuration of a very thin thermopile array in a wafer-level housing with only two wafers;

[0062] Figure 7 This illustrates the configuration of a very thin thermal array for surface mountable housings (SMD housings);

[0063] Figure 8 A further configuration of the thermopile array with an additional bottom wafer is shown, wherein the additional bottom wafer contains further signal or image processing components; and

[0064] Figure 9 This illustrates a configuration of a very thin infrared array with thermopile wafers mounted upside down. Detailed Implementation

[0065] It should be understood that Figures 1 to 9 The details of each chip are shown separately. In fact, these chips are much larger and each contains multiple adjacent structures described above. These structures are monolithically divided into separate thermal infrared sensor arrays after manufacturing.

[0066] Figure 1 The basic structure of a very thin infrared sensor array in a vacuum wafer-level package, after each wafer is mounted but before monolithization, is shown. It has an upper cover wafer 1, a thinned central wafer 3, and a bottom wafer 4. In the cover wafer 1, there are cavities 10 above each set of sensor pixels 5.

[0067] according to Figure 1The infrared sensor array includes multiple groups of infrared sensor arrays having multiple sensor pixels 5, narrow strips 5', and cavities 10. The multiple sensor pixels 5 are arranged adjacent to each other or in groups of four or more in a regular pattern. The narrow strips 5' on the central wafer 3 remain empty, so that there are no sensor pixels 5 between groups. The cavities 10 are located above each group of sensor pixels 5 in the cover wafer 1. Each cavity 10 is separated from each other by rods 1', which are supported on the strips 5' and mechanically stabilize the cover wafer 1.

[0068] For example, four sets of sensor pixels 5 can be arranged in a distributed manner in a partition on the central chip 3, such that the strips 5' intersect in a cross shape. Then, the cavity 10 in the cover chip 1 can be set accordingly, such that the rod 1' also intersects in a cross shape and is supported on the strips 5' of the central chip 3.

[0069] The maximum number of sensor pixels 5 or corresponding groups that can be manufactured on the central wafer 3 is limited only by the size of the sensor pixels 5 and the lateral dimension of the wafer.

[0070] The cover wafer 1, with the filter layer 2, is the thickest and, together with the rod 1' supported on the strip 5', imparts stability to the wafer assembly to be supplied. The central wafer 3 includes a plurality of thermal sensor pixels 5 and cavities 11 in the central wafer 3 below each sensor pixel 5, the sensor pixels 5 and cavities 11 being defined by films 5'' connected to the surrounding central wafer 3. On each film 5'', an IR radiation absorber in the form of an umbrella-shaped portion 7 ( Figure 2 Cavity 11 is laterally defined by a substantially vertical wall in the central wafer 3, and at the top according to the figure, cavity 11 is defined by a membrane.

[0071] To avoid repetition, these explanations also apply in principle to the embodiments described further.

[0072] The bottom wafer 4 has an introduced getter 14 located below each group of sensor pixels 5. After proper mounting, the bottom wafer 4 is typically significantly thinned to a thickness of less than 50-100 µm. During closure, the sensor pixels 5, having cavities 10 and 11 that surround them in an adiabatic manner, are hermetically sealed in a vacuum environment. If necessary, the getter 14 is ignited to suppress the effect of degassing on a stable vacuum.

[0073] In order to transmit the electrical signal generated by the pixel 5, there are contact pads 15 for the line bridge 17 on the bottom wafer 4 in the edge region outside the cover wafer 1.

[0074] Figure 2 A method for fabricating a three-part wafer (cap wafer 1, central wafer 3, and bottom wafer 4) for wafer-level packaging (WLP) is shown.

[0075] In the first step, on a double-sided polished silicon wafer ( Figure 2 In (a), as described above, the cover wafer 1 is subsequently provided with a cavity 10 ( Figure 2 b), and then apply an anti-reflective layer or filter layer 2 to both sides. Figure 2 c). These filter layers 2 can also be applied to optical lenses, which can be located above the cavity 10. However, the cost of a single lens is significantly higher than the cost of a filter in a wafer assembly.

[0076] On the central chip 3 (sensor chip), sensor pixels 5 are generated. Figure 2 d) and preferably, it is provided with an additional three-dimensional absorber structure, namely, the umbrella-shaped portion 7 on the membrane 5''. Figure 2 e), and in order to increase the fill factor on sensor pixel 5, umbrella-shaped portion 7 extends regionally beyond the size of the film 5'' located below without contacting adjacent umbrella-shaped portions 5''.

[0077] The other CMOS structure 8 is integrated on the upper side of the bottom chip 4. Figure 2 f), and for each chip (i.e., for each group of sensor pixels 5), at least one cavity 13 is created in the bottom wafer 4 for introducing getter 14 ( Figure 2 g). Since the fabrication of CMOS structure 8 is well-known, it will not be discussed in detail here.

[0078] The CMOS structure 8 includes CMOS evaluation circuitry and optional additional circuitry for signal processing and image processing. Integration of the EEPROM is also particularly advantageous, allowing the measurement and calibration values ​​of each sensor pixel 5 to be subsequently stored within the infrared sensor array itself. Furthermore, the central wafer 3 preferably has a through contact 6 extending from the CMOS side with electrical terminals to the underside of the wafer. Figure 7 ).

[0079] At a location below the rear pixel area, a cavity 13 is preferably formed in the bottom wafer 4 or below each group of sensor pixels 5 by conventional silicon wet etching or dry etching steps, and a getter 14 is deposited in the cavity to enable the generation of a long-term stable vacuum. This area may be small and located below and beside the pixels, but must be connected to the front side of the central wafer 3 by one or more holes etched in the film 5''.

[0080] Figure 3 The first embodiment shows the assembly of three separate wafers to form a complete wafer stack, wherein a thin wafer assembly is formed in a wafer-level package through the assembly steps of the three separate wafers, and the cavity 11 is etched from the back side of the central wafer 3 below the sensor pixel 5.

[0081] Cover wafer 1 and central thermopile wafer (i.e., central wafer 3) Figure 3 a), for example, by wafer bonding or adhesive bonding to form a fixed component ( Figure 3 c). This is followed by thinning the sensor chip 3 from the back or bottom side. Figure 3 d), the step of deep etching the sensor chip 3 ( Figure 3 e), thereby creating cavities 11 below each pixel 5, and aligning and mounting the bottom chip 4 on the central chip 3. Figure 3 f). Finally, bottom chip 4 ( Figure 3 The thinning of g) is also performed from the back side, and via the line bridge 17 or alternatively via the through contact 6 between the sensor pixels 5. Figure 7 The wiring support completes the electrical contact of the mezzanine arrangement. Figure 3 h).

[0082] Although other thermal sensor methods, such as thermoelectric or thermal radiation sensor pixels, are also possible, the sensor principle will be described below with reference to the example of thermopile pixels, whose design is basically known.

[0083] For the sake of completeness, however, it should be mentioned that, with Figure 1 Conversely, the umbrella-shaped portion 7 on the membrane 5'' is suspended from the cavity 11 by a narrow beam 11', as... Figure 9 As shown in g, slits 11'' for heat insulation are formed between beam 11' and membrane 5'' and between beam 11' and the edge of the central wafer 3 that laterally surrounds cavity 11. At the thermopile pixel, a high-temperature resistant structure extends on beam 11', with its "hot" contacts located on membrane 5'' and its "cold" contacts located on the edge surrounding cavity 11 and serving as a heat sink.

[0084] It should also be mentioned that this particular variant is obtained by connecting the inverted bottom wafer 4 to the thermopile wafer, wherein the inverted wafer assembly is applied to the underside of the film 5''. Figure 9 f、 Figure 9 g).

[0085] During the assembly process, in the first main step, the cover wafer 1, having the cavity 10 and the applied filter layer 2, is aligned relative to the central wafer 3. Figure 3 (b) allows the sensitive sensor pixel 5 to protrude into the cavity of the cover wafer 10 together with the corresponding absorber layer located thereon (e.g., the umbrella-shaped portion 7 on the film 5'').

[0086] For example, the alignment of the three wafers can be achieved by using a suitable infrared microscope through a dry or wet etch structure in the cover wafer 1.

[0087] The two wafers (cover wafer 1 and central wafer 3) are mechanically and hermetically connected to each other. Figure 3 c). This is accomplished using eutectic wafer bonding methods known per se (e.g., anodic bonding, soldering or fusion of glass frits, adhesive bonding, or soldering). While the glass frit method is preferred due to its well-known properties, eutectic bonding, particularly using the SLID method with solid-liquid interdiffusion, is also highly advantageous. Bonding temperatures are sometimes significantly lower than 400°C, thus ensuring full CMOS compatibility. Of course, materials must be carefully selected based on the desired CMOS compatibility.

[0088] A liquid eutectic is formed at the interface between the two wafers during bonding. During cooling, material bonding then forms between the wafers. Due to this material bonding, in addition to excellent hermeticity, the resulting stack exhibits very high stability, which is beneficial for subsequent process steps.

[0089] Then see Figure 3 d. Thinning the back side of the central wafer 3 (e.g., by mechanical methods such as grinding and polishing). The remaining thickness of the central wafer 3 or the wafer having the sensor pixel 5 should not exceed 200-300 µm, preferably less than 20-50 µm, and then the film 5'' is etched away from the back side below the sensor pixel 5, for example by dry etching (DRIE), thereby forming an insulating cavity 11 (see...). Figure 3 e). In this case, the through contact 6 (so-called through hole 6, for example, see Figure 5 , 7 Alternatively, 8) it can also be formed from the central wafer 3 through to the bottom wafer 4, which has an additional module for the CMOS signal processing 8. Similarly, for the through contacts 6, it was found that they can be manufactured with significantly smaller lateral dimensions and more precisely through a greatly thinned central wafer or wafer 3.

[0090] In the context of this invention, thinning before the DRIE etching process and the fabrication of the through contact 6 has several important functions:

[0091] - The thickness of the central wafer 3, which is typically 400-500 μm, can be reduced to a very small substrate thickness, preferably less than 20-50 μm, thereby reducing the overall structure thickness.

[0092] - The very thin residual substrate of the central wafer 3 can be etched more precisely using DRIE etching because, as the wafer thickness decreases, the tolerances (so-called tilt) during the etching process naturally have little or no effect on the transfer accuracy of the etching mask used for etching. DRIE allows the etching mask to be transferred to the side facing the top cover wafer 1 with very high precision, making very small pixel structures possible.

[0093] - Due to the very thin central wafer 3, the lateral dimension of the through contact 6 can be reduced very significantly.

[0094] - Due to this smaller etching depth, the DRIE etching process (which is typically performed primarily as a single-wafer process) can be faster and therefore more economical.

[0095] In the next assembly step, the bottom wafer 4 with CMOS circuitry 8 on the front and the cavity 13 for getter 14 are aligned on the front with the two upper wafers (cover wafer 1 and central wafer 3) that have already been assembled with each other. Figure 3 f), and is mechanically bonded securely via wafer bonding. This bottom wafer 4 is subsequently thinned on the body side (back side). Figure 3 g), and may require or exist electrical through-hole contacts 6 (so-called through-silicon vias TSV) to form and contact the bottom wafer 4.

[0096] To achieve the highest possible temperature resolution, the central wafer 3 should be hermetically sealed in a vacuum environment. This may already be accomplished in normal wafer-level packaging.

[0097] While an additional getter is not necessarily required, it has been found that the introduced getter 14 is preferably activated by thermal excitation (“heating”) during or after wafer bonding, which helps maintain a stable vacuum over a long period. Electrically activated getter 14 is also possible, and for this, a corresponding power supply line must be introduced into the bottom wafer 4.

[0098] In principle, the getter can also be contained in the cover wafer 1 (see...). Figure 6 a) Or at the edge of the central wafer 3 near the sensor pixel 5. Since the central wafer 3 is functionally required to have holes (through the slit 11'' in the film 5'' and the hole in the substrate), however, the most efficient and preferred method is to house the getter 14 in the bottom wafer 4 below the sensor pixel 5. This is because the arrangement of the slit 11'' and the hole in the central wafer 3 facilitates gas exchange from top to bottom.

[0099] In the final step, after monolithization into individual independent array chips, a mezzanine consisting of three interconnected and thinned wafers is mounted on a wiring support (in...). Figure 3 (not shown in h) and makes electrical contact via, for example, wire bonding bridge 17 ( Figure 3 h). This wiring support can be a circuit board (PCB, such as the circuit board in a mobile phone), a metal casing, or a so-called QFN casing with a very thin bottom.

[0100] In this way, the thickness of the overall assembly of the monolithic wafer according to the present invention does not need to be significantly increased compared to the thickness of the monolithic wafer. This is because, as an overall assembly with a thickness of, for example, only 500 μm, it can be easily handled (processed, measured, and transported) and can be divided into individual chips.

[0101] like Figure 4 As shown, a particularly easy-to-manufacture configuration of the thermopile array has no TSVs (through-vessels).

[0102] like Figure 3 As shown in a-3d, the first four steps are executed accordingly. Here, for the sake of brevity, this method is combined with... Figure 4 a and Figure 4 b in.

[0103] Next is the backside etching step ( Figure 4 c) During this period, a cavity 11 is formed instead of a through contact portion. This cavity 11 is used to provide heat insulation for the film of the sensor pixel 5 located above the cavity. The bottom wafer 4 is provided with a cavity 13 for the getter 14, and the getter 14 is introduced ( Figure 4 d), and the bottom chip 4 is connected to the two upper chips that have been mounted on each other and thinned out ( Figure 4 e). On the upper side of the central wafer 3, which has sensor pixels 5 and CMOS signal processing 8, conventional pads 15 are applied to the outer edge of each chip.

[0104] For example, before separating the components into individual chips using a thin saw blade, these chips are exposed by sawing from above into the wafer assembly using a wider saw blade. After the pads 15 are exposed and before the wafer stack is monolithized, the thermopile arrays can be tested for functionality using a conventional automated wafer sampler, even while still within the wafer assembly.

[0105] In the final step ( Figure 4 In f), the monolithic thermopile sensor array chip, consisting of three wafer segments, is electrically connected to an external module using wire bridges 17 via conventional wire bonding methods. Through these wire bridges 17 and simple adhesive or solder connections, the entire array chip can be mounted, for example, on a chip carrier board on a circuit board, in a ceramic or metal housing, or particularly preferably in a so-called QFN package with a very thin bottom, thus maintaining the advantages of a flat housing.

[0106] The basic principle of the very thin wafer-level package for a thermal sensor with particularly small sensor pixels 5 can also be configured for a variant in which the thermally insulating cavities 10, 11 for sensor pixels 5 are not etched from below through the central wafer, but are introduced from above through a sacrificial layer technique known per se (so-called surface micromachining).

[0107] This variant is in Figure 5 The image shows a configuration of a high-resolution thermal sensor in a vacuum wafer-level package (WLP) with three wafers, and a cavity 16 for thermal insulation of sensor pixel 5 is etched from above the central wafer 3 using a known sacrificial layer technique.

[0108] Below each sensor pixel 5 in the central wafer 3 having thermal sensor pixels 5, a cavity 16 is created in the central wafer 3 using a sacrificial layer technique known per se through a slit 11'' in the film 5''. Figure 5 b). This can be accomplished, for example, using a sacrificial layer known per se (e.g., porous silicon) or as an oxide in SOI technology, or by anisotropically wet etching the bulk silicon beneath the film of sensor pixel 5. The separated material is led outward through slits 11'' in film 5''.

[0109] The cavity 16 created below each sensor pixel 5 ensures that the slit film 5'' of the infrared-sensitive functional layer with sensor pixel 5 is thermally insulated from the silicon substrate (central wafer 3) and allows for high sensor signal in a subsequent vacuum environment.

[0110] If an anisotropic etching method is used, then even for very small pixels (e.g., less than 50 μm), there is a shallower etching depth of only tens of micrometers, which can correspondingly greatly reduce the thickness of the central wafer 3, while the cavity 16 is not etched outward to the underside of the central wafer 3, which will prevent vacuum sealing.

[0111] During installation, the central chip 3 ( Figure 5 b) Through wafer bonding ( Figure 5 c) Securely connected to cover chip 1 in an equivalent manner ( Figure 5 a), then thinned to a smaller thickness ( Figure 5 d). For example in Figure 3 As in the previous exemplary embodiments, an electrical direct contact 6 (TSV) is provided between the front and back sides of the central chip 3, and the sensor pixel 5 or the signal processing channel 8 of the first stage is integrated on the central chip 3. Figure 5 e). Furthermore, at least one hole should preferably be etched through the central wafer (not shown), or one or more cavities 16 should be anisotropically etched through the entire wafer, or the wafer should be thinned to expose the cavities 16, thereby allowing the getter 14 in the cavity 13 of the bottom wafer 4 to pass through. Figure 5 f) can ensure a stable vacuum in the cavities 10 and 16 below and above the sensor pixel 5.

[0112] In principle, the getter can also be deposited in the cavity 10 of the cover wafer with a filter layer (see [reference]). Figure 6 a) Although there is more space in the bottom chip 4, there is also less interference effect on the sensor pixel 5 and the filter layer during the activation of the getter 14.

[0113] The bottom wafer 4, which has an additional CMOS signal processing component 8, is securely and hermetically connected to the cover wafer 1 via conventional wafer bonding machinery. Figure 5 g), and the bottom wafer 4 is thinned to a very small thickness so that the triple components of the WLP can also be very thin (less than 0.5 mm to less than 1.0 mm).

[0114] As a special form (unlike all other solutions with three or more wafers in the assembly), there is also a particularly simple configuration in which the cavity 16 of the thermopile array is etched from above (as shown in the image). Figure 6 (As shown).

[0115] Figure 6 The configuration of a high-resolution thermal sensor in a vacuum wafer-level package is shown, which has only two wafers, namely a cover wafer 1 and a central wafer 3, wherein a cavity 16 for thermal insulation of sensor pixels 5 is etched out from above the central wafer 3 by a known sacrificial layer technique.

[0116] The first step is based on... Figure 5 It is done in a way that is equivalent to the variant. However, with Figure 5 Compared to the solutions in the middle, Figure 6 The configuration shown does not require any through contact 6 or bottom wafer 4.

[0117] In this case, the getter 14 must be placed at the outermost edge of the cavity 10 of the cover chip 1 at the widest possible distance, and this outermost edge is close to the filter layer 2 opposite to the sensor pixel 5. Figure 6 a) allows the sensor array to have an unrestricted field of view.

[0118] After wafer-to-wafer bonding is performed between the cover wafer 1 and the central wafer 3 with the cavity 16 below the sensor pixel 5, the (central) wafer 3 with the pixel 5 is thinned in the assembly. Figure 6 b), and through the pads 15 and contact bridges 17 at the chip edge ( Figure 6 c) Electrical contacts are fed to external electronic components of the array chip. It should be understood that this may require multiple pads 15 with line bridges 17.

[0119] Although this dual-wafer solution according to the invention appears very simple, it has certain disadvantages compared to all other solutions according to the invention with three or more wafers:

[0120] - The integration density is significantly lower than previous solutions because there is no signal processing to be "transferred" to the bottom wafer, which is not present here, and the getter 14 must be housed next to the filter layer 2 in the cavity 10 of the cover wafer 1.

[0121] - Although the final thickness of the array may be very small after thinning of the (central) chip 3. Figure 6 The solution in the article achieves this goal, but the lateral dimension of the (central) chip 3 must be larger to accommodate signal processing on the entire pixel side on chip 3. This increases the external size of the array chip, or fewer sensor pixels 5 can be accommodated on a chip of the same size.

[0122] - Due to the lower integration while maintaining the same overall size, there is a loss in temperature resolution and / or spatial resolution (minimum pixel size) compared to the aforementioned solutions.

[0123] In this variant, the thickness of the central wafer 3 needs to be reduced less, or left with a thickness similar to that of the cavity 10 of the cover wafer 1. This presents fewer problems with bending of the chips in both the cover wafer 1 and the central wafer 3 due to the internal vacuum.

[0124] In another embodiment, the particularly flat "mezzanine" consisting of three wafers can be configured in a "surface mountable" (SMD) manner (see [reference]). Figure 7 ).

[0125] In this case, the sensor chips in both the central wafer 3 and the bottom wafer 4 must be equipped with the known through contacts 6 and 18 (TSV vias). Figure 7 a).

[0126] In the current prior art, such through contacts 6, 18 can have a lateral dimension of a few micrometers. Very thin wafers are a prerequisite for achieving this. In this way, they can be accommodated both in the corner regions of each sensor pixel 5 (which may result in the signal processing 8 on the entire pixel side being repositioned into the bottom wafer 4) and in the edge regions of the central wafer 3 near the pixel field (focal plane), so that a portion of the signal processing 8 can be placed into the bottom wafer 4.

[0127] The through contact 6 terminates with contact pads (not shown separately), thereby allowing the through contact 18 (electrical contact) to pass between the two wafers on the bottom wafer 4 after installation.

[0128] The back side of the bottom wafer 4 receives solder bumps 9. After thinning, the solder bumps 9 are placed on the through contact portion 18 of the thinned bottom wafer 4. Figure 7 b).

[0129] To achieve surface mountability, the bottom chip 4 includes:

[0130] - A through contact 18 (TSV) has a particularly small diameter and extends from the surface of the CMOS structure 8 to the underside of the central wafer 3 and the bottom wafer 4. Contacts for the interface are fed outward from the through contact 18 to external modules for other signal processing or to the voltage supply.

[0131] - Solder bump 9, which is disposed on the lower end of the through contact 18, so as to mechanically and electrically connect the sensor chip (central wafer 3) to the wiring support (e.g., circuit board, not shown) below.

[0132] However, some details should be noted during the installation of the three chips:

[0133] For example, the wafers must be oriented very precisely relative to each other, which can be achieved, for example, by etching holes using a dry etching technique (DRIE) or a similar etching method on the cover wafer 1, so that comparison marks can be aligned. Infrared alignment methods are also applicable here, since silicon wafers are transparent to infrared radiation.

[0134] Alignment holes or multiple asymmetrical holes or notches in the corners of the upper cover wafer 1 (filter wafer) can help with precise, positioned mounting of the wafer stack during SMD processes.

[0135] In one particular embodiment, a through contact 6 leading to the bottom wafer 4 is introduced into the central wafer 3 at the corner of each sensor pixel 5, where CMOS signal processing is performed.

[0136] In another specific embodiment, another bottom wafer 19 (CMOS wafer) may be mounted below the bottom wafer 4, which has sensor-side (analog / digital) signal processing (see [reference]). Figure 8 The additional bottom chip 19 can contain additional image processing capabilities, such as an image processor, large data storage, or other digital computing units. With the same external dimensions (length / width) and only slightly greater thickness, the sensor chip can therefore have more image processing capabilities.

[0137] Therefore, as described above, the original bottom wafer 4 is pre-mounted in the wafer stack. Figure 8 a) and thinning. However, after contact formation, solder bumps are not applied to the bottom wafer 4, but are only allowed to be applied to the contact pads 20, which are then electrically connected to the additional bottom wafer 19. Figure 8b). An additional bottom wafer 19, having additional signal processing components 22 (e.g., an image processor or a relatively large digital image memory), is then aligned with the upper wafer, forming a through contact 21 in the second bottom wafer 19 that matches the bottom wafer 4, and a corresponding via is prepared for the final electrical contact of the entire module of the wafer stack, the via completing the final electrical contact through a contact bump 9' at the lower end of the interconnection 21. Figure 8 e).

[0138] The upper wafer and the additional bottom wafer 19 are securely mechanically connected to the bottom wafer 4 by conventional wafer bonding methods, and a contact (electrical interconnection) is formed between the wafer sides that are stacked on top of each other. Figure 8 d).

[0139] In the final process step, the attached bottom wafer 19 is thinned and subsequently formed with contact bumps 9 for SMD mounting (e.g., solder, conductive adhesive, etc.) (see [link to process details]). Figure 8 e).

[0140] After thinning, the total thickness of the resulting quadruple wafer stack may be less than 0.5 mm to less than 1 mm, because the cover wafer 1 (filter wafer) is still the thickest. As long as the wafer stack as a whole has sufficient mechanical stability for wafer processing, the three wafers arranged below can be thinned to less than 100 µm in the assembly, respectively.

[0141] Figure 9 A further configuration of the thermopile array in a wafer-level package is shown, which also does not require a TSV. However, compared to Figure 4 different( Figure 4 It also does not have TSV), however, due to the inverted mounting, direct electrical contact is possible through the corresponding contact pad 25 of the central wafer 3 and the contact pad 24 of the bottom wafer 4. Figure 9 a, Figure 9 g), these contact pads have integrated advanced image processing. Therefore, evaluation electronics can even be fully integrated onto the bottom chip 4, freeing up space for more sensor pixels 5. Thus, pixel density can be increased even further.

[0142] Figure 9 This illustrates a thermopile array in a wafer-level package, featuring an inverted, very thin central wafer 3 without through-holes (through-contact portions). Figure 9 af), Figure 9 g shows an enlarged single unit with an umbrella-shaped portion 7 on the membrane 5''.

[0143] This is a particularly economical variant. The front side of the bottom wafer 4 is located on the front side of the central wafer 3. The two front sides are oriented relative to each other, and each front side has corresponding contact pads and solder paste, or has means (not shown) for providing electrical contact. Then, the contact pads 24 on the bottom wafer 4 are directly aligned with the contact pads 25 on the central wafer 3. Figure 9 a). The two wafers are then mechanically bonded together securely using conventional wafer bonding methods, after which the central wafer 3 is significantly thinned, ideally to less than 15 µm. Figure 9 b).

[0144] The cavity 11 of the pixel is then fabricated using DRIE, and a three-dimensional absorber structure, namely the umbrella-shaped portion 7, is introduced into the cavity 11. Figure 9 c). The cover wafer 1 is thinned and a cavity and filter layer are inserted ( Figure 9 d). The cover wafer 1 is then securely mechanically bonded to the wafer assembly consisting of the bottom wafer 4 and the central wafer 3 using conventional wafer bonding methods. Figure 9 e).

[0145] The entire chip assembly, consisting of three chips, was then inverted so that the bottom chip 4 is now at the bottom. Figure 9 f). The chip can now be placed and bonded to a suitable substrate, and electrically connected to the substrate below (not shown) via wire bonding bridge 17.

[0146] To apply the chip onto an underlying substrate such as a printed circuit board (PCB), solder bumps as mentioned in the previous embodiments can also be applied. The wire bonding bridge 17 is redundant in this case. Because of this method, since the CMOS electronics on the bottom wafer and the central wafer (4, 3) are in direct contact via corresponding contact pads 24, 25, through-contacts are not required.

[0147] To illustrate, Figure 9 g shows details of the pixel area. The umbrella-shaped portion 7 of the sensor pixel 5 is located on the membrane 5'' in the cavity 11 (opposite to the previous embodiment). The contact pads 24 of the bottom wafer 4 are electrically connected to the contact pads 25 of the central wafer 3. The signal processing 8 (CMOS processing) is located on the bottom wafer 4.

[0148] For completeness, it should be mentioned that, in principle, even more thin wafers can be added to the wafer stack. Power-saving semiconductor technologies, particularly for signal processing and microprocessor circuitry on the lower wafers, are desirable, ensuring that the overall power loss does not significantly impact the so-called thermal shock problem of heat-sensitive wafers. Excessive power loss in the wafer stack can lead to prolonged transients after power-on and cause measurement errors.

[0149] Figure 3-9 The exemplary embodiments described herein have cavities 11, 16 etched from the front or back for mounting in a QFN package via wire bonding in COB technology or via SMD auto-mount, and some embodiments also use an additional bottom wafer 19 with additional signal processing components, and these embodiments can of course be combined with each other in any desired manner.

[0150] Through all the embodiments described, the goal of constructing a particularly flat, vacuum-sealed, and mechanically stable thermopile array has been achieved.

[0151] In addition, Figure 4 and Figure 6 The simplified variant in this embodiment has two significant advantages over the prior art:

[0152] On the one hand, almost the entire area of ​​the central chip 3 can be used for the sensor pixel 5 itself, while the equally large area required for signal processing channels 8 is arranged on the bottom chip 4 below. Thus, a minimum size of the sensor mezzanine is achieved, which in turn is an advantage of small infrared camera modules in so-called "mobile devices" (e.g., smartphones), which achieve particularly high integration or high packaging density.

[0153] On the other hand, the central chip 3 with sensor pixel 5 can be manufactured using a technology particularly suited to thermopile structures, while the bottom chips (or additional bottom chips) 4, 19 can be manufactured using "mixed-signal" CMOS technology, which does not require the integration of special thermopile structures or does not need to consider them.

[0154] according to Figure 9 Because of the inverted mounting, the entire signal processing can even be accommodated on the bottom chip 19 below.

[0155] The second objective of a particularly high-resolution (space and thermal) thermopile array is achieved through three measures according to the invention:

[0156] - Central wafer 3, particularly in the scheme of etching cavity 11 from the back of the wafer (i.e., according to...) Figure 3 , 4 (7 and 8, 9), after thinning to such a small remaining thickness, it becomes possible to construct smaller thermopile pixels than previously known, i.e., the silicon edge of the sensor pixel 5 surrounding the cavity 11 after DRIE etching (used for thermal separation and as a heat sink for cold contacts) can be reduced to a few micrometers. Therefore, the remaining film size is larger relative to the pixel size, i.e., smaller pixels become possible (e.g., less than 25-50 µm).

[0157] - The signal electronics (ROIC) are preferably housed on the bottom wafers 4, 19 via very small through-contacts 6 (with a small diameter). The space there is larger than the space next to the thermopile array on the central wafer 3. Ideally, almost the entire chip area can be used for the focal plane array (…). Figure 9 ).

[0158] - If the bottom chip 4 (or as Figure 5 , 7 The other bottom chip 19 in 8 can be used with almost the entire chip area of ​​the signal processing channel (SPC), so in a high-resolution array, fewer sensor pixels 5 must share the signal processing channel, or more area can be reserved for a single preamplifier. The more SPCs running in parallel, the smaller the noise bandwidth, and the noise of the preamplifier also decreases with the increase in area. Both of these measures reduce noise and improve the noise-limited temperature resolution (NETD) of the pixel.

[0159] This function will be briefly explained with reference to thermal array sensors with thermopile pixels. In principle, the following also applies to other thermal sensor principles, such as thermoelectric sensors or microbolometers.

[0160] The thermopile structure is integrated on a silicon chip in a known manner, which is fabricated on a wafer (a central wafer 3 containing sensor pixels 5). The thermopile array contains a large number of individual sensor pixels 5, which are typically arranged in rows and columns in a matrix.

[0161] Following the actual CMOS process, sensor pixel 5 is produced using a special CMOS-compatible microsystems technology method. Sensor pixel 5 is located, for example, on a thin dielectric layer such as silicon dioxide, silicon nitride, silicon carbide, or a combination thereof.

[0162] Following the CMOS process of central wafer 3, the MEMS process is performed. In the first stage of the MEMS process (still before mounting cover wafer 1), the passivation layer above the thermocouple is thinned, and the slit 11'' behind the beam 11' for thermal insulation is introduced from the top side of the wafer to the silicon bulk boundary. This is typically done by so-called dry etching or a similar anisotropic method.

[0163] The central portion of membrane 5'' is equipped with an infrared absorbing layer ( Figure 2 d). For this purpose, a three-dimensional umbrella-shaped portion 7 (shielding structure) is preferably produced to impart a shielding structure to the sensor pixel 5 ( Figure 2 e) Exceptionally high fill factor. An additional absorption layer can be applied to the umbrella-shaped portion 7 to further increase infrared sensitivity.

[0164] Further MEMS steps are performed only after the cover wafer 1 and the central wafer are mounted, using known wafer bonding methods. Figure 3 ac).

[0165] In all variants, the thermopile sensor pixel 5 ( Figure 3 e) The cavity 11 below is etched, wherein the ideal back-side etching of the cavity 11 below the pixel is performed only after the central wafer 3 or the wafer with the sensor pixel 5, and in the wafer assembly, the cover wafer 1 is thinned to a smaller thickness, thereby improving the accuracy of the etching. However, in principle, etching at another point is also possible if, in particular, the CMOS compatibility requirements of the wafer manufacturing plant allow and reliable wafer processing is ensured.

[0166] After the central thermopile wafer 3 is thinned ( Figure 3 d), according to the present invention, the cavity 11 is formed from the back side by DRIE dry etching ( Figure 3 e) Introduce a central wafer 3 that has been significantly thinned (typically less than 50-100 μm).

[0167] Following the second MEMS stage, a self-supporting film 5'' is formed on the front side of the central wafer 3 by the aforementioned dielectric layer and insulating slits 11'' for the rods (beams 11'). Besides providing thermal insulation for the subsequent sensitive IR pixels, the self-supporting film 5'' also allows for gas exchange (vacuum between the upper and lower sides of the sensor pixels) and the effective function of getters (e.g., ...). Figure 3 f and Figure 3 g), as mentioned above.

[0168] The thermal contact and thermoelectric element are located on a thin film 5'' at the center of the thermopile sensor pixel 5. Between the thermal contact area in the center of the film 5'' and the silicon heat sink, a thermocouple is supported on a beam 11' (narrow connecting element). The beam 11' is thermally insulated from the center of the film 5'' and the silicon heat sink (the silicon material surrounding the cavity 11) through a slit 11'' in the film 5'', and thus reduces heat transfer from the thermal contact on the film 5'' to the silicon heat sink.

[0169] Semiconductor materials with high Seebeck coefficients can be used for thermocouples. Polycrystalline silicon, amorphous silicon layers, SiGe layers, and special implanted layers with high thermoelectric coefficients (e.g., bismuth or antimony and their compounds) are all possible.

[0170] Like all the other wafers below, the cover wafer 1 is preferably made of silicon, since all wafers then have the same coefficient of thermal expansion, although in principle other materials, such as glass substrates or other organic and inorganic materials, can also satisfy the required optical properties (e.g., Ge or so-called chalcogenides).

[0171] The bottom chips 4, 19 are preferably made of silicon, although they may also be composed of other materials (such as glass), but the disadvantage is lower integration because they lack signal processing capabilities or have far fewer signal processing capabilities than silicon chips. The bottom chips 4, 19 may also be composed of organic materials and, for example, contain organic electronics to simplify their use on flexible supports, such as in foldable smartphones.

[0172] The processes and arrangements known in the fabrication and assembly of individual wafers are deliberately discussed only very briefly here, as they are already known.

[0173] Vacuum-filled wafer-level casing should be understood as a wafer-level casing that has been evacuated, or as a wafer-level casing in which a vacuum exists.

[0174] List of reference numerals

[0175] 1. The upper cover chip

[0176] 1' pole

[0177] 2. Filter layer

[0178] 3. Central chip

[0179] 4 Bottom chip

[0180] 5 sensor pixels

[0181] 5' strip

[0182] 5'' membrane

[0183] 6 Straight through contact part

[0184] 7. Umbrella-shaped section (radiation collector)

[0185] 8 CMOS signal processing channels

[0186] 9. Contact bumps

[0187] 9' Contact bump

[0188] 10. Cavity in the filter layer

[0189] 11. Cavity

[0190] 11' Liang

[0191] 11'' slit

[0192] 12 pixels with umbrella-shaped portions

[0193] 13. Cavity

[0194] 14. Getter

[0195] 15 pads

[0196] 16. Cavity

[0197] 17-line bridge

[0198] 18 Straight through contact part

[0199] 19 Additional bottom chip

[0200] 20 Contact pads

[0201] 21 Contact pads

[0202] 22 Signal Processing

[0203] 23 Contact pads

[0204] 24 Contact pads

[0205] 25 Contact pads

Claims

1. A method for producing a thermal infrared sensor array in a vacuum-filled wafer-level housing, the wafer-level housing having a thickness of less than 1.2 mm, the wafer-level housing comprising at least two wafers, the two wafers being a cover wafer (1) and a central wafer (3), the central wafer (3) having a plurality of sensitive infrared-sensitive sensor pixels (5) respectively located on a slit-film (5'') above an adiabatic cavity (11), Its features are, First, at least one cavity (10) is formed on the inner side of the cover wafer (1), and is firmly mechanically connected to the central wafer (3) with infrared-sensitive sensor pixels (5) by wafer bonding. Then, the central wafer (3) is thinned from the back side of the wafer to a predetermined thickness. At least one bottom wafer (4) is fixed to the back side of the central wafer (3) by wafer bonding, and the bottom wafer (4) is thinned after wafer bonding.

2. The method according to claim 1, characterized in that, After the central wafer (3) has been thinned to a predetermined thickness, the thermally insulating cavity (11) passes through the slit (11'') in the thin film (5'') from the front and enters the central wafer (3) to be etched under the slit thin film (5'') of each infrared-sensitive sensor pixel (5).

3. The method according to claim 1, characterized in that, After the central wafer (3) has been thinned to the predetermined thickness, an adiabatic cavity (11) is etched from the back side into the central wafer (3) under the thin film (5'') of each infrared-sensitive sensor pixel (5).

4. The method according to any one of claims 1-3, characterized in that, After wafer bonding, the thickness of the central wafer (3) is reduced to less than 300 μm.

5. The method according to any one of claims 1-3, characterized in that, In addition to the sensor pixels (5), at least a portion of the signal preprocessing of the sensor pixels is integrated on the central chip (3).

6. The method according to claim 1, characterized in that, After the central wafer (3) is thinned, the through contact (6) is introduced from the front side of the central wafer (3) to the back side of the central wafer (3).

7. The method according to any one of claims 1-3, characterized in that, After wafer bonding, the thickness of the bottom wafer (4) is reduced to less than 300 μm.

8. The method according to any one of claims 1-3, characterized in that, The bottom chip (4) is equipped with a part of the signal processing of the sensor array.

9. The method according to any one of claims 1-3, characterized in that, The bottom chip (4) has a through contact (18) from the front to the back.

10. The method according to any one of claims 1-3, characterized in that, The bottom chip (4) located at the bottom has metal sputtering on its underside, which enables the bottom chip (4) to be SMD mounted by soldering, welding or adhesive bonding.

11. The method according to any one of claims 1-3, characterized in that, The bottom wafer (4) has at least one cavity (10) in which a getter (14) for stabilizing the vacuum is introduced, and the getter (14) is subsequently activated by the getter (14) through an aperture in the sensor pixel (5) or at least one additional aperture in the central wafer (3) to ensure the airtightness of the cavity (10) in the cover wafer (1) above the sensor pixel (5).

12. The method according to any one of claims 1-3, characterized in that, At least one additional bottom wafer (19) containing additional signal processing components, image processors or chips for artificial intelligence is disposed below the bottom wafer (4).

13. The method according to any one of claims 1-3, characterized in that, The cover plate (1) is made of infrared-transmitting material.

14. The method according to any one of claims 1-3, characterized in that, An infrared-transmitting anti-reflective layer or filter layer is applied to both sides of the cover wafer (1).

15. The method according to claim 14, characterized in that, The infrared transmission antireflective layer has a long-pass or band-pass coating to block a predetermined wavelength range.

16. The method according to claim 6, characterized in that, The through contact (6) of the central wafer (3) is mechanically and electrically connected to the contact pad (20) on the front side of the bottom wafer (4), connected to the through contact (18) of the bottom wafer (4) and the through contact (21) of the other bottom wafer (19), and the through contact (6) of the central wafer (3) is then thinned, and the through contact (21) in the other bottom wafer (19) is provided with contact pad (9').

17. The method according to any one of claims 1-3, characterized in that, After being mechanically connected to the cover wafer (1), the thickness of the central wafer (3) is reduced to less than 15 µm.

Citation Information

Patent Citations

  • Etching of infrared sensor membrane

    EP2889909A2

  • Method of making a thermopile detector and package

    US20080128620A1

  • Infrared sensor and infrared sensor module

    US8519336B2

  • Method for hermetically sealing with reduced stress

    WO2015004166A1

  • Wafer-level vacuum packaged infrared detector and manufacturing method thereof

    CN102583220A