Light emitting device, display device and manufacturing method

By employing an electron transport layer structure with a core-encased shell in organic light-emitting devices, the problem of poor performance of electron transport layer materials is solved, achieving efficient carrier balance and extended device lifetime, while improving luminous efficiency and interface stability.

CN114566598BActive Publication Date: 2026-11-20BOE TECHNOLOGY GROUP CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202011354418.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-11-27
Publication Date
2026-11-20
Estimated Expiration
2040-11-27

AI Technical Summary

Technical Problem

Existing organic light-emitting display products face challenges in achieving high resolution, resulting in high technical difficulty and low yield. Poor performance of electron transport layer materials leads to short lifespan of light-emitting devices, carrier imbalance, and low luminous efficiency.

Method used

An electron transport layer structure with a core-shell is adopted. By adjusting the particle size and thickness of the core and shell, the difference between the number of electrons and holes reaching the light-emitting layer per unit time is controlled within a preset threshold range, which promotes carrier balance. Furthermore, the chemical stability and electron injection efficiency are improved by selecting the shell material.

Benefits of technology

It improves the lifespan and luminous efficiency of light-emitting devices, reduces the turn-on voltage, enhances carrier balance and interface stability, and improves luminous performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114566598B_ABST
    Figure CN114566598B_ABST
Patent Text Reader

Abstract

The application discloses a light-emitting device, a display device and a manufacturing method, which aims at improving the poor performance of the electron transport layer material in the light-emitting device, reducing the service life of the light-emitting device, and solving the problems of carrier imbalance and low light-emitting efficiency. The light-emitting device comprises an electron transport layer between the light-emitting layer and the cathode layer; the material of the electron transport layer comprises a core and a shell layer wrapping the core; when the number of electrons reaching the light-emitting layer per unit time is greater than the number of holes, and the difference between the number of electrons reaching the light-emitting layer per unit time and the number of holes exceeds a preset threshold range, the particle size of the core is reduced and / or the thickness of the shell layer is increased; when the number of electrons reaching the light-emitting layer per unit time is less than the number of holes, and the difference between the number of electrons reaching the light-emitting layer per unit time and the number of holes exceeds a preset threshold range, the particle size of the core is increased and / or the thickness of the shell layer is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of display technology, and more particularly to a light-emitting device, a display apparatus, and a method for manufacturing it. Background Technology

[0002] Organic light-emitting diodes (OLEDs) were once widely recognized as the promising next-generation display technology to replace liquid crystal displays (LCDs). However, with rising consumer spending power, high-resolution products have become the focus of display product development. High-resolution OLEDs struggle to compete with LCDs because the organic layer structure is typically fabricated using mask evaporation, a method plagued by alignment difficulties, low yield, and the inability to achieve smaller luminescent areas. This lack of precise control over the evaporation area fails to meet the rapidly growing demand for high-resolution displays. Furthermore, using printing methods to replace mask evaporation for OLED fabrication also yields extremely limited resolution. Therefore, high-resolution OLEDs face serious challenges: high technical difficulty, low yield, and high price.

[0003] On the other hand, with the in-depth development of quantum dot technology, the research on electroluminescent quantum dot light-emitting diodes has become increasingly in-depth, and the quantum efficiency has been continuously improved, basically reaching the level of industrialization. Further adopting new processes and technologies to realize its industrialization has become the future trend.

[0004] Currently, the structure of traditional light-emitting devices includes a hole injection layer (HI), a hole transport layer (HT), a light-emitting layer (QD layer), and an electron transport layer (ET). However, the poor performance of the electron transport layer material reduces the lifetime of the light-emitting device. Summary of the Invention

[0005] This invention provides a light-emitting device, a display device, and a manufacturing method to improve the problems of poor performance of electron transport layer materials in light-emitting devices, reduced device lifespan, carrier imbalance, and low luminous efficiency.

[0006] This invention provides a light-emitting device, comprising: an anode, a light-emitting layer, and a cathode stacked sequentially; and an electron transport layer located between the light-emitting layer and the cathode layer, wherein the difference between the number of electrons and the number of holes reaching the light-emitting layer per unit time is less than a preset threshold range. The electron transport layer is made of a core and a shell enclosing the core. The conductivity of the core and the shell is used to regulate the number of electrons reaching the light-emitting layer per unit time. When the number of electrons reaching the light-emitting layer per unit time is greater than the number of holes, and the difference between the number of electrons and the number of holes reaches the light-emitting layer per unit time exceeds a preset threshold range... The particle size of the core is reduced and / or the thickness of the shell is increased to ensure that the difference between the number of electrons and holes reaching the light-emitting layer per unit time is within a preset threshold range, thereby promoting the balance of electrons and holes in the light-emitting layer. When the difference between the number of electrons reaching the light-emitting layer per unit time being less than the number of holes and the number of electrons reaching the light-emitting layer per unit time being greater than the number of holes exceeds the preset threshold range, the particle size of the core is increased and / or the thickness of the shell is decreased to ensure that the difference between the number of electrons and holes reaching the light-emitting layer per unit time is within the preset threshold range, thereby promoting the balance of electrons and holes in the light-emitting layer.

[0007] In one possible implementation, the gap between the cathode layer and the electron transport layer is further filled with a first filling layer, the material of which is the same as that of the shell layer; and / or, the gap between the electron transport layer and the light-emitting layer is filled with a second filling layer, the material of which is the same as that of the shell layer.

[0008] In one possible implementation, the thickness of the first filling layer is greater than or equal to the thickness of the electron transport layer; or, the thickness of the second filling layer is greater than or equal to the thickness of the electron transport layer.

[0009] In one possible implementation, the thickness of the second filling layer is greater than or equal to the thickness of the light-emitting layer.

[0010] In one possible implementation, the first filling layer is an annealed film layer to have the same crystal phase as the shell layer; and / or, the second filling layer is an annealed film layer to have the same crystal phase as the shell layer.

[0011] In one possible implementation, the shell is made of a metal oxide.

[0012] In one possible implementation, the metal oxide contains a metal in its highest valence state.

[0013] In one possible implementation, the material of the shell includes one or a combination of the following:

[0014] SnO2;

[0015] Cu2O;

[0016] Fe2O3;

[0017] TiO2;

[0018] ZrO2;

[0019] CoO;

[0020] WO3;

[0021] In2O3;

[0022] Al2O3;

[0023] Fe3O4.

[0024] In one possible implementation, the core material comprises one or a combination of the following: ZnO, ZnMgO, ZnAlO, ZnLiO, and ZnAgO.

[0025] In one possible implementation, the shell has a thickness of 0.1 nm to 100 nm; the core is a nanoparticle with a particle size between 0.1 nm and 100 nm.

[0026] In one possible implementation, the electron transport rate of the shell material is less than that of the core material.

[0027] In one possible implementation, the conduction band bottom level depth of the shell is greater than that of the core; the valence band top level depth of the shell is greater than that of the core.

[0028] In one possible implementation, the band gap width of the shell is negatively correlated with the thickness of the shell.

[0029] In one possible implementation, the depth of the conduction band bottom level of the shell is negatively correlated with the thickness of the shell.

[0030] In one possible implementation, the light-emitting layer is an organic light-emitting layer; or, the light-emitting layer is a quantum dot light-emitting layer.

[0031] In one possible implementation, when the light-emitting layer is a quantum dot light-emitting layer, the light-emitting layer includes a plurality of light-emitting portions of quantum dots with different particle sizes, and the second filling layer includes a plurality of control portions corresponding to the light-emitting portions, wherein the thickness of the control portions is positively correlated with the corresponding quantum dot particle size.

[0032] In one possible implementation, the light-emitting device further includes a substrate, wherein the anode, the light-emitting layer, the electron transport layer and the cathode are sequentially disposed on one side of the substrate; or the cathode, the electron transport layer, the light-emitting layer and the anode are sequentially disposed on one side of the substrate.

[0033] In one possible implementation, a hole injection layer is further disposed between the anode and the light-emitting layer, and a hole transport layer is further disposed between the hole injection layer and the light-emitting layer.

[0034] This invention also provides a display device, including the light-emitting device as described in this invention embodiment.

[0035] This invention also provides a method for manufacturing a light-emitting device as described in this invention, comprising:

[0036] An anode, a light-emitting layer, an electron transport layer, and a cathode are sequentially stacked.

[0037] The formation of the electron transport layer includes:

[0038] The first solution containing core particles is formed;

[0039] A second solution containing the elements contained in the shell is formed;

[0040] The second solution is added to the first solution, mixed evenly, and heated to form the core containing the shell.

[0041] In one possible implementation, the manufacturing method further includes:

[0042] A first thin film is formed between the cathode layer and the electron transport layer, the material of the first thin film being the same as that of the shell layer.

[0043] In one possible implementation, the manufacturing method further includes:

[0044] A second thin film is formed between the electron transport layer and the light-emitting layer, and the material of the second thin film is the same as that of the shell layer.

[0045] In one possible implementation, after forming the second filler layer and before forming the cathode layer, the fabrication method further includes:

[0046] The first thin film, the electron transport layer, and the second thin film are subjected to an annealing process to convert the first thin film into a first filler layer and the second thin film into a second filler layer.

[0047] The beneficial effects of the embodiments of the present invention are as follows: The light-emitting device provided by the embodiments of the present invention includes an electron transport layer. The material of the electron transport layer includes a core and a shell layer that encapsulates the core. The shell layer can encapsulate the core to isolate it from external water and oxygen, thereby improving the chemical stability of the core, improving the light-emitting device's resistance to water and oxygen, and increasing the lifespan of the light-emitting device. Moreover, the shell layer can passivate the surface defects of the core, improving the problem that when a light-emitting device with only a core is applied, the defects on the surface of the core will quench the light emission of the light-emitting layer in the light-emitting device. At the same time, the shell layer can lower the energy level barrier for electrons to migrate from the electron transport layer to the light-emitting layer, which is more conducive to electron injection. This can give the light-emitting device a lower turn-on voltage and a higher current density, resulting in better light-emitting performance. Furthermore, the balance of charge carriers in the light-emitting device can be controlled by regulating the core and shell. When the number of electrons reaching the light-emitting layer per unit time is greater than the number of holes, and the difference between the number of electrons reaching the light-emitting layer per unit time and the number of holes exceeds a preset threshold range, the particle size of the core is reduced and / or the thickness of the shell is increased to promote the balance of holes and electrons in the light-emitting layer. When the number of electrons reaching the light-emitting layer per unit time is less than the number of holes, and the difference between the number of electrons reaching the light-emitting layer per unit time and the number of holes exceeds a preset threshold range, the particle size of the core is increased and / or the thickness of the shell is decreased to promote the balance of holes and electrons in the light-emitting layer. Attached Figure Description

[0048] Figure 1 This is one of the structural schematic diagrams of the light-emitting device provided in the embodiments of the present invention;

[0049] Figure 2 This is a schematic diagram of the structure of a light-emitting device provided in an embodiment of the present invention;

[0050] Figure 3 This is a second schematic diagram of the structure of the light-emitting device provided in an embodiment of the present invention;

[0051] Figure 4 This is the third schematic diagram of the structure of the light-emitting device provided in the embodiment of the present invention;

[0052] Figure 5 A schematic diagram comparing the effects of light-emitting devices with and without shells on quantum dot luminescence, provided in an embodiment of the present invention.

[0053] Figure 6 A schematic diagram of the energy levels of the shell and core provided for an embodiment of the present invention;

[0054] Figure 7 A schematic diagram of the energy levels of a quantum dot light-emitting device provided in an embodiment of the present invention;

[0055] Figure 8A schematic diagram of the luminous brightness of a quantum dot light-emitting device provided in an embodiment of the present invention;

[0056] Figure 9 A schematic diagram of the current density of a quantum dot light-emitting device provided in an embodiment of the present invention;

[0057] Figure 10 This is the fourth schematic diagram of the structure of the light-emitting device provided in the embodiment of the present invention;

[0058] Figure 11 This is the fifth schematic diagram of the structure of the light-emitting device provided in the embodiment of the present invention;

[0059] Figure 12 This is the sixth schematic diagram of the structure of the light-emitting device provided in the embodiment of the present invention;

[0060] Figure 13 This is the seventh schematic diagram of the structure of the light-emitting device provided in the embodiment of the present invention;

[0061] Figure 14 This is a schematic diagram illustrating the fabrication of a light-emitting device provided in an embodiment of the present invention. Detailed Implementation

[0062] To make the objectives, technical solutions, and advantages of the embodiments of this disclosure clearer, the technical solutions of the embodiments of this disclosure will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some, not all, of the embodiments of this disclosure. All other embodiments obtained by those skilled in the art based on the described embodiments of this disclosure without creative effort are within the scope of protection of this disclosure.

[0063] Unless otherwise defined, the technical or scientific terms used in this disclosure shall have the ordinary meaning understood by one of ordinary skill in the art to which this disclosure pertains. The terms “first,” “second,” and similar terms used in this disclosure do not indicate any order, quantity, or importance, but are merely used to distinguish different components. Terms such as “comprising” or “including” mean that the element or object preceding the word encompasses the elements or objects listed following the word and their equivalents, without excluding other elements or objects. Terms such as “connected” or “linked” are not limited to physical or mechanical connections, but can include electrical connections, whether direct or indirect. Terms such as “upper,” “lower,” “left,” and “right” are used only to indicate relative positional relationships, and these relative positional relationships may change accordingly when the absolute position of the described objects changes.

[0064] To keep the following description of the embodiments of this disclosure clear and concise, detailed descriptions of known functions and known components are omitted.

[0065] The structure of quantum dot light-emitting devices includes a hole injection layer (HI), a hole transport layer (HT), a quantum dot (QD) layer, and an electron transport layer (ET). ZnO nanoparticles are commonly used as the electron transport material in the ET layer. However, due to the amphoteric nature of ZnO nanoparticles, they are susceptible to water and oxygen damage, exhibiting poor stability and causing abnormal brightness curves during device aging, thus reducing the lifetime of the quantum dot light-emitting device. Furthermore, the electron transport rate of ZnO nanoparticles is often greater than that of the hole transport material, leading to an imbalance in carrier injection in the quantum dot light-emitting device. This causes the exciton recombination region to shift towards the HT layer, reducing device performance. Simultaneously, surface defects in ZnO nanoparticles quench excitons, further degrading device performance. Moreover, the hole transport rate is lower than that of ZnO nanoparticles, resulting in an imbalance in carrier injection and reducing the device's luminous efficiency.

[0066] In view of this, see Figure 1 and Figure 2 As shown, this embodiment of the invention provides a light-emitting device comprising an anode 101, a light-emitting layer 104, and a cathode 106 stacked sequentially, and an electron transport layer 105 located between the light-emitting layer 104 and the cathode layer 106 such that the difference between the number of electrons and the number of holes reaching the light-emitting layer 104 per unit time is within a preset threshold range. Specifically, the preset threshold can be understood as a numerical range, and when the difference between the number of electrons and the number of holes reaching the light-emitting layer 104 per unit time is within this numerical range, the luminous efficiency of the light-emitting device meets the preset requirements.

[0067] The electron transport layer 105 is made of a core 1 and a shell 2 that surrounds the core 1. The conductivity of the core 1 and the shell 2 is used to control the rate at which electrons can be transferred from the cathode layer 106 to the light-emitting layer 104.

[0068] When the number of electrons reaching the light-emitting layer 104 per unit time is greater than the number of holes, and the difference between the number of electrons reaching the light-emitting layer 104 per unit time and the number of holes exceeds a preset threshold range, the particle size of the core 1 is reduced and / or the thickness of the shell 2 is increased so that the difference between the number of electrons and the number of holes reaching the light-emitting layer 104 per unit time is within the preset threshold range.

[0069] When the number of electrons reaching the luminescent layer 104 per unit time is less than the number of holes, and the difference between the number of electrons reaching the luminescent layer 104 per unit time and the number of holes exceeds a preset threshold range, the particle size of the core 1 is increased and / or the thickness of the shell 2 is decreased, so that the difference between the number of electrons and holes reaching the luminescent layer 104 per unit time is within the preset threshold range. The shell 2 can encapsulate the core 1 to isolate it from external water and oxygen.

[0070] The light-emitting device provided in this embodiment of the invention includes an electron transport layer 105. The material of the electron transport layer 105 includes a core and a shell layer encapsulating the core. The shell layer can encapsulate the core to isolate it from external water and oxygen, thereby improving the chemical stability of the core, improving the light-emitting device's resistance to water and oxygen, and increasing the lifespan of the light-emitting device. Moreover, the shell layer can passivate the surface defects of the core, improving the problem that when a light-emitting device with only a core is applied, the defects on the surface of the core will quench the light emission of the light-emitting layer in the light-emitting device. At the same time, the shell layer can reduce the energy level barrier for electrons to migrate from the electron transport layer to the light-emitting layer, which is more conducive to electron injection. This can give the light-emitting device a lower turn-on voltage and a higher current density, resulting in better light-emitting performance. Furthermore, the balance of charge carriers in the light-emitting device can be controlled by adjusting the core 1 and the shell 2. When the number of electrons arriving at the light-emitting layer 104 per unit time is greater than the number of holes, and the difference between the number of electrons arriving at the light-emitting layer 104 per unit time and the number of holes exceeds a preset threshold range, the particle size of the core is reduced and / or the thickness of the shell is increased to promote the balance of holes and electrons in the light-emitting layer 104. When the number of electrons arriving at the light-emitting layer 104 per unit time is less than the number of holes, and the difference between the number of electrons arriving at the light-emitting layer 104 per unit time and the number of holes exceeds a preset threshold range, the particle size of the core is increased and / or the thickness of the shell is decreased to promote the balance of holes and electrons in the light-emitting layer 104.

[0071] In practical implementation, when the number of electrons reaching the luminescent layer 104 per unit time is greater than the number of holes, and the difference between the number of electrons reaching the luminescent layer 104 per unit time and the number of holes exceeds a preset threshold, the conduction band bottom energy level of the electron transport layer should be shallowed. This increases the barrier for electrons to inject into the electron transport layer from the cathode, thereby reducing the number of electrons entering the electron transport layer from the cathode, ultimately ensuring that the number of electrons and holes reaching the luminescent layer 104 per unit time is equal. Specifically, the particle size of the synthesized core nanoparticles can be reduced to achieve the goal of shallowing the conduction band bottom energy level of the electron transport layer.

[0072] In practical implementation, when the number of electrons reaching the light-emitting layer 104 per unit time is greater than the number of holes, and the difference between the number of electrons reaching the light-emitting layer 104 per unit time and the number of holes exceeds a preset threshold range, the electron transport rate can be reduced to eventually make the number of electrons and holes reaching the light-emitting layer 104 per unit time equal. Specifically, the thickness of the shell can be appropriately increased to reduce the electron transport rate (i.e., the electron transport rate in shell 2 is less than the electron transport rate in core 1). Of course, considering that when the thickness of shell 2 increases, the bottom energy level of the electron transport layer conduction band is close to the cathode, which may lower the energy level barrier and increase the electron injection amount, in practical implementation, light-emitting devices with different shell 2 thicknesses can be designed to obtain the optimal shell 2 thickness.

[0073] In practical implementation, when the number of electrons reaching the luminescent layer 104 per unit time is less than the number of holes, and the difference between the number of electrons reaching the luminescent layer 104 per unit time and the number of holes exceeds a preset threshold, the conduction band bottom energy level of the electron transport layer should be deepened. This lowers the barrier for electrons to inject into the electron transport layer from the cathode electrode, thereby increasing the number of electrons entering the electron transport layer from the cathode, ultimately ensuring that the number of electrons and holes reaching the luminescent layer 104 per unit time is equal. Specifically, the particle size of the synthesized core nanoparticles can be increased to achieve the goal of deepening the conduction band bottom energy level of the electron transport layer.

[0074] In practical implementation, when the number of electrons reaching the light-emitting layer 104 per unit time is less than the number of holes, and the difference between the number of electrons reaching the light-emitting layer 104 per unit time and the number of holes exceeds a preset threshold range, the electron transport rate can be increased to ultimately make the number of electrons and holes reaching the light-emitting layer 104 per unit time equal. Specifically, the thickness of the shell can be appropriately reduced to increase the electron transport rate.

[0075] In specific implementations, the electron transport layer in this embodiment of the invention can be applied to an organic light-emitting device, that is, the light-emitting layer 104 can be an organic light-emitting layer. Specifically, the light-emitting device in this embodiment of the invention can also be applied to a quantum dot light-emitting device, that is, the light-emitting layer 104 can be a quantum dot light-emitting layer.

[0076] For specific implementation, see Figure 3 As shown, at least the gap between the cathode layer 106 and the shell layer 2 is filled with a first filler layer 1051, and the material of the first filler layer 1051 is the same as that of the shell layer 2. Specifically, the filling position of the first filler layer 1051 can vary depending on the manufacturing conditions, for example, combined with... Figure 3As shown, if the first filling layer 1051 is formed by magnetron sputtering, the depth reached by the first filling layer 1051 is limited, and it can only fill the gap between the side of the shell layer 2 facing the cathode layer 106 and the cathode layer 106. If the first filling layer 1051 is formed by liquid spin coating, the first filling layer 1051 can penetrate into the gap below the shell layer 2, and partially or completely fill the gap on the side of the shell layer 2 away from the cathode layer 106. Specifically, the light-emitting layer 104 can be a quantum dot light-emitting layer. In traditional device structures, both ZnO nanoparticles (electron transport material) and quantum dot luminescent materials are nanomaterials. During the thin film deposition process, due to the particle size of the materials themselves, pores and gaps are generated. During device operation, electrons can only be transported through the contact surface between the two, causing the luminescent surface to lose uniformity. This also easily leads to point discharge or a sharp increase in local temperature, resulting in dead pixels and reducing device lifespan. However, in this embodiment of the invention, the gap between the cathode layer 106 and the electron transport layer 105 is filled with a first filling layer 1051. The material of the first filling layer 1051 is the same as that of the shell layer 2, which can fill the gaps on the surface of the core / shell structure nanoparticles in the electron transport layer. Filling defects improves the uniformity and stability of charge carrier transport, prevents localized tip discharge, and flattens the surface of the core / shell structure, facilitating subsequent film formation, improving interface problems, enhancing interface stability, and allowing the core / shell nanoparticles to be fully encapsulated by the shell material, thus improving nanoparticle stability. Moreover, since the first filling layer and the shell of the core / shell nanoparticles use the same material, after high-temperature annealing and recrystallization, a unified crystal phase can be formed with fewer interface defects. In contrast, using different materials results in interfacial stress due to lattice mismatch, increasing interfacial defects. At the same time, the flat surface is conducive to the deposition of subsequent film layers (e.g., cathodes), forming a uniform contact interface with the subsequent film layers.

[0077] Specifically, in combination Figure 3 As shown, at least the gap between the shell layer 2 and the light-emitting layer 104 is filled with a second filling layer 1052, and the material of the second filling layer 1052 is the same as that of the shell layer 2. Specifically, the light-emitting layer 104 can be a quantum dot light-emitting layer. Similarly, the filling position of the second filling layer 1052 can vary depending on the fabrication conditions; for example, combined with… Figure 2As shown, if the second filling layer 1052 is formed by magnetron sputtering, the depth reached by the second filling layer 1052 is limited, and it can only fill the gap between the side of the shell layer 2 facing the light-emitting layer 104 and the light-emitting layer 104. If the second filling layer 1052 is formed by liquid spin coating, the second filling layer 1052 can penetrate into the gap below the light-emitting quantum dots, and also partially or completely fill the gap on the side of the light-emitting quantum dots facing the anode 101. In this embodiment of the invention, the shell layers of the core / shell structure nanoparticles are all formed with the same film layer (first filling layer 1051 and second filling layer 1052) as the shell material to form a unified crystal phase, which can reduce interface defects and fully encapsulate the core, thereby enhancing the stability of the core.

[0078] Specifically, the thickness of the first filling layer 1051 is greater than or equal to the thickness of the electron transport layer 105; or, the thickness of the second filling layer 1052 is greater than or equal to the thickness of the electron transport layer 105. For example, specifically, the thickness of the first filling layer 1051 being greater than or equal to the thickness of the electron transport layer 105 can be applied to a positive light-emitting device. During fabrication, the anode 101, the light-emitting layer 104, the electron transport layer 105, and the cathode 106 are formed sequentially. That is, the electron transport layer 105 is formed first, and then the first filling layer 1051 is used to fill it, so that the thickness of the first filling layer 1051 is greater than or equal to the thickness of the electron transport layer 105, which can make it flat before the electrodes are made. For example, if the thickness of the second filling layer 1052 is greater than or equal to the thickness of the electron transport layer 105, it can be applied to an inverted device, in which the cathode 106, electron transport layer 105, light-emitting layer 104 and anode 101 are formed in sequence. That is, the electron transport layer 105 is made first, and then the second filling layer 1052 is used to fill it, so that the thickness of the second filling layer 1052 is greater than or equal to the thickness of the electron transport layer 105, which can make it flat, and then the light-emitting layer 104 is made.

[0079] Specifically, the thickness of the second filling layer 1052 is greater than or equal to the thickness of the light-emitting layer 104. This approach is applicable to upright structures, i.e., the light-emitting layer 104 (which can be a quantum dot light-emitting layer) is fabricated first, followed by the second filling layer 1052. By making the thickness of the second filling layer 1052 greater than or equal to the thickness of the light-emitting layer 104, the surface of the quantum dot light-emitting layer can be made smooth, which is beneficial for the subsequent fabrication of the electron transport layer 105.

[0080] For specific implementation, see Figure 4As shown, the light-emitting layer 104 includes multiple light-emitting portions F with quantum dots of different sizes, and the second filling layer 1052 includes multiple control portions T corresponding to the light-emitting portions F. The thickness of the control portion T is positively correlated with the corresponding quantum dot particle size. Specifically, the light-emitting layer 104 includes: a first light-emitting portion F1 with quantum dots of a first size, a second light-emitting portion F2 with quantum dots of a second size, and a third light-emitting portion F3 with quantum dots of a third size, wherein the range of the first size is larger than the range of the second size, and the range of the second size is larger than the range of the third size; correspondingly, the control portion T includes: a first control portion T1 corresponding to the first light-emitting portion F1, a second control portion T2 corresponding to the second light-emitting portion F2, and a third control portion T3 corresponding to the third light-emitting portion F3; the thickness of the first control portion T1 is greater than the thickness of the second control portion T2, and the thickness of the second control portion T2 is greater than the thickness of the third control portion T3. Specifically, quantum dots of different sizes can correspond to quantum dots that emit different colors of light. For example, quantum dots of the first size can correspond to quantum dots that emit red light, quantum dots of the second size can correspond to quantum dots that emit green light, and quantum dots of the third size can correspond to quantum dots that emit blue light.

[0081] Specifically, in the design process of the light-emitting device, a first filling layer 1051 with a thickness of 5nm-10nm and a second filling layer 1052 with a thickness of 5nm-10nm are fabricated on both sides of the core / shell structure nanoparticles. The thickness of the second filling layer 1052 is determined by the size of the quantum dots in the quantum dot light-emitting layer. For example, when the particle size of red quantum dots is 8nm, the interface gaps and roughness caused by quantum dot accumulation are approximately 8nm. In this case, a 10nm thick shell material needs to be deposited to fill the gaps on the quantum dot surface and flatten the interface. When the particle size of green quantum dots is 5nm, the interface gaps and roughness caused by quantum dot accumulation are approximately 5nm. In this case, an 8nm thick shell material needs to be deposited to fill the gaps on the quantum dot surface and flatten the interface. When the particle size of blue quantum dots is 2nm, the interface gaps and roughness caused by quantum dot accumulation are approximately 2nm. In this case, a 5nm thick shell material needs to be deposited to fill the gaps on the quantum dot surface and flatten the interface.

[0082] In specific implementation, the first filling layer 1051 is a film layer processed by an annealing process to have the same crystal phase as the shell layer 2; the second filling layer 1052 is a film layer processed by an annealing process to have the same crystal phase as the shell layer 2. In this embodiment of the invention, the first filling layer 1051 and the second filling layer 1052 are both film layers processed by an annealing process. After high-temperature annealing and recrystallization, a uniform crystal phase can be formed, resulting in fewer interface defects. In contrast, dissimilar materials generate interface stress due to lattice mismatch, increasing interface defects.

[0083] For details, see Figure 5 As shown, the photoluminescence spectrum of the first film structure in the 600nm-650nm range is higher than that of the second film structure in the 600nm-650nm range. The first film structure is a quantum dot film covering the light-emitting device provided in the embodiments of the present invention (e.g., a structure of Glass / (ZnO / SnO2) / RQD, where ZnO is the core 1 of the light-emitting device, SnO2 is the shell 2 of the light-emitting device, and RQD is a red quantum dot film). The second film structure is a quantum dot film covering only the core 1 (e.g., a structure of Glass / ZnO / RQD, where ZnO is the core 1 of the light-emitting device, and RQD is a red quantum dot film). Due to the presence of defects on the surface of the core 1 (e.g., zinc oxide), the light emission of the quantum dot light-emitting layer formed by the light-emitting device will be quenched. However, by wrapping the core 1 with the shell 2, the surface defects of the core can be passivated, thereby improving the light emission intensity of the quantum dot light-emitting layer.

[0084] In specific implementations, the shell layer 2 is made of metal oxide. In this embodiment of the invention, the shell layer 2 is made of metal oxide, which, compared to encapsulating other types of materials (e.g., organic materials), allows the light-emitting device to have better water and oxygen resistance, better stability, and thus improve the lifespan of the light-emitting device. Specifically, water and oxygen resistance can be understood as not reacting chemically with water or oxygen, or reducing the rate of chemical reaction with water or oxygen.

[0085] Specifically, in a metal oxide, the metal is in its highest valence state. For example, in the metal oxide Fe₂O₃, Fe is in its highest valence state. In this embodiment of the invention, the metal is in its highest valence state in the shell 2 of the metal oxide, which can give the light-emitting device more stable chemical properties and thus better resistance to water and oxygen. Specifically, in a metal oxide, the metal being in its highest valence state can be understood as the maximum number of electrons that the metal can lose within the metal oxide.

[0086] Specifically, the material of shell 2 includes one or a combination of the following:

[0087] SnO2;

[0088] Cu2O;

[0089] Fe2O3;

[0090] TiO2;

[0091] ZrO2;

[0092] CoO;

[0093] WO3;

[0094] In2O3;

[0095] Al2O3;

[0096] Fe3O4.

[0097] In this embodiment of the invention, the essence of improving the water and oxygen resistance of the core is to isolate the contact between water and oxygen and the core. Therefore, metal oxides that are not in the highest oxidation state can also improve the water and oxygen resistance of the core. Moreover, metal oxides that are not in the highest oxidation state can also absorb some water and oxygen, thereby enhancing the water and oxygen resistance of the core.

[0098] For specific implementation, see Figure 6 As shown, the conduction band bottom energy level depth of shell 2 is greater than that of core 1. In this embodiment of the invention, the conduction band bottom energy level depth of shell 2 is greater than that of core 1. When this light-emitting device is used in a light-emitting device, the energy level barrier for electron migration from the electron transport layer to the light-emitting layer can be reduced, which is more conducive to electron injection. This allows the light-emitting device to have a lower turn-on voltage and a higher current density, resulting in better light-emitting performance.

[0099] For specific implementation, see Figure 6 As shown, the valence band top level depth of shell 2 is greater than that of core 1. In this embodiment of the invention, the greater valence band top level depth of shell 2 compared to core 1 enables the electron transport layer to block holes. When this electron transport layer is applied to a light-emitting device, holes can be confined to the light-emitting layer, reducing leakage current and improving the radiative recombination efficiency of holes and electrons in the light-emitting layer.

[0100] For details, see Figure 7 , Figure 8 , Figure 9 As shown, where, Figure 7 This is an energy level structure diagram illustrating the application of a light-emitting device provided in an embodiment of the present invention in a quantum dot light-emitting device. Figure 8 This is a schematic diagram showing the luminous intensity of a light-emitting device under different voltages. Figure 9 This diagram illustrates the current density of a light-emitting device at different voltages. The specific structure of the quantum dot light-emitting device (e.g.) Figure 8 and Figure 9 The structure (shown by the dashed line) may include: an anode (specifically, indium tin oxide, ITO), a hole injection layer (specifically, polyethylene dioxythiophene-poly(styrene sulfonate), PEDOT:PSS), a hole transport layer (specifically, TFB), a quantum dot emitting layer (specifically, a red quantum dot emitting layer RQD emitting red light), an electron transport layer (specifically, ZnO coated with SnO2), and a cathode (specifically, Al). To more clearly illustrate the improved performance of the light-emitting device provided in the embodiments of the present invention, a control device (such as...) is fabricated. Figure 8 and Figure 9 For comparison, the structure of the control device is identical to that of the quantum dot light-emitting device provided in this application, except that the electron transport layer is made of ZnO. Specifically, the structure of the control device may include, sequentially disposed on one side of the substrate, an anode (specifically, the material can be indium tin oxide ITO), a hole injection layer (specifically, the material can be polyethylene dioxythiophene-poly(styrene sulfonate), PEDOT:PSS), a hole transport layer (specifically, the material can be TFB), a quantum dot light-emitting layer (specifically, the material can be a red quantum dot light-emitting layer RQD emitting red light), an electron transport layer (specifically, the material can be ZnO), and a cathode (specifically, the material can be Al). Figure 4 , Figure 5 and Figure 6 It is known that the synthesized core-shell ZnO / SnO2 nanoparticles have a conduction band (-3.8 eV) and a valence band (-7.8 eV). The energy level difference between the conduction band and the Al electrode is only 0.4 eV, which is beneficial for electron injection into the ZnO / SnO2 layer. The LUMO (-4.5 eV) is higher than that of the RQD, which is beneficial for electron transport to the RQD layer. At the same time, the energy difference between the valence band peak (-7.8 eV) of the ZnO / SnO2 nanoparticles and the HOMO energy level of the RQD reaches 1.2 eV, which enables them to block holes, confining holes to the QD layer, reducing leakage current, and improving the radiative recombination efficiency of holes and electrons in the RQD layer. When the light-emitting device provided in this embodiment of the invention is used in a light-emitting device, the encapsulated shell can reduce the energy level barrier for electron migration from the electron transport layer to the light-emitting layer, which is more conducive to electron injection. This can give the light-emitting device a lower turn-on voltage and a higher current density, resulting in better light-emitting performance.

[0101] In practical implementation, the thickness of shell 2 is negatively correlated with its band gap width; specifically, the thickness of shell 2 is negatively correlated with its conduction band bottom energy level. That is, as the thickness of shell 2 increases, its band gap width narrows, and its conduction band bottom energy level decreases. In practical implementation, the thickness of shell 2 can be controlled based on the reaction time during its fabrication; the longer the reaction time, the greater the thickness of shell 2. For example, after 20 hours of reaction, the thickness of shell 2 is approximately 4 nm; after 10 hours, the thickness is approximately 2 nm. Specifically, the thickness of shell 2 ranges from 0.1 nm to 100 nm. It should be noted that the thickness of shell 2 can be specifically understood as its thickness along the radial direction of core 1.

[0102] In practical implementation, core 1 is composed of nanoparticles. Specifically, the material of core 1 is ZnO, ZnMgO, ZnAlO, ZnLiO, or ZnAgO. The particle size of core 1 is negatively correlated with its band gap width. That is, as the particle size of the core nanoparticles decreases, the band gap width widens, and the conduction band bottom rises. In practical implementation, the particle size of the final synthesized core nanoparticles can be controlled by adjusting the holding temperature of the precursor solution and the reaction temperature during the synthesis process. Higher temperatures result in larger particle sizes. For example, the particle size of ZnO nanoparticles synthesized at 0℃ is approximately 2.5 nm; at 25℃, it is approximately 4.1 nm; and at 50℃, it is approximately 5.3 nm. Specifically, the particle size of core 1 ranges from 0.1 nm to 100 nm.

[0103] The following tables, Tables 1 and 2, show the correlation between the performance of the synthesized core and shell under different conditions:

[0104] Table 1. Particle size, conduction band, valence band, and band gap of ZnO nanoparticles synthesized at different temperatures:

[0105] Temperature (°C) Particle size (nm) Conductor band (eV) Valence band (eV) Band gap (eV) 0 2.5 -3.6 -7.33 3.73 25 4.1 -3.7 -7.28 3.58 50 5.3 -3.8 -7.25 3.45

[0106] Table 2. Thickness, conduction band, valence band, and band gap of the SnO2 shell in core-shell ZnO (2.5 nm) / SnO2 nanoparticles synthesized at different reaction times:

[0107] Time (h) Thickness (nm) Conductor band (eV) Valence band (eV) Band gap (eV) 10 2 -3.7 -7.9 4.2 20 4 -3.9 -7.9 4

[0108] For specific implementation, see Figure 10 As shown, the light-emitting device provided in this embodiment of the invention can be an upright structure, that is, the light-emitting device further includes a substrate 100, wherein the anode 101, the light-emitting layer 104, the electron transport layer 105 and the cathode 106 are sequentially disposed on one side of the substrate 100.

[0109] For specific implementation, see Figure 11 As shown, the light-emitting device provided in this embodiment of the invention can be an inverted structure. The light-emitting device also includes a substrate 100, wherein a cathode 106, an electron transport layer 105, a light-emitting layer 104 and an anode 101 are sequentially disposed on one side of the substrate 100.

[0110] For specific implementation, see Figure 12 and Figure 13 As shown, a hole injection layer 102 is provided between the anode 101 and the light-emitting layer 104, and a hole transport layer 103 is provided between the hole injection layer 102 and the light-emitting layer 104.

[0111] In practical implementation, the material of the quantum dot light-emitting layer can include one of the following:

[0112] CdS;

[0113] CdSe;

[0114] ZnSe;

[0115] InP;

[0116] PbS;

[0117] CsPbCl3;

[0118] CsPbBr3;

[0119] CsPhI3;

[0120] CdS encapsulated with ZnS;

[0121] CdSe encapsulated with ZnS;

[0122] InP encapsulated with ZnS;

[0123] PbS encapsulated with ZnS;

[0124] CsPbCl3 encapsulated with ZnS;

[0125] CsPbBr3 encapsulated with ZnS;

[0126] CsPhI3 containing ZnS.

[0127] Based on the same inventive concept, embodiments of the present invention also provide a display device, including the light-emitting device as provided in embodiments of the present invention.

[0128] Based on the same inventive concept, see [link to inventive concept] Figure 14 As shown, this embodiment of the invention also provides a method for manufacturing a light-emitting device as provided in this embodiment of the invention, comprising:

[0129] Step S10: Form an anode, a light-emitting layer, an electron transport layer, and a cathode that are stacked sequentially;

[0130] The formation of the electron transport layer includes:

[0131] Step S100: Form a first solution containing core particles; specifically, it may be to form a first solution containing ZnO nanoparticles.

[0132] Specifically, forming a first solution containing ZnO nanoparticles may include:

[0133] Zn(OAc)2 is dissolved in a mixed solvent of dimethyl sulfoxide and dimethoxyethanol to form a first precursor solution;

[0134] Tetramethylammonium hydroxide pentahydrate is dissolved in ethanol to form a second precursor solution;

[0135] After the first precursor solution and the second precursor solution are respectively kept at a first temperature for a first time;

[0136] While stirring, the first precursor solution is rapidly injected into the second precursor solution, the first temperature is maintained, and the stirring is carried out for a second duration.

[0137] Add twice the volume of ethyl acetate, precipitate, centrifuge, and purify.

[0138] The purified ZnO nanoparticles were redispersed in anhydrous ethanol, and ethanolamine stabilizer was added to form a stable ZnO nanoparticle colloidal solution.

[0139] Step S200: Form a second solution containing the elements contained in the shell; specifically, this can be achieved by slowly adding tin tetrachloride dropwise into dichloromethane under anhydrous and oxygen-free conditions while continuously stirring to form a transparent and homogeneous second solution.

[0140] Step S300: Add the second solution to the first solution, mix well and heat to form a core containing a shell;

[0141] Specifically, adding a second solution to a first solution, mixing thoroughly, and heating to form a core containing a shell can include:

[0142] While stirring, add the ZnO nanoparticle colloidal solution to the second solution, mix well, and then pour the mixture into a high-pressure reactor.

[0143] The reactor was placed in an oven at a second temperature and the reaction was maintained at that temperature for a third time.

[0144] The temperature of the reactor was lowered to the third temperature, and ethyl acetate was added to precipitate white core / shell structured ZnO / SnO2 nanoparticles.

[0145] After centrifugation, discard the supernatant, add anhydrous ethanol, and redisperse the white precipitate.

[0146] Ethanolamine is added to form a transparent and uniform colloidal solution of ZnO / SnO2 nanoparticles.

[0147] Specifically, the manufacturing method provided in this embodiment of the invention further includes: forming a first thin film between the cathode layer and the electron transport layer, wherein the material of the first thin film is the same as the material of the shell layer.

[0148] Specifically, the manufacturing method provided in this embodiment of the invention further includes: forming a second thin film between the electron transport layer and the light-emitting layer, wherein the material of the second thin film is the same as the material of the shell layer.

[0149] In a specific implementation, in this embodiment of the invention, after the formation of the second filling layer and before the formation of the cathode layer, the manufacturing method provided by this embodiment of the invention further includes: performing an annealing process on the first thin film, the electron transport layer, and the second thin film to convert the first thin film into the first filling layer and the second thin film into the second filling layer.

[0150] This invention also provides a specific method for manufacturing a light-emitting device, as follows:

[0151] I. Synthesis of core / shell structured ZnO / SnO2 nanoparticles:

[0152] A. Preparation of ZnO nanoparticle cores:

[0153] Preparation of precursor solution 1 (first precursor solution): Weigh 220 mg (1 mmol) of Zn(OAc)2 and dissolve it in a mixed solvent of 10 mL dimethyl sulfoxide and 8 mL dimethoxyethanol;

[0154] Preparation of precursor solution 2 (second precursor solution): Weigh 330 mg (1.85 mmol) of tetramethylammonium hydroxide pentahydrate (TMAH) and dissolve it in 3.3 mL of ethanol;

[0155] After precursor solution 1 and precursor solution 2 were kept at 0℃ for 30 min, precursor solution 1 was rapidly injected into precursor solution 2 under vigorous stirring, and the reaction system was kept at 0℃ and stirred vigorously for 3 h.

[0156] After the reaction was completed, ethyl acetate of twice the volume was added to the system to precipitate and centrifuge to purify the synthesized ZnO nanoparticles. The purified ZnO nanoparticles were redispersed in 20 mL of anhydrous ethanol and 0.2 mL of ethanolamine stabilizer was added to form a stable ZnO nanoparticle colloidal solution. The ZnO nanoparticles synthesized in this step serve as the core of the subsequent core / shell structure ZnO / SnO2 nanoparticles.

[0157] B. Synthesis of core / shell structured ZnO / SnO2 nanoparticles:

[0158] Precursor solution 3: In an anhydrous and oxygen-free environment, slowly add 1.5 mL of tin tetrachloride to 10 mL of dichloromethane and stir continuously to prepare a transparent and homogeneous solution.

[0159] While stirring, 20 mL of the ZnO nanoparticle core colloidal solution synthesized in step A above was slowly added to precursor solution 3. After the system was mixed evenly, the mixture was poured into a high-pressure reactor (50 mL). The reactor was then placed in an oven at 100°C and kept at that temperature for 20 hours. After the reactor temperature was lowered to 25°C, 20 mL of ethyl acetate was added, and a white core / shell structure ZnO / SnO2 nanoparticle precipitate was formed. After centrifuging the mixture, the supernatant was discarded, and 20 mL of anhydrous ethanol was added to redisperse the white precipitate. Then, 0.5 mL of ethanolamine was added to form a transparent and uniform ZnO / SnO2 nanoparticle colloidal solution.

[0160] II. Fabrication of QLED Devices:

[0161] Taking red quantum dot devices as an example, the device structure is designed as ITO / PEDOT:PSS / TFB / RQD / (ZnO / SnO2) / Al. This invention designs and synthesizes core-shell structured ZnO / SnO2 nanoparticles as light-emitting devices, which are not limited to red quantum dots, but are applicable to quantum dot light-emitting diodes of any color, and are not limited to quantum dot materials (CdS, CdSe, ZnSe, InP, PbS, CsPbCl3, CsPbBr3, CsPhI3, CdS / ZnS, CdSe / ZnS, InP / ZnS, PbS / ZnS, CsPbCl3 / ZnS, CsPbBr3 / ZnS, CsPhI3 / ZnS, etc. quantum dots).

[0162] The device fabrication process is as follows:

[0163] 1. Clean the ITO glass substrate (substrate) with anhydrous ethanol and deionized water by ultrasonic cleaning for 15 minutes each, then dry it. Then treat the substrate with ultraviolet light for 10 minutes to improve the surface work function of ITO.

[0164] 2. After the above treatment, a hole injection layer PEDOT:PSS is spin-coated onto the ITO substrate, and the surface morphology of HI is improved by annealing at 120℃ for 15 min.

[0165] 3. Spin-coat hole transport layer material TFB onto the surface of the HI layer and anneal at 120℃ for 15 min to remove the solvent;

[0166] 4. A red quantum dot layer was spin-coated onto the TFB film and annealed at 100°C for 15 min to form a flat QD layer.

[0167] 5. Using a sputtering coating device, a 5nm-10nm SnO2 thin film is sputtered on the surface of the QD layer to fill the gaps and defects between quantum dots, enabling the quantum dots to make close contact with the electron transport material and to planarize its surface.

[0168] 6. Spin-coating electron transport material core / shell structured ZnO / SnO2 nanoparticles onto a planarized SnO2 QD surface;

[0169] 7. Using a sputter coating device, a 5nm-10nm SnO2 thin film is sputtered onto the surface of ZnO / SnO2 nanoparticles to fill the gaps and defects between the ZnO / SnO2 nanoparticles, making the surface flattened and facilitating the subsequent deposition of a flat and uniform electrode film; (In this device structure, ZnO nanoparticles are fully encapsulated by SnO2 material, maximizing the filling of surface defects of ZnO nanoparticles, improving the stability of ZnO nanoparticles, and improving device efficiency and lifespan);

[0170] 8. Annealing at 150℃ for 20 minutes improves the interfacial environment, allowing the thin SnO2 layer to form a unified crystalline phase with the SnO2 shell layer of the core-shell ZnO / SnO2 structure, resulting in denser interfacial contact and reduced interfacial defects. This is also the reason for using shell materials to prepare films on both sides of the core / shell ZnO nanoparticle film. After high-temperature annealing and recrystallization, the same material can form a unified crystalline phase with fewer interfacial defects, while dissimilar materials generate interfacial stress due to lattice mismatch, increasing interfacial defects.

[0171] 9. Vacuum evaporation of Al electrodes;

[0172] 10. Use a glass cover to encapsulate the device and complete its fabrication.

[0173] This invention also provides another method for manufacturing a light-emitting device, as follows:

[0174] Taking red-light multi-electron quantum dot devices as an example, core-shell structured ZnO / Al2O3 nanoparticles were designed and synthesized as electron transport materials (the insulation of Al2O3 material can significantly reduce the electron transport rate of ZnO, which is beneficial to improving the injection balance of charge carriers in the device. At the same time, Al2O3 material can fill the surface defects of ZnO nanoparticles, improve the water and oxygen resistance of ZnO, and improve the device performance). The device structure was designed as ITO / PEDOT:PSS / TFB / RQD / Al2O3(ZnO / Al2O3)Al2O3 / Al.

[0175] The fabrication process of the light-emitting device is as follows:

[0176] 1. Clean the ITO glass substrate with anhydrous ethanol and deionized water using ultrasonic cleaning for 15 minutes each, then dry it. Finally, treat the substrate with ultraviolet light for 10 minutes to improve the surface work function of ITO.

[0177] 2. After the above treatment, a hole injection layer PEDOT:PSS is spin-coated onto the ITO substrate, and the surface morphology of HI is improved by annealing at 120℃ for 15 min.

[0178] 3. Spin-coat the hole transport layer material (specifically TFB) onto the surface of the hole injection layer (HI) and anneal it at 120°C for 15 min to remove the solvent;

[0179] 4. Spin-coat a red quantum dot layer onto the hole transport layer and anneal it at 100°C for 15 min to form a flat QD layer;

[0180] 5. Using a sputter coating device, a 5nm-10nm Al2O3 thin film is sputtered on the surface of the QD layer to fill the gaps and defects between quantum dots, enabling the quantum dots to make close contact with the electron transport material and to planarize its surface.

[0181] 6. Spin-coat the Al2O3 planarized QD surface with core / shell structured ZnO / Al2O3 nanoparticles for electron transport material, and anneal at 120℃ for 15 min to remove solvent and organic matter;

[0182] 7. Using a sputter coating device, a 5-10 nm Al2O3 thin film is sputtered onto the surface of ZnO / Al2O3 nanoparticles to fill the gaps and defects between the ZnO / Al2O3 nanoparticles, making the surface flat and facilitating the subsequent deposition of a flat and uniform electrode film; (In this device structure, ZnO nanoparticles are fully encapsulated by Al2O3 material, maximizing the filling of surface defects of ZnO nanoparticles, improving the stability of ZnO nanoparticles, and improving device efficiency and lifespan);

[0183] 8. Annealing at 150℃ for 20 minutes improves the interfacial environment, allowing the thin Al2O3 layer to form a unified crystalline phase with the shell Al2O3 of the core-shell ZnO / Al2O3 structure, resulting in denser interfacial contact and reduced interfacial defects. This is also the reason for using shell materials to prepare films on both sides of the core / shell ZnO nanoparticle film. After high-temperature annealing and recrystallization, the same material can form a unified crystalline phase with fewer interfacial defects, while dissimilar materials generate interfacial stress due to lattice mismatch, increasing interfacial defects.

[0184] 9. Vacuum evaporation of Al electrodes;

[0185] 10. Use a glass cover to encapsulate the device and complete its fabrication.

[0186] The beneficial effects of the embodiments of the present invention are as follows: The light-emitting device provided by the embodiments of the present invention includes an electron transport layer. The material of the electron transport layer includes a core and a shell layer that encapsulates the core. The shell layer can encapsulate the core to isolate it from external water and oxygen, thereby improving the chemical stability of the core, improving the light-emitting device's resistance to water and oxygen, and increasing the lifespan of the light-emitting device. Moreover, the shell layer can passivate the surface defects of the core, improving the problem that when a light-emitting device with only a core is applied, the defects on the surface of the core will quench the light emission of the light-emitting layer in the light-emitting device. At the same time, the shell layer can lower the energy level barrier for electrons to migrate from the electron transport layer to the light-emitting layer, which is more conducive to electron injection. This can give the light-emitting device a lower turn-on voltage and a higher current density, resulting in better light-emitting performance. Furthermore, the balance of charge carriers in the light-emitting device can be controlled by regulating the core and shell. When the number of electrons arriving at the light-emitting layer per unit time is greater than the number of holes, and the difference between the number of electrons arriving at the light-emitting layer per unit time and the number of holes exceeds a preset threshold range, the particle size of the core is reduced and / or the thickness of the shell is increased to promote the balance of holes and electrons in the light-emitting layer. When the number of electrons arriving at the light-emitting layer per unit time is less than the number of holes, and the difference between the number of electrons arriving at the light-emitting layer per unit time and the number of holes exceeds a preset threshold range, the particle size of the core is increased and / or the thickness of the shell is decreased to promote the balance of holes and electrons in the light-emitting layer 104.

[0187] Obviously, those skilled in the art can make various modifications and variations to this invention without departing from its spirit and scope. Therefore, if these modifications and variations fall within the scope of the claims of this invention and their equivalents, this invention also intends to include these modifications and variations.

Claims

1. A light-emitting device, characterized in that, include: An anode, a light-emitting layer, and a cathode are stacked in sequence, and an electron transport layer is located between the light-emitting layer and the cathode layer, such that the difference between the number of electrons and the number of holes reaching the light-emitting layer per unit time is within a preset threshold range; The electron transport layer is made of a core and a shell that encloses the core. The conductivity of the core and the shell is used to control the number of electrons that reach the light-emitting layer per unit time. When the number of electrons reaching the light-emitting layer per unit time is greater than the number of holes, and the difference between the number of electrons reaching the light-emitting layer per unit time and the number of holes exceeds the preset threshold range, the particle size of the core is reduced and / or the thickness of the shell is increased, so that the difference between the number of electrons and the number of holes reaching the light-emitting layer per unit time is within the preset threshold range. When the number of electrons reaching the light-emitting layer per unit time is less than the number of holes, and the difference between the number of electrons reaching the light-emitting layer per unit time and the number of holes exceeds the preset threshold range, the particle size of the core is increased and / or the thickness of the shell is decreased, so that the difference between the number of electrons and the number of holes reaching the light-emitting layer per unit time is within the preset threshold range.

2. The light-emitting device as described in claim 1, characterized in that, At least the gap between the cathode layer and the shell layer is filled with a first filling layer, the material of which is the same as that of the shell layer; and / or, at least the gap between the shell layer and the light-emitting layer is filled with a second filling layer, the material of which is the same as that of the shell layer.

3. The light-emitting device as described in claim 2, characterized in that, The thickness of the first filling layer is greater than or equal to the thickness of the electron transport layer; or, the thickness of the second filling layer is greater than or equal to the thickness of the electron transport layer.

4. The light-emitting device as described in claim 2, characterized in that, The thickness of the second filling layer is greater than or equal to the thickness of the light-emitting layer.

5. The light-emitting device as described in claim 2, characterized in that, The first filling layer is an annealed film layer to have the same crystal phase as the shell layer; and / or, the second filling layer is an annealed film layer to have the same crystal phase as the shell layer.

6. The light-emitting device as described in claim 1, characterized in that, The shell is made of metal oxide.

7. The light-emitting device as described in claim 6, characterized in that, In the metal oxide, the metal is in its highest valence state.

8. The light-emitting device as described in claim 5, characterized in that, The material of the shell includes one or a combination of the following: SnO2; Cu2O; Fe2O3; TiO2; ZrO2; CoO; WO3; In2O3; Al2O3; Fe3O4.

9. The light-emitting device as described in claim 1, characterized in that, The core material includes one or a combination of the following: ZnO, ZnMgO, ZnAlO, ZnLiO, and ZnAgO.

10. The light-emitting device as claimed in claim 1, characterized in that, The shell has a thickness of 0.1 nm to 100 nm; the core consists of nanoparticles with a particle size between 0.1 nm and 100 nm.

11. The light-emitting device according to any one of claims 1-10, characterized in that, The electron transport rate of the shell material is less than that of the core material.

12. The light-emitting device according to any one of claims 1-10, characterized in that, The depth of the conduction band bottom level of the shell is greater than the depth of the conduction band bottom level of the core; the depth of the valence band top level of the shell is greater than the depth of the valence band top level of the core.

13. The light-emitting device according to any one of claims 1-10, characterized in that, The band gap width of the shell is negatively correlated with the thickness of the shell.

14. The light-emitting device according to any one of claims 1-10, characterized in that, The depth of the conduction band bottom level of the shell is negatively correlated with the thickness of the shell.

15. The light-emitting device according to any one of claims 1-10, characterized in that, The light-emitting layer is an organic light-emitting layer; or, the light-emitting layer is a quantum dot light-emitting layer.

16. The light-emitting device according to any one of claims 2-5, characterized in that, When the light-emitting layer is a quantum dot light-emitting layer, the light-emitting layer includes multiple light-emitting portions of quantum dots with different particle sizes, and the second filling layer includes multiple control portions corresponding to the light-emitting portions, the thickness of the control portions being positively correlated with the corresponding quantum dot particle size.

17. The light-emitting device according to any one of claims 1-10, characterized in that, The light-emitting device further includes a substrate, wherein the anode, the light-emitting layer, the electron transport layer and the cathode are sequentially disposed on one side of the substrate; or the cathode, the electron transport layer, the light-emitting layer and the anode are sequentially disposed on one side of the substrate.

18. The light-emitting device as claimed in claim 17, characterized in that, A hole injection layer is further disposed between the anode and the light-emitting layer, and a hole transport layer is further disposed between the hole injection layer and the light-emitting layer.

19. A display device, characterized in that, Including the light-emitting device as described in any one of claims 1-18.

20. A method for manufacturing a light-emitting device as described in any one of claims 1-18, characterized in that, include: An anode, a light-emitting layer, an electron transport layer, and a cathode are sequentially stacked. The formation of the electron transport layer includes: The first solution containing core particles is formed; A second solution containing the elements contained in the shell is formed; The second solution is added to the first solution, mixed evenly, and heated to form the core containing the shell.

21. The manufacturing method as described in claim 20, characterized in that, The manufacturing method further includes: A first thin film is formed between the cathode layer and the electron transport layer, the material of the first thin film being the same as that of the shell layer.

22. The manufacturing method as described in claim 21, characterized in that, The manufacturing method further includes: A second thin film is formed between the electron transport layer and the light-emitting layer, and the material of the second thin film is the same as that of the shell layer.

23. The manufacturing method as described in claim 22, characterized in that, After forming the first thin film and before forming the cathode layer, the fabrication method further includes: The first film, the electron transport layer, and the second film are subjected to an annealing process to convert the first film into a first filler layer and the second film into a second filler layer.

Citation Information

Patent Citations

  • Nanoparticle material and light-emitting device

    CN105658762A

  • Core-shell nano material and preparation method thereof and quantum dot light emitting diode

    CN110752319A