Trench gate super junction IGBT device structure and manufacturing method
By adopting a trench gate structure in superjunction IGBT devices, the number of trenching processes is reduced, the device damage problem is solved, and the yield and tolerability are improved.
Patent Information
- Application Number
- CN202210277956.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-03-21
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2042-03-21
AI Technical Summary
In the current fabrication process of superjunction IGBT devices, the multiple trenching processes cause severe damage to the devices, affecting the yield and reliability.
The trench gate superjunction IGBT device structure is adopted. By setting a deep trench structure including a first deep trench region and a second deep trench region in the N-base region, the P-type region and the trench gate region are formed by the same trench, and an insulating region is added between them, which reduces the number of trenching processes and improves the device's breakdown resistance.
This effectively reduces the damage to the device caused by the multi-stage trenching process, improves the yield of IGBT devices, and enhances the device's load-bearing capacity and breakdown resistance.
Smart Images

Figure CN114823885B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of semiconductor power device technology, and in particular to a trench gate superjunction IGBT device structure and fabrication method. Background Technology
[0002] Existing superjunction IGBT device structures are mainly formed through two processes: the first is multiple epitaxial doping, and the second is deep trench filling P-type silicon process. Among these two processes, the superjunction withstand layer formed by the trench filling process is easier to achieve a smaller aspect ratio than the superjunction withstand layer formed by multiple epitaxial technology. At the same time, the doping distribution of the N and P regions of the formed superjunction is also more uniform, which is beneficial to reducing Ron.sp.
[0003] In the process of forming trench-type superjunction IGBT devices using the deep trench filling P-type silicon process, two trenching processes are typically required. First, a deep trench filling P-type silicon process is used to form a lateral PN superjunction structure, and then a shallow trench is dug to form the trench gate structure. Trenching is necessary in both processes, but this process can cause stress on the wafer. Multiple trenching processes are more likely to lead to increased leakage current, decreased reliability, and increased fragmentation, thus reducing yield.
[0004] Therefore, there is a need for a superjunction IGBT device structure and fabrication method to solve how to design the device structure and trenching process in order to reduce device damage caused by the trenching process during IGBT device fabrication without affecting the operating conditions of the superjunction IGBT device, thereby improving the yield of IGBT devices. Summary of the Invention
[0005] To address the technical problem of reduced device yield caused by multiple trenching processes in existing deep trench filling P-type silicon-forming trench-type superjunction IGBT devices, this invention provides a trench-gate superjunction IGBT device structure, the specific technical solution of which is as follows:
[0006] The trench gate superjunction IGBT device structure provided by this invention includes an N-base region and further includes:
[0007] Several deep trenches are disposed within the N-base region, the deep trenches including a first deep trench region and a second deep trench region;
[0008] The first deep trench region is located below the deep trench, and the first deep trench region is filled with P-type silicon to form a P-type silicon region. The P-type silicon region and the adjacent N-base region form a lateral PN junction.
[0009] The second deep trench region is located above the deep trench, and the second deep trench region is filled with polysilicon to form a polysilicon gate region;
[0010] A gate insulating region is disposed between the first deep trench region and the second deep trench region to insulate the first deep trench region from the second deep trench region.
[0011] A gate oxide layer is disposed on the inner sidewall of the second deep trench region.
[0012] The trench gate superjunction IGBT device structure provided by this invention, by setting a deep trench structure including a first deep trench region and a second deep trench region in the N-base region, allows the first deep trench region forming the P-type region of the superjunction and the second deep trench region forming the trench gate to be formed by the same trench. Compared with the traditional trenching method, this saves the trenching process, effectively reduces the impact of the multi-trenching process on the device under dual stress, reduces device damage caused by the trenching process during IGBT device fabrication, and improves the yield of IGBT devices. Furthermore, an insulating region is added between the first deep trench region and the second deep trench region. The insulating region has better insulation capability than the sidewall gate oxide layer, thereby helping to improve the breakdown resistance of the gate bottom and enhance the device's withstand performance.
[0013] In some embodiments, the trench gate superjunction IGBT device structure provided by the present invention further includes:
[0014] The Pwell region is located between adjacent second deep trench regions;
[0015] The Nplus region is located above and adjacent to the Pwell region;
[0016] A front metal area is positioned above the Nplus area;
[0017] An interlayer dielectric layer is disposed between the front metal region and the Nplus region.
[0018] In some embodiments, two adjacent Nplus regions are provided between adjacent second deep trench regions, and there is a gap between adjacent Nplus regions. The trench gate superjunction IGBT device structure provided by the present invention further includes:
[0019] The connecting hole penetrates the interlayer dielectric layer in the vertical direction and passes through the gap to the adjacent Nplus region, serving to connect the front metal region and the Pwell region;
[0020] The Pplus area is located below the connection hole within the Pwell area.
[0021] In some embodiments, the connection hole is filled with the front metal corresponding to the front metal area;
[0022] The Nplus region, the Pplus region, and the front metal region form an ohmic contact.
[0023] In some embodiments, an N-type FS buffer layer, a P+ collector region, and a back metal region are disposed sequentially from top to bottom below the N-base region;
[0024] The P+ collector region and the back metal region form an ohmic contact.
[0025] In some implementations, the depths of the first deep trench area and the depths of the second deep trench area are set according to a preset ratio.
[0026] In some embodiments, the present invention also provides a method for fabricating a trench gate superjunction IGBT device, which, based on providing an N-base region, includes the following steps:
[0027] Several deep trenches are dug within the N-base region;
[0028] After filling the deep trench with P-type silicon, the P-type silicon is etched back to form a first deep trench region, so that the first deep trench region and the adjacent N-base region form a lateral PN junction;
[0029] An insulating material is deposited on the P-type silicon within the first deep trench region to form a gate insulating region;
[0030] A gate oxide layer is formed on the deep trench sidewall above the gate insulating region by thermal oxidation;
[0031] Polysilicon material is filled inside the gate oxide layer, and a polysilicon gate region is formed by etching. The polysilicon gate region is used as the second deep trench region.
[0032] In some embodiments, after using the polysilicon gate region as the second deep trench region, the method further includes:
[0033] Trivalent ions are injected into a preset Pwell pattern region and thermally diffused to form a Pwell region, wherein the Pwell pattern region is disposed between adjacent second deep trench regions;
[0034] Pentavalent ions are injected into a preset Nplus pattern region and thermally diffused to form an Nplus region. The Nplus pattern region is located above the Pwell region and adjacent to the Pwell region. Two adjacent Nplus regions are set between adjacent second deep trench regions, and there is a gap between adjacent Nplus regions.
[0035] An interlayer dielectric layer is deposited above the Nplus region;
[0036] The interlayer dielectric layer is etched in the region corresponding to the position directly above the gap in the interlayer dielectric layer, and silicon over-etching is performed to form a connection hole, so that the connection hole penetrates the interlayer dielectric layer and passes through the gap to pass through the adjacent Nplus region;
[0037] Trivalent ion implantation is performed on the connecting hole, and a Pplus region is formed by thermal diffusion in the Pwell region below the connecting hole;
[0038] A front metal region is formed by sputtering a front metal material over the interlayer dielectric layer.
[0039] In some embodiments, after sputtering a front metal material over the interlayer dielectric layer to form a front metal region, the method further includes:
[0040] Pentavalent ions are implanted under the N-substrate, and an N-type FS buffer layer is formed after laser annealing.
[0041] Trivalent ions are implanted under the N-type FS buffer layer, and P+ collector region is formed after laser annealing.
[0042] A back metal region is formed by sputtering back metal below the P+ collector region.
[0043] In some embodiments, the implantation energy of pentavalent ions in the N-type FS buffer layer is higher than the implantation energy of trivalent ions in the P+ collector region.
[0044] The trench gate superjunction IGBT device structure and fabrication method provided by this invention have the following technical advantages:
[0045] By setting a deep trench structure including a first deep trench region and a second deep trench region in the N-base region, the first deep trench region forming the P-type region of the superjunction and the second deep trench region forming the trench gate are formed by the same trench. Compared with the traditional trenching method, this saves trenching process, effectively reduces the impact of the multi-trenching process on the device under dual stress, reduces device damage caused by trenching process during IGBT device fabrication, improves the yield of IGBT devices, and adds an insulating region between the first deep trench region and the second deep trench region. The insulating region has better insulation capability than the sidewall gate oxide layer, which helps to improve the breakdown resistance of the gate bottom and improve the device's withstand performance. Attached Figure Description
[0046] To more clearly illustrate the technical solutions in the embodiments of the present invention, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0047] Figure 1 This is an example diagram of the trench gate superjunction IGBT device structure provided by the present invention;
[0048] Figure 2A flowchart of the method for fabricating a trench gate superjunction IGBT device provided by the present invention;
[0049] Figure 3 Another flowchart of the method for fabricating trench gate superjunction IGBT devices provided by the present invention.
[0050] The diagram is labeled as follows: Back metal region-1, P+ collector region-2, N-type FS buffer layer-3, N-base region-4, deep trench-5, first deep trench region-5.1, second deep trench region-5.2, P-type silicon region-6, gate insulating region-7, gate oxide layer-8, polysilicon gate region-9, Pwell region-10, Pplus region-11, Nplus region-12, via-13, interlayer dielectric layer-14, and front metal region-15. Detailed Implementation
[0051] In the following description, specific details such as particular system architectures and technologies are set forth for illustrative purposes and not for limitation, in order to provide a thorough understanding of the embodiments of this application. However, those skilled in the art will understand that this application can also be implemented in other embodiments without these specific details. In other instances, detailed descriptions of the hierarchy and block structure in well-known IGBT devices are omitted to avoid unnecessary detail from hindering the description of this application.
[0052] It should be understood that, when used in this specification and the appended claims, the term "comprising" indicates the presence of the described features, integrals, steps, operations, elements and / or components, but does not exclude the presence or addition of one or more other features, integrals, steps, operations, elements, components and / or sets.
[0053] To keep the drawings concise, only the parts relevant to the invention are shown schematically in each figure, and they do not represent the actual structure of the product. Furthermore, for ease of understanding, in some figures, components with the same structure or function are shown only schematically, or only one is labeled. In this document, "a" not only means "only one," but can also mean "more than one."
[0054] It should also be further understood that the term “and / or” as used in this application specification and the appended claims means any combination of one or more of the associated listed items and all possible combinations, and includes such combinations.
[0055] Furthermore, in the description of this application, the terms "first," "second," etc., are used only to distinguish descriptions and should not be construed as indicating or implying relative importance.
[0056] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the specific implementation methods of the present invention will be described below with reference to the accompanying drawings. Obviously, the drawings described below are merely some embodiments of the present invention. For those skilled in the art, other drawings and other implementation methods can be obtained based on these drawings without any creative effort.
[0057] One embodiment of the present invention, such as Figure 1 As shown, the trench gate superjunction IGBT device structure provided by the present invention includes an N-base region 4, a deep trench 5, a P-type silicon region 6, a gate insulating region 7, a gate oxide layer 8, and a polysilicon gate region 9.
[0058] In this configuration, several deep trenches 5 are disposed within the N-base region 4. Each deep trench 5 includes a first deep trench region 5.1 and a second deep trench region 5.2. The first deep trench region 5.1 is located below the deep trench 5 and is filled with P-type silicon to form a P-type silicon region 6. The P-type silicon region 6 forms a lateral PN junction with the adjacent N-base region 4. The second deep trench region 5.2 is located above the deep trench 5 and is filled with polysilicon to form a polysilicon gate region 9. A gate insulating region 7 is disposed between the first deep trench region 5.1 and the second deep trench region 5.2 to insulate between them. A gate oxide layer 8 is disposed on the inner sidewall of the second deep trench region 5.2. The gate oxide layer 8 on the sidewall of the gate insulating region 7 achieves the insulating effect of the gate insulating region 7.
[0059] The trench gate superjunction IGBT device structure provided in this embodiment uses a deep trench structure including a first deep trench region and a second deep trench region in the N-base region. This allows the first deep trench region forming the P-type region of the superjunction and the second deep trench region forming the trench gate to be formed by the same trench. Compared with the traditional trenching method, this saves on trenching processes, effectively reduces the impact of multiple trenching processes on the device under dual stress, reduces device damage caused by trenching processes during IGBT device fabrication, and improves the yield of IGBT devices. Furthermore, an insulating region is added between the first deep trench region and the second deep trench region. The insulating region has better insulation capabilities than the sidewall gate oxide layer, thereby helping to improve the breakdown resistance of the gate bottom and enhance the device's withstand performance.
[0060] In one embodiment, such as Figure 1 As shown, the trench gate superjunction IGBT device structure provided by the present invention is characterized by further including a back metal region 1, a P+ collector region 2, an N-type FS buffer layer 3, a Pwell region 10, a Pplus region 11, an Nplus region 12, a connection hole 13, an interlayer dielectric layer 14, and a front metal region 15.
[0061] The Pwell region 10 is located between adjacent second deep trench regions 5.2, the Nplus region 12 is located above and adjacent to the Pwell region 10, the front metal region 15 is located above the Nplus region 12, and the interlayer dielectric layer 14 is located between the front metal region 15 and the Nplus region 12.
[0062] Specifically, two adjacent Nplus regions 12 are provided between adjacent second deep trench regions 5.2, and there is a gap between adjacent Nplus regions 12. The connecting hole 13 penetrates the interlayer dielectric layer 14 in the vertical direction and passes through the adjacent Nplus regions 12 through the gap to connect the front metal region 15 and the Pwell region 10. The Pplus region 11 is located below the connecting hole 13 in the Pwell region 10. The connecting hole 13 is filled with the front metal corresponding to the front metal region 15. The Nplus regions 12, Pplus regions 11 and the front metal region 15 form an ohmic contact.
[0063] Below the N-base region 4, from top to bottom, are arranged an N-type FS buffer layer 3, a P+ collector region 2, and a back metal region 1, with the P+ collector region 2 and the back metal region 1 forming an ohmic contact.
[0064] In one embodiment, the depth of the first deep trench area 5.1 and the depth of the second deep trench area 5.2 can be set according to a preset ratio based on user requirements.
[0065] In one embodiment, the trench gate superjunction IGBT device fabrication method provided by the present invention, based on providing an N-base region, includes the following steps:
[0066] S1 excavates several deep trenches within the N-base region.
[0067] After filling the deep trench with P-type silicon, S2 etches back the P-type silicon to form the first deep trench region, so that the first deep trench region and the adjacent N-base region form a lateral PN junction.
[0068] S3 deposits insulating material on P-type silicon within the first deep trench region to form a gate insulating region.
[0069] S4 forms a gate oxide layer on the deep trench sidewall above the gate insulating region through thermal oxidation.
[0070] Specifically, the gate oxide layer on the sidewall of the gate insulating region achieves the insulation effect of the gate insulating region.
[0071] S5 fills the gate oxide layer with polysilicon material and etches it to form a polysilicon gate region, which is then used as the second deep trench region.
[0072] The trench gate superjunction IGBT device fabrication method provided in this embodiment creates a deep trench structure including a first deep trench region and a second deep trench region in the N-base region. This allows the first deep trench region forming the P-type region of the superjunction and the second deep trench region forming the trench gate to be formed by the same trench. Compared with the traditional trenching method, this method saves on trenching processes, effectively reduces the impact of multiple trenching processes on the device under dual stress, reduces device damage caused by trenching processes during IGBT device fabrication, and improves the yield of IGBT devices. Furthermore, an insulating region is added between the first deep trench region and the second deep trench region. The insulating region has better insulation capabilities than the sidewall gate oxide layer, thereby helping to improve the breakdown resistance of the gate bottom and enhance the device's withstand performance.
[0073] In one embodiment, the method further includes the following after step S5:
[0074] S6 injects trivalent ions into a pre-defined Pwell pattern region and thermally diffuses to form the Pwell region.
[0075] Specifically, the Pwell graphic area is located between adjacent second deep groove areas.
[0076] S7 injects pentavalent ions into a pre-defined Nplus pattern region and thermally diffuses to form the Nplus region.
[0077] Specifically, the Nplus graphic area is located above and adjacent to the Pwell area, and two adjacent Nplus areas are set between adjacent second deep trench areas, with gaps between adjacent Nplus areas.
[0078] S8 deposits an interlayer dielectric layer above the Nplus region.
[0079] S9 etches the interlayer dielectric layer in the region directly above the void in the interlayer dielectric layer and performs silicon over-etching to form a connection hole, so that the connection hole penetrates the interlayer dielectric layer and passes through the void through the adjacent Nplus region.
[0080] S10 performs trivalent ion implantation into the connecting hole, and thermal diffusion forms the Pplus region in the Pwell region below the connecting hole.
[0081] S11 sputters front metal material over the interlayer dielectric layer to form a front metal region.
[0082] S12 is implanted with pentavalent ions under an N-substrate, and after laser annealing, an N-type FS buffer layer is formed.
[0083] Specifically, before performing step S12, the back side of the device can be thinned to a preset thickness in advance.
[0084] S13 is implanted with trivalent ions under the N-type FS buffer layer, and after laser annealing, a P+ collector region is formed.
[0085] Specifically, the implantation energy of pentavalent ions in the N-type FS buffer layer is higher than that of trivalent ions in the P+ collector region.
[0086] S14 sputters back metal below the P+ collector region to form a back metal region.
[0087] In the above embodiments, the descriptions of each embodiment have different focuses. For parts that are not described in detail or recorded in a certain embodiment, please refer to the relevant descriptions of other embodiments.
[0088] It should be noted that the above embodiments can be freely combined as needed. The above description is only a preferred embodiment of the present invention. It should be pointed out that for those skilled in the art, several improvements and modifications can be made without departing from the principle of the present invention, and these improvements and modifications should also be considered within the scope of protection of the present invention.
Claims
1. A trench-gate superjunction IGBT device structure, including an N-base region, characterized in that, Also includes: Several deep trenches are disposed within the N-base region, the deep trenches including a first deep trench region and a second deep trench region; The first deep trench region is located below the deep trench, and the first deep trench region is filled with P-type silicon to form a P-type silicon region. The P-type silicon region and the adjacent N-base region form a lateral PN junction. The second deep trench region is located above the deep trench, and the second deep trench region is filled with polysilicon to form a polysilicon gate region; A gate insulating region is disposed between the first deep trench region and the second deep trench region to insulate the first deep trench region from the second deep trench region. A gate oxide layer is disposed on the inner sidewall of the second deep trench region; Below the N-base region, from top to bottom, are arranged an N-type FS buffer layer, a P+ collector region, and a back metal region; The P+ collector region and the back metal region form an ohmic contact; The depths of the first deep trench area and the depths of the second deep trench area are set according to a preset ratio; The deep trench formation process is as follows: Several deep trenches are excavated within the N-base region; After filling the deep trench with P-type silicon, the P-type silicon is etched back to form a first deep trench region, so that the first deep trench region and the adjacent N-base region form a lateral PN junction; An insulating material is deposited on the P-type silicon within the first deep trench region to form a gate insulating region; A gate oxide layer is formed on the deep trench sidewall above the gate insulating region by thermal oxidation; Polysilicon material is filled inside the gate oxide layer, and a polysilicon gate region is formed by etching. The polysilicon gate region is used as the second deep trench region.
2. The trench gate superjunction IGBT device structure according to claim 1, characterized in that, Also includes: The Pwell region is located between adjacent second deep trench regions; The Nplus region is located above and adjacent to the Pwell region; A front metal area is positioned above the Nplus area; An interlayer dielectric layer is disposed between the front metal region and the Nplus region.
3. The trench gate superjunction IGBT device structure according to claim 2, characterized in that, Two adjacent Nplus regions are provided between adjacent second deep trench regions, and there is a gap between adjacent Nplus regions. The system also includes: The connecting hole penetrates the interlayer dielectric layer in the vertical direction and passes through the gap to the adjacent Nplus region, serving to connect the front metal region and the Pwell region; The Pplus area is located below the connection hole within the Pwell area.
4. The trench gate superjunction IGBT device structure according to claim 3, characterized in that, The connection hole is filled with the front metal corresponding to the front metal area; The Nplus region, the Pplus region, and the front metal region form an ohmic contact.
5. The method for fabricating a trench-gate superjunction IGBT device as described in claim 1, characterized in that, based on providing an N-base region, Including the following steps: Several deep trenches are excavated within the N-base region; After filling the deep trench with P-type silicon, the P-type silicon is etched back to form a first deep trench region, so that the first deep trench region and the adjacent N-base region form a lateral PN junction; An insulating material is deposited on the P-type silicon within the first deep trench region to form a gate insulating region; A gate oxide layer is formed on the deep trench sidewall above the gate insulating region by thermal oxidation; Polysilicon material is filled inside the gate oxide layer, and a polysilicon gate region is formed by etching. The polysilicon gate region is used as the second deep trench region.
6. The method for fabricating a trench-gate superjunction IGBT device according to claim 5, characterized in that, After using the polysilicon gate region as the second deep trench region, the method further includes: Trivalent ions are injected into a preset Pwell pattern region and thermally diffused to form a Pwell region, wherein the Pwell pattern region is disposed between adjacent second deep trench regions; Pentavalent ions are injected into a preset Nplus pattern region and thermally diffused to form an Nplus region. The Nplus pattern region is located above the Pwell region and adjacent to the Pwell region. Two adjacent Nplus regions are set between adjacent second deep trench regions, and there is a gap between adjacent Nplus regions. An interlayer dielectric layer is deposited above the Nplus region; The interlayer dielectric layer is etched in the region corresponding to the position directly above the gap in the interlayer dielectric layer, and silicon over-etching is performed to form a connection hole, so that the connection hole penetrates the interlayer dielectric layer and passes through the gap to pass through the adjacent Nplus region; Trivalent ion implantation is performed on the connecting hole, and a Pplus region is formed by thermal diffusion in the Pwell region below the connecting hole; A front metal region is formed by sputtering a front metal material over the interlayer dielectric layer.
7. The method for fabricating a trench-gate superjunction IGBT device according to claim 6, characterized in that, After sputtering a front metal material over the interlayer dielectric layer to form a front metal region, the method further includes: A pentavalent ion is implanted beneath the N-base region, and an N-type FS buffer layer is formed after laser annealing. Trivalent ions are implanted under the N-type FS buffer layer, and P+ collector region is formed after laser annealing. A back metal region is formed by sputtering back metal below the P+ collector region.
8. The method for fabricating a trench-gate superjunction IGBT device according to claim 7, characterized in that, The implantation energy of pentavalent ions in the N-type FS buffer layer is higher than that of trivalent ions in the P+ collector region.
Citation Information
Patent Citations
Shield grid trench MOSFET device and manufacturing method thereof
CN105702739A