Anode oxide film repair device and method

By designing anodic film layer repair device, using suction cups and DC power supplies to locally repair the anodic film, the problem of long workpiece removal and repair cycles in the existing technology is solved, and efficient anodic film repair is achieved, suitable for single-use assembly and electronic components products.

CN114892234BActive Publication Date: 2024-11-05SICHUAN FANHUA AVIATION INSTR & ELECTRICAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210460373.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-04-28
Publication Date
2024-11-05
Estimated Expiration
2042-04-28

AI Technical Summary

Technical Problem

The prior art When local scratches and damage to the anodic aluminum and aluminum alloy workpieces are assembled or used, the workpiece needs to be removed for overall repair, resulting in waste of working hours and increased manufacturing costs, especially for disposable assembly and electronic components. When the device is product, the repair cycle is too long.

Method used

An anodized film layer repair device was designed, including a suction cup, a repair tank and a DC power supply. The damaged area is sealed through the suction cup, and local repairs are performed using anodized electrolyte and a DC power supply to avoid dismantling the workpiece and simplifying the repair process.

Benefits of technology

It realizes local repair of the anodic film layer, reduces the repair cycle, is suitable for one-time assembly and electronic component products, avoids workpiece disassembly and transport, and improves repair efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114892234B_ABST
    Figure CN114892234B_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of anodizing, and discloses an anodizing film repairing device and method. The repairing device comprising a suction cup, a repairing tank and a direct current power supply is used to repair a product with a damaged anodizing film. The suction cup comprises a conical section and a cylindrical section, the conical section has a conical opening, the cylindrical section is provided with a through hole connected to the contraction end of the conical opening along the central axis, and the top edge of the cylindrical section has a thread for screwing with the repairing tank. The repairing tank comprises a tank body and a tank cover, the tank body has a cavity for accommodating anodizing electrolyte, and the tank side edge at the opening end of the cavity is provided with a thread for screwing with the top of the cylindrical section and the tank cover. A lead plate is provided in the cavity, and a direct current power supply is provided outside the tank body, the negative pole of the direct current power supply extends into the cavity in the tank body and is connected to the lead plate, and the positive pole of the direct current power supply is externally connected to a wire. A sealing window connecting the cavity with the outside is provided at one end of the tank body away from the cavity opening, and the sealing window is detachably provided with a sealing cover.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of anodizing technology, and more specifically, to an anodized film repair device and method, which is a method for repairing an anodized film after anodized aluminum and aluminum alloy workpieces are locally scratched during assembly or use, resulting in exposed substrates. Background Art

[0002] Aluminum and aluminum alloys are widely used in the manufacturing industry. In order to enhance their corrosion resistance or enhance their appearance, aluminum and aluminum alloys are usually anodized to form an anodized film with a thickness of 4μm-20μm on their surface. Since the anodizing process requires direct contact with strong acids and alkalis, assembled products or semi-finished products usually cannot be directly anodized, especially products with electronic components, which cannot be directly immersed in anodizing electrolytes for anodizing. When anodized aluminum and aluminum alloy workpieces are scratched during assembly or use, resulting in partial exposure of the substrate, the current repair method is to first remove the damaged workpiece, then remove the anodized film from the damaged workpiece as a whole, polish the scratched area to repair the scratches, and then re-anodize the damaged workpiece as a whole. The disadvantages of this repair method are: 1. Removing the damaged workpiece consumes time, and for some one-time assembled products, removing the damaged workpiece will cause some workpieces or components to be scrapped, increasing the manufacturing cost; 2. The damaged workpiece needs to be transferred between the anodizing workshop and the machining workshop, increasing the repair cycle.

[0003] Therefore, in order to improve the repair efficiency and avoid the step of removing the workpiece in the repair process, while repairing the scratches and damaged anodized film on the workpiece, a simple method of local repair of the anodized film on the surface of aluminum and aluminum alloy workpieces was attempted. Summary of the invention

[0004] The purpose of the present invention is to provide an anodized film repair device and method to realize the repair function of the anodized film, facilitate local repair of damaged anodized film of products, avoid disassembly of damaged workpieces from the products, and be suitable for disposable assembly products and products with electronic components. It is flexible and portable to avoid transportation of damaged workpieces and effectively reduce the repair cycle.

[0005] The present invention is achieved through the following technical solutions:

[0006] An anodic oxide film repair device is used to repair products with damaged anodic oxide films, comprising a suction cup, a repair tank, and a DC power supply;

[0007] The suction cup comprises a conical section and a cylindrical section, wherein the conical section has a conical opening, the cylindrical section is provided with a through hole connected to the conical opening contraction end along the central axis, and the top edge of the cylindrical section has a thread for screwing with the repair tank;

[0008] The repair tank comprises a tank body and a tank cover, wherein the tank body has a cavity for containing anodizing electrolyte, and the tank side edge at the open end of the cavity is provided with a thread for screwing with the top of the columnar section and the tank cover;

[0009] A lead plate is provided in the cavity, a DC power supply is provided outside the can body, the negative pole of the DC power supply extends into the cavity in the can body and is connected to the lead plate, and the positive pole of the DC power supply is externally connected to a wire;

[0010] A sealing window communicating the cavity with the outside is arranged at one end of the can body away from the cavity opening, and a sealing cover is detachably mounted on the sealing window.

[0011] Furthermore, the positive electrode of the DC power supply is connected to a conductive clip via a wire.

[0012] At the same time, the present invention also includes a method for repairing an anodic oxide film layer, using an anodic oxide film layer repairing device as described above to repair a product with a damaged anodic oxide film, specifically comprising the following steps:

[0013] Step S1: Surface pretreatment: determine the suction cup model according to the damaged area so that the tapered opening of the tapered section can completely cover the damaged area; remove the damaged area and the peripheral anodized film layer to form the area to be repaired, and the area to be repaired can be completely covered by the tapered opening; smooth and clean the area to be repaired so that the surface roughness of the area to be repaired is consistent and the product base surface of the area to be repaired is completely exposed;

[0014] Step S2: Preparation for repair: completely cover the conical opening of the conical section of the suction cup and seal the gap between the conical section and the product surface; screw the body of the repair tank to the cylindrical section of the suction cup, store the anodic oxidation electrolyte in the cavity inside the tank body, and ensure that the anodic oxidation electrolyte is filled into the conical section and contacts the area to be repaired, connect the anode of the power supply device to the product, and set the DC power supply working parameters;

[0015] Step S3: Repair phase: start the DC power supply, and the repair device repairs the anodized film layer in the area to be repaired;

[0016] Step S4: Post-processing stage: turn off the DC power supply and separate the repair device from the product.

[0017] Further optimized, in step S3, during the operation of the repair device, the sealing cover on the sealing window adds pure water ice cubes into the cavity in the can body through the sealing window.

[0018] Further optimized, step S4 also includes cleaning and drying the product and the suction cup.

[0019] Compared with the prior art, the present invention has the following advantages and beneficial effects:

[0020] The present invention provides an anodized film repair device and method, which facilitates the local repair of damaged anodized film layers of products and avoids disassembling damaged workpieces from the products. It is suitable for disposable assembly products and products with electronic components. It is flexible and portable and avoids the transportation of damaged workpieces, effectively reducing the beneficial effect of the repair cycle. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] The technical solution will be described clearly and completely below in conjunction with the accompanying drawings. It is obvious that the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments.

[0022] Figure 1 A schematic diagram of the structure of a suction cup of an anodized film repair device provided by the present invention;

[0023] Figure 2 It is a structural schematic diagram of the tank body and the DC power supply in the present invention;

[0024] Figure 3 It is a schematic diagram of the structure of the can cover in the present invention;

[0025] Figure 4 A schematic diagram of the use status of an anodized film repair device provided by the present invention.

[0026] Among them: 1. Product; 3. Columnar section; 4. Conical section; 5. Can body; 6. Can cover; 7. Cavity; 8. Lead plate; 9. Wire; 10. DC power supply; 11. Sealed window. DETAILED DESCRIPTION

[0027] The above contents of the invention are further described in detail below in conjunction with the specific implementation methods of the embodiments. However, this should not be understood as the scope of the above subject matter of the invention being limited to the following examples. Various substitutions or changes made according to common technical knowledge and customary means in the art without departing from the above technical ideas of the invention should be included in the scope of the invention.

[0028] Embodiment 1:

[0029] An anodic oxide film repairing device of this embodiment is used to repair a product 1 with a damaged anodic oxide film, and includes a suction cup, a repair tank, and a DC power supply 10;

[0030] The suction cup includes a conical section 4 and a cylindrical section 3, wherein the conical section 4 has a conical opening, the cylindrical section 3 is provided with a through hole connected to the conical opening contraction end along the central axis, and the top edge of the cylindrical section 3 has a thread for screwing with the repair tank;

[0031] The repair tank comprises a tank body 5 and a tank cover 6. The tank body 5 has a cavity 7 for containing anodizing electrolyte inside. The edge of the tank body 5 at the open end of the cavity 7 is provided with a thread for screwing with the top of the columnar section 3 and the tank cover 6.

[0032] A lead plate 8 is provided in the cavity 7, a DC power supply 10 is provided outside the can body 5, a negative electrode of the DC power supply 10 extends into the cavity 7 in the can body 5 and is connected to the lead plate 8, and a positive electrode of the DC power supply 10 is externally connected to a wire 9;

[0033] The end of the can body 5 away from the opening of the cavity 7 is provided with a sealing window 11 connecting the cavity 7 with the outside, and the sealing window 11 is detachably mounted with a sealing cover;

[0034] The positive electrode of the DC power source 10 is connected to a conductive clip via a wire 9 .

[0035] Embodiment 2:

[0036] This embodiment provides an anodic oxide film repair method, using an anodic oxide film repair device as described in Example 1 to repair the surface of an aluminum or aluminum alloy product 1 with a damaged anodic oxide film, specifically comprising the following steps:

[0037] Step S1: Surface pretreatment: determine the suction cup model according to the damaged area so that the tapered opening of the tapered section 4 can completely cover the damaged area; remove the damaged area and the peripheral anodized film layer to form the area to be repaired, and the area to be repaired can be completely covered by the tapered opening; smooth and clean the area to be repaired so that the surface roughness of the area to be repaired is consistent, and the base surface of the product 1 in the area to be repaired is completely exposed;

[0038] Specifically, the area to be repaired can be smoothed by mechanical grinding with a file, grinder, sandpaper, scouring pad, etc. to remove scratches; the area to be repaired can be cleaned by using an organic cleaning agent to remove solid particles and oil stains on the surface of the area to be repaired;

[0039] Step S2: Preparation for repair: completely cover the conical opening of the conical section 4 of the suction cup, and seal the gap between the conical section 4 and the surface of the product 1 with materials such as sealant to ensure tightness; invert the body 5 of the repaired tank to remove the tank cover 6, invert the product 1 and the suction cup to screw the body 5 of the repaired tank to the cylindrical section 3 of the suction cup, and store anodizing electrolyte in the cavity 7 inside the tank body 5. The anodizing electrolyte can be selected to have a concentration of 180 to 220 g / L of sulfuric acid, after connecting the suction cup and the tank body 5 of the repair tank, ensure that the anodizing electrolyte can submerge more than one-third of the length of the lead plate 8, and ensure that the anodizing electrolyte is filled into the conical section 4 and contacts the area to be repaired, connect the anode of the power supply device to the product 1, so that the DC power supply 10, the lead plate 8, the anodizing electrolyte, and the area to be repaired are connected to form an electronic circuit, and set the working parameters of the DC power supply 10, such as selecting the output voltage of the DC power supply 10 to be 15V~17V, and the output time to be 20min~40min; work within the process temperature range of 13℃~26℃;

[0040] Step S3: Repair phase: start the DC power supply 10, and the repair device repairs the anodized film layer in the area to be repaired;

[0041] Step S4: Post-processing stage: turn off the DC power supply 10, and invert the product 1, the suction cup and the body 5 of the repair tank again to separate the repair device and the product 1.

[0042] In order to better implement this embodiment, it is further optimized that in the step S3, during the operation of the repair device, when the temperature of the anodized electrolyte is about to exceed the maximum value of the process temperature range, the sealing cover on the sealing window 11 adds pure water ice cubes into the cavity 7 in the tank body 5 through the sealing window 11 to cool the anodized electrolyte, thereby ensuring that the entire repair process is always operated within the process temperature range;

[0043] In order to better implement this embodiment, further optimization is performed in step S4, which also includes cleaning and drying the product 1 and the suction cup. Distilled water or other cleaning liquids can be used for cleaning. After cleaning and drying, the distilled water in the suction cup is poured out first, and the remaining liquid is blown dry with silk cloth or hot air to complete the entire repair process.

[0044] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. Any simple modification or equivalent change made to the above embodiment based on the technical essence of the present invention shall fall within the protection scope of the present invention.

Claims

1. A method for repairing an anodic oxide film layer, using a repair device to repair a product (1) with a damaged anodic oxide film, characterized in that: The repair device comprises a suction cup, a repair tank, and a DC power supply (10); The suction cup comprises a conical section (4) and a cylindrical section (3), the conical section (4) having a conical opening, the cylindrical section (3) being provided with a through hole connected to the contracted end of the conical opening along the central axis, and the top edge of the cylindrical section (3) having a thread for screwing with the repair tank; The repair tank comprises a tank body (5) and a tank cover (6); the tank body (5) has a cavity (7) inside for containing anodizing electrolyte; the edge of the tank body (5) at the open end of the cavity (7) is provided with a thread for screwing with the top of the columnar segment (3) and the tank cover (6); A lead plate (8) is provided in the cavity (7), a DC power supply (10) is provided outside the can body (5), a negative electrode of the DC power supply (10) extends into the cavity (7) in the can body (5) and is connected to the lead plate (8), and a positive electrode of the DC power supply (10) is externally connected to a wire (9); An end of the can body (5) away from the opening of the cavity (7) is provided with a sealing window (11) connecting the cavity (7) with the outside, and a sealing cover is detachably mounted on the sealing window (11); The repair method specifically comprises the following steps: Step S1, surface pretreatment: determining the suction cup model according to the damaged area so that the conical opening of the conical section (4) can completely cover the damaged area; removing the anodized film layer in the damaged area and the periphery to form an area to be repaired, wherein the area to be repaired can be completely covered by the conical opening; smoothing and cleaning the area to be repaired so that the surface roughness of the area to be repaired is uniform and the base surface of the product (1) in the area to be repaired is completely exposed; Step S2, preparation for repair: completely cover the conical opening of the conical section (4) of the suction cup, and seal the gap between the conical section (4) and the surface of the product (1); screw the body (5) of the repair tank to the cylindrical section (3) of the suction cup, store the anodic oxidation electrolyte in the internal cavity (7) of the body (5), and ensure that the anodic oxidation electrolyte is filled into the conical section (4) and contacts the area to be repaired, connect the anode of the power supply device to the product (1), and set the working parameters of the DC power supply (10); Step S3, repair stage: starting the DC power supply (10), and the repair device repairs the anodized film layer of the area to be repaired; during the operation of the repair device, the sealing cover on the sealing window (11) adds pure water ice cubes into the cavity (7) in the can body (5) through the sealing window (11); Step S4, post-processing stage: turning off the DC power supply (10) and separating the repair device from the product (1); and further comprising cleaning and drying the product (1) and the suction cup; After cleaning and drying, pour out the distilled water in the suction cup first, then use silk cloth or hot air to blow away the remaining liquid to complete the entire repair process.