Semiconductor device and method of manufacturing the same

By setting a high-impurity breakdown prevention region in the upper part of the well region of LDMOS and forming the base region in combination with specific processes, the breakdown problem caused by the rise of LDMOS breakdown voltage is solved, and a balance between breakdown voltage and cost control is achieved.

CN115050805BActive Publication Date: 2026-11-24FUJI ELECTRIC CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202210112626.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2021-03-08
Filing Date
2022-01-29
Publication Date
2026-11-24
Estimated Expiration
2042-01-29

AI Technical Summary

Technical Problem

As the breakdown voltage of an LDMOS device increases, the impurity concentration in the n-type well region decreases, making it easier for the depletion layer between the drain region and the semiconductor substrate to expand and break down. This leads to a decrease in breakdown voltage, and in order to prevent breakdown, the device size is increased, thereby increasing the chip cost.

Method used

A high-impurity breakdown prevention region is set in the upper part of the well region of LDMOS, and a high-impurity base region, drift region, carrier supply region and carrier receiving region are formed through specific ion implantation and thermal treatment processes to ensure voltage withstand while suppressing the increase in chip size.

Benefits of technology

By setting a breakdown prevention region on the upper part of the well region, the breakdown between the drain region and the semiconductor layer is prevented, thus avoiding an increase in device area and controlling chip area, achieving voltage withstand while reducing cost.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115050805B_ABST
    Figure CN115050805B_ABST
Patent Text Reader

Abstract

This invention provides a semiconductor device and a method for manufacturing the same, which can ensure voltage withstand capability while suppressing the increase in chip size. The semiconductor device includes: a semiconductor layer (1) of a first conductivity type; a well region (2) of a second conductivity type disposed on the upper part of the semiconductor layer; a base region (4a, 4b) of the second conductivity type disposed on the upper part of the well region; a carrier supply region (6a, 6b) of the first conductivity type disposed on the upper part of the base region; a drift region (3) of the first conductivity type disposed on the upper part of the well region and disposed separately from the base region; a carrier receiving region (5) of the first conductivity type disposed on the upper part of the drift region; a gate electrode (11a, 11b) disposed on the upper surface of the well region sandwiched between the base region and the drift region through a gate insulating film (12); and a breakdown prevention region (9a, 9b) of the second conductivity type disposed on the upper part of the well region, the impurity concentration of which is different from that of the base region.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to a semiconductor device and a method for manufacturing the same. Background Technology

[0002] Laterally diffused MOS transistors (hereinafter referred to as "LDMOS") are one of the semiconductor devices commonly used in high-voltage applications. LDMOS achieves high voltage withstand capability by mitigating the electric field intensity when high voltage is applied through a drift region with a relatively low impurity concentration located between the source and drain regions (see Patent Document 1).

[0003] In the case of a p-channel LDMOS, an n-type well region is formed for device isolation. The n-type well region is formed deep in the p-type semiconductor substrate to ensure sufficient isolation breakdown voltage. The impurity concentration of the n-type well region is appropriately adjusted according to the breakdown voltage and on-state resistance of the semiconductor device.

[0004] Existing technical documents

[0005] Patent documents

[0006] Patent Document 1: Japanese Patent No. 4645861 Specification Summary of the Invention

[0007] The problem the invention aims to solve

[0008] As the breakdown voltage of an LDMOS device increases, the impurity concentration in the n-type well region tends to decrease. When the impurity concentration in the n-type well region decreases, there are concerns that the depletion layer between the drain region and the semiconductor substrate is prone to propagation and breakdown, leading to a decrease in the breakdown voltage between the drain region and the semiconductor substrate. When it is necessary to ensure an adequate distance between the drain region and the semiconductor substrate, the increased device size results in a larger chip size, thus increasing costs.

[0009] In view of the above problems, the object of the present invention is to provide a semiconductor device and a method thereof that can ensure voltage resistance while suppressing the increase in chip size.

[0010] Solution for solving the problem

[0011] One aspect of the present invention is a semiconductor device comprising: (a) a semiconductor layer of a first conductivity type; (b) a well region of a second conductivity type disposed on the upper portion of the semiconductor layer; (c) a base region of the second conductivity type disposed on the upper portion of the well region, having a higher impurity concentration than the well region; (d) a carrier supply region of the first conductivity type disposed on the upper portion of the base region; (e) a drift region of the first conductivity type disposed on the upper portion of the well region, separately disposed from the base region; (f) a carrier receiving region of the first conductivity type disposed on the upper portion of the drift region, having a higher impurity concentration than the drift region; (g) a gate electrode disposed on the upper surface of the well region sandwiched between the base region and the drift region, separated by a gate insulating film; and (h) a breakdown prevention region of the second conductivity type disposed on the upper portion of the well region, having a higher impurity concentration than the well region, wherein the impurity concentration of the breakdown prevention region is different from that of the base region.

[0012] Other aspects of the present invention relate to a method for manufacturing a semiconductor device, the method comprising the following steps: (a) forming a well region of a second conductivity type on top of a semiconductor layer of a first conductivity type; (b) forming a base region of a second conductivity type with a higher impurity concentration than the well region on top of the well region; (c) forming a breakdown prevention region of a second conductivity type on top of the well region with a higher impurity concentration than the well region and a different impurity concentration than the base region; (d) forming a drift region of a first conductivity type on top of the well region, separate from the base region; (e) forming a carrier supply region of a first conductivity type on top of the base region; (f) forming a carrier receiving region of a first conductivity type with a higher impurity concentration than the drift region on top of the drift region; and (g) forming a gate electrode on the upper surface of the well region sandwiched between the base region and the drift region, separated by a gate insulating film.

[0013] The effects of the invention

[0014] According to the present invention, a semiconductor device and a method thereof that can ensure voltage withstand capability while suppressing the increase in chip size can be provided. Attached Figure Description

[0015] Figure 1 This is a top view showing a semiconductor device according to an embodiment of the present invention.

[0016] Figure 2 From Figure 1 A cross-sectional view observed along the AA direction.

[0017] Figure 3 From Figure 1 A cross-sectional view observed along the BB direction.

[0018] Figure 4 This is a cross-sectional view of the semiconductor device involved in the comparative example.

[0019] Figure 5A This is used to illustrate the manufacturing method of the semiconductor device involved in the embodiments of the present invention. Figure 2 The corresponding process cross-sectional diagram.

[0020] Figure 5B This is used to illustrate the manufacturing method of the semiconductor device involved in the embodiments of the present invention. Figure 3 The corresponding process cross-sectional diagram.

[0021] Figure 6A This is a continuation of the method for manufacturing a semiconductor device according to embodiments of the present invention. Figure 5A The cross-sectional diagram of the subsequent process.

[0022] Figure 6B This is a continuation of the method for manufacturing a semiconductor device according to embodiments of the present invention. Figure 5B The cross-sectional diagram of the subsequent process.

[0023] Figure 7A This is a continuation of the method for manufacturing a semiconductor device according to embodiments of the present invention. Figure 6A The cross-sectional diagram of the subsequent process.

[0024] Figure 7B This is a continuation of the method for manufacturing a semiconductor device according to embodiments of the present invention. Figure 6B The cross-sectional diagram of the subsequent process.

[0025] Figure 8A This is a continuation of the method for manufacturing a semiconductor device according to embodiments of the present invention. Figure 7A and Figure 7B The following is a top view.

[0026] Figure 8B From Figure 8A A cross-sectional view observed along the AA direction.

[0027] Figure 8C From Figure 8A A cross-sectional view observed along the BB direction.

[0028] Figure 8D From Figure 8A A cross-sectional view observed in the CC direction.

[0029] Figure 9A This is a continuation of the method for manufacturing a semiconductor device according to embodiments of the present invention. Figure 8B The cross-sectional diagram of the subsequent process.

[0030] Figure 9B This is a continuation of the method for manufacturing a semiconductor device according to embodiments of the present invention. Figure 8CThe cross-sectional diagram of the subsequent process.

[0031] Figure 10A This is a continuation of the method for manufacturing a semiconductor device according to embodiments of the present invention. Figure 9A The cross-sectional diagram of the subsequent process.

[0032] Figure 10B This is a continuation of the method for manufacturing a semiconductor device according to embodiments of the present invention. Figure 9B The cross-sectional diagram of the subsequent process.

[0033] Figure 11A This is a continuation of the method for manufacturing a semiconductor device according to embodiments of the present invention. Figure 10A The cross-sectional diagram of the subsequent process.

[0034] Figure 11B This is a continuation of the method for manufacturing a semiconductor device according to embodiments of the present invention. Figure 10B The cross-sectional diagram of the subsequent process.

[0035] Figure 12A This is a continuation of the method for manufacturing a semiconductor device according to embodiments of the present invention. Figure 11A The cross-sectional diagram of the subsequent process.

[0036] Figure 12B This is a continuation of the method for manufacturing a semiconductor device according to embodiments of the present invention. Figure 11B The cross-sectional diagram of the subsequent process.

[0037] Figure 13 This is a top view illustrating a semiconductor device according to a first modified embodiment of the present invention.

[0038] Figure 14 This is a top view illustrating a method for manufacturing a semiconductor device according to a first variation of an embodiment of the present invention.

[0039] Figure 15 This is a top view illustrating a method for manufacturing a semiconductor device according to a second variation of an embodiment of the present invention.

[0040] Figure 16 This is a cross-sectional view of a semiconductor device according to a third variation of an embodiment of the present invention.

[0041] Figure 17 This is a cross-sectional view of a semiconductor device according to a fourth variation of an embodiment of the present invention.

[0042] Figure 18 This is a process cross-sectional view of a semiconductor device used to illustrate a fourth variation of an embodiment of the present invention.

[0043] Figure 19 This is a top view illustrating a semiconductor device according to a fifth variation of an embodiment of the present invention. Detailed Implementation

[0044] Hereinafter, embodiments and variations of the present invention will be described with reference to the accompanying drawings. In the drawings, identical or similar parts are labeled with the same or similar reference numerals, and repeated descriptions are omitted. The drawings are schematic, and the relationship between thickness and planar dimensions, the ratio of thicknesses of each layer, etc., may sometimes differ from actual conditions. Furthermore, the drawings may include parts with different dimensional relationships or ratios. Additionally, the embodiments shown below are illustrative of apparatuses and methods for embodying the technical concept of the present invention; the technical concept of the present invention does not specify the material, shape, structure, or arrangement of structural components as described below.

[0045] In this specification, "carrier supply region" refers to the semiconductor region that supplies majority carriers (majority carriers) as the main current, such as the source region of a MIS-type field-effect transistor (MISFET) or a MIS-type electrostatic induction transistor (MISSIT), the emitter region of an insulated-gate bipolar transistor (IGBT), and the anode region of a MIS-controlled electrostatic induction thyristor (MIS-controlled SI thyristor). "Carrier receiving region" refers to the semiconductor region that receives majority carriers as the main current, such as the drain region of a MISFET or MISSIT, the collector region of an IGBT, and the cathode region of a MIS-controlled SI thyristor. In semiconductor devices that operate in a bipolar configuration, such as IGBTs and MIS-controlled SI thyristors, carriers (carriers) of the opposite conductivity type are injected with majority carriers from the carrier receiving region.

[0046] Furthermore, the definitions of up and down, etc., in the following description are merely for ease of explanation and are not intended to limit the technical concept of the present invention. For example, if the object is rotated 90° and observed, the term "up and down" becomes "left and right," and if the object is rotated 180° and observed, the relationship between the terms "up and down" will be reversed, which is self-evident.

[0047] Furthermore, the following explanation illustrates, exemplified by the case where the first conductivity type is p-type and the second conductivity type is n-type. However, the conductivity types can also be chosen in reverse order, with the first conductivity type being n-type and the second conductivity type being p-type. Additionally, the + and - symbols attached to n and p indicate semiconductor regions with relatively higher or lower impurity concentrations compared to semiconductor regions without + and - symbols, respectively. However, even semiconductor regions with the same n and n symbols do not necessarily have strictly identical impurity concentrations.

[0048] (Implementation Method)

[0049] <Structure of Semiconductor Devices>

[0050] Figure 1 A top view of a semiconductor device according to an embodiment of the present invention is shown. Figure 2 With From Figure 1 The cross-sectional view observed in the AA direction corresponds to this. Figure 3 With From Figure 1 The cross-sectional view observed along the BB direction corresponds to this. Figure 1 For convenience, details regarding the Chinese text have been omitted. Figure 2 and Figure 3 The illustrations of the element isolation insulating film 10, gate insulating film 12, gate electrodes 11a and 11b, interlayer insulating film 13, drain electrode 14, source electrode 15 and 16, and substrate contact electrodes 17 and 18 on the upper side of semiconductor layer 1 correspond to the top view of semiconductor layer 1. Furthermore, in Figure 1 For convenience, dashed lines are used to represent the characters. Figure 2 The gate electrodes 11a and 11b are shown.

[0051] The semiconductor device involved in the embodiments of the present invention is as follows: Figures 1-3 As shown, a semiconductor layer 1 having a first conductivity type (p-type) and a second conductivity type (n-type) disposed on the upper part of the semiconductor layer 1. - Type 2) of the trap area.

[0052] Semiconductor layer 1 can be, for example, a silicon (Si) substrate or other semiconductor substrate. Alternatively, a semiconductor substrate made of a wide-bandgap semiconductor (such as silicon carbide (SiC), gallium nitride (GaN), diamond, or aluminum nitride (AlN) with a wider bandgap than silicon can be used as semiconductor layer 1. Semiconductor layer 1 can also be a p-type semiconductor region disposed on the upper part of a p-type or n-type semiconductor substrate.

[0053] like Figure 1 and Figure 2 As shown on the left, an n-type impurity concentration with a higher concentration than that of the trap region 2 is provided in the upper part of the trap region 2. - The base region (channel forming region) 4a is of the type. A p-type base is disposed on the upper part of the base region 4a. + A carrier supply region (source region) 6a of type 6a. Above the base region 4a, in connection with the source region 6a, is provided an n-type substrate with a higher impurity concentration compared to the base region 4a. + Contact area 7a of type 7. (e.g.) Figure 1 As shown, the source region 6a and the contact region 7a have strip-shaped planar patterns along... Figure 1 It extends in the vertical direction. For example... Figure 2 As shown, the upper surfaces of the source region 6a and the contact region 7a are connected to the source electrode 15.

[0054] like Figure 1 and Figure 2 As shown on the right, an n-type impurity concentration with a higher concentration than that of the well region 2 is provided in the upper part of the well region 2. - The base region 4b is of the type. A p-type base is disposed on the upper part of the base region 4b. + The source region 6b is of the type 6. Above the base region 4b, in connection with the source region 6b, is an n-type source region with a higher impurity concentration compared to the base region 4b. + Contact area 7b of type. (e.g.) Figure 1 As shown, the source region 6b and the contact region 7b have strip-shaped planar patterns along... Figure 1 It extends in the vertical direction. For example... Figure 2 As shown, the upper surfaces of the source region 6b and the contact region 7b are connected to the source electrode 16.

[0055] like Figures 1-3 As shown in the center of the left-right direction, a p is provided at the upper part of the trap region 2. - A carrier transport region (drift region) 3 of the type is provided. A p-type impurity concentration with a higher concentration than that of the drift region 3 is provided at the upper part of the drift region 3. + Type 5 carrier receiving region (drain region). For example... Figure 1 As shown, the well region 2 has a rectangular planar pattern. The drain region 5 has a strip-shaped planar pattern along... Figure 1 It extends vertically. The drain region 5 is located in... Figure 1 The source regions 6a and 6b are separated by the well region 2 and the drift region 3 in the left-right direction. That is, in the embodiment of the present invention, two p-channel LDMOS are symmetrically arranged left and right, and the two LDMOS share the drain region 5. Furthermore, in addition to the two LDMOS, various semiconductor elements such as transistors can be mixed in the semiconductor layer 1. Figure 2 As shown, the upper surface of the drain region 5 is connected to the drain electrode 14.

[0056] like Figure 2 and Figure 3 As shown, a device isolation insulating film 10 is provided on the upper surface of the semiconductor layer 1. The device isolation insulating film 10 is composed of a field oxide film, such as a local insulating film (LOCOS film) selectively (locally) formed by the local silicon oxidation (LOCOS) method.

[0057] like Figure 1 and Figure 2 As shown on the left, a gate electrode 11a, separated by a gate insulating film 12, is disposed on the upper surface of the base region 4a and the well region 2, between the source region 6a and the drift region 3. Figure 1 and Figure 2As shown on the right, a gate electrode 11b is disposed on the upper surface of the base region 4b and the well region 2, which is sandwiched between the source region 6b and the drift region 3, and is separated by a gate insulating film 12.

[0058] As the gate insulating film 12, for example, in addition to silicon oxide film (SiO2 film), any single layer film or composite film obtained by stacking multiple of them can be used, such as silicon oxynitride film (SiON film), strontium oxide film (SrO film), silicon nitride film (Si3N4 film), aluminum oxide film (Al2O3 film), magnesium oxide film (MgO film), yttrium oxide film (Y2O3 film), hafnium oxide film (HfO2 film), zirconium oxide film (ZrO2 film), tantalum oxide film (Ta2O5 film), bismuth oxide film (Bi2O3 film).

[0059] Materials used as gate electrodes 11a and 11b include, for example, polysilicon layers (doped polysilicon layers) with high concentrations of p-type impurities such as boron (B) or n-type impurities such as phosphorus (P), and high-melting-point metals.

[0060] An interlayer insulating film 13 is disposed on the gate electrodes 11a and 11b. The interlayer insulating film 13 can be an undoped silicon oxide film (SiO2 film) free of phosphorus (P) and boron (B), referred to as "NSG". Alternatively, the interlayer insulating film 13 can also be a silicon oxide film with added phosphorus (PSG film), a silicon oxide film with added boron (BSG film), a silicon oxide film with added boron and phosphorus (BPSG film), a silicon nitride film (Si3N4 film), or a laminate of these films.

[0061] like Figures 1-3 As shown, p is disposed on the upper part of semiconductor layer 1 in a manner that surrounds the drift region 3. + Type 8 substrate contact area. For example... Figure 1 As shown, the substrate contact area 8 has, for example, a ring-shaped planar pattern. Figure 2 As shown, the upper surface of the substrate contact area 8 is connected to the substrate contact electrodes 17 and 18. By applying a substrate potential (e.g., ground potential) to the substrate contact area 8 via the substrate contact electrodes 17 and 18, the semiconductor layer 1 is fixed at the substrate potential.

[0062] like Figure 1 and Figure 3 As shown, an n-type impurity concentration with a higher concentration than that of the well region 2 is provided in the upper part of the well region 2. - Type 5 breakdown prevention regions 9a and 9b. Breakdown prevention regions 9a and 9b function to prevent breakdown between the drain region 5 and the semiconductor layer 1. Figure 1 and Figure 3The example illustrates the case where the breakdown prevention regions 9a and 9b are separated from the drift region 3; however, the breakdown prevention regions 9a and 9b can also be connected to the drift region 3. For example... Figure 1 As shown, the breakdown prevention zones 9a and 9b are in Figure 1 The drain region 5 and the semiconductor layer 1 are positioned vertically in the region facing each other. Breakdown prevention regions 9a and 9b are configured to sandwich the drain region 5 and the drift region 3 in between. Figure 1 In the left and right directions, the width W0 of the breakdown prevention regions 9a and 9b is wider than the width of the drain region 5.

[0063] The impurity concentration in the breakdown prevention regions 9a and 9b is higher than that in the well region 2, but lower than that in the base regions 4a and 4b. In an embodiment of the invention, the depth D2 of the breakdown prevention regions 9a and 9b is equal to the depth D1 of the base regions 4a and 4b. The depth D2 of the breakdown prevention regions 9a and 9b may also be shallower than the depth D1 of the base regions 4a and 4b. Although described later, the breakdown prevention regions 9a and 9b and the base regions 4a and 4b are formed simultaneously through the same ion implantation and heat treatment processes.

[0064] The depth D2 of the penetration prevention zones 9a and 9b is the same as the depth D3 of the drift zone 3. The depth D2 of the penetration prevention zones 9a and 9b can also be deeper or shallower than the depth D3 of the drift zone 3.

[0065] <First Comparative Example>

[0066] Here, the semiconductor device involved in the first comparative example is described. Figure 4 This refers to the semiconductor device involved in the first comparative example and the semiconductor device involved in the embodiments of the present invention. Figure 3 The corresponding cross section. For example... Figure 4 As shown, the semiconductor device involved in the first comparative example differs from the semiconductor device involved in the embodiments of the present invention in that it does not have a breakdown prevention region provided on the upper part of the well region 2.

[0067] In the semiconductor device involved in the first comparative example, when the impurity concentration in the well region 2 is low, the depletion layer from p - The drift region 3 of the type gradually moves towards n - The p-type well region 2 extends to the p-type semiconductor layer 1, causing breakdown between the drain region 5 and the semiconductor layer 1, resulting in a decrease in breakdown voltage. To prevent breakdown, the distance D0 of the well region 2 needs to be sufficiently ensured, but this increases the device area, and the increased chip area leads to higher costs.

[0068] In contrast, the semiconductor device according to embodiments of the present invention, such as Figure 1 and Figure 3As shown, breakdown prevention regions 9a and 9b are provided on the upper part of the well region 2, which can prevent breakdown between the drain region 5 and the semiconductor layer 1, suppress the increase of device area, and thus suppress chip area, thereby enabling low-cost manufacturing.

[0069] <Second Comparative Example>

[0070] Next, the semiconductor device involved in the second comparative example will be described. The semiconductor device involved in the second comparative example is related to... Figures 1-3 The semiconductor device according to the embodiment of the present invention shown has the same structure, but differs in that the impurity concentrations of the breakdown prevention regions 9a and 9b are equivalent to the impurity concentrations of the base regions 4a and 4b. In the semiconductor device according to the second comparative example, during the ion implantation process for forming the base regions 4a and 4b, ion implantation is also performed on the breakdown prevention regions 9a and 9b, and the base regions 4a and 4b and the breakdown prevention regions 9a and 9b are formed simultaneously through subsequent heat treatment. However, during the ion implantation process for forming the base regions 4a and 4b, since implantation conditions suitable for the impurity concentrations of the base regions 4a and 4b are used, the impurity concentrations of the breakdown prevention regions 9a and 9b are sometimes unsuitable.

[0071] In contrast, the semiconductor device according to an embodiment of the present invention makes the impurity concentrations of the breakdown prevention regions 9a and 9b different from the impurity concentrations of the base regions 4a and 4b within the same device, thereby enabling the impurity concentrations of the breakdown prevention regions 9a and 9b to be adjusted to impurity concentrations suitable for preventing breakdown.

[0072] <Methods for Manufacturing Semiconductor Devices>

[0073] Next, refer to Figures 5A to 12B This section will explain a method for manufacturing a semiconductor device according to embodiments of the present invention. Here, the focus is primarily on... Figure 2 and Figure 3 The cross-section of the semiconductor device shown is illustrated. Furthermore, the manufacturing method of the semiconductor device described below is just one example; it is self-evident that various other manufacturing methods can be used, including variations thereof, as long as they fall within the scope of the main points described in the specification.

[0074] First, a p-type Si substrate or other semiconductor layer 1 is prepared. Next, a photoresist film 20 is coated on the upper surface of the semiconductor layer 1, and a pattern is formed on the photoresist film 20 using photolithography. For example... Figure 5A and Figure 5B As shown, a patterned photoresist film 20 is used as a mask to implant n-type impurity ions such as phosphorus (P). After removing the photoresist film 20, a heat treatment is performed, thereby activating the n-type impurity ions. The result is as follows: Figure 6A and Figure 6B As shown, n is selectively formed on the upper part of semiconductor layer 1. - Type 2 trap region.

[0075] Next, a photoresist film 21 is coated on the upper surface of the semiconductor layer 1 and the well region 2, and a pattern is formed on the photoresist film 21 using photolithography. For example... Figure 7A and Figure 7B As shown, a patterned photoresist film 21 is used as a mask for implanting p-type impurity ions such as boron (B). After removing the photoresist film 21, a photoresist film 22 is recoated on the upper surface of the semiconductor layer 1 and the well region 2, as shown. Figure 8A As shown, photolithography is used to form a pattern on the photoresist film 22.

[0076] Figure 8B Showing from Figure 8A The cross section observed along the AA direction. Figure 8C Showing from Figure 8A The cross section observed in the BB direction. Figure 8D Showing from Figure 8A The cross-section observed in the CC direction. For example... Figure 8A As shown, the photoresist film 22 has a resist pattern comprising: slit-shaped (strip-shaped) openings 22a and 22b corresponding to the breakdown prevention regions 9a and 9b, and rectangular, full-surface openings 22c and 22d corresponding to the base regions 4a and 4b. The slits of the openings 22a and 22b are along... Figure 8A Extending vertically, and in Figure 8A Multiple are arranged side by side in the left and right directions.

[0077] like Figures 8B to 8D As shown, a patterned photoresist film 22 is used as a mask for ion implantation to implant n-type impurity ions such as phosphorus (P). The ion implantation conditions are set to be suitable for the base regions 4a and 4b. Therefore, as... Figure 8B As shown, ion implantation is performed by opening the entire surface of the openings 22c and 22d used to form the base regions 4a and 4b. On the other hand, ion implantation is performed through methods such as... Figure 8C and 8D As shown, the openings 22a and 22b used to form the breakdown prevention regions 9a and 9b are slit-shaped, which can limit the amount of ion implantation, thereby making the impurity concentration in the breakdown prevention regions 9a and 9b a concentration suitable for preventing breakdown.

[0078] like Figure 8AAs shown, the impurity concentration in the breakdown prevention zones 9a and 9b can be adjusted to a concentration suitable for preventing breakdown by adjusting the density (shielding rate) of the slits in the openings 22a and 22b, the slit width (width of the non-opening portion) W1 of the openings 22a and 22b, the slit interval (width of the opening) S1, and the ratio of the slit interval S1 to the slit width W1 S1 / W1. The higher the shielding rate of the slits in the openings 22a and 22b, the lower the impurity concentration in the breakdown prevention zones 9a and 9b, and the shallower the depth of the breakdown prevention zones 9a and 9b. For example, by adjusting the shielding rate of openings 22a and 22b to approximately 50%, the slit width W1 to approximately 0.5 μm, the slit spacing S1 to approximately 0.5 μm, and the ratio of slit spacing S1 to slit width W1 S1 / W1 to approximately 1, the impurity concentration in breakdown prevention regions 9a and 9b can be approximately half that in base regions 4a and 4b. Figures 8B to 8D After the n-type impurity ions are implanted, the photoresist film 22 is removed.

[0079] Next, heat treatment is performed, thereby activating the p-type and n-type impurity ions. The result is as follows: Figure 9A and Figure 9B As shown, p is selectively formed in the upper part of the trap region 2. - Type 3 drift region. Furthermore, n-type drift regions are selectively formed in the upper part of trap region 2. - Type 9a, 9b and n - The base regions 4a and 4b are of the p-type type. The breakdown prevention regions 9a and 9b are regions integrally formed with the same impurity concentration after the n-type impurities injected through the slits of the openings 22a and 22b diffuse laterally. The impurity concentration of the breakdown prevention regions 9a and 9b differs from that of the base regions 4a and 4b, and is lower than that of the base regions 4a and 4b. Furthermore, it is used to form p-type base regions 4a and 4b. - Heat treatment of drift region 3 and for forming n - Type 9a, 9b and n - The heat treatment of the base regions 4a and 4b of the type can also be carried out separately rather than together.

[0080] Next, as Figure 10A and Figure 10B As shown, a device isolation insulating film 10 is formed on the upper surface of semiconductor layer 1 using methods such as the LOCOS method. Next, a gate insulating film 12 is formed on the upper surface of semiconductor layer 1 using methods such as thermal oxidation or chemical vapor deposition (CVD). Furthermore, a polysilicon layer with a high concentration of n-type or p-type impurities (doped polysilicon layer) is deposited using a CVD method with doped gases. Then, a portion of the doped polysilicon layer and the gate insulating film 12 are selectively removed using photolithography and dry etching. As a result, as shown... Figure 11A and Figure 11B As shown, a pattern of gate electrodes 11a and 11b, consisting of a gate insulating film 12 and a doped polysilicon layer, is formed.

[0081] Next, a photoresist film is coated on the upper surfaces of semiconductor layer 1 and gate electrodes 11a and 11b, and a pattern is formed on the photoresist film using photolithography. The patterned photoresist film is used as a mask for implantation of p-type impurity ions such as boron (B). After removing the photoresist film, a photoresist film is recoated on the upper surfaces of semiconductor layer 1 and gate electrodes 11a and 11b, and a pattern is formed on the photoresist film using photolithography. The patterned photoresist film is used as a mask for implantation of n-type impurity ions such as phosphorus (P). After removing the photoresist film, a heat treatment is performed, thereby activating the p-type and n-type impurity ions. As a result, as... Figure 12A and Figure 12B As shown, p is formed in the upper part of the base region 4a. + Type 6a and n source pole regions + The contact region 7a is of the type. Furthermore, a p-type contact region is formed on the upper part of the base region 4b. + Type 6b and n source pole regions + The contact area 7b is of the type. Furthermore, p is selectively formed in the upper part of the drift region 3. + Type 5 drain region. Furthermore, p-type drain regions are selectively formed on the upper part of semiconductor layer 1. + Type 8 substrate contact area.

[0082] Next, an interlayer insulating film 13 is deposited using CVD or similar methods to cover the gate electrodes 11a and 11b. Then, a portion of the interlayer insulating film 13 is selectively removed using photolithography or dry etching to form contact holes that expose the upper surfaces of the source regions 6a and 6b, the drain region 5, the contact regions 7a and 7b, and the substrate contact region 8. Furthermore, the contact holes are filled with a metal film using sputtering, photolithography, and dry etching to form the drain electrode 14 connected to the drain region 5, the source electrodes 15 and 16 connected to the source regions 6a and 6b and the contact regions 7a and 7b, and the substrate contact electrodes 17 and 18 connected to the substrate contact region 8. Thus, Figures 1-3 The semiconductor device involved in the embodiments of the present invention shown is completed.

[0083] According to the semiconductor device manufacturing method of the present invention, by forming breakdown prevention regions 9a and 9b on the upper part of the well region 2, it is possible to prevent breakdown between the drain region 5 and the semiconductor layer 1, suppress the increase of device area, and thus suppress chip area, thereby enabling low-cost manufacturing.

[0084] Furthermore, during the ion implantation process for forming base regions 4a and 4b, ion implantation for forming breakdown prevention regions 9a and 9b is also performed simultaneously. Since the breakdown prevention regions 9a and 9b, with impurity concentrations equal to those of the base regions 4a and 4b, are formed concurrently with the base regions 4a and 4b, the ion implantation conditions are set to conditions suitable for the base regions 4a and 4b. Therefore, sometimes the impurity concentrations for the breakdown prevention regions 9a and 9b are unsuitable. On the other hand, when a dedicated photolithography and ion implantation process is added to ensure that the impurity concentrations of the breakdown prevention regions 9a and 9b are suitable for preventing breakdown, the cost increases.

[0085] In contrast, according to the semiconductor device manufacturing method of the present invention, in the ion implantation process for forming base regions 4a and 4b, by making the openings 22a and 22b for forming breakdown prevention regions 9a and 9b into slits, breakdown prevention regions 9a and 9b with different impurity concentrations than those of the base regions 4a and 4b can be formed simultaneously with the formation of base regions 4a and 4b. Therefore, the impurity concentration of the breakdown prevention regions 9a and 9b can be made to a concentration suitable for preventing breakdown, and manufacturing can be achieved cost-effectively without the need for additional dedicated photolithography and ion implantation processes for forming the breakdown prevention regions 9a and 9b.

[0086] (First variation)

[0087] The semiconductor device involved in the first variation of the embodiments of the present invention differs from the semiconductor device involved in the embodiments of the present invention in that, as Figure 13 As shown, the breakdown prevention zones 9a and 9b have been expanded. Figure 13 The width W2 in the left-right direction. Breakdown prevention zones 9a and 9b are located in... Figure 13 The width W2 in the left and right directions is greater than p - The width of the drift region 3 is wide. The other structures of the semiconductor device involved in the first variation of the embodiment of the present invention are the same as those involved in the semiconductor device involved in the embodiment of the present invention, therefore, repeated descriptions are omitted.

[0088] The semiconductor device according to the first variation of the present invention, even when the width W2 of the breakdown prevention regions 9a and 9b is increased, achieves the same effect as the semiconductor device according to the embodiment of the present invention.

[0089] When manufacturing the semiconductor device according to the first modified example of the embodiments of the present invention, such as Figure 14 As shown, when forming the photoresist film 22, the area used to form the slit-shaped openings 22a and 22b of the breakdown prevention regions 9a and 9b can be expanded accordingly to the width W2 of the breakdown prevention regions 9a and 9b.

[0090] (Second variation)

[0091] The difference between the semiconductor device manufacturing method according to the second variation of the embodiments of the present invention and the semiconductor device manufacturing method according to the embodiments of the present invention is that, as Figure 15 As shown, when forming the resist pattern of the photoresist film 22, the slits of the openings 22a and 22b corresponding to the breakdown prevention regions 9a and 9b are in different directions. The slits of the openings 22a and 22b are along... Figure 15 Extending to the left and right, in Figure 15 Multiple semiconductor devices are arranged side-by-side in the vertical direction. The other processes of the semiconductor device manufacturing method according to the second variation of the present invention are the same as those according to the semiconductor device manufacturing method according to the embodiments of the present invention, therefore, repeated descriptions are omitted.

[0092] The semiconductor device manufacturing method according to the second variation of the present invention achieves the same effect as the semiconductor device manufacturing method according to the present invention, even if the slits of the photoresist film 22 corresponding to the openings 22a and 22b of the breakdown prevention regions 9a and 9b are different. Furthermore, the shape of the slits of the openings 22a and 22b is not particularly limited; for example, they may be oblique slits, or they may be a grid pattern obtained by combining slits in orthogonal directions.

[0093] (Third variation)

[0094] The semiconductor device involved in the third variation of the embodiments of the present invention differs from the semiconductor device involved in the embodiments of the present invention in that, as Figure 16 As shown, the depth D2 of the penetration prevention zones 9a and 9b is shallower than that of the drift zone 3. The depth D2 of the penetration prevention zones 9a and 9b is shallower than that of the drift zone 3. Figure 2 The base regions 4a and 4b shown have a shallow depth D1. The other structures of the semiconductor device involved in the third variation of the embodiment of the present invention are the same as those involved in the semiconductor device involved in the embodiment of the present invention, therefore, repeated descriptions are omitted.

[0095] The semiconductor device according to the third variation of the embodiment of the present invention, even when the depth D2 of the breakdown prevention regions 9a and 9b is shallow, achieves the same effect as the semiconductor device according to the embodiment of the present invention.

[0096] When manufacturing the semiconductor device according to the third variation of the embodiment of the present invention, the depth D2 of the breakdown prevention regions 9a and 9b can be made shallow by adjusting the density of the slits of the openings 22a and 22b corresponding to the breakdown prevention regions 9a and 9b.

[0097] (Fourth variation)

[0098] The semiconductor device involved in the fourth variation of the embodiments of the present invention differs from the semiconductor device involved in the embodiments of the present invention in that, as Figure 17 As shown, the impurity concentration ratio of base regions 4a and 4b is... Figure 3 The breakdown prevention zones 9a and 9b shown have low impurity concentrations. For example... Figure 17 As shown, the depth D1 of the base regions 4a and 4b is shallower than the depth D3 of the drift region 3, and also shallower than... Figure 3 The breakdown prevention regions 9a and 9b shown have a shallow depth D2. Furthermore, the depth D1 of the base regions 4a and 4b can be equal to the depth D3 of the drift region 3, and can also be... Figure 3 The depth D2 of the breakdown prevention regions 9a and 9b shown is the same. The other structures of the semiconductor device according to the fourth variation of the embodiment of the present invention are the same as those according to the embodiment of the present invention, therefore repeated descriptions are omitted.

[0099] The semiconductor device according to the fourth variation of the embodiment of the present invention, even if the impurity concentration of the base regions 4a and 4b is similar to that of the semiconductor device, is still applicable. Figure 3 Even when the impurity concentrations of the breakdown prevention regions 9a and 9b shown are different and lower than those of the breakdown prevention regions 9a and 9b, they still achieve the same effect as the semiconductor device involved in the embodiments of the present invention.

[0100] When manufacturing the semiconductor device according to the fourth variation of the embodiments of the present invention, such as Figure 18 As shown, when forming the photoresist pattern of the photoresist film 22, the openings 22a and 22b corresponding to the breakdown prevention regions 9a and 9b are set as rectangular patterns instead of slits. On the other hand, the openings 22c and 22d corresponding to the base regions 4a and 4b are set as slit patterns.

[0101] In Figure 18 When the photoresist pattern of the photoresist film 22 shown is used as a mask for implanting n-type impurity ions, the implantation conditions are set to be suitable for forming breakdown prevention regions 9a and 9b. The impurity concentration and depth of the base regions 4a and 4b can be adjusted by adjusting the density of the slits in the openings 22c and 22d. As a result, the base regions 4a and 4b and the breakdown prevention regions 9a and 9b can be formed in such a way that the impurity concentration of the base regions 4a and 4b is lower than that of the breakdown prevention regions 9a and 9b, and the depth D1 of the base regions 4a and 4b is shallower than the depth D2 of the breakdown prevention regions 9a and 9b.

[0102] (Fifth variation)

[0103] The semiconductor device involved in the fifth variation of the embodiments of the present invention differs from the semiconductor device involved in the embodiments of the present invention in that, as Figure 19 As shown, it has an LDMOS. Figure 19 The LDMOS shown corresponds to Figure 1 The leftmost LDMOS in the two LDMOS transistors shown. The breakdown prevention region 9a has a C-shaped planar pattern to surround p. - The drift region 3 of the type is arranged in a manner that surrounds it. The other structures of the semiconductor device according to the fifth variation of the embodiment of the present invention are the same as those according to the semiconductor device according to the embodiment of the present invention, therefore, repeated descriptions are omitted.

[0104] The semiconductor device according to the fifth variation of the present invention, even when having an LDMOS, performs the same effect as the semiconductor device according to the embodiments of the present invention.

[0105] When manufacturing the semiconductor device according to the fifth variation of the present invention, when forming the resist pattern of the photoresist film 22, the slit of the opening corresponding to the breakdown prevention region 9a can be formed into a C-shaped pattern.

[0106] (Other implementation methods)

[0107] As described above, the present invention has been illustrated through embodiments and variations, but it should not be construed that the discussions and drawings, which form part of this disclosure, are intended to limit the invention. Based on this disclosure, those skilled in the art will recognize various alternative embodiments, examples, and application techniques. For instance, the structures disclosed in the embodiments and variations of the present invention can be appropriately combined without creating contradictions.

[0108] Explanation of reference numerals in the attached figures

[0109] 1: Semiconductor layer; 2: Well region; 3: Drift region; 4a, 4b: Base region; 5: Drain region; 6a, 6b: Source region; 7a, 7b: Contact region; 8: Substrate contact region; 9a, 9b: Breakdown prevention region; 10: Component isolation insulating film; 11a, 11b: Gate electrode; 12: Gate insulating film; 13: Interlayer insulating film; 14: Drain electrode; 15, 16: Source electrode; 17, 18: Substrate contact electrode; 20, 21, 22: Photoresist film; 22a, 22b, 22c, 22d: Openings.

Claims

1. A semiconductor device, characterized by comprising: Possessing: a semiconductor layer of a first conductivity type; a well region of a second conductivity type provided on an upper portion of the semiconductor layer; a base region of the second conductivity type provided on an upper portion of the well region, which is higher in impurity concentration than the well region; a carrier supply region of the first conductivity type provided on an upper portion of the base region; a drift region of the first conductivity type provided on an upper portion of the well region, which is provided separately from the base region; a carrier receiving region of the first conductivity type provided on an upper portion of the drift region, which is higher in impurity concentration than the drift region; a gate electrode provided on an upper surface of the well region between the base region and the drift region via a gate insulating film; and a breakdown prevention region of the second conductivity type provided on an upper portion of the well region, which is higher in impurity concentration than the well region, the impurity concentration of the breakdown prevention region being different from the impurity concentration of the base region, wherein, in a planar pattern, the breakdown prevention region is provided in a region where the carrier receiving region and the well region face each other in a direction orthogonal to a direction in which the carrier receiving region and the carrier supply region face each other.

2. The semiconductor device according to claim 1, wherein the impurity concentration of the breakdown prevention region is lower than the impurity concentration of the base region.

3. The semiconductor device according to claim 1 or 2, wherein the depth of the breakdown prevention region is shallower than the depth of the base region.

4. The semiconductor device according to claim 1, wherein the impurity concentration of the breakdown prevention region is higher than the impurity concentration of the base region.

5. The semiconductor device according to claim 1 or 4, wherein the depth of the breakdown prevention region is deeper than the depth of the base region.

6. The semiconductor device according to any one of claims 1, 2, or 4, wherein in a planar pattern, the breakdown prevention region is provided in a region where the drift region and the well region face each other in the orthogonal direction. including the following steps:

7. A method for manufacturing a semiconductor device, characterized by forming a well region of a second conductivity type on an upper portion of a semiconductor layer of a first conductivity type; forming a base region of the second conductivity type on an upper portion of the well region, which is higher in impurity concentration than the well region; forming a breakdown prevention region of the second conductivity type on an upper portion of the well region, which is higher in impurity concentration than the well region and different in impurity concentration from the base region; forming a drift region of the first conductivity type on an upper portion of the well region separately from the base region; forming a carrier supply region of the first conductivity type on an upper portion of the base region; forming a carrier receiving region of the first conductivity type on an upper portion of the drift region, which is higher in impurity concentration than the drift region; and forming a gate electrode on an upper surface of the well region between the base region and the drift region via a gate insulating film, wherein the step of forming the base region and the step of forming the breakdown prevention region include: forming a resist pattern having a first opening portion for forming the base region and a slit-shaped second opening portion for forming the breakdown prevention region; performing implantation of impurity ions of the second conductivity type using the resist pattern as a mask; and The base region and the breakdown prevention region, which has a lower impurity concentration compared to the base region, are simultaneously formed through heat treatment. or, The steps of forming the base region and forming the breakdown prevention region include: A resist pattern is formed having a slit-shaped first opening for forming the base region and a second opening for forming the breakdown prevention region; The resist pattern is used as a mask to implant impurity ions of a second conductivity type; and The base region and the breakdown prevention region, which has a high impurity concentration compared to the base region, are simultaneously formed through heat treatment.

Citation Information

Patent Citations

  • Semiconductor device and its manufacture

    JP2000174218A

  • Semiconductor device

    JP2017123498A