Semiconductor structure and method of manufacturing the same

By doping impurities on a semiconductor substrate to form a semiconductor substrate with a gradual change in impurity concentration, VDMOS can be fabricated, which solves the problems of high cost and low efficiency caused by epitaxial growth, and achieves reduced on-resistance and improved reverse recovery characteristics of parasitic diodes.

CN115148603BActive Publication Date: 2026-11-20WUXI CHINA RESOURCES HUAJING MICROELECTRONICS
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202110343343.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-03-30
Publication Date
2026-11-20
Estimated Expiration
2041-03-30

AI Technical Summary

Technical Problem

In the existing VDMOS fabrication process, the epitaxial growth of semiconductor substrates is inefficient and costly, resulting in high on-resistance per unit area and harsh reverse recovery characteristics of parasitic diodes.

Method used

A semiconductor substrate is doped with impurities of the first conductivity type, with the impurity concentration gradually increasing from the surface to the interior to form a semiconductor substrate. A VDMOS is then formed on the substrate through a diffusion process, which reduces the on-resistance per unit area and improves the reverse recovery characteristics of the parasitic diode.

Benefits of technology

It reduces the on-resistance per unit area, improves the reverse recovery characteristics of parasitic diodes, and solves the problems of high cost and low efficiency caused by epitaxial growth.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115148603B_ABST
    Figure CN115148603B_ABST
Patent Text Reader

Abstract

The present disclosure provides a semiconductor structure and a preparation method thereof. The preparation method of the semiconductor structure comprises: providing a semiconductor substrate with a first conductivity type; doping an impurity with the first conductivity type into the semiconductor substrate to obtain a semiconductor substrate, the semiconductor substrate comprising opposite first and second surfaces, and the concentration of the impurity gradually increasing from the first surface to the second surface; and forming a VDMOS using the semiconductor substrate. The present disclosure can reduce manufacturing cost and improve product performance.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This disclosure relates to the field of semiconductor technology, and in particular to a semiconductor structure and its fabrication method. Background Technology

[0002] With the rapid development of technology, vertical double-diffused metal-oxide-semiconductor field-effect transistors (VDMOS) have found increasingly widespread applications in social production and daily life. Currently, in the fabrication of VDMOS, the semiconductor substrate used is formed by epitaxially growing N-drift regions on an N+ substrate. However, this epitaxial growth process is costly. Summary of the Invention

[0003] The purpose of this disclosure is to provide a semiconductor structure and a method for fabricating the same, which can reduce manufacturing costs and improve product performance.

[0004] According to one aspect of this disclosure, a method for fabricating a semiconductor structure is provided, comprising:

[0005] Provide a semiconductor substrate having a first conductivity type;

[0006] The semiconductor substrate is doped with impurities of a first conductivity type to obtain a semiconductor substrate, the semiconductor substrate comprising a first surface and a second surface opposite to each other, the concentration of the impurities gradually increasing from the first surface to the second surface;

[0007] VDMOS is formed using the semiconductor substrate.

[0008] Further, the process of doping the semiconductor substrate with impurities of a first conductivity type to obtain a semiconductor substrate, the semiconductor substrate comprising a first surface and a second surface opposite to each other, wherein the concentration of the impurities gradually increases from the first surface to the second surface, further includes:

[0009] Both opposite surfaces of the semiconductor substrate are doped with impurities of a first conductivity type;

[0010] The semiconductor substrate is obtained by thinning one or both surfaces of the semiconductor substrate.

[0011] Further, the process of doping the semiconductor substrate with impurities of a first conductivity type to obtain a semiconductor substrate, the semiconductor substrate comprising a first surface and a second surface opposite to each other, wherein the concentration of the impurities gradually increases from the first surface to the second surface, further includes:

[0012] The semiconductor substrate is obtained by doping one surface of the semiconductor substrate with an impurity having a first conductivity type.

[0013] Furthermore, the method of forming VDMOS using the semiconductor substrate further includes:

[0014] A source and a gate are formed on a first surface of the semiconductor substrate, and a drain is formed on a second surface of the semiconductor substrate to form a VDMOS.

[0015] Furthermore, the doping of the semiconductor substrate with impurities having a first conductivity type further includes:

[0016] The semiconductor substrate is doped with impurities of a first conductivity type through a diffusion process at a preset temperature.

[0017] Furthermore, the diffusion time of the diffusion process is 288h-432h, and / or the preset temperature is 1200℃-1300℃.

[0018] According to one aspect of this disclosure, a semiconductor structure is provided, the semiconductor structure being a VDMOS, the semiconductor structure comprising:

[0019] A semiconductor substrate includes a first surface and a second surface that are opposite to each other, wherein the concentration of impurities in the semiconductor substrate gradually increases from the first surface to the second surface.

[0020] Furthermore, the semiconductor substrate is a single-crystal material.

[0021] Furthermore, the semiconductor structure includes:

[0022] The source electrode is disposed on the first surface of the semiconductor substrate;

[0023] A gate is disposed on the first surface of the semiconductor substrate;

[0024] The drain electrode is disposed on the second surface of the semiconductor substrate.

[0025] Furthermore, the thickness of the semiconductor substrate ranges from 290 μm to 400 μm, and / or the concentration of impurities in the semiconductor substrate ranges from 1 × 10⁻⁶. 14 Number of atoms / cm 3 Up to 7×10 19 Number of atoms / cm 3 .

[0026] The semiconductor structure and its fabrication method disclosed herein involve a gradual increase in impurity concentration from the first surface to the second surface of the semiconductor substrate, which solves the problems of low efficiency and high cost caused by epitaxial growth in related technologies. At the same time, compared with VDMOS fabricated using semiconductor substrates in related technologies, the VDMOS fabricated herein can reduce the on-resistance per unit area, and the parasitic diode in the VDMOS has softer reverse recovery characteristics. Attached Figure Description

[0027] Figure 1 This is a schematic diagram of a semiconductor substrate in related technologies.

[0028] Figure 2 yes Figure 1 Impurity concentration diagram of the structure shown.

[0029] Figure 3 yes Figure 1 The electric field intensity diagram of the structure shown.

[0030] Figure 4 This is a flowchart of a method for fabricating a semiconductor structure according to an embodiment of the present disclosure.

[0031] Figure 5 This is a schematic diagram of the semiconductor substrate used in the method for fabricating the semiconductor structure according to an embodiment of the present disclosure.

[0032] Figure 6 This is a diagram showing the impurity concentration of the doped semiconductor substrate in the semiconductor structure fabrication method of the present disclosure.

[0033] Figure 7 This is a schematic diagram of the semiconductor substrate in the method for fabricating the semiconductor structure according to the embodiments of this disclosure.

[0034] Figure 8 yes Figure 7 Impurity concentration diagram of the structure shown.

[0035] Figure 9 yes Figure 7 The electric field intensity diagram of the structure shown.

[0036] Figure 10 This is another schematic diagram of the semiconductor substrate in the method for fabricating the semiconductor structure according to the present disclosure.

[0037] Figure 11 This is the reverse recovery current diagram of the parasitic diode.

[0038] Explanation of reference numerals in the attached figures: 1. Semiconductor substrate; 2. Semiconductor substrate; 201. First surface; 202. Second surface; 3. N+ substrate; 4. N- drift region. Detailed Implementation

[0039] Exemplary embodiments will now be described in detail, examples of which are illustrated in the accompanying drawings. When the following description relates to the drawings, unless otherwise indicated, the same numbers in different drawings denote the same or similar elements. The embodiments described in the following exemplary embodiments do not represent all embodiments consistent with this disclosure. Rather, they are merely examples of apparatuses consistent with some aspects of this disclosure as detailed in the appended claims.

[0040] The terminology used in this disclosure is for the purpose of describing particular embodiments only and is not intended to limit the disclosure. Unless otherwise defined, the technical or scientific terms used in this disclosure should be understood in their ordinary sense by one of ordinary skill in the art to which this disclosure pertains. The terms “first,” “second,” and similar terms used in this disclosure and the claims do not indicate any order, quantity, or importance, but are merely used to distinguish different components. Similarly, the terms “a” or “one,” and similar terms do not indicate a quantity limitation, but rather indicate the presence of at least one. “A plurality” or “several” indicates two or more. Unless otherwise stated, the terms “front,” “rear,” “lower,” and / or “upper,” and similar terms are for ease of description only and are not limited to a location or spatial orientation. The terms “comprising,” “including,” and similar terms mean that the elements or objects preceding “comprising,” encompass the elements or objects listed following “comprising,” and their equivalents, and do not exclude other elements or objects. The terms “connected,” “linked,” and similar terms are not limited to physical or mechanical connections and can include electrical connections, whether direct or indirect. The singular forms “a,” “the,” and “the” used in this disclosure and the appended claims are also intended to include the plural forms, unless the context clearly indicates otherwise. It should also be understood that the term “and / or” as used herein refers to and includes any or all possible combinations of one or more of the associated listed items.

[0041] In related technologies, such as Figure 1 As shown, in the fabrication of VDMOS, the semiconductor substrate used is formed by epitaxially growing an N-drift region 4 on an N+ substrate 3. This N-drift region 4 constitutes the high-resistivity layer of the VDMOS to improve its breakdown voltage. This epitaxial growth method is inefficient and has high manufacturing costs; simultaneously, as... Figure 2 As shown, the impurity concentration at thickness 0 is the impurity concentration at the surface of the N-drift region 4 facing away from the N+ substrate 3; the impurity concentration at thickness a is the impurity concentration at the interface between the N+ substrate 3 and the N-drift region 4; and the impurity concentration at thickness b is the impurity concentration at the surface of the N+ substrate 3 facing away from the N-drift region 4. It can be seen that the impurity concentration at the interface between the N+ substrate 3 and the N-drift region 4 is abrupt. On the one hand, a thicker N-drift region 4 is needed to ensure voltage withstand capability, resulting in a larger on-resistance per unit area (Rsp). On the other hand, during reverse recovery of the parasitic diode, minority carriers are quickly swept out of the high-resistivity layer, resulting in a stiff reverse recovery characteristic. Furthermore, the electric field intensity diagram of the semiconductor substrate formed by epitaxially growing the N-drift region 4 on the N+ substrate 3 is shown in the figure. Figure 3As shown, the electric field strength at the interface of N+ substrate 3 / N- drift region 4 is not equal to 0, therefore, its electric field is of the through type.

[0042] This disclosure provides a method for fabricating a semiconductor structure. For example... Figure 4 As shown, the method for fabricating this semiconductor structure may include steps S100-S130, wherein:

[0043] Step S100: Provide a semiconductor substrate having a first conductivity type.

[0044] Step S110: Doping a semiconductor substrate with an impurity having a first conductivity type to obtain a semiconductor substrate. The semiconductor substrate includes a first surface and a second surface that are opposite to each other. The concentration of the impurity gradually increases from the first surface to the second surface.

[0045] Step S120: Form VDMOS using a semiconductor substrate.

[0046] The semiconductor structure fabrication method of this disclosure provides a method where the concentration of impurities gradually increases from the first surface to the second surface of the semiconductor substrate, thus solving the problems of low efficiency and high cost caused by epitaxial growth in related technologies. At the same time, compared with VDMOS fabricated using semiconductor substrates in related technologies, the VDMOS (vertical double-diffused metal-oxide-semiconductor field-effect transistor) fabricated in this disclosure can reduce the on-resistance per unit area, and the parasitic diode in the VDMOS has softer reverse recovery characteristics.

[0047] The steps of the method for fabricating the semiconductor structure according to the present disclosure will be described in detail below:

[0048] In step S100, a semiconductor substrate having a first conductivity type is provided.

[0049] like Figure 5 As shown, the semiconductor substrate 1 is a single-crystal material, such as single-crystal silicon, which has a first conductivity type. In this embodiment, the conductivity type of the semiconductor substrate 1 is N-type. The semiconductor substrate 1 may include two opposite surfaces.

[0050] In step S110, an impurity having a first conductivity type is doped into a semiconductor substrate to obtain a semiconductor substrate. The semiconductor substrate includes a first surface and a second surface that are opposite to each other, and the concentration of the impurity gradually increases from the first surface to the second surface.

[0051] In one embodiment of this disclosure, such as Figure 5 As shown, step S110 may include: doping both opposite surfaces of the semiconductor substrate 1 with impurities having a first conductivity type. Figure 6In the diagram, the impurity concentration at a thickness of 0 represents the impurity concentration at one surface of semiconductor substrate 1; the impurity concentration at a thickness of c represents the impurity concentration inside semiconductor substrate 1; and the impurity concentration at a thickness of d represents the impurity concentration at the other surface of semiconductor substrate 1. Figure 6 It can be seen that the concentration of the impurity gradually decreases from the surface of the semiconductor substrate 1 to the interior of the semiconductor substrate 1. In other words, the concentration of the impurity gradually increases from the interior of the semiconductor substrate 1 to one surface of the semiconductor substrate 1, and the concentration of the impurity also gradually increases from the interior of the semiconductor substrate 1 to the other surface of the semiconductor substrate 1. The concentrations of the impurity at the two opposite surfaces of the semiconductor substrate 1 can be the same, or they can be different.

[0052] like Figure 7 As shown, after doping both opposite surfaces of the semiconductor substrate 1 with impurities of a first conductivity type, step S110 may further include: thinning one or both surfaces of the semiconductor substrate 1 to obtain the semiconductor substrate 2. It is understood that this disclosure can thin only one surface of the semiconductor substrate 1 to obtain the semiconductor substrate 2, or it can thin both surfaces of the semiconductor substrate 1 to obtain the semiconductor substrate 2. Specifically, this disclosure can grind the surface of the semiconductor substrate 1 to thin the semiconductor substrate 1, thereby forming the semiconductor substrate 2. The semiconductor substrate 2 includes opposite first surfaces 201 and second surfaces 202. The ground surface of the two opposite surfaces of the semiconductor substrate 1 forms the first surface 201 of the semiconductor substrate 2, and the unground surface of the two opposite surfaces of the semiconductor substrate 1 forms the second surface 202 of the semiconductor substrate 2. Figure 8 In this context, the impurity concentration at the thickness of 0 is the impurity concentration at the first surface 201 of the semiconductor substrate 2; the impurity concentration at the thickness of e is the impurity concentration at the second surface 202 of the semiconductor substrate 2. Figure 8 It can be seen that the impurity concentration at the first surface 201 is less than that at the second surface 202. From the first surface 201 to the second surface 202, the impurity concentration gradually increases. In other words, the impurity concentration in the semiconductor substrate 2 gradually increases along the thickness direction of the semiconductor substrate 2. Figure 9 The electric field intensity diagram of the semiconductor substrate 2 prepared according to this disclosure is shown. Figure 9 In the figure, the electric field intensity when the thickness is equal to 0 is the electric field intensity at the first surface 201 of the semiconductor substrate 2; the electric field intensity when the thickness is equal to e is the electric field intensity at the second surface 202 of the semiconductor substrate 2. Figure 9 It is known that the electric field of the semiconductor substrate 2 is non-punch-through type. Compared with the semiconductor substrate 2 with a punch-through type electric field in the related art, the present disclosure can reduce the thickness of the high-resistivity drift region when the same breakdown voltage is achieved, thereby reducing the on-resistance per unit area (Rsp).

[0053] In another embodiment of this disclosure, such as Figure 7 and Figure 10 As shown, step S110 may include: doping a surface of a semiconductor substrate 1 with an impurity having a first conductivity type to obtain a semiconductor substrate 2. The undoped surface of the semiconductor substrate 1 forms the first surface 201 of the semiconductor substrate 2, and the doped surface forms the second surface 202 of the semiconductor substrate 2.

[0054] like Figure 5 and Figure 10 As shown, this disclosure allows for the doping of a semiconductor substrate 1 with an impurity of a first conductivity type via ion implantation or diffusion processes. The impurity can be phosphorus, but this disclosure does not specifically limit its application. For example, doping the semiconductor substrate 1 with an impurity of the first conductivity type may include doping the semiconductor substrate 1 with an impurity of the first conductivity type via a diffusion process at a preset temperature. The preset temperature can be 1200℃-1300℃, such as 1200℃, 1250℃, 1260℃, 1280℃, 1300℃, etc. The diffusion time at the preset temperature can be 288h-432h, i.e., 12 days-18 days, such as 12 days, 14 days, 17 days, 18 days, etc. The diffusion process at the preset temperature can employ liquid source diffusion. Taking phosphorus as an example, the liquid source used can be phosphorus oxychloride, etc. In other embodiments of this disclosure, the diffusion process can also employ solid source diffusion or gas source diffusion.

[0055] In addition, such as Figure 7 As shown, the thickness of the semiconductor substrate 2 can range from 290 μm to 400 μm, with specific values ​​such as 290 μm, 300 μm, 360 μm, and 400 μm. The impurity concentration in the semiconductor substrate 2 can range from 1 × 10⁻⁶. 14 Number of atoms / cm 3 Up to 7×10 19 Number of atoms / cm 3 That is, the number of impurity atoms in each cubic centimeter of semiconductor substrate 2 can range from 1 × 10⁻⁶. 14 Up to 7×10 19 .

[0056] In step S120, a VDMOS is formed using a semiconductor substrate.

[0057] For example, step 120 may include: forming a source and a gate on a first surface of a semiconductor substrate, and forming a drain on a second surface of the semiconductor substrate to form a VDMOS. The VDMOS may also include a termination structure to improve the lateral breakdown voltage capability of the semiconductor structure. Specifically, taking an N-type semiconductor substrate as an example, step 120 may include: performing ring lithography on the first surface of the semiconductor substrate; ring implanting P-type ions and forming a P-type breakdown voltage region after push junction to form a termination structure; forming a gate oxide layer and a gate on the first surface of the semiconductor substrate; forming a well region with a second conductivity type in the semiconductor substrate on both sides of the gate, the second conductivity type being opposite to the first conductivity type; forming a source region with a first conductivity type in the well region, and forming a source on the source region; and forming a drain on the second surface of the semiconductor substrate.

[0058] Figure 11 The reverse recovery current diagrams of parasitic diodes in semiconductor structures prepared using this disclosure and in semiconductor structures formed using semiconductor substrate 2 in the related art are shown. Figure 11 middle, I d I represents the forward current. RRM This represents the maximum reverse recovery current. The (t1-t0) and (t4-t3) stages are mainly the process of extracting minority carriers injected during forward propagation, while the (t2-t1) and (t5-t4) stages are the process of the space charge region rapidly expanding to the maximum breakdown voltage. Minority carrier injection during forward propagation is related to the forward current. Therefore, under the same forward current, (t1-t0) and (t4-t3) are approximately the same. However, since the space charge region length of parasitic diodes in related technologies is short, while the space charge region length of the parasitic diode of this disclosure is long, it takes longer to build the space charge region to achieve the same withstand voltage. This results in (t5-t4) being greater than (t2-t1), which in turn leads to the softness factor (t2-t1) / (t1-t0) of parasitic diodes in related technologies being smaller than the softness factor (t5-t4) / (t4-t3) of parasitic diodes of this disclosure. Therefore, the reverse recovery characteristic of the parasitic diode of this disclosure is softer, avoiding large voltage and current spikes during the switching process of the device and solving the EMI problem.

[0059] This disclosure also provides a method for fabricating a semiconductor substrate. This method is the same as the method for fabricating the semiconductor substrate in the above-described methods for fabricating semiconductor structures.

[0060] like Figure 7As shown, this disclosure also provides a semiconductor substrate 2. The semiconductor substrate 2 may include a first surface 201 and a second surface 202 that are opposite to each other, and the impurity concentration in the semiconductor substrate 2 gradually increases from the first surface 201 to the second surface 202.

[0061] This disclosure also provides a semiconductor structure. This semiconductor structure may include the semiconductor substrate described in the above embodiments. The semiconductor structure may be a VDMOS (Vertical Double-Diffused Metal-Oxide-Semiconductor Field-Effect Transistor).

[0062] like Figure 7 As shown, the thickness of the semiconductor substrate 2 can range from 290 μm to 400 μm, with specific values ​​such as 290 μm, 300 μm, 360 μm, and 400 μm. The impurity concentration in the semiconductor substrate 2 can range from 1 × 10⁻⁶. 14 Number of atoms / cm 3 Up to 7×10 19 Number of atoms / cm 3 That is, the number of impurity atoms in each cubic centimeter of semiconductor substrate 2 can range from 1 × 10⁻⁶. 14 Up to 7×10 19 The semiconductor structure may include a source, a gate, and a drain. The source is disposed on the first surface 201 of the semiconductor substrate 2. The gate is disposed on the first surface 201 of the semiconductor substrate 2. The drain is disposed on the second surface 202 of the semiconductor substrate 2.

[0063] The semiconductor substrate preparation method, semiconductor substrate, semiconductor structure preparation method and semiconductor structure provided in this disclosure belong to the same inventive concept. The relevant details and beneficial effects can be referred to each other, and will not be repeated here.

[0064] The above description is merely a preferred embodiment of this disclosure and is not intended to limit this disclosure in any way. Although this disclosure has been disclosed above with reference to a preferred embodiment, it is not intended to limit this disclosure. Any person skilled in the art can make some modifications or alterations to the above-disclosed technical content to create equivalent embodiments without departing from the scope of the technical solution of this disclosure. Any simple modifications, equivalent changes, and alterations made to the above embodiments based on the technical essence of this disclosure without departing from the content of the technical solution of this disclosure shall still fall within the scope of the technical solution of this disclosure.

Claims

1. A method for fabricating a semiconductor structure, characterized in that, include: Provide a semiconductor substrate having a first conductivity type; The semiconductor substrate is doped with impurities of a first conductivity type to obtain a semiconductor substrate, the semiconductor substrate comprising a first surface and a second surface opposite to each other, the concentration of the impurities gradually increasing from the first surface to the second surface; VDMOS is formed using the semiconductor substrate; The process of doping the semiconductor substrate with impurities of a first conductivity type to obtain a semiconductor substrate, the semiconductor substrate comprising a first surface and a second surface opposite to each other, wherein the concentration of the impurities gradually increases from the first surface to the second surface, further comprising: Both opposite surfaces of the semiconductor substrate are doped with impurities of a first conductivity type; The semiconductor substrate is obtained by thinning one or both surfaces of the semiconductor substrate.

2. The method for preparing a semiconductor structure according to claim 1, characterized in that, The method of forming VDMOS using the semiconductor substrate further includes: A source and a gate are formed on a first surface of the semiconductor substrate, and a drain is formed on a second surface of the semiconductor substrate to form a VDMOS.

3. The method for preparing the semiconductor structure according to any one of claims 1 to 2, characterized in that, The doping of the semiconductor substrate with impurities having a first conductivity type further includes: The semiconductor substrate is doped with impurities of a first conductivity type through a diffusion process at a preset temperature.

4. The method for preparing a semiconductor structure according to claim 3, characterized in that, The diffusion time of the diffusion process is 288h-432h, and / or the preset temperature is 1200℃-1300℃.

5. A semiconductor structure, characterized in that, The semiconductor structure is prepared by the method for preparing the semiconductor structure according to any one of claims 1-4, wherein the semiconductor structure is a VDMOS, and the semiconductor structure comprises: A semiconductor substrate includes a first surface and a second surface that are opposite to each other, wherein the concentration of impurities in the semiconductor substrate gradually increases from the first surface to the second surface.

6. The semiconductor structure according to claim 5, characterized in that, The semiconductor substrate is a single-crystal material.

7. The semiconductor structure according to claim 5, characterized in that, The semiconductor structure includes: The source electrode is disposed on the first surface of the semiconductor substrate; A gate is disposed on the first surface of the semiconductor substrate; The drain electrode is disposed on the second surface of the semiconductor substrate.

8. The semiconductor structure according to claim 5, characterized in that, The thickness of the semiconductor substrate ranges from 290 μm to 400 μm, and / or the concentration of impurities in the semiconductor substrate ranges from 1 × 10⁻⁶. 14 Number of atoms / cm 3 Up to 7×10 19 Number of atoms / cm 3 .

Citation Information

Patent Citations

  • Rocket motor

    JP1995083114A