By combining a host material with a specific structure and a delayed fluorescence material, the problem that the host material in the delayed fluorescence material combination of the prior art cannot achieve full light emission performance is solved, and an organic light-emitting element with low voltage drive, long lifetime and high luminous efficiency is realized.

CN115280535BActive Publication Date: 2026-07-17KYULUX INC

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
KYULUX INC
Filing Date
2021-02-04
Publication Date
2026-07-17

AI Technical Summary

Technical Problem

In the existing technology, the host material of delayed fluorescence material combinations cannot achieve sufficient luminescence performance, especially in terms of driving voltage and luminescence lifetime, where there is room for improvement.

Method used

A combination of a host material with a specific structure and a delayed fluorescence material is used, specifically including compounds with specific structures, compounds represented by general formulas (1), (2) and (3), and a delayed fluorescence material to form a composition for use as the luminescent layer of an organic light-emitting element.

Benefits of technology

This has resulted in an organic light-emitting element that features low voltage drive, long lifespan, and high luminous efficiency, thereby improving light-emitting performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115280535B_ABST
    Figure CN115280535B_ABST
Patent Text Reader

Abstract

本发明的课题在于改善使用了延迟荧光材料的有机发光元件的发光效率、驱动电压及寿命。本发明提供一种由下述通式的化合物组成的延迟荧光材料用主体材料。R1~R5为不包含氰基的取代基,n1~n5为0~4,Ar为单环亚芳基或单环杂亚芳基。