Phase change random access memory and method of manufacturing the same
By using a vertical architecture design and a phased low-temperature process to manufacture PCRAM memory, the compatibility problem between high-temperature processes and phase change material regions was solved, achieving high areal density and efficient memory cell manufacturing, thus improving the performance and stability of the memory.
Patent Information
- Application Number
- CN202210319455.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2022-01-21
- Filing Date
- 2022-03-29
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2042-03-29
AI Technical Summary
Existing PCRAM memory faces difficulties in increasing transistor density during manufacturing, and there is incompatibility between high-temperature processes and low-temperature formation processes of phase change material regions, resulting in limitations on the areal density and manufacturing efficiency of memory cells.
The vertical architecture design separates the FET logic layer from the memory layer. The FET logic is fabricated using SOI or SiGe/Si epitaxial substrates. Embedded back-side heated transistors are formed through low-temperature processes to increase the areal density of memory cells. Phase change material regions are also formed through low-temperature processes.
This design achieves high areal density memory cells, avoids damage to the carrier wafer caused by high-temperature processes, improves manufacturing efficiency and the stability of the memory layer, and enhances the current switching capability of the memory cells.
Smart Images

Figure CN115312562B_ABST
Abstract
Description
Technical Field
[0001] This disclosure relates to a phase-change random access memory and a method for manufacturing the same. Background Technology
[0002] The following text discusses the fields of electronic memory, phase change random access memory (PCRAM), PCRAM manufacturing, and related fields. Summary of the Invention
[0003] In a non-limiting embodiment, a method of manufacturing a phase-change random access memory (PCM) is provided. The method includes: forming a field-effect transistor (FET) logic layer of the PCM on a first wafer, wherein forming the FET logic layer includes forming at least one heated FET for each memory cell of the PCM, a first surface of the FET logic layer adjoining the first wafer; bonding a second surface of the FET logic layer relative to the first surface to a carrier wafer; bonding the second surface of the FET logic layer relative to the first surface to the carrier wafer; removing the first wafer to expose the first surface of the FET logic layer, wherein the second surface of the FET logic layer remains bonded to the carrier wafer; and after removing the first wafer, forming a storage layer of the PCM on the exposed first surface of the FET logic layer, wherein forming the storage layer includes forming a phase-change material region for each memory cell electrically connected to a channel of the at least one heated FET.
[0004] In a non-limiting embodiment, the phase-change random access memory (PCM) includes: a wafer; a field-effect transistor (FET) logic layer disposed on the wafer, wherein at least one heated FET of each memory cell of the PCM is included in the FET logic layer; and a storage layer disposed on the FET logic layer, wherein a phase-change material region of each memory cell is included in the storage layer, wherein the phase-change material region is electrically connected to a channel of the at least one heated FET.
[0005] In a non-limiting embodiment, the phase-change random access memory includes: a wafer; a storage layer, wherein a chalcogenide material region of each storage cell is included in the storage layer; and a field-effect transistor (FET) logic layer disposed between the wafer and the storage layer, wherein at least one heating FET of each storage cell is included in the FET logic layer, wherein the at least one heating FET is electrically connected to the chalcogenide material region to heat the chalcogenide material region. Attached Figure Description
[0006] Various aspects of this disclosure will be understood by reading the following detailed description in conjunction with the accompanying drawings. It should be understood that the devices and / or structures shown in the drawings are not necessarily drawn to scale. Therefore, for clarity of discussion, the dimensions of various features may be arbitrarily increased and / or decreased.
[0007] Figure 1 The memory cell of a vertical PCRAM architecture, in which the storage cell includes a second heated field-effect transistor (FET), is illustrated in equivalent circuit diagram.
[0008] Figure 2 A method for manufacturing a vertically structured PCRM, including a second heating FET, is illustrated.
[0009] Figures 3 to 5 The diagram illustrates the manufacturing process of the first chip used to manufacture PCRAM.
[0010] Figure 6 and Figure 7 The sequential steps of fabricating the FET logic layer of a vertical architecture PCRAM are illustrated using a cross-sectional schematic diagram.
[0011] Figure 8 , Figure 9 and Figure 10 The sequential steps of bonding the FET logic layer to the carrier wafer are illustrated using a cross-sectional schematic diagram.
[0012] Figures 11 to 16 The sequential steps of fabricating the storage layer of a vertical architecture PCRAM are illustrated in cross-sectional schematic diagram, using the base of the deposition region that forms the metal plug as the phase change material.
[0013] Figures 17 to 19 The sequential steps of an alternative method for forming a metal plug at the base of a deposition region that serves as a phase-change material are illustrated using a cross-sectional schematic diagram.
[0014] Figures 20 to 22 A schematic cross-sectional view is used to illustrate the phase change material deposited on the metal plug. Figure 20 It is a series of steps that begin with the fabrication of the storage layer of vertical architecture PCRAM via back end-of-line (BEOL) metal interconnects.
[0015] Figures 23 to 25 An additional embodiment of a vertically structured PCRAM including a second heating FET is illustrated in cross-sectional schematic.
[0016] Figure 26 A vertical PCRAM cell excluding the second heating FET is illustrated using an equivalent circuit diagram. Detailed Implementation
[0017] The following disclosure provides numerous different embodiments or instances for implementing various features of the provided subject matter. Specific examples of components and arrangements are described below to simplify this disclosure. Of course, these are merely examples and not intended to be limiting. For example, in the following description, forming a first feature on or over a second feature may include embodiments in which the first and second features are formed in direct contact, and may also include embodiments in which an additional feature may be formed between the first and second features such that the first and second features are not in direct contact. Furthermore, reference numerals and / or letters may be repeated throughout this disclosure. Such repetition is for the sake of brevity and clarity and does not in itself imply a relationship between the various embodiments and / or configurations discussed.
[0018] Furthermore, for ease of explanation, spatially relative terms such as "beneath," "below," "lower," "above," and "upper" may be used herein to describe the relationship between one element or feature shown in the figures and another element or feature. In addition to the orientations illustrated in the figures, these spatially relative terms are also intended to encompass different orientations of elements in use or operation. Devices may have other orientations (rotated 90 degrees or in other orientations), and the spatially relative descriptive terms used herein shall be interpreted accordingly. Unless explicitly stated otherwise, components with the same reference number are assumed to have the same material composition and thickness within the same thickness range.
[0019] Various semiconductor technologies have benefited from random access memory (RAM) with high areal density of memory cells. However, physical limitations make it challenging to increase transistor density in memory (such as flash memory and dynamic random access memory, DRAM) by reducing its size.
[0020] Integrating logic and passive components is another method to increase the cell density of RAM. PCRAM uses phase change materials, such as chalcogenide materials, as passive data storage cells. By passing current through the phase change material, the crystalline phase of the phase change material can switch between a crystalline phase with low resistance and a glassy (or crystalline) phase with high resistance. A large current sufficient to induce a phase change is used to write to the PCRAM cell, and a small current insufficient to induce a phase change is used to detect the resistivity of the phase change material to read from the PCRAM cell. For write operations, generally short, high-amplitude electrical pulses cause rapid heating and cooling to produce an amorphous state, while long, lower-amplitude (but still high-amplitude) electrical pulses are used to transform the material into a crystalline state.
[0021] Generally, PCRAM architecture includes an integrated circuit (IC), where each PCRAM memory cell includes a phase change material region and a driving FET. This approach can limit the areal density of the memory cells. Device speed is also limited by the current density that the FET can apply to the phase change material region. The low current density problem can be solved by adding a second FET to each memory cell. However, this may increase the area of each memory cell and thus negatively impact the areal density of the PCRAM cell. Furthermore, PCRAM fabrication is also challenging. FET fabrication generally requires high-temperature processes, while the formation of the phase change material region (e.g., a chalcogenide material region) is typically performed at low temperatures.
[0022] This document discloses embedded dual-sided heated PCRAM devices and methods for stacking device structures to improve device density. In an illustrative process embodiment, the method includes: using silicon oninsulator (SOI) or SiGe / Si epitaxial substrates for FET logic fabrication processes (e.g., FinFET or gate all-around (GAA) metal-oxide-semiconductor FET, MOSFET processes) and front-end-of-line (FEOL) and middle-end-of-line (MEOL) processes; bonding to a carrier wafer and flipping the bonding structure to perform silicon back-side thinning stopping at the SOI oxide or insulating layer (or SiGe layer); patterning back-side contact openings and forming metal silicides / plugs; and using the flipped wafer as a substrate to form embedded back-side PCRAM and optionally form back-side heated transistors for improving heating efficiency.
[0023] Compared to designs in which FET logic and passive components (e.g., chalcogenide phase-change materials) are arranged side-by-side on the same plane, some embodiments disclosed herein include embedded back-side PCRAM and back-side heated transistors to advantageously increase the areal density of memory cells.
[0024] Please refer to Figure 1 The diagram illustrates a vertically integrated PCRAM memory cell 10 with an equivalent circuit diagram. The described PCRAM memory cell 10 includes a phase change material region 12, which in the illustrated embodiment is a germanium antimony telluride (GST) material, such as Ge₂Sb₂Te₅. More generally, another phase change material, such as a chalcogenide material, can be used. Two examples of phase change materials include the described GST material or a titanium antimony telluride (TST) composition. Figure 1 As shown, the phase change material region 12 operates as a variable resistor, having high resistance when GST is in an amorphous or glassy state and low resistance when GST is in a crystalline state. (More generally, the resistance of the phase change material region 12 is switched to an appropriate degree to define two different storage states).
[0025] The storage cell 10 further includes a heating FET 14, which is also in Figure 1 The label "MOS1" indicates that the heating FET 14 is a MOSFET. In the storage cell 10, the phase change material region 12 is electrically connected to at least one heating FET 14 and is fed through the source S and drain D of this at least one heating FET 14 (e.g., ...). Figure 1 The current between the heating FET 14 and the storage cell 10 is heated. The gate of the heating FET 14 is connected to the write line WL1 of the storage cell 10, which controls the writing of the storage cell 10 (that is, to switch the electrical state of the storage cell 10 between a logic state in which the phase change material region 12 is in a high resistance state and another logic state in which the phase change material region 12 is in a low resistance state).
[0026] The described memory cell 10 further includes a second heating transistor 16, which is also electrically connected to the phase change material region 12 of the memory cell 10 via a channel current. The second heating transistor 16... Figure 1 It is also labeled as "MOS2". However, as will be explained, generally speaking, the first heating FET 14 and the second heating transistor 16 have different structures and / or are made of different materials.
[0027] like Figure 1 Further illustrations, and in particular references Figure 1In illustration A, it should be understood that PCRAM cell 10 is one of the storage cells of PCRAM1. Figure 1 As illustrated in Illustration A, PCRAM 1 includes a plurality of PCRAM storage cells 10 arranged in a two-dimensional array. (See again...) Figure 1 The main diagram (showing a circuit diagram of a memory cell 10) has a vertical architecture. The fabrication of PCRAM 1 is illustrated in [the diagram / illustration]. Figure 1 The main diagram is shown in the upper left corner, using a first wafer 20 and a second wafer 22, wherein the second wafer 22 is also referred to herein as carrier wafer 22. A FET logic layer 24 is formed on the first wafer 20, and at least one heating FET 14 of each memory cell 10 of the PCRAM 1 is included in the FET logic layer 24. After the FET logic layer 24 is formed, it is transferred from the first wafer 20 to the second wafer (or carrier wafer) 22. After the transfer, a memory layer 26 including a phase change material region 12 and a second heating transistor 16 is formed on the FET logic layer 24. Additional metallization steps provide appropriate electrical interconnects to form the PCRAM 1 including an array of memory cells 10.
[0028] This vertical architecture offers several advantages. The resulting vertical architecture of the PCRAM 1 allows the memory cell 10 to have a high areal density on the final wafer (i.e., the second wafer (carrier wafer) 22, on which the PCRAM 1 is bonded). This is due to the memory layer 26 of the memory cell 10, which has phase change material regions 12, being vertically separated from the underlying FET logic layer 24. Compared to a design where the logic FETs are laterally distributed between the phase change material regions, the vertical architecture design allows the FET logic layer 24 and the memory layer 26 to be stacked more tightly (i.e., achieving a higher areal density).
[0029] Another advantage is that dividing the process into fabricating the FET logic layer 24 first and then the memory layer 26 allows for the application of optimal process temperature conditions for each layer during formation. In particular, fabricating FET logic circuit systems typically uses higher temperatures (e.g., including at least one process performed at a temperature of at least 700°C, and FET process operations often performed at 800°C to 900°C or higher). In contrast, phase change material regions, such as chalcogenide materials, are typically fabricated at temperatures of 500°C or lower. For example, GST is sometimes formed at a temperature of about 400°C. Therefore, the processing of the first wafer 20 can be completed at high temperatures (e.g., at 700°C or higher in some embodiments), and the formation of the memory layer 26 after transfer to the second wafer 22 can be completed, for example, at 500°C or lower in some embodiments. With the disclosed vertical manufacturing method, the high-temperature manufacturing of the FET logic layer 24 can be completed before the low-temperature manufacturing of the memory layer 26, thus advantageously ensuring that the memory layer 26 is not exposed to the high temperatures used to form the FET logic layer 24.
[0030] Furthermore, the lower temperature used to form the memory layer 26 facilitates the transfer of the FET logic layer 24 from the first wafer 20 to the second wafer (carrier wafer) 22. This is because a low-temperature process after the transfer avoids damage to the bonding between the carrier wafer 22 and the FET logic layer 24. For example, in some illustrated embodiments, a bonding is formed between highly planar oxide layers formed on the bonding surfaces of the second wafer (carrier wafer) and the FET logic layer 24 using fusion bonding. This fusion bonding process may be unstable during higher-temperature FET processes, but remains stable at the lower temperature used to manufacture the memory layer 26.
[0031] exist Figure 1 In the illustrated example, storage layer 26 also includes a second heating transistor 16 in each storage cell 10. This generates a larger current for switching the state of the phase-change material region 12. Nevertheless, placing the second heating transistor 16 in storage layer 26 does not occupy space in FET logic layer 24, thus increasing the areal density of storage cell 10 while still increasing the switching current.
[0032] To maintain a low-temperature process for the memory layer 26, the second heated transistor 16 may be of a different type and / or made of a different material than the heated FET 14 of the FET logic layer 24. For example, in some non-limiting embodiments, the heated FET 14 is a gate all-around (GAA) FET using silicon channels, while the second heated transistor 16 has channels comprising indium gallium zinc oxide (InGaZnO) heavily doped to N-type (n+ type) to improve conductivity. The InGaZnO channels of the second heated transistor 16 can be formed at a lower process temperature than the process temperature of the silicon channels of the heated FET 14. For example, in some embodiments, the second heated transistor 16 can be formed at a temperature of 500ºC or lower (approximately 400ºC in some embodiments). This facilitates the integration of the second heated transistor 16 into the memory layer 26 to provide advantages such as increased areal density as described above.
[0033] Figure 1 Other reference numerals shown will be explained with reference to cross-sectional schematic diagrams illustrating some non-limiting embodiments.
[0034] Please refer to Figure 2 Explained using a flowchart Figure 1 The manufacturing method of PCRAM 1 with a vertical architecture is shown. Figures 3 to 22 Drawing in the form of a sectional view Figure 2 Various embodiments of the method and the sequential steps of the pattern are shown. Nevertheless, Figure 2 First, an overview of the method is provided herein. The process begins with a first wafer 20. Figure 2 One of the blocks graphically represents what was previously shown in Figure 1 The first wafer 20 includes an etch stop layer that will be removed during a subsequent operation 38 of the process. If the first wafer 20 is a commercially available silicon-on-insulator (SOI) wafer, the insulating layer of the SOI wafer can serve as the etch stop layer. Alternatively, the first wafer 20 may include a silicon wafer on which an etch stop layer is deposited and subsequently epitaxial silicon is formed (see reference). Figures 3 to 5(See the cross-sectional schematic diagram shown). In operations 30 and 32, a FET logic layer 24 is formed on the first wafer 20. More specifically, operation 30 is a front-end-of-line (FEOL) process, performed on the first wafer 20 to form a heating FET 14 for the memory cell 10 of the PCRAM 1. The subsequent operation 32 is a middle-end-of-line (MEOL) process to form the bottom metal (also known as the M0 metal) of the first metal layer that forms the heating FET 14 that contacts the memory cell 10 of the PCRAM 1.
[0035] Subsequently, the FET logic layer 24 is transferred from the first wafer 20 to the second wafer (carrier wafer) 22. The carrier wafer 22 may be a silicon wafer, or more generally, any type of wafer providing suitable structural support for the manufactured PCRAM 1. At this point, in operation 34, high-density plasma (HDP) oxide deposition is performed on the Mo metal of the FET logic layer 24, and the formed HDP oxide is planarized using chemical mechanical polishing (CMP). A similar oxide is also formed on the carrier wafer 22 (not shown in the flowchart). Subsequently, in operation 36, the FET logic layer 24 (more specifically, the HDP oxide deposited and planarized thereon) is bonded to the second wafer 22 (more specifically, the HDP oxide deposited and planarized thereon) using a suitable bonding process (e.g., fusion bonding). Finally, in operation 38, the first wafer 20 is removed from the FET logic layer 24, completing the transfer to the second wafer 22. The removal of operation 38 may require one or more chemical etching, mechanical polishing, chemical-mechanical etching and / or similar methods.
[0036] Next, the storage layer 26 is fabricated. In operation 40, dielectric isolation is deposited. Then, operation 42 is performed to pattern and dry-etch to form contact openings, thus opening via paths to the drain of the heating FET 14. In operation 44, a metal silicide layer is formed on the drain of the heating FET 14, and a contact plug is formed to contact this metal silicide layer. In operation 46, a phase change material region 12 is formed on the plug, and a second heating transistor 16 is also formed. In operation 48, back-end processes are performed to form the metal interconnects of the storage cell 10. Furthermore, in operation 50, an oxide through-hole is formed to connect the gate of the heating FET 14 to the write line WL1 of the storage cell 10.
[0037] Please refer to Figures 3 to 5A cross-sectional schematic diagram showing the sequential steps of the process is used to illustrate the method for manufacturing the first wafer 20. For example... Figure 3 As shown, starting from silicon wafer 60. (As...) Figure 4 As shown, an etch stop layer 62 is formed on silicon wafer 60. After the FET logic layer 24 is bonded to the second wafer (carrier wafer) 22, the etch stop layer 62 will act as an etch stop during the removal of the first wafer 20. After forming the etch stop layer 62, an epitaxial silicon layer 64 is deposited on the etch stop layer 62 to form the starting silicon surface for forming the FET logic layer 24. The etch stop layer 62 may include components that are chemically sufficiently different from silicon to act as an etch stop and can serve as a carrier for subsequent silicon epitaxial growth (e.g., ...). Figure 5 Any material on the surface (as shown in the drawing).
[0038] In some non-limiting embodiments, the etch stop layer comprises a silicon germanium (SiGe) layer having about 20% to 30% silicon, i.e., where x is 20% to 30% Si. 1-x G x The SiGe layer has a larger lattice constant than silicon, so in some embodiments the SiGe layer is boron-doped to produce lattice contraction and reduce the lattice constant difference between SiGe and silicon.
[0039] In other non-limiting embodiments, the etch stop layer 62 is an oxide layer, such that the resulting first wafer 20 is a silicon-on-insulator (SOI) wafer. In some embodiments, the first wafer 20 may be a commercially available SOI wafer, wherein the etch stop layer 62 is a buried silicon dioxide layer. This commercially available SOI wafer may be formed by bonding / etch-back, separation by implantation of oxygen (SIMOX), or the like. During SIMOX, oxygen is implanted to form the silicon dioxide etch stop layer 62, and the overlying silicon layer 64 may be, for example, the original silicon surface or an epitaxial silicon surface grown after ion implantation.
[0040] The foregoing are merely exemplary examples, and more generally, the following methods may be employed: Figure 5 The first wafer 20 can be formed by any process that includes a structural silicon substrate (silicon wafer 60), an etch stop layer 62, and a crystalline silicon layer (epitaxy silicon layer 64) of sufficient quality to serve as a substrate for epitaxial deposition of the FET logic layer 24.
[0041] Please refer to Figure 6 The reference is shown in a cross-sectional schematic diagram. Figure 2 An example of a heated FET 14 manufactured by the front-end process of Operation 30 is shown. Figure 6 A heating FET 14 fabricated on a first wafer 20 is shown, and more specifically, a heating FET 14 fabricated on an epitaxial silicon layer 64 of the first wafer 20 is shown. The illustrated heating FET 14 is a gate-all-around (GAA) FET 14, which includes a gate metal 70 (also labeled "MG") and a high-dielectric-constant dielectric 72. It should be understood that the gate metal 70 may include conductive materials other than metals. As a non-limiting exemplary example, the high-dielectric-constant dielectric 72 is, for example, hafnium oxide (HfO2) and surrounds a channel 74 (in some non-limiting embodiments, such as a silicon channel) around the GAA FET (i.e., the heating FET 14). The gate metal 70, the high-dielectric-constant dielectric 72, and the channel 74 define a transistor architecture. For example, spacers 76, 78, and 79 made of silicon nitride (SiN) and / or silicon carbonitride (SiCN), along with an inter-layer dielectric (ILD) material 80, provide electrical isolation for various components. The illustrated SiN spacer 79 acts as an etch stop during the removal of the first wafer 20 in subsequent operation 38. The illustrated GAA FET (i.e., heated FET 14) uses SiGe as the drain (D) and source (S) junctions. The GAA FET (i.e., heated FET 14) is fabricated using suitable processes. These processes include, for example, the use of sacrificial layers, etch-back techniques, etc., to form the illustrated three-dimensional GAA FET (i.e., heated FET 14).
[0042] Although the heated FET 14 is illustrated using a GAA FET architecture, this is merely an exemplary example. In general, the heated FET 14 may be a GAA FET of other architectures, other forms of three-dimensional FETs (e.g., a fin FET), or a planar FET. Because the illustrated GAA FET is only a non-limiting example of the heated FET 14, therefore... Figure 6 The following diagrams only label some of the GAA FETs.
[0043] Please refer to Figure 7 Shown in cross-sectional view Figure 2The illustrated operation 32 (MEOL process) is an exemplary example. The MEOL process provides a first metallization layer (referred to herein as M0 metal 81) to provide electrical contact for the gate of the heated FET 14. The MEOL process includes an additional layer of ILD material 82 providing support and electrical isolation for the conductive via 84, metal contacts (and traces 86). The conductive via 84 may, for example, comprise tungsten, while the metal contacts and traces 86 may comprise copper or a copper alloy. This is merely a non-limiting exemplary example. Figure 7 Only the M0 metal 81 that contacts the gate of the heated FET 14 is shown. However, the M0 metal 81 may additionally include conductive interconnects (not shown), such as write traces. The conductive trace 86 serves as the write line for the heated FET 14 (i.e., Figure 1 The write line shown is WL1. In some diagrams, the conductive trace 86 is labeled "WL1" (see reference). Figures 20 to 26 ). Figure 1 The circuit diagram also shows conductive trace 86.
[0044] You should understand Figure 7 (More broadly speaking) Figures 6 to 22 The diagram illustrates a single memory cell 10 of PCRAM 1. Therefore, the M0 metal 81 of PCRAM 1 extends across all memory cells 10 of the PCRAM 1 under fabrication, and optionally includes write lines, or other conductive traces, etc., traversing multiple columns and rows of memory cells. The heating FETs 14 and the M0 metal 81 of all memory cells 10 of the fabricated PCRAM 1 extend across the PCRAM 1 under fabrication and are collectively referred to herein as the FET logic layer 24 (also shown in...). Figure 1 ).
[0045] As described above, Figure 2 Operations 30, 32 and Figure 6 , 7 The fabrication of the FET logic layer includes process operations performed at relatively high temperatures (at least 700ºC in some embodiments, and 800ºC to 900ºC or higher in others). Because high temperatures can adversely affect the degradation of the components carrying the wafer bonding and / or the memory layer 26, Figure 2 The subsequent operations 34, 36, 38, 40, 42, 44, 46, 48, and 50 shown can generally be performed at lower temperatures (500ºC or lower in some embodiments, or 400ºC or lower in other, more restrictive embodiments). Therefore, the disclosed manufacturing method advantageously separates the process into high-temperature fabrication of the FET logic layer and subsequent low-temperature processes.
[0046] Please refer to Figures 8 to 10 To show using a cross-sectional schematic diagram Figure 2An exemplary example of the bonding between the carrier wafer 22 and the FET logic layer 24 in operations 34 and 36 shown. Figure 8 The illustration shows the result of high-density plasma (HDP) oxide deposition in operation 34, which is formed on FET logic layer 24. Figure 8 The heating FET 14 and the HDP oxide layer 90 on the M0 metal 81. Please refer to... Figure 9 Similarly, an HDP oxide layer 92 is formed on the carrier wafer 22. The exposed surfaces of the HDP oxide layers 90 and 92 are planarized using chemical mechanical polishing (CMP). Figure 9 This shows that the planarized HDP oxide layers 90 and 92 are bonded together to complete the bonding of the carrier wafer 22 and the FET logic layer 24. Figure 10 The resulting structure after flipping over is shown. Appropriately, the planarized contact surfaces of the HDP oxide layers 90 and 92 are joined by fusion bonding induced by thermal annealing. Without being limited to any particular theory, fusion bonding can be interpreted as the chemical bonding of the hydroxyl functional groups of the HDP oxide layers.
[0047] Alternatively, the first surface 100 of the formed FET logic layer 24 is attached to the silicon wafer 60 by epitaxy or other deposition techniques to fabricate the FET logic layer 24 on the silicon wafer 60. It should be noted that the first surface is not a surface exposed during the fabrication of the FET logic layer, but rather corresponds to the interface between the formed FET logic layer and the underlying first wafer 20. The second surface 102 of the FET logic layer 24, relative to the first surface 100 of the FET logic layer, is bonded to the carrier wafer 22. The second surface 102 is exposed at the end of the fabrication of the FET logic layer 24, and more specifically, the second surface 102 corresponds to the upper surface of the M0 metal 81. During wafer bonding (… Figure 9 After (as shown), the joint structure is flipped (as shown). Figure 10 As shown), this positions the first wafer 20 on top, facilitating the subsequent removal step to expose the first surface 100.
[0048] Please refer to Figure 11 and Figure 12 Using a sectional view diagram to illustrate Figure 2 An example of the removal step in operation 38 shown. Figure 11The diagram shows the device after the removal of silicon wafer 60 and etch stop layer 62. In a suitable method, a large portion of the thickness of silicon wafer 60 is removed using a rapid process, such as grinding, and the remaining thinned silicon is removed using an etchant with a high selectivity for silicon relative to the material of etch stop layer 62. Subsequently, an etchant with a high selectivity for the material of etch stop layer 62 relative to silicon is used to remove etch stop layer 62, such that... Figure 11 Only the epitaxial silicon layer 64 remains, as shown. Finally, the epitaxial silicon layer 64 is removed using an etchant that has a high selectivity for silicon compared to the material of the heated FET 14 deposited directly on the epitaxial silicon layer 64 (e.g., compared to the source S-drain D junction of the GAA FET 14 and compared to the SiN and / or SiCN spacer walls 79). The resulting structure is shown in... Figure 12 The first surface 100 of the FET logic layer 24 is exposed at this time.
[0049] Please refer to Figure 13 Using a cross-sectional diagram to illustrate in Figure 2 A dielectric isolation layer 106 is formed in the dielectric isolation deposition of operation 40. The dielectric isolation layer 106 may typically comprise any dielectric material. In some non-limiting embodiments, the dielectric isolation layer 106 comprises silicon dioxide.
[0050] Please refer to Figures 14 to 16 Using a sectional view diagram to illustrate Figure 2 Examples of operations 42 and 44 involving patterning and dry etching to form contact openings and to form metal silicide contacts and contact plugs. Figure 14 The diagram illustrates the formation of a patterned photoresist 110 on a dielectric isolation layer 106. For example, an opening 112 of the patterned photoresist 110 is defined by spin-on deposition of the photoresist, exposure with a suitable photomask (not shown), and subsequent development. The dielectric isolation layer 106 is then etched through the opening 112 to define an opening 114 within the dielectric isolation layer 106, and the patterned photoresist is subsequently stripped to form... Figure 15 The structure shown. For example, TiSi is deposited in opening 114. x Or, a metal silicide of nickel, cobalt, or platinum group metals is in contact with 116, and then as follows Figure 16 The deposition shown is, for example, a conductive plug 118 made of a low-resistivity metal (e.g., tungsten, molybdenum, cobalt, ruthenium, iridium, etc.). This produces, as... Figure 16 The structure shown. (As illustrated) Figure 16 As shown, the metal silicide contact 116 and the conductive plug 118 form the drain D for the heated FET 14 (as shown). Figure 1Electrical contact between (as shown). As described, the top of the conductive plug 118 serves as the landing site for the subsequent phase change material region 12 (see reference). Figure 20 ).
[0051] Please refer to Figures 17 to 19 A cross-sectional schematic diagram illustrates an alternative method for forming the metal silicide contact 116 and the conductive plug 118. In this method, it begins with... Figure 10 The device to be processed, as shown, has most of the thickness of the silicon wafer 60 removed using a rapid process, such as grinding, followed by removal of the remaining thinned silicon using an etchant that has a high selectivity for silicon compared to the material of the etch stop layer 62. Figure 17 As shown, this makes the etch stop layer 62 the topmost exposed surface. Figure 18 As shown, a patterned photoresist 120 with an opening is subsequently formed, and etching is performed through this opening to form an opening 124 in the etch stop layer 62 and the underlying epitaxial silicon layer 64. Next, a metal silicide contact 116 and a conductive plug 118 are formed in the opening 124 to form... Figure 19 The structure shown.
[0052] Please refer to Figure 20 , Figure 21 Using a sectional view diagram to illustrate Figure 2 An example of operation 46 is used to form a phase change material region 12 and a second heating transistor 16. Figures 20 to 21 The instance begins at Figure 16 The element to be processed is shown, but it can also be started similarly from... Figure 19 The component to be processed. In any case, the ILD material 130 is formed and patterned to define an opening leading to the top of the conductive plug 118, and a phase change material region 12 is deposited in this opening to contact the top of the conductive plug 118. This formation... Figure 20 The structure shown. The conductive plug 118 contacts the metal silicide 116, thus forming an electrical connection between the phase change material region 12 and the drain D of the heating FET 14. Figure 1This connection is also illustrated using an electrical diagram. The phase change material region 12 may include a germanium antimony telluride (GST) composition. However, as previously explained, other phase change materials may be used, such as another chalcogenide material (e.g., titanium antimony telluride (TST) composition). In yet another non-limiting embodiment, the phase change material region 12 is a GST composition having a stoichiometric ratio of Ge2Sb2Te5. In some non-limiting embodiments, the phase change material region 12 is deposited at a relatively low temperature (e.g., 500ºC or lower). In some more limiting embodiments, the phase change material region 12 is deposited at a temperature of 400ºC or lower.
[0053] Subsequently, as Figure 21 As shown, a second heating transistor 16 is formed. Next, another ILD material 132 is deposited as an insulating spacer, and this ILD material 132 is patterned using a photolithography process to form an opening that contacts the upper electrode 134 of the phase change material region 12. Further, inter-metal dielectric (IMD) material is deposited and patterned, and conductive material is deposited to form the second heating transistor 16 on the ILD material 132. The second heating transistor 16 includes a transistor channel 140, a transistor gate 142, and conductive interconnects 144, 146, and 148. (See reference...) Figure 1 Advantageously, the memory layer 26 (including the second heated transistor 16) is formed at a low temperature. In some non-limiting embodiments, the memory layer 26 is formed at a temperature of, for example, 500ºC or lower. In some more limiting embodiments, the memory layer 26 is formed at a temperature of 400ºC or lower. Therefore, the second heated transistor 16 suitably has materials and transistor architecture that can be manufactured at the desired low temperature (500ºC or lower in some instances). Thus, the second heated transistor 16 is configured as a FET having a channel 140 and a gate 142. In a non-limiting example, the channel 140 comprises a thin film of indium gallium zinc oxide (IGZO), and the gate 142 comprises a high-dielectric-constant dielectric material, for example, hafnium oxide. Figure 21 In the example shown, the upper electrode 134 provides an electrical connection between the drain of the IGZO channel 140 of the second heating transistor 16 and the phase change material region 12, and the conductive interconnect 144 forms the bit line BL of the storage cell 10 of the PCRAM 1 (e.g., Figure 1 (As shown). Conductive interconnect 146 provides an electrical connection between the source S of the first heating FET 14 and the source of the IGZO channel 140 (also shown in...). Figure 1The conductive interconnect 148 contacts the gate 142 of the second heating transistor 16, and thus forms the second write line (i.e., Figure 1 The write line WL2 is shown.
[0054] Please refer to Figure 22 Using a sectional view diagram to illustrate Figure 2 An example of the BEOL process in operation 48. The BEOL process in operation 48 forms one or more layers of metal 150 (e.g., M1 metal, M2 metal, etc.) to provide electrical connections to the conductive interconnects 144 serving as bit lines in PCRAM 1 and the conductive interconnects 148 serving as write lines WL2 in PCRAM 1. Furthermore, Figure 2 Operation 50 may include further BEOL processing to provide an electrical connection to trace 86, which serves as write line WL1, via oxide perforation (not shown).
[0055] Reference should be understood Figures 3 to 22 The examples described are non-limiting and can have various variations. For example, the heating FET 14 can vary in architecture, such as being a GAA FET, FinFET, planar FET, etc. The second heating transistor 16 can vary in structure, for example, using another channel material that can be fabricated at low temperatures (500ºC or lower in some embodiments, and 400ºC or lower in more limiting embodiments). Various electrical interconnects such as trace 86, conductive plug 118, upper electrode 134, conductive interconnects 144, 146, 148, etc., can differ in configuration details from those shown. Furthermore, N-channel FETs or P-channel FETs can be considered as heating FETs. In some embodiments, the upper electrode 134 is smaller in height than the conductive plug 118, which serves as the lower electrode.
[0056] Please refer to Figures 23 to 25 Some variations of the embodiments will be described. Figures 23 to 25 In the text, the labels correspond to similar ones. Figure 22 Features of the illustrated embodiment. Figure 23 The embodiments shown are different Figure 22 The example shown. Figure 23 The illustrated embodiment provides a second metal silicide contact 116-2 and a second conductive plug 118-2 formed as part of the FET logic layer 24 in the same manner as the metal silicide contact 116 and conductive plug 118, except that the second metal silicide contact 116-2 and the second conductive plug 118-2 contact the source S of the heated FET 14. The advantage of this method is that the conductive interconnect 146 providing the electrical connection between the source of the IGZO channel 140 and the source S of the heated FET 14 can be shortened to... Figure 23The conductive interconnect 146-2 shown lands on the second conductive plug 118-2. This avoids forming the conductive interconnect 146 as a via extending into the FET logic layer 24 during the formation of the storage layer 26.
[0057] Figure 24 The illustrated embodiments are similar to Figure 23 The embodiment shown omits the left half of the GAA FET structure.
[0058] Figure 25 The embodiments shown are similar to Figure 22 The illustrated embodiment, however, includes the GAA FET structure on the left and connects it to provide a second heating FET 14-3 to provide additional heating for the phase change material region 12. Therefore, Figure 25 The illustrated embodiment has three heating transistors (including heating FETs 14, 14-3 and heating transistor 16) connected to heat the phase change material region 12, which further improves heating efficiency.
[0059] The aforementioned embodiment of PCRAM with a vertical architecture also advantageously includes a second heating transistor 16 located in the memory layer 26, in addition to the heating FET 14. As mentioned above, this improves heating efficiency.
[0060] Please refer to Figure 26 However, if the additional heating efficiency provided by the second heating transistor 16 is not required, the second heating transistor 16 can be omitted. Figure 26 Drawing similar to Figure 1 The PCRAM shown is omitted, except for the second heating transistor 16. Figure 26 In the text, the labels correspond to similar ones. Figure 1 Features of the illustrated embodiments. It should be understood that... Figure 26 The vertical architecture of the embodiment retains the advantage of high areal packing density due to the vertical arrangement of the phase change material region 12 and the heating FET 14.
[0061] Various embodiments will be further described below.
[0062] In a non-limiting embodiment, a method of manufacturing a phase-change random access memory (PCM) is provided. The method includes: forming a field-effect transistor (FET) logic layer of the PCM on a first wafer, wherein forming the FET logic layer includes forming at least one heated FET for each memory cell of the PCM, a first surface of the FET logic layer adjoining the first wafer; bonding a second surface of the FET logic layer relative to the first surface to a carrier wafer; bonding the second surface of the FET logic layer relative to the first surface to the carrier wafer; removing the first wafer to expose the first surface of the FET logic layer, wherein the second surface of the FET logic layer remains bonded to the carrier wafer; and after removing the first wafer, forming a storage layer of the PCM on the exposed first surface of the FET logic layer, wherein forming the storage layer includes forming a phase-change material region for each memory cell electrically connected to a channel of the at least one heated FET.
[0063] In a non-limiting embodiment, a method of manufacturing a phase-change random access memory (PCM) is provided. The method includes: forming a field-effect transistor (FET) logic layer of the PCM on a first wafer, wherein forming the FET logic layer includes forming at least one heated FET for each memory cell of the PCM, a first surface of the FET logic layer adjoining the first wafer; bonding a second surface of the FET logic layer relative to the first surface to a carrier wafer; bonding the second surface of the FET logic layer relative to the first surface to the carrier wafer; removing the first wafer to expose the first surface of the FET logic layer, wherein the second surface of the FET logic layer remains bonded to the carrier wafer; and after removing the first wafer, forming a storage layer of the PCM on the exposed first surface of the FET logic layer, wherein forming the storage layer includes forming a phase-change material region for each memory cell electrically connected to a channel of the at least one heated FET. The storage layer forming the phase-change random access memory on the exposed first surface of the field-effect transistor logic layer further includes: forming a second heating transistor for each storage cell to be connected to the corresponding storage cell via a channel.
[0064] In some embodiments, the phase change material region and the second heated transistor are formed at a temperature of 500ºC or lower. In some embodiments, forming the field-effect transistor logic layer includes performing at least one process operating at a temperature of at least 700ºC. In some embodiments, forming the second heated transistor includes depositing the channel of the second heated transistor comprising an indium gallium zinc oxide component. In some embodiments, the at least one heated field-effect transistor is a fin field-effect transistor or a gate-all-around field-effect transistor. In some embodiments, forming the memory layer includes: forming a metal silicide layer on the drain of the fin field-effect transistor or the gate-all-around field-effect transistor; forming a conductive via comprising a metal or a metal alloy on the metal silicide layer; and forming the phase change material region on the conductive via. In some embodiments, bonding the second surface of the field-effect transistor logic layer to the carrier wafer includes: disposing an oxide layer on the second surface of the field-effect transistor logic layer; performing chemical mechanical polishing on the oxide layer disposed on the second surface of the field-effect transistor logic layer; and after the chemical mechanical polishing, bonding the oxide layer disposed on the second surface of the field-effect transistor logic layer to another oxide layer disposed on the carrier wafer. In some embodiments, the first wafer comprises a silicon wafer having an etch stop layer disposed thereon, an epitaxial silicon layer disposed thereon on the etch stop layer, wherein the field-effect transistor logic layer is formed on the epitaxial silicon layer, and removing the first wafer comprises removing the silicon wafer, wherein removing the silicon wafer comprises etching at least a portion of the silicon wafer using the etch stop layer as an etch stop. In some embodiments, the etch stop layer comprises a silicon-germanium layer or an oxide layer. In some embodiments, the phase change material region comprises a chalcogenide material. In some embodiments, the chalcogenide material comprises a germanium-antimony-tellurium composition or a titanium-antimony-tellurium composition.
[0065] In a non-limiting embodiment, the phase-change random access memory (PCM) includes: a wafer; a field-effect transistor (FET) logic layer disposed on the wafer, wherein at least one heated FET of each memory cell of the PCM is included in the FET logic layer; and a storage layer disposed on the FET logic layer, wherein a phase-change material region of each memory cell is included in the storage layer, wherein the phase-change material region is electrically connected to a channel of the at least one heated FET.
[0066] In a non-limiting embodiment, the phase-change random access memory (PCM) includes: a wafer; a field-effect transistor (FET) logic layer disposed on the wafer, wherein at least one heated FET of each memory cell of the PCM is included in the FET logic layer; and a storage layer disposed on the FET logic layer, wherein a phase-change material region of each memory cell is included in the storage layer, wherein the phase-change material region is electrically connected to a channel of the at least one heated FET. A second heated transistor of each memory cell is further included in the storage layer, the second heated transistor including a channel electrically connected to the phase-change material region.
[0067] In some embodiments, the channel of the second heating transistor comprises indium gallium zinc oxide. In some embodiments, the at least one heating field-effect transistor is a finned field-effect transistor or a gate-all-around field-effect transistor. In some embodiments, the phase change material region comprises a chalcogenide material. In some embodiments, the phase change material region comprises germanium-antimony-tellurium or titanium-antimony-tellurium.
[0068] In a non-limiting embodiment, the phase-change random access memory includes: a wafer; a storage layer, wherein a chalcogenide material region of each storage cell is included in the storage layer; and a field-effect transistor (FET) logic layer disposed between the wafer and the storage layer, wherein at least one heating FET of each storage cell is included in the FET logic layer, wherein the at least one heating FET is electrically connected to the chalcogenide material region to heat the chalcogenide material region.
[0069] In a non-limiting embodiment, the phase-change random access memory includes: a wafer; a storage layer, wherein a chalcogenide material region of each storage cell is included in the storage layer; and a field-effect transistor (FET) logic layer disposed between the wafer and the storage layer, wherein at least one heating FET of each storage cell is included in the FET logic layer, wherein the at least one heating FET is electrically connected to the chalcogenide material region to heat the chalcogenide material region. A second heating transistor of each storage cell is further included in the storage layer, and the second heating transistor is electrically connected to the chalcogenide material region to heat the chalcogenide material region.
[0070] The foregoing has outlined features of several embodiments to enable those skilled in the art to better understand the nature of this disclosure. Those skilled in the art should understand that they can readily use this disclosure as a basis for designing or modifying other processes and structures to achieve the same purposes and / or advantages as the embodiments described herein. Those skilled in the art should also recognize that such equivalent constructions do not depart from the spirit and scope of this disclosure, and that they can make various changes, substitutions, and modifications without departing from the spirit and scope of this disclosure.
Claims
1. A method for manufacturing a phase-change random access memory, comprising: A field-effect transistor (FET) logic layer of the phase-change random access memory is formed on a first wafer, wherein forming the FET logic layer includes forming at least one heated FET for each memory cell of the phase-change random access memory, and a first surface of the FET logic layer is attached to the first wafer. The second surface of the field-effect transistor logic layer, relative to the first surface, is bonded to the carrier wafer; The first wafer is removed to expose the first surface of the field-effect transistor logic layer, wherein the second surface of the field-effect transistor logic layer remains bonded to the carrier wafer; as well as After the first wafer is removed, a storage layer of the phase-change random access memory is formed on the exposed first surface of the field-effect transistor logic layer. Forming the storage layer includes forming phase-change material regions for each storage cell that are electrically connected to channels of the at least one heated field-effect transistor. These phase-change material regions are heated by channel currents flowing between the drain and source of the at least one heated field-effect transistor in the storage cell. The removal of the first wafer to expose the first surface of the field-effect transistor logic layer includes exposing the at least one heated field-effect transistor of each memory cell. Furthermore, forming the storage layer also includes: A metal silicide layer is formed on the drain of the at least one heated field-effect transistor; Conductive vias comprising metal or metal alloy are formed on the metal silicide layer; and The phase change material region is formed on the conductive via.
2. The method for manufacturing a phase-change random access memory according to claim 1, wherein the memory layer forming the phase-change random access memory on the exposed first surface of the field-effect transistor logic layer further comprises: A second heating transistor is formed for each storage cell, with channels connecting to the corresponding storage cell.
3. The method for manufacturing a phase change random access memory according to claim 2, wherein the phase change material region and the second heating transistor are formed at a temperature of 500ºC or lower.
4. The method for manufacturing a phase-change random access memory according to claim 3, wherein forming the field-effect transistor logic layer comprises performing at least one process at a temperature of at least 700ºC.
5. The method for manufacturing a phase-change random access memory according to claim 2, wherein forming the second heating transistor includes depositing the channel of the second heating transistor comprising an indium gallium zinc oxide composition.
6. The method for manufacturing a phase-change random access memory according to claim 1, wherein the at least one heated field-effect transistor is a finned field-effect transistor or a gate-all-around field-effect transistor.
7. The method for manufacturing a phase change random access memory according to claim 1, wherein the phase change material region comprises germanium-antimony-tellurium or titanium-antimony-tellurium.
8. The method for manufacturing a phase-change random access memory according to claim 1, wherein bonding the second surface of the field-effect transistor logic layer to the carrier wafer comprises: An oxide layer is disposed on the second surface of the field-effect transistor logic layer; The oxide layer disposed on the second surface of the logic layer of the field-effect transistor is subjected to chemical mechanical polishing; as well as After the chemical mechanical polishing, the oxide layer disposed on the second surface of the field-effect transistor logic layer is bonded to another oxide layer disposed on the carrier wafer.
9. The method for manufacturing a phase-change random access memory according to claim 1, wherein the first wafer comprises a silicon wafer, an etch stop layer is disposed on the silicon wafer, an epitaxial silicon layer is disposed on the etch stop layer, wherein the field-effect transistor logic layer is formed on the epitaxial silicon layer, and removing the first wafer comprises: Removing the silicon wafer, wherein removing the silicon wafer includes etching at least a portion of the silicon wafer using the etch stop layer as an etch stop.
10. The method for manufacturing a phase change random access memory according to claim 9, wherein the etch stop layer comprises a silicon-germanium layer or an oxide layer.
11. The method for manufacturing a phase change random access memory according to claim 1, wherein the phase change material region comprises a chalcogenide material.
12. The method of manufacturing a phase-change random access memory according to claim 1, wherein the phase-change material regions of each memory cell are electrically connected to be heated by a channel current flowing between the drain and source of the at least one heated field-effect transistor of the memory cell.
13. A method for manufacturing a phase-change random access memory, comprising: A field-effect transistor logic layer of the phase-change random access memory formed on a first wafer, wherein the field-effect transistor logic layer includes at least one heated field-effect transistor of each storage cell of the phase-change random access memory. The field-effect transistor logic layer on the first wafer will be bonded to the second wafer; With the field-effect transistor logic layer still bonded to the second wafer, the first wafer is removed to expose the surface of the field-effect transistor logic layer, wherein the exposed surface of the field-effect transistor logic layer includes exposing the at least one heated field-effect transistor for each memory cell; and After bonding the field-effect transistor (FET) logic layer on the first wafer to the second wafer, a memory layer is formed on the surface where the FET logic layer is exposed. The memory layer includes phase-change material regions for each memory cell, wherein the phase-change material regions are electrically connected to the channels of the at least one heated FET, and the phase-change material regions are heated by channel current flowing between the drain and source of the at least one heated FET in the memory cell. Furthermore, forming the storage layer includes: A metal silicide layer is formed on the drain of the at least one heated field-effect transistor; Conductive vias comprising metal or metal alloy are formed on the metal silicide layer; and The phase change material region is formed on the conductive via.
14. The method of claim 13, wherein a second heating transistor for each storage cell is further included in the storage layer, the second heating transistor including a channel electrically connected to the phase change material region.
15. The method of claim 14, wherein the channel of the second heating transistor comprises indium gallium zinc oxide.
16. The method of claim 13, wherein the at least one heated field-effect transistor is a finned field-effect transistor or a gate-surround field-effect transistor.
17. The method of claim 13, wherein the phase change material region comprises a chalcogenide material.
18. The method of claim 17, wherein the phase change material region comprises germanium-antimony-tellurium or titanium-antimony-tellurium.
19. A method for manufacturing a phase-change random access memory, comprising: Forming a field-effect transistor logic layer of the phase-change random access memory on a first wafer includes forming at least one heated field-effect transistor for each memory cell of the phase-change random access memory, wherein a first surface of the formed field-effect transistor logic layer is attached to the first wafer. The field-effect transistor logic layer is transferred from the first wafer to the second wafer; After the field-effect transistor (FET) logic layer is transferred from the first wafer to the second wafer, a storage layer of the phase-change random access memory (PDRAM) is formed on the FET logic layer. The storage layer of the PDRAM includes chalcogenide phase-change material regions formed for each memory cell. The chalcogenide phase-change material regions of each memory cell are electrically connected to the channel of the at least one heated FET. The chalcogenide phase-change material regions are heated by the channel current flowing between the drain and source of the at least one heated FET in the memory cell. The storage layer is formed at a temperature of 500°C or lower. Furthermore, the storage layer forming the phase-change random access memory includes: A metal silicide layer is formed on the drain of the at least one heated field-effect transistor; Conductive vias comprising metal or metal alloy are formed on the metal silicide layer; and The chalcogenide phase change material region is formed on the conductive via.
20. The method according to claim 19, wherein the chalcogenide phase change material region comprises germanium-antimony-tellurium or titanium-antimony-tellurium components.
Citation Information
Patent Citations
Semiconductor memory device and method of fabricating the same
CN1574410A
3D semiconductor device and structure
US20200243487A1