Injection molding bending mechanism
By adopting the combination technology of continuous heating, external extrusion and water-cooled circulation pump in the bending mechanism of the injection molded parts, the possible rebound and deformation problems after bending of the injection molded parts are solved, and the stability and production efficiency of the injection molded parts are improved, and the safety is improved.
Patent Information
- Application Number
- CN202210888305.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-07-27
- Publication Date
- 2025-04-01
- Estimated Expiration
- 2042-07-27
AI Technical Summary
Due to the good plasticity of the injection molded parts during the bending process, they may deform or rebound when they are not completely cooled after heating and bending.
An injection molded part bending mechanism is adopted, and rapid cooling and molding is achieved through continuous heating and external extrusion, and a water-cooled circulation pump is used. The mechanism includes a bending device, a cooling device and a push rod. Through the cooperation of snaps, grooves and water-cooled circulation pump, the injection molded parts are quickly cooled after bending, avoiding rebound and deformation.
It effectively avoids the problem of rebound or deformation after injection molding, improves the stability and production efficiency of injection molding parts, and improves safety through alarm devices.
Smart Images

Figure CN115320074B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of bending mechanisms, in particular to an injection molded part bending mechanism. Background Art
[0002] Injection molded parts refer to various injection molded products produced by injection molding machines, including various packages, parts, etc. They are mainly made of materials such as polyethylene or polypropylene and added with a variety of organic solvents.
[0003] In the prior art, when an injection molded part is bent, it is usually heated at the bend. After stamping and bending, the next injection molded part is bent directly. However, some injection molded parts have good plasticity and may deform and rebound when they are not completely cooled after heating and bending.
[0004] Therefore, an injection molded part bending mechanism is proposed. Summary of the invention
[0005] The object of the present invention is to provide an injection molded part bending mechanism, which solves the problems raised in the above-mentioned background technology through continuous heating and external extrusion, and rapid cooling and shaping.
[0006] To achieve the above object, the present invention provides the following technical solutions:
[0007] An injection molded part bending mechanism, comprising:
[0008] Controller;
[0009] A base, wherein a controller is fixedly mounted on an outer side wall of the base;
[0010] Conveyor belt, the base is equipped with a transmission belt;
[0011] A hydraulic punch, wherein the outer side wall of the base is fixedly connected with a connecting seat, and the hydraulic punch is fixedly installed on the connecting seat;
[0012] A push rod, wherein the push rod is fixedly mounted on the inner side wall of the base;
[0013] Also includes:
[0014] A bending device, wherein a plurality of the bending devices are placed on the conveyor belt, and the bending devices slide relative to the base;
[0015] A cooling device is fixedly installed inside each of the plurality of bending devices.
[0016] Preferably, the bending device includes a plurality of shells fixedly mounted on the conveyor belt, a No. 1 spring is fixedly mounted at four corners of the upper end of the shell, an extrusion plate is fixedly connected to the upper ends of the four No. 1 springs, the extrusion plate is V-shaped, a guide rod is slidably mounted inside one side wall of the shell, the guide rod is fixedly connected to the extrusion plate, two forming plates are symmetrically fixedly connected inside the shell, an empty groove is formed between the two forming plates, a plurality of No. 2 springs are fixedly connected to the middle of the bottom of the empty groove, a support plate is fixedly connected to the top of the plurality of No. 2 springs, and the support plate is located directly below the middle of the extrusion plate.
[0017] Preferably, grooves are symmetrically provided at the upper ends of both side walls of the shell, and two buckles cooperating with the grooves are fixedly mounted at the lower end of the extrusion plate.
[0018] Preferably, an elastic block cooperating with the guide rod is provided inside one side wall of the shell, a heating wire is provided inside the support plate, and the elastic block is electrically connected to the heating wire.
[0019] Preferably, two through slots penetrating to the groove are provided on the outer side wall of the shell, two No. 4 springs are symmetrically and fixedly connected inside the two through slots, and a movable rod for pushing the buckle is commonly connected between the four No. 4 springs.
[0020] Preferably, the cooling device includes a water-cooling circulation pump fixedly installed inside the molding plate on one side, a plurality of water-cooling circulation pipes are fixedly connected under the surfaces of the two molding plates, and the plurality of water-cooling circulation pipes are connected to the water-cooling circulation pump pipeline, an elastic button is fixedly installed on the molding plate on one side of the water pump circulation pump, and the elastic button is electrically connected to the water-cooling circulation pump, and an alarm device for detecting whether the water-cooling circulation pipe is leaking is provided inside the two molding plates.
[0021] Preferably, the alarm device includes a collection box fixedly installed at the bottom of the outer shell, two connection rods are provided in the middle of the collection box, two warning lights corresponding to the two forming plates are provided on the outer surface of the outer shell, and the connection rods are electrically connected to the warning lights, and a water channel for collecting water is fixedly connected between the forming plate and the collection box.
[0022] Preferably, the power can be supplied only after the head of the power rod contacts water.
[0023] Preferably, two support bars are fixedly installed on both sides of the outer wall of the shell, and trigger plates are hinged on the two support bars. No. 3 springs are fixedly installed on both sides of the outer wall of the shell, and the two No. 3 springs are fixedly connected to the trigger plates, and the trigger plates are electrically connected to the controller.
[0024] Preferably, a striker is provided on the inner wall of the base, an input end of the striker is fixedly connected to a cylinder, and round rods cooperating with grooves on the outer wall of the shell are provided on both sides of the striker.
[0025] Compared with the prior art, the present invention has the following beneficial effects:
[0026] 1. The injection molding bending mechanism described in the present invention is provided with buckles, grooves and a water-cooled circulating pump, so that after the bending is completed, the injection molding is buckled with the buckles and the grooves, and then squeezed by the extrusion plate and the molding plate, and then the injection molding is quickly cooled by the water-cooled circulating pump, so as to achieve the effect of rapid molding and avoid the possibility of rebound and deformation of the injection molding after molding.
[0027] 2. The injection molding part bending mechanism described in the present invention can provide a collection box and a warning light to promptly remind the staff when the water-cooling circulation pipe is broken or damaged, allowing the staff to repair and replace it, and can objectively observe the condition of the water-cooling circulation pipe inside the shell, thereby improving safety.
[0028] 3. The injection molded part bending mechanism described in the present invention can automatically pop out the molded injection molded part by setting a collision rod and a push rod, and can be automatically pushed out and collected after reaching the specified position, thereby reducing the burden on the staff and further improving the production efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] Figure 1 It is a three-dimensional structural diagram of the present invention;
[0030] Figure 2 is a cross-sectional view of the present invention;
[0031] Figure 3 For the present invention Figure 2 A partial enlarged view of the middle part;
[0032] Figure 4 For the present invention Figure 3 A partial enlarged view of point B in the middle;
[0033] Figure 5 For the present invention Figure 3 A partial enlarged view of point C in the middle;
[0034] Figure 6 For the present invention Figure 3 A partial enlarged view of point D in the middle;
[0035] Figure 7 It is a structural diagram of the present invention when being bent;
[0036] Figure 8 For the present invention Figure 7 A partial enlarged view of point E in the middle;
[0037] Fig. 9 It is a partial structural schematic diagram of the present invention.
[0038] In the figure: 1. controller; 2. base; 3. conveyor belt; 4. hydraulic punch; 51. shell; 52. groove; 53. extrusion plate; 54. support plate; 6. spring No. 1; 7. spring No. 2; 8. buckle; 9. moving rod; 10. forming plate; 11. water-cooling circulation pump; 12. impact rod; 13. round rod; 14. push rod; 15. guide rod; 16. elastic block; 17. water-cooling circulation pipe; 18. elastic button; 19. collection box; 20. connecting rod; 21. water channel; 22. warning light; 23. support bar; 24. trigger plate; 25. spring No. 3; 26. through groove; 27. spring No. 4. DETAILED DESCRIPTION
[0039] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0040] See also Figures 1 to 9 The present invention provides an injection molding bending mechanism, and the technical solution is as follows:
[0041] An injection molded part bending mechanism, comprising:
[0042] Controller 1;
[0043] A base 2, wherein a controller 1 is mounted on an outer side wall of the base 2;
[0044] A conveyor belt 3, wherein the conveyor belt 3 is installed on the surface of the base 2;
[0045] A hydraulic punch 4, wherein the hydraulic punch 4 is fixedly connected to a hydraulic cylinder, the hydraulic cylinder is fixedly connected to a connecting seat, and the connecting seat is fixedly connected to the base 2;
[0046] A push rod 14, wherein the push rod 14 is fixedly connected to the inner wall of the base 2;
[0047] Also includes:
[0048] Bending devices, a plurality of said bending devices are placed on the conveyor belt 3, and said bending devices slide relative to the base 2;
[0049] A cooling device is fixedly installed inside each of the plurality of bending devices.
[0050] When in use, first, the staff puts the injection molded part into the bending device, operates the controller 1 to start the machine, and the conveyor belt 3 drives the bending device to stop just below the hydraulic punch 4. At this time, the hydraulic punch 4 presses down to bend. After the bending is completed, the cooling device is started, so that the injection molded part is quickly cooled after bending. The conveyor belt 3 drives the bending device and the bent injection molded part to the push rod 14 and then stops. The push rod 14 pushes the bent injection molded part out, and the bending device returns to the staff along the conveyor belt 3. By setting the cooling device, the injection molded part can be quickly cooled after the bending is completed, avoiding the problem of rebound and deformation of the injection molded part after bending.
[0051] As an embodiment of the present invention, the bending device includes: the bending device includes a plurality of shells 51 fixedly installed on the conveyor belt 3, four corners of the upper end of the shell 51 are fixedly installed with No. 1 springs 6, the upper ends of the four No. 1 springs 6 are commonly fixedly connected with an extrusion plate 53, the extrusion plate 53 is V-shaped, a guide rod 15 is slidably installed inside a side wall of the shell 51, the guide rod 15 is fixedly connected to the extrusion plate 53, two forming plates 10 are symmetrically fixedly connected inside the shell 51, an empty groove is formed between the two forming plates 10, a plurality of No. 2 springs 7 are fixedly connected in the middle of the bottom of the empty groove, a support plate 54 is commonly fixedly connected to the top of the plurality of No. 2 springs 7, and the support plate 54 is located directly below the middle of the extrusion plate 53.
[0052] During use, the staff puts the injection molded part on the support plate 54, and the shell 51 is driven by the conveyor belt 3 to the bottom of the hydraulic punch 4 and stops. At this time, the hydraulic punch 4 is pressed down, and the hydraulic punch 4 drives the extrusion plate 53 to move downward, thereby squeezing the injection molded part into the shell 51, compressing the No. 1 spring 6, and the guide rod 15 moves downward to squeeze the support plate 54 and the No. 2 spring 7 into the shell 51 until the spring limit. At this time, the extrusion plate 53 and the two forming plates 10 squeeze and bend the injection molded part. After completing the bending action, the hydraulic punch 4 moves upward to recover. By setting the extrusion plate 53 and the two forming plates 10, the injection molded part is bent. Then, through the guide rod 15, it is avoided that the No. 1 spring 6 will swing randomly when pressed down, causing problems in the bending of the injection molded part, thereby improving stability.
[0053] As an embodiment of the present invention, grooves 52 are symmetrically provided at the upper ends of both side walls of the housing 51 , and two buckles 8 cooperating with the grooves 52 are fixedly mounted at the lower end of the extrusion plate 53 .
[0054] When in use, when the hydraulic punch 4 drives the extrusion plate 53 to press down, when it is extruded to a certain extent, the buckles 8 on both sides enter the grooves 52, and then the buckles 8 are engaged with the grooves 52, so that the extrusion plate 53 and the shell 51 are fixed, so that the injection molded part can maintain a bent state between the extrusion plate 53 and the molding plate 10. By setting the buckles 8 and the grooves 52, the injection molded part can be stably maintained in a bent state between the extrusion plate 53 and the molding plate 10, thereby avoiding rebound and deformation of the injection molded part after bending, thereby improving stability.
[0055] As an embodiment of the present invention, an elastic block 16 cooperating with the guide rod 15 is provided inside a side wall of the housing 51, a heating wire is provided inside the support plate 54, and the elastic block 16 is electrically connected to the heating wire.
[0056] During use, when the hydraulic punch 4 drives the extrusion plate 53 to press down, the extrusion plate 53 drives the guide rod 15 to move downward. When the injection molded part has not yet contacted the forming plate 10, the guide rod 15 squeezes the elastic block 16 toward the outer wall of the shell 51. The elastic block 16 is squeezed and gives an electrical signal to the heating wire. The heating wire starts to heat up, and then the support plate 54 is heated, so that the injection molded part to be bent is heated. By arranging the guide rod 15, the elastic block 16 and the heating wire in cooperation, the injection molded part can be preheated before bending, so that the injection molded part can be bent more smoothly, thereby improving the stability of the bending.
[0057] As an embodiment of the present invention, two through grooves 26 that penetrate into the groove 52 are opened on the outer wall of the shell 51, and two No. 4 springs 27 are symmetrically fixedly connected inside the two through grooves 26. The four No. 4 springs 27 are commonly connected to each other with a movable rod 9 for pushing the buckle 8.
[0058] When in use, after the bending is completed, the buckle 8 is engaged with the groove 52. After the shape is fixed, it hits the movable rod 9, and the movable rod 9 hits the buckle 8, so that the buckle 8 is separated from the groove 52, and the extrusion plate 53 is driven to move upward with the restoring force of the No. 1 spring 6, so that the extrusion plate 53 is separated from the shell 51, allowing the formed injection molded part to be separated. Due to the elastic force of the No. 4 spring 27, the movable rod 9 is restored to its initial state to avoid deviation when the movable rod 9 is hit next time. By setting the movable rod 9, the injection molded part can be automatically separated without manual operation, thereby improving production efficiency.
[0059] As an embodiment of the present invention, the cooling device includes a water-cooling circulation pump 11 fixedly installed inside the molding plate 10 on one side, and multiple water-cooling circulation pipes 17 are fixedly connected under the surface of the two molding plates 10, and the multiple water-cooling circulation pipes 17 are all connected to the water-cooling circulation pump 11 pipeline. An elastic button 18 is fixedly installed on the molding plate 10 on the side of the water pump circulation pump, and the elastic button 18 is electrically connected to the water-cooling circulation pump 11. An alarm device for detecting whether the water-cooling circulation pipe 17 is leaking is provided inside the two molding plates 10.
[0060] When in use, when the hydraulic punch 4 drives the extrusion plate 53 to press down, the injection molded part is pressed down, and then the support plate 54 compresses the No. 2 spring 7. When the buckle 8 is buckled with the groove 52, the No. 2 spring 7 is compressed to the extreme, the support plate 54 contacts the elastic button 18, and the elastic button 18 is squeezed into the inside of the molding plate 10 by the support plate 54. The elastic button 18 gives an electrical signal to the water-cooling circulation pump 11, so that the water-cooling circulation pump 11 starts, and cold water flows in the water-cooling circulation pipe 17, so that the molded injection molded part is quickly cooled down. When the buckle 8 is disengaged from the groove 52, due to the restoring force of the No. 2 spring 7, the support plate 54 and the molded injection molded part are driven to move upward, the elastic button 18 loses pressure, and stops giving the water-cooling circulation pump 11 an electrical signal, and the water-cooling circulation pump 11 stops. By setting the support plate 54, the elastic button 18 and the water-cooling circulation pump 11 in coordination, the molded injection molded part is quickly cooled down, thereby avoiding the possibility of rebound and deformation of the molded injection molded part, thereby improving stability.
[0061] As an embodiment of the present invention, the alarm device includes a collection box 19 fixedly installed at the bottom of the outer shell 51, and two connection rods 20 are provided in the middle of the collection box 19. The outer surface of the outer shell 51 is provided with two warning lights 22 corresponding to the two forming plates 10, and the connection rods 20 are electrically connected to the warning lights 22. A water channel 21 for collecting water is fixedly connected between the forming plates 10 and the collection box 19.
[0062] During use, when the water-cooling circulation pump 11 is started, cold water flows in the water-cooling circulation pipe 17 to cool the molded injection molded parts. Because the hydraulic punch 4 drives the extrusion plate 53 to press down, vibration may be generated. Long-term operation may cause the water-cooling circulation pipe 17 to rupture or be damaged, and then cause the cold water in the water-cooling circulation pipe 17 to flow out. The outflowing cold water flows into the collecting box 19 along the water channel 21 or the inner wall of the outer shell 51, contacts the power rod 20 to be energized, and the warning light 22 on the outer wall of the outer shell 51 starts to flash to alarm. By providing the collecting box 19 and the warning light 22, the staff can be reminded in time when the water-cooling circulation pipe 17 is ruptured or damaged, allowing the staff to repair and replace it, and can objectively observe the condition of the water-cooling circulation pipe 17 inside the outer shell 51, thereby improving safety.
[0063] As an implementation mode of the present invention, the power supply can only be conducted after the head of the power rod 20 contacts water.
[0064] During use, when the support plate 54 is heated, or due to some external factors, some water will be collected in the collection box 19. When the water level is not enough to touch the head of the connecting rod 20, the connecting rod 20 is not powered on, and the warning light 22 will not flash. When the water-cooling circulation pipe 17 is broken or damaged, the cold water inside leaks out, and the water level in the collection box 19 will soon touch the head of the connecting rod 20, the connecting rod 20 is powered on, and the warning light 22 flashes to alarm. This avoids some external factors that cause the warning light 22 to flash to alarm, thereby improving accuracy.
[0065] As an embodiment of the present invention, two support bars 23 are fixedly installed on both sides of the outer wall of the shell 51, and a trigger plate 24 is hinged on the two support bars 23. No. 3 springs 25 are fixedly installed on the outer walls of both sides of the shell 51, and the two No. 3 springs 25 are fixedly connected to the trigger plate 24, and the trigger plate 24 is electrically connected to the controller 1.
[0066] When in use, the top of the support plate 54 and the two molding plates 10 are slightly away from the top of the shell 51, just enough to allow the injection molded parts to be stuck. When placing the injection molded parts, the staff inserts the injection molded parts into the shell 51, and the four sides of the injection molded parts are completely flush with the inner wall of the shell 51 to place them flat. When the staff places the injection molded parts, they do not completely insert the injection molded parts into the shell 51, or one side is tilted, or even the injection molded parts are not placed flat. The conveyor belt 3 drives multiple shells 51 to move, and the staff does not place the injection molded parts flat when placing them. , resulting in problems with the bending of the injection molded parts. During extrusion, the injection molded parts will be squeezed out or even broken. The overflowed and broken injection molded parts will touch the trigger plates 24 on both sides. The trigger plates 24 are squeezed outward and rotated, driving the No. 3 spring 25 to extend outward, and then giving an electrical signal to the controller 1 to stop the entire conveyor belt 3. By setting the trigger plate 24 and the controller 1 to cooperate with each other, it can be automatically stopped in time when a situation occurs, avoiding problems affecting the subsequent machine operation, further reducing the output of unqualified bent injection molded parts, and improving production efficiency.
[0067] As an embodiment of the present invention, a striker 12 is provided on the inner wall of the base 2, and a cylinder is fixedly connected to the input end of the striker 12. Round rods 13 that cooperate with the grooves 52 on the outer wall of the shell 51 are provided on both sides of the striker 12.
[0068] When in use, the shell 51 moves with the conveyor belt 3 to the front of the impact rod 12 and stops. The conveyor belt 3 is the existing technology and can stably stop in front of the impact rod 12. At this time, the impact rod 12 starts, and the two round rods 13 just enter the through groove 26 and hit the movable rod 9, so that the movable rod 9 pushes the buckle 8, and then the buckle 8 disengages from the groove 52. After the impact rod 12 hits the movable rod 9, it is quickly recovered to prevent the shell 51 from hitting the round rod 13 and causing it to move during movement. By arranging the impact rod 12 and the movable rod 9 to cooperate with each other, when the shell 51 stops in front of the impact rod 12, the buckle 8 can be disengaged from the groove 52, thereby improving production efficiency.
[0069] Working principle: When in use, first, the staff puts the injection molded part on the support plate 54, operates the controller 1 to start the machine, and multiple shells 51 move with the conveyor belt 3. When the shell 51 moves to the bottom of the hydraulic punch 4, the conveyor belt 3 stops. At this time, the hydraulic punch 4 presses down, and the hydraulic punch 4 drives the extrusion plate 53 to move downward, and then squeezes the injection molded part into the shell 51, compressing the No. 1 spring 6, and the guide rod 15 moves downward. When the injection molded part has not yet contacted the molding plate 10, the guide rod 15 squeezes the elastic block 16 toward the outer wall of the shell 51. The elastic block 16 is squeezed and gives an electrical signal to the heating wire. The heating wire begins to heat up, and then the support plate 54 is heated, so that the bending part of the injection molded part is preheated, and the hydraulic punch 4 squeezes the support plate 54 and the No. 2 spring 7 into the shell 51 until the No. 2 spring 7 is extreme. At this time, the buckles 8 on both sides enter the groove 52, and then the buckle 8 is engaged with the groove 52, so that the extrusion plate 53 and the shell 51 are fixed. At the same time, the extrusion plate 53 and the two The molding plate 10 squeezes and bends the injection molded part into shape, and at the same time, the support plate 54 contacts the elastic button 18, and the elastic button 18 is squeezed into the inside of the molding plate 10 by the support plate 54. The elastic button 18 gives an electrical signal to the water cooling circulation pump 11, so that the water cooling circulation pump 11 starts, and cold water flows in the water cooling circulation pipe 17, so that the molded injection molded part is quickly cooled. The housing 51 moves with the conveyor belt 3 to the front of the striker 12 and stops. At this time, the striker 12 starts, and the two round rods 13 just enter the through groove 26 and strike The striking rod 9 pushes the buckle 8, and the buckle 8 disengages from the groove 52. Due to the restoring force of the No. 2 spring 7, the support plate 54 and the molded injection molded part are driven upward, the elastic button 18 loses pressure, and the electrical signal to the water-cooling circulation pump 11 stops. The conveyor belt 3 drives the shell 51 and the bent injection molded part to the push rod 14 and then stops. The push rod 14 pushes the bent injection molded part out, and the shell 51 returns to the staff along the conveyor belt 3, and this process is repeated.
[0070] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. An injection molded part bending mechanism, comprising: Controller (1); A base (2), wherein a controller (1) is fixedly mounted on an outer side wall of the base (2); A conveyor belt (3), the base (2) is equipped with a conveyor belt; The hydraulic punch (4) is fixedly connected to the outer wall of the base (2) with a connecting seat, and a hydraulic Punch (4); A push rod (14), wherein the push rod (14) is fixedly mounted on the inner side wall of the base (2); Features: A bending device, wherein a plurality of the bending devices are placed on a conveyor belt (3), and the bending devices slide relative to the base (2); A cooling device, wherein a cooling device is fixedly installed inside each of the bending devices; The bending device comprises a plurality of shells (51) fixedly mounted on the conveyor belt (3), a No. 1 spring (6) being fixedly mounted on the four corners of the upper end of the shell (51), the upper ends of the four No. 1 springs (6) being fixedly connected to an extrusion plate (53) in a V-shape, a guide rod (15) being slidably mounted inside a side wall of the shell (51), the guide rod (15) being fixedly connected to the extrusion plate (53), two forming plates (10) being symmetrically fixedly connected inside the shell (51), an empty slot being formed between the two forming plates (10), a plurality of No. 2 springs (7) being fixedly connected to the middle of the bottom of the empty slot, a support plate (54) being fixedly connected to the tops of the plurality of No. 2 springs (7), and the support plate (54) being located directly below the middle of the extrusion plate (53); The upper ends of the two side walls of the housing (51) are symmetrically provided with grooves (52), and the lower end of the extrusion plate (53) is fixedly provided with two buckles (8) that cooperate with the grooves (52); An elastic block (16) cooperating with the guide rod (15) is provided inside a side wall of the housing (51), a heating wire is provided inside the support plate (54), and the elastic block (16) is electrically connected to the heating wire; Two through slots (26) penetrating to the groove (52) are provided on the outer wall of the housing (51), two No. 4 springs (27) are symmetrically fixedly connected inside the two through slots (26), and a movable rod (9) for pushing the buckle (8) is commonly connected between the four No. 4 springs (27); The cooling device comprises a water-cooling circulation pump (11) fixedly mounted inside the molding plate (10) on one side, a plurality of water-cooling circulation pipes (17) fixedly connected below the surfaces of the two molding plates (10), and the plurality of water-cooling circulation pipes (17) are all connected to the water-cooling circulation pump (11) pipeline, an elastic button (18) is fixedly mounted on the molding plate (10) on the side of the water pump circulation pump, and the elastic button (18) is electrically connected to the water-cooling circulation pump (11), and an alarm device for detecting whether the water-cooling circulation pipe (17) is leaking is provided inside the two molding plates (10); The alarm device comprises a collection box (19) fixedly mounted on the bottom of the housing (51), two connecting rods (20) are arranged in the middle of the collection box (19), two warning lights (22) corresponding to the two forming plates (10) are arranged on the outer surface of the housing (51), and the connecting rods (20) are electrically connected to the warning lights (22), and a water channel (21) for collecting water is fixedly connected between the forming plates (10) and the collection box (19); The power supply can only be turned on after the head of the power rod (20) contacts water; Two support bars (23) are fixedly mounted on both sides of the outer wall of the housing (51), and a trigger plate (24) is hinged on each of the two support bars (23). No. 3 springs (25) are fixedly mounted on both sides of the outer wall of the housing (51), and the two No. 3 springs (25) are fixedly connected to the trigger plate (24), and the trigger plate (24) is electrically connected to the controller (1); The inner wall of the base (2) is provided with a striker rod (12), the input end of the striker rod (12) is fixedly connected to a cylinder, and round rods (13) are provided on both sides of the striker rod (12) and cooperate with the grooves (52) on the outer wall of the shell (51).
Citation Information
Patent Citations
Plastic guide pipe bending equipment
CN113561456A
Bending mechanism for injection molded part
CN114683526A