3D memory device with trench isolator and method of fabrication
By controlling the etchant temperature to ensure consistent etching rates between the isolation layer and the buffer layer, the etching process is simplified, solving the problem of inconsistent etching in the manufacturing of 3D storage devices. This achieves efficient and low-cost flat surface formation and improves product yield.
Patent Information
- Application Number
- CN202210683169.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-06-16
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2042-06-16
AI Technical Summary
In the manufacturing process of existing 3D storage devices, inconsistent etching of the isolation layer and buffer layer leads to increased manufacturing time and cost, and CMP process introduces defects such as scratches or dents.
By controlling the temperature of the etchant, the etching rates of the first isolation layer and the first buffer layer tend to be consistent. Hydrofluoric acid is used as the etchant to simplify the etching process, avoid CMP process, and directly control the etching time to achieve a flat surface.
It improved manufacturing efficiency, reduced costs, avoided defects caused by CMP process, and improved product qualification rate.
Smart Images

Figure CN115332152B_ABST
Abstract
Description
Technical Field
[0001] This disclosure relates to the fields of memory and semiconductor technology, and more specifically, to a 3D memory device and trench isolation device and a method of manufacturing them. Background Technology
[0002] Three-dimensional memory architecture can overcome the density limitations of planar memory. Three-dimensional non-volatile memory (3D NAND), also known as 3D memory devices, forms a stacked structure through alternating layers of gate conductors and insulating layers. Typically, an isolation section is placed on the bottom gate conductor layer to divide it into multiple pages, enabling page erasure during data erasure. However, due to structural characteristics and process limitations, the yield rate and manufacturing efficiency of this type of three-dimensional memory need improvement. Summary of the Invention
[0003] The purpose of this disclosure is to provide an improved 3D memory device and manufacturing method, which uses the same etchant to etch the first isolation layer and the first buffer layer, and controls the etching rates of the two to be consistent, thereby saving manufacturing time and cost while obtaining a flat surface of the second gate insulating layer.
[0004] According to a first aspect of this disclosure, a method for manufacturing a 3D memory device is provided, comprising: sequentially stacking a first gate insulating layer, a first gate sacrificial layer, a second gate insulating layer, and a first buffer layer on a first substrate along the thickness direction of the first substrate; forming a first groove extending from the surface of the first buffer layer toward the first substrate and at least penetrating the first gate sacrificial layer; forming a first isolation layer on the first buffer layer, wherein a portion of the first isolation layer fills the first groove; and etching the first isolation layer and the first buffer layer with a first etchant, wherein the etching stops near the surface of the second gate insulating layer, wherein the first isolation layer and the first buffer layer are made of different materials, and in the step of etching the first isolation layer and the first buffer layer, the temperature of the first etchant is controlled to reach a preset temperature so that the etching rates of the first isolation layer and the first buffer layer tend to be consistent.
[0005] Optionally, after etching the first isolation layer and the first buffer layer, the manufacturing method further includes: using a second etchant to etch the first buffer layer to remove the first buffer layer remaining on the surface of the second gate insulating layer, wherein the temperature of the second etchant is controlled so that the etching rate of the first buffer layer is greater than the etching rate of the first isolation layer.
[0006] Optionally, the material of the first isolation layer includes an oxide layer, the material of the first buffer layer includes a nitride layer, and both the first etchant and the second etchant include hydrofluoric acid.
[0007] Optionally, the temperature of the second etchant is higher than the temperature of the first etchant.
[0008] Optionally, after etching the first isolation layer and the first buffer layer with the first etchant, the manufacturing method further includes: replacing the first gate sacrificial layer with a bottom gate conductor layer, wherein the first isolation layer in the first groove serves as the first isolation portion of the bottom gate conductor layer.
[0009] According to a second aspect of this disclosure, a 3D storage device is provided, which is formed using the manufacturing method described above.
[0010] According to a third aspect of this disclosure, a method for manufacturing a trench isolation device is provided, comprising: forming a second buffer layer on a second substrate; forming a second trench extending from the surface of the second buffer layer into the second substrate; forming a second isolation layer on the second buffer layer, wherein a portion of the second isolation layer fills the second trench; and etching the second isolation layer and the second buffer layer with a third etchant, the etching stopping near the surface of the second substrate, wherein the second isolation layer and the second buffer layer are made of different materials, and in the step of etching the second isolation layer and the second buffer layer, the temperature of the third etchant is controlled to reach a preset temperature so that the etching rates of the second isolation layer and the second buffer layer tend to be consistent.
[0011] Optionally, after etching the second isolation layer and the second buffer layer, the manufacturing method further includes: etching the second buffer layer with a fourth etchant to remove the second buffer layer remaining on the surface of the second substrate, wherein the temperature of the fourth etchant is controlled so that the etching rate of the second buffer layer is greater than the etching rate of the second isolation layer.
[0012] Optionally, the material of the second isolation layer includes an oxide layer, the material of the second buffer layer includes a nitride layer, and both the third etchant and the fourth etchant include hydrofluoric acid.
[0013] Optionally, the temperature of the fourth etchant is higher than the temperature of the third etchant.
[0014] Optionally, after etching the second isolation layer and the second buffer layer with a third etchant, the manufacturing method further includes: forming a plurality of doped regions in the substrate; and forming a gate structure on the substrate, wherein the isolation layer in the second trench serves as a second isolation portion of the active region.
[0015] According to a fourth aspect of this disclosure, a trench isolation device is provided, which is formed using the manufacturing method described above.
[0016] According to the 3D memory device and manufacturing method provided in the embodiments of this disclosure, when removing the structural layer above the horizontal height of the second gate insulating layer surface, the first isolation layer and the first buffer layer are etched using the same etchant, and the temperature of the etchant is controlled so that the etching rates of the first isolation layer and the first buffer layer tend to be consistent. Since the total thickness and etching rate of the first isolation layer and the first buffer layer to be removed are known, it is relatively easy to stop the etching near the surface of the second gate insulating layer by only controlling the etching time, thereby saving manufacturing time and cost while obtaining a flat second gate insulating layer surface.
[0017] Furthermore, when a portion of the first buffer layer remains on the surface of the second gate insulating layer, the temperature of the second etchant can be controlled to make the etching rate of the first buffer layer greater than the etching rate of the first isolation layer, thereby completely removing the first buffer layer.
[0018] Therefore, the manufacturing method of the 3D storage device according to the present disclosure improves product manufacturing efficiency and reduces costs. Attached Figure Description
[0019] The above and other objects, features and advantages of this disclosure will become clearer from the following description of embodiments of this disclosure with reference to the accompanying drawings.
[0020] Figure 1a and 1b The circuit diagram and structural schematic diagram of the storage cell string of the 3D storage device are shown respectively.
[0021] Figure 2 A perspective view of a 3D storage device is shown.
[0022] Figure 3 It shows along Figure 2 A schematic diagram of the cross-section taken by line AA.
[0023] Figure 4 A first structural schematic diagram of the 3D storage device manufacturing method of this disclosure is shown.
[0024] Figure 5 A second structural schematic diagram of the 3D storage device manufacturing method of this disclosure is shown.
[0025] Figure 6 A third structural schematic diagram of the 3D storage device manufacturing method of this disclosure is shown.
[0026] Figure 7 A fourth structural schematic diagram of the 3D storage device manufacturing method of this disclosure is shown.
[0027] Figure 8A fifth structural schematic diagram of the 3D storage device manufacturing method of this disclosure is shown.
[0028] Figure 9 A sixth structural schematic diagram of the 3D storage device manufacturing method of this disclosure is shown.
[0029] Figure 10 A seventh structural schematic diagram of the 3D storage device manufacturing method of this disclosure is shown.
[0030] Figure 11 The eighth structural schematic diagram of the 3D storage device manufacturing method of this disclosure is shown.
[0031] Figure 12 A ninth structural schematic diagram of the 3D storage device manufacturing method of this disclosure is shown.
[0032] Figure 13 A tenth structural schematic diagram of the 3D storage device manufacturing method of this disclosure is shown.
[0033] Figure 14 An eleventh structural schematic diagram of the 3D storage device manufacturing method of this disclosure is shown.
[0034] Figure 15 A schematic diagram of the twelfth structure of the 3D storage device manufacturing method of this disclosure is shown.
[0035] Figure 16 The thirteenth structural schematic diagram of the 3D storage device manufacturing method of this disclosure is shown.
[0036] Figure 17 The fourteenth structural schematic diagram of the 3D storage device manufacturing method of this disclosure is shown.
[0037] Figure 18 A first structural schematic diagram of the trench isolation device manufacturing method of this disclosure is shown.
[0038] Figure 19 A second structural schematic diagram of the trench isolation device manufacturing method of this disclosure is shown.
[0039] Figure 20 A third structural schematic diagram of the trench isolation device manufacturing method of this disclosure is shown.
[0040] Figure 21 A schematic diagram showing the effect of temperature on the etching rate of hydrofluoric acid on oxide and nitride layers. Detailed Implementation
[0041] The present disclosure will now be described in more detail with reference to the accompanying drawings. In the various drawings, the same elements are indicated by similar reference numerals. For clarity, the various parts in the drawings are not drawn to scale. Furthermore, some well-known parts may not be shown. For simplicity, a semiconductor structure obtained after several steps can be depicted in a single figure.
[0042] It should be understood that when describing the structure of a device, when referring to a layer or region as being "above" or "on top of" another layer or region, it can mean that it is directly above another layer or region, or that there are other layers or regions between it and another layer or region. Furthermore, if the device is flipped, that layer or region will be located "below" or "under" another layer or region.
[0043] Many specific details of this disclosure, such as the structure, materials, dimensions, processing methods, and techniques of the devices, are described below to provide a clearer understanding of the disclosure. However, as those skilled in the art will understand, this disclosure may be implemented without following these specific details.
[0044] This disclosure may be presented in various forms, some of which will be described below.
[0045] Figure 1a and 1b The circuit diagram and structural schematic diagram of the storage cell string of the 3D storage device are shown respectively. In this embodiment, the storage cell string shown includes four storage cells. It is understood that this disclosure is not limited thereto, and the number of storage cells in the storage cell string can be any number, for example, 32 or 64.
[0046] like Figure 1a As shown, the first end of the memory cell string 100 is connected to the bit line (BL), and the second end is connected to the source line (SL). The memory cell string 100 includes multiple transistors connected in series between the first and second ends, including: a first selection transistor (drain-side selection transistor) Q1, storage transistors M1 to M4, and a second selection transistor (source-side selection transistor) Q2. The gate of the first selection transistor Q1 is connected to the selection gate for drain (SGD), also known as the top gate selection line. The gate of the second selection transistor Q2 is connected to the selection gate for source (SGS), also known as the bottom gate selection line. The gates of storage transistors M1 to M4 are respectively connected to the corresponding word lines WL1 to WL4.
[0047] like Figure 1bAs shown, the selection transistors Q1 and Q2 of the memory cell string 100 each include a top gate conductor layer 122 and a bottom gate conductor layer 123, respectively, and the memory transistors M1 to M4 each include a middle gate conductor layer 121. The gate conductor layers 121, 122, and 123 are arranged in the same order as the transistors in the memory cell string 100, and adjacent gate conductor layers are separated from each other by an interlayer insulating layer, thereby forming a gate stack structure. Further, the memory cell string 100 includes a channel pillar 110. The channel pillar 110 is adjacent to or penetrates the gate stack structure. In the middle portion of the channel pillar 110, a tunneling dielectric layer 112, a charge storage layer 113, and a gate dielectric layer 114 are sandwiched between the gate conductor layer 121 and the channel layer 111, thereby forming the memory transistors M1 to M4. At both ends of the channel pillar 110, a gate dielectric layer 114 is sandwiched between the gate conductor layers 122 and 123 and the channel layer 111, thereby forming selection transistors Q1 and Q2.
[0048] In this embodiment, the channel layer 111 is composed of, for example, polysilicon; the tunneling dielectric layer 112 and the gate dielectric layer 114 are each composed of oxides, such as silicon oxide; the charge storage layer 113 is composed of an insulating layer containing quantum dots or nanocrystals, such as silicon nitride containing metal or semiconductor particles; and the gate conductor layer 121 is composed of a conductive material, such as tungsten, copper, polysilicon, graphite, etc. The channel layer 111 provides the channel region for the select transistor and the storage transistor, and the doping type of the channel layer 111 is the same as the type of the select transistor and the storage transistor. For example, for an N-type select transistor and a storage transistor, the channel layer 111 can be N-type doped polysilicon.
[0049] In this embodiment, the core of the channel post 110 is a channel layer 111, and the tunneling dielectric layer 112, charge storage layer 113, and gate dielectric layer 114 form a stacked structure surrounding the sidewalls of the core. In an alternative embodiment, the core of the channel post 110 is an additional insulating layer, and the channel layer 111, tunneling dielectric layer 112, charge storage layer 113, and gate dielectric layer 114 form a stacked structure surrounding the insulating layer.
[0050] In this embodiment, select transistors Q1 and Q2, and storage transistors M1 to M4 use a common channel layer 111 and gate dielectric layer 114. In channel pillar 110, channel layer 111 provides the source / drain regions and channel layer for the plurality of transistors. In an alternative embodiment, the channel layers and gate dielectric layers for select transistors Q1 and Q2, and the channel layers and gate dielectric layers for storage transistors M1 to M4, can be formed in separate steps. In channel pillar 110, the channel layers of select transistors Q1 and Q2 are electrically connected to the channel layers of storage transistors M1 to M4.
[0051] In some other embodiments, the selection transistor Q1 can also be fabricated with a structure similar to that of the storage transistors M1 to M4. Specifically, a tunneling dielectric layer 112, a charge storage layer 113, and a gate dielectric layer 114 are sandwiched between the gate conductor layer 122 and the channel layer 111 at the upper part of the channel pillar 110, thereby forming the selection transistor Q1. Since the selection transistor Q1 has the same structure as the storage transistors M1 to M4, the fabrication process of the channel pillar can be simplified.
[0052] Figure 2 This diagram shows a perspective view of a 3D memory device. X, Y, and Z represent the length, width, and height directions of the 3D memory device, respectively. For clarity, [the diagram is missing here]. Figure 2 The individual insulating layers in the 3D storage device are not shown.
[0053] The 3D storage device shown in this embodiment includes 16 4x4 storage cell strings 100, each storage cell string 100 including 4 storage cells, thereby forming a 4x4x4 storage cell array with a total of 64 storage cells. It is understood that this disclosure is not limited thereto; the 3D storage device may include any number of storage cell strings, for example, 1024, and the number of storage cells in each storage cell string may be any number, for example, 32 or 64.
[0054] In the 3D memory device, each memory cell string includes its own channel pillar 110 and a common gate conductor layer 121, 122, and 123. The gate conductor layers 121, 122, and 123 are arranged in the same stacking order as the transistors in the memory cell string 100. Adjacent gate conductor layers are separated from each other by an interlayer insulating layer, thus forming a gate stack structure. The interlayer insulating layer is not shown in the figure. The internal structure of the channel pillar 110 is as follows... Figure 1b As shown, no further detailed description will be provided here. The channel pillars 110 penetrate the gate stack structure and are arranged in an array. The first ends of multiple channel pillars 110 in the same column are connected to the same bit line (i.e., one of bit lines BL1 to BL4), and the second ends are connected to the first substrate 101. The second ends form a common source connection through the first substrate 101.
[0055] The gate conductor layer 122 of the drain-side select transistor Q1 is divided into different gate lines by a gate line slit 103 and an isolation trench 105 (top gate line cut-out). The gate lines of multiple channel pillars 110 in the same row along the X direction are connected to the same drain select gate line (i.e., one of drain select gate lines SGD1 to SGD4) through a conductive channel 135.
[0056] The gate conductor layers 121 of storage transistors M1 and M4 are connected together in different layers. If the gate conductor layers 121 of storage transistors M1 and M4 are divided into different gate lines by gate gaps 103, the gate lines on the same layer reach the interconnect layer 132 through their respective conductive channels 131, thereby interconnecting with each other, and then connected to the same word line (i.e., one of word lines WL1 to WL4) through conductive channels 133.
[0057] The gate conductor layer 123 of the source-side select transistor Q2 is divided into different gate lines by the gate line gap 103 and the first groove 104 (bottom gate line cutout). The gate lines of multiple channel pillars 110 in the same row are connected to the same source select gate line SGS (i.e., one of the source select gate lines SGS1 to SGS4) through the conductive channel 134.
[0058] Figure 3 It shows along Figure 2 A schematic diagram of the cross-section taken by line AA.
[0059] like Figure 3 As shown, multiple channel pillars 110 penetrate the stacked structure to reach the well region 102 in the first substrate 101. Gate gaps 103 divide the stacked structure into a first region 11 and a second region 12, wherein the gate conductor layers 121, 122, and 123 of the first region 11 and the second region 12 are all separated by gate gaps 103. In the first region 11, a first recess 104 and an isolation portion 104a (first isolation portion) therein separate the bottom gate conductor layer 123 to correspond to the first sub-region 11a and the second sub-region 11b, respectively; an isolation trench 105 separates the top gate conductor layer 122 to correspond to the first sub-region 11a and the second sub-region 11b, respectively. Similarly, in the second region 12, the first groove 104 and the isolation portion 104a therein separate the bottom gate conductor layer 123 to correspond to the third sub-region 12a and the fourth sub-region 12b, respectively; the isolation trench 105 separates the top gate conductor layer 122 to correspond to the third sub-region 12a and the fourth sub-region 12b, respectively. However, the embodiments of this disclosure are not limited to this, and the various sub-regions in the first region 11 and the second region 12 can be divided in other ways as needed. The sidewalls of the gate gap 103 are covered with insulating material 103a, and a conductive channel 141 is formed in the gate gap 103. Preferably, a doped region 142 is formed in the well region 102, and the conductive channel 141 is connected to the doped region 142 in the well region 102. However, the embodiments of this disclosure are not limited to this, and the gate gap 103 can also be completely filled with an insulating layer, and a conductive channel is formed on the back side of the first substrate 101 to connect with the well region 102.
[0060] The following will be through Figures 4 to 17 The manufacturing method of the 3D storage device according to the embodiments of this disclosure will be described in detail, wherein, Figures 3 to 17 It can be regarded as along Figure 2 A cross-sectional view of the section cut by line AA.
[0061] like Figure 4 As shown, a well region 102 is formed in the first substrate 101, and a first gate insulating layer 151a, a first gate sacrificial layer 152a, a second gate insulating layer 151b and a first buffer layer 160 are sequentially stacked on the first substrate 101 along the height direction.
[0062] In this embodiment, the first gate insulating layer 151a and the second gate insulating layer 151b are, for example, oxide layers, specifically including but not limited to silicon oxide layers. The first gate sacrificial layer 152a and the first buffer layer 160 are, for example, nitride layers, specifically including but not limited to silicon nitride layers.
[0063] Furthermore, a first groove 104 is formed extending from the surface of the first buffer layer 160 toward the first substrate 101, such as... Figure 5 As shown, the first groove 104 needs to penetrate at least the first gate sacrificial layer 152a.
[0064] In this step, for example, an etching process is used to form the first groove 104, and the etching time is controlled so that the etching stops after penetrating the first gate sacrificial layer 152a. The first buffer layer 160 is used to protect the surface of the second gate insulating layer 151b during the etching step. In this embodiment, the bottom of the first groove 104 is located in the first gate insulating layer 151a. In some other embodiments, the bottom of the first groove 104 may also penetrate the first gate insulating layer 151a. In this embodiment, the first groove 104 extends along the length direction to divide the first gate sacrificial layer 152a into multiple sections. The number of first grooves 104 can be set as needed.
[0065] Furthermore, a first isolation layer 170 is formed on the first buffer layer 160, and the first isolation layer 170 fills the first groove 104, such as Figure 6 As shown.
[0066] In this step, for example, a deposition process is used to form a first isolation layer 170, wherein the material of the first isolation layer 170 is, for example, an oxide layer, including but not limited to silicon oxide.
[0067] Furthermore, the first isolation layer on the first buffer layer 160 is removed, and the first isolation layer remaining in the first groove 104 serves as the first isolation portion 104a, as shown below. Figure 7 As shown.
[0068] In this step, for example, a chemical mechanical polishing (CMP) process is used to remove the first isolation layer on the first buffer layer 160.
[0069] Further, the first buffer layer 160 is removed. In the first embodiment, the first buffer layer 160 can be etched using a mixture of hydrofluoric acid and phosphoric acid, such as... Figure 8 As shown. However, after removing the first buffer layer 160, the surface of the second gate insulating layer 151b and the sidewall of the first isolation portion 104a will form an angle (at the dashed box 01). In subsequent processes, multiple layers of gate sacrificial layers and gate insulating layers need to be alternately stacked and deposited on top of the second gate insulating layer 151b. To ensure the flatness of the alternately stacked and deposited multiple layers of gate sacrificial layers and gate insulating layers, a CMP process is needed to remove the first isolation portion 104a that protrudes above the second gate insulating layer 151b; or an oxide layer can be deposited first to cover the protruding part of the first isolation portion 104a, and then a CMP process can be used for surface planarization, which is a more complex process.
[0070] In the second embodiment, the first buffer layer 160 can be directly removed using a CMP process, such as... Figure 9 As shown. However, in this embodiment, since the first buffer layer 160 is made of silicon nitride, which is very hard, hard small particles will be generated during the grinding process, damaging the softer first isolation portion 104a and causing defects such as scratches or dents (dashed box 02). In addition, the grinding cost of the silicon nitride first buffer layer 160 is very high, and in the actual production process, since the thickness of the first buffer layer 160 is very thin, each batch needs to undergo a grinding test before grinding, and the grinding time of this batch needs to be adjusted according to the test results, resulting in poor process stability. Moreover, both the first and second embodiments require the use of CMP process. Since the CMP process generates particles, the wafer needs to be cleaned after CMP is completed, which adds a cleaning step.
[0071] To address the problems in the two embodiments described above for removing the first buffer layer 160, this disclosure provides a third embodiment. For example... Figure 10 As shown, after the first isolation layer 170 is formed, the first isolation layer 170 and the first buffer layer 160 are etched using a first etchant.
[0072] In this step, the temperature of the first etchant is controlled to reach a preset temperature so that the etching rates of the first isolation layer 170 and the first buffer layer 160 tend to be consistent, close to 1:1. The required etching time can be obtained based on the total thickness t1 of the structural layers (first isolation layer 170 and first buffer layer 160) above the horizontal height of the second gate insulating layer 151b surface and the etching rate of the first etchant. This allows the etching to stop near the surface of the second gate insulating layer 151b, resulting in... Figure 11 The semiconductor structure shown has a second gate insulating layer 151b flush with the surface of the first isolation portion 104a.
[0073] In some specific embodiments, when the first isolation layer 170 is deposited, a small depression is formed on the surface of the first isolation layer 170 corresponding to the first groove 104. When the etching of the first isolation layer 170 at the depression has reached the vicinity of the surface of the second gate insulating layer 151b, there is still residue in the first buffer layer 160. Figure 12 As shown. Therefore, a second etchant is also needed to etch the first buffer layer 160 to remove any remaining first buffer layer 160 on the surface of the second gate insulating layer 151b. The temperature of the second etchant is controlled so that the etching rate of the first buffer layer 160 is greater than the etching rate of the first isolation layer 170. In this embodiment, both the first and second etchants include hydrofluoric acid, such as... Figure 21 As shown, the etching rate of hydrofluoric acid on the oxide layer and the nitride layer is close to 1:1 when the temperature reaches the preset temperature a, and increases with increasing temperature when the preset temperature a is exceeded. In some specific embodiments, the etching rate of the second etchant on the first buffer layer 160 and the first isolation layer 170 can be made greater than 1000:1 by adjusting the concentration of hydrofluoric acid in the second etchant and the temperature of the second etchant.
[0074] Compared to the first and second embodiments, the third embodiment of this disclosure has a very simple step in removing the first buffer layer 160. It is relatively easy to stop the etching near the surface of the second gate insulating layer 151b by simply controlling the etching time, thereby saving manufacturing time while obtaining a flat surface. Moreover, the CMP process is no longer required, so there are no defects such as scratches or dents caused by the CMP process, as well as particle residue problems. Furthermore, the etching process is more cost-effective and has better process stability than the CMP process.
[0075] Furthermore, the gate sacrificial layer 152 and the gate insulating layer 151 are alternately stacked on the flat semiconductor structure surface, as follows: Figure 13 As shown.
[0076] Furthermore, multiple channel pillars 110 are formed through the stacked structure, and an isolation trench is formed through the top gate sacrificial layer 152, and an isolation portion 105a is formed in the isolation trench.
[0077] Furthermore, the multiple gate sacrificial layers 152 are replaced with multiple gate conductor layers 121, 122, and 123.
[0078] In this step, for example, anisotropic etching is first performed on the insulating stack structure. Anisotropic etching can be performed using dry etching methods, such as ion milling, plasma etching, reactive ion etching, or laser ablation. For example, by controlling the etching time, the etching is stopped near the first substrate 101 to form a structure like... Figure 15 The grid line gap 103 is shown.
[0079] Then, for example, a wet etching process is used to remove multiple gate sacrificial layers 152 through multiple gate line gaps 103 to form gaps 106 between adjacent gate insulating layers 151, such as... Figure 16 As shown.
[0080] Next, conductive material, including but not limited to tungsten, is filled into the gate line gaps 103 and voids 106. Finally, a back-etching process is used to reform the gate line gaps 103. The remaining conductive material in the voids 106 constitutes the gate conductor layers 121, 122, and 123. Figure 17 As shown. In subsequent steps, the material used to form the conductive channels is formed as follows. Figure 3 The structure shown can also be filled with insulating material in the grid gap 103.
[0081] According to the manufacturing method of the 3D memory device provided in the embodiments of this disclosure, when removing the structural layer above the horizontal height of the surface of the second gate insulating layer, the etching rate of the first isolation layer and the first buffer layer is made to be consistent by etching the first isolation layer and the first buffer layer and controlling the temperature of the etchant. Since the total thickness and etching rate of the first isolation layer and the first buffer layer to be removed are known, it is relatively easy to stop the etching near the surface of the second gate insulating layer by controlling the etching time, thereby saving manufacturing time and cost while obtaining a flat surface of the second gate insulating layer.
[0082] Furthermore, when a portion of the first buffer layer remains on the surface of the second gate insulating layer, the temperature of the second etchant can be controlled to make the etching rate of the first buffer layer greater than the etching rate of the first isolation layer, thereby completely removing the first buffer layer.
[0083] Therefore, the manufacturing method of the 3D storage device according to the present disclosure improves the product yield and manufacturing efficiency.
[0084] like Figures 18 to 20 As shown, this disclosure also provides a method for manufacturing a trench isolation device, comprising: forming a second buffer layer on a second substrate 201; forming a second trench 203 extending from the surface of the second buffer layer 202 into the second substrate 201; forming a second isolation layer 204 on the second buffer layer 202, wherein the second isolation layer 204 fills the second trench 203; and etching the second isolation layer 204 and the second buffer layer 202 with a third etchant, wherein the etching stops near the surface of the second substrate 201, wherein the second isolation layer 204 and the second buffer layer 202 are made of different materials, and in the step of etching the second isolation layer 204 and the second buffer layer 202, the temperature of the third etchant is controlled so that the etching rates of the second isolation layer 204 and the second buffer layer 202 tend to be consistent.
[0085] After the step of etching the second isolation layer 204 and the second buffer layer 202, the manufacturing method further includes: etching the second buffer layer 202 with a fourth etchant to remove the second buffer layer 202 remaining on the surface of the second substrate 201, wherein the temperature of the fourth etchant is controlled so that the etching rate of the second buffer layer 202 is greater than the etching rate of the second isolation layer 204.
[0086] The second isolation layer 204 is made of an oxide layer, the second buffer layer 202 is made of a nitride layer, and both the third and fourth etchants contain hydrofluoric acid. The temperature of the fourth etchant is higher than that of the third etchant.
[0087] After etching the second isolation layer 204 and the second buffer layer 202 with a third etchant, the manufacturing method further includes: forming a plurality of doped regions 224 and 225 in the second substrate 201; and forming a gate structure on the second substrate 201, the gate structure including a gate dielectric layer 221, a gate conductor 222 and a sidewall 223, wherein the second isolation layer 204 in the second recess 203 serves as the isolation portion 210 (second isolation portion) of the active region.
[0088] The steps for removing the second buffer layer 202 disclosed herein are very simple. It is relatively easy to stop the etching near the surface of the second substrate 201 simply by controlling the etching time, thereby saving manufacturing time while obtaining a flat surface. Furthermore, the CMP process is no longer required, thus avoiding defects such as scratches or dents and particle residue problems caused by the CMP process. Moreover, the etching process is more cost-effective and has better process stability than the CMP process.
[0089] The above description does not provide detailed explanations of the technical aspects of each layer's patterning, etching, etc. However, those skilled in the art should understand that various technical means can be used to form layers and regions of the desired shape. Furthermore, to form the same structure, those skilled in the art can also design methods that are not entirely identical to those described above. Additionally, although various embodiments have been described above, this does not mean that the measures in the various embodiments cannot be used advantageously in combination.
[0090] The embodiments of this disclosure have been described above. However, these embodiments are for illustrative purposes only and are not intended to limit the scope of this disclosure. The scope of this disclosure is defined by the appended claims and their equivalents. Various substitutions and modifications can be made by those skilled in the art without departing from the scope of this disclosure, and all such substitutions and modifications should fall within the scope of this disclosure.
Claims
1. A method for manufacturing a 3D storage device, comprising: A first gate insulating layer, a first gate sacrificial layer, a second gate insulating layer, and a first buffer layer are sequentially stacked on a first substrate along the thickness direction of the first substrate. A first groove is formed, which extends from the surface of the first buffer layer toward the first substrate and at least penetrates the first gate sacrificial layer. A first isolation layer is formed on the first buffer layer, and a portion of the first isolation layer fills the first groove; and The first isolation layer and the first buffer layer are etched using a first etchant, and the etching stops near the surface of the second gate insulating layer. The first isolation layer and the first buffer layer are made of different materials. In the step of etching the first isolation layer and the first buffer layer, the temperature of the first etchant is controlled to reach a preset temperature so that the etching rates of the first isolation layer and the first buffer layer tend to be consistent. The material of the first isolation layer includes an oxide layer, the material of the first buffer layer includes a nitride layer, and the first etchant includes hydrofluoric acid.
2. The manufacturing method of claim 1, after the step of etching the first isolation layer and the first buffer layer, the manufacturing method further comprises: The first buffer layer is etched using a second etchant to remove any remaining first buffer layer on the surface of the second gate insulating layer. Specifically, the temperature of the second etchant is controlled so that the etching rate of the first buffer layer is greater than the etching rate of the first isolation layer.
3. The manufacturing method according to claim 2, wherein, The second etching agent includes hydrofluoric acid.
4. The manufacturing method according to claim 3, wherein, The temperature of the second etchant is higher than that of the first etchant.
5. The manufacturing method according to any one of claims 1-4, after the step of etching the first isolation layer and the first buffer layer with a first etchant, the manufacturing method further includes: Replace the first gate sacrificial layer with the bottom gate conductor layer. The first isolation layer within the first groove serves as the first isolation portion of the bottom gate conductor layer.
6. A 3D storage device, formed using the manufacturing method described in any one of claims 1-5.
7. A method for manufacturing a trench isolation device, comprising: A second buffer layer is formed on the second substrate; A second groove is formed, which extends from the surface of the second buffer layer into the second substrate; A second isolation layer is formed on the second buffer layer, and a portion of the second isolation layer fills the second groove; as well as The second isolation layer and the second buffer layer are etched using a third etchant, and the etching stops near the surface of the second substrate. The second isolation layer and the second buffer layer are made of different materials. During the etching steps of the second isolation layer and the second buffer layer, the temperature of the third etchant is controlled to reach a preset temperature so that the etching rates of the second isolation layer and the second buffer layer tend to be consistent. The material of the second isolation layer includes an oxide layer, the material of the second buffer layer includes a nitride layer, and the third etchant includes hydrofluoric acid.
8. The manufacturing method according to claim 7, after the step of etching the second isolation layer and the second buffer layer, the manufacturing method further includes: The second buffer layer is etched using a fourth etchant to remove any remaining second buffer layer on the surface of the second substrate. Specifically, the temperature of the fourth etchant is controlled so that the etching rate of the second buffer layer is greater than the etching rate of the second isolation layer.
9. The manufacturing method according to claim 8, wherein, The fourth etching agent includes hydrofluoric acid.
10. The manufacturing method according to claim 9, wherein, The temperature of the fourth etchant is higher than that of the third etchant.
11. The manufacturing method according to any one of claims 7-10, after the step of etching the second isolation layer and the second buffer layer with a third etchant, the manufacturing method further includes: Multiple doped regions are formed in the second substrate; as well as A gate structure is formed on the second substrate. The isolation layer within the second groove serves as the second isolation portion of the active region.
12. A trench isolation device, formed using the manufacturing method described in any one of claims 7-11.
Citation Information
Patent Citations
Method for manufacturing isolation structure of shallow groove