By combining the design of suspension agglomeration unit and conditioning unit, the problem of unstable calcination quality of magnesium oxide powder was solved, and the activity stability of magnesium oxide powder and the controllability of citric acid method color change time were achieved, thus meeting the quality requirements of building material grade magnesium oxide powder.

CN115682707BActive Publication Date: 2026-07-17LIAONING DONGDA POWDER ENG TECH CO LTD

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
LIAONING DONGDA POWDER ENG TECH CO LTD
Filing Date
2022-11-10
Publication Date
2026-07-17

AI Technical Summary

Technical Problem

The calcination quality of products from existing magnesium oxide powder calcining furnaces is unstable, making it difficult to meet the activity requirements of building material-grade magnesium oxide powder. In particular, the color change time of the citric acid method is difficult to control within 40s to 350s.

Method used

The design combines a suspension agglomeration unit and a conditioning unit. Through high-temperature cyclone separation, suspension agglomeration and conditioning treatment, the residence time of materials in the furnace and the gas-solid contact surface are increased, and the activity of magnesium oxide powder is controlled to ensure that it is adjustable and controllable within 40s~350s.

Benefits of technology

The activity of magnesium oxide powder is stabilized, meeting the quality requirements of building material grade magnesium oxide powder. The color change time of citric acid method is adjustable, and the active MgO mass fraction of the produced magnesium oxide powder is 70%~40%.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115682707B_ABST
    Figure CN115682707B_ABST
Patent Text Reader

Abstract

本发明提供一种氧化镁粉焙烧装置,涉及氧化镁粉生产设备技术领域。其中,氧化镁粉焙烧装置包括炉体以及与炉体相连接的卸料单元。炉体包括投料单元,靠近卸料单元侧的投料单元的端部连接有悬浮团聚单元,远离投料单元侧的悬浮团聚单元的端部连接有燃料燃烧单元,靠近卸料单元侧的燃料燃烧单元的端部连接有调质单元,燃料燃烧单元还连接有助燃单元。其中,远离悬浮团聚单元侧的投料单元的端部处设置有旋风投料设备,投料单元的侧周设置有高温旋风分离单元,高温旋风分离单元还连接至悬浮团聚单元。本发明技术方案生产出的氧化镁粉的活性稳定,并且生产出的氧化镁粉的柠檬酸法变色时间可在40s~350s可调可控,完全符合氧化镁粉的要求。