Coating apparatus and coating method capable of easily adjusting coating thickness

By utilizing the design of a water tank partition and roller unit in the coating device, an ultra-thin coating can be formed without changing the traditional process conditions, solving the problem of difficult coating thickness control in the existing technology and improving the battery characteristics and production efficiency of secondary batteries.

CN115768563BActive Publication Date: 2026-11-24LG ENERGY SOLUTION LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202180031536.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2021-06-30
Filing Date
2021-12-14
Publication Date
2026-11-24
Estimated Expiration
2041-12-14

AI Technical Summary

Technical Problem

Existing technologies struggle to stably form coatings of extremely thin thickness without altering traditional coating process operations, thus affecting the battery characteristics of secondary batteries.

Method used

A coating apparatus is employed, comprising a water tank, a roller unit, and a heating unit. The water tank is divided into two areas by a partition, which respectively contains a polar solution and a coating solution. The coating thickness is precisely controlled by adjusting the height of the coating solution and the conveying speed of the substrate film.

Benefits of technology

Without altering traditional operating conditions, an ultra-thin coating was formed, improving the battery characteristics of the secondary battery. Furthermore, the process is simple and reduces the generation of pollutants.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115768563B_ABST
    Figure CN115768563B_ABST
Patent Text Reader

Abstract

The present invention relates to a coating apparatus capable of achieving an ultra-thin coating thickness, and more specifically, to a coating apparatus for continuously forming a coating on each surface of a substrate film (100), the coating apparatus comprising: a water tank (210) located on a movement path of the substrate film (100); a water tank partition (220) vertically located inside the water tank (210), the water tank partition being configured to divide the internal space of the water tank (210) into two regions, such as a first water tank portion (211) and a second water tank portion (212); a roller unit (300) configured to continuously convey the substrate film (100); and a heating unit (400) located outside the water tank (210), wherein the water tank partition (220) is spaced a predetermined distance from the inner bottom surface of the water tank (210).
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application claims the benefit of priority to Korean Patent Application No. 2021-0085734, filed on June 30, 2021, the entire contents of which are incorporated herein by reference.

[0002] The present invention relates to a coating apparatus and coating method for a separator or current collector for a secondary battery, and more specifically, to a coating apparatus and coating method for a separator or current collector for a secondary battery capable of adjusting the coating thickness by adjusting the height of the coating solution layer, thereby achieving an extremely thin coating thickness. Background Technology

[0003] With the increasing demand for portable electronic devices such as smartphones, tablets, and laptops, the demand for secondary batteries, which serve as the energy source for these devices, has also increased dramatically. Among these, lithium-ion secondary batteries, characterized by high energy density and long battery life, are the most widely used.

[0004] Lithium-ion secondary batteries are assembled by manufacturing electrode assemblies. These assemblies are stacked with positive and negative electrodes stacked alternately, with separators inserted between the positive and negative electrodes. The electrode assemblies are then inserted into a battery casing made of a can or bag of predetermined size and shape, and electrolyte is injected into the battery casing. The electrolyte permeates into the space between the positive and negative electrodes and the separator through capillary force.

[0005] To ensure that lithium-ion batteries maintain a long lifespan while possessing high capacity and high energy density, the electrode components must be thoroughly impregnated with the electrolyte. If the electrode components are not completely impregnated with the electrolyte, the reactions between the electrodes will be disrupted, the battery resistance will increase, the external characteristics of the battery will deteriorate, and the battery capacity will drop sharply. As a result, battery performance may decline, battery life may be shortened, and the battery may overheat or explode due to high internal resistance.

[0006] In many cases, the positive electrode, negative electrode, and separator are hydrophobic, while the electrolyte is hydrophilic. Therefore, a considerable amount of time and strict process conditions are required to improve the permeability of the electrodes and separator to the electrolyte.

[0007] If the coating thickness formed on the porous substrate is too small, the thermal safety of the separator is low. If the coating thickness is too large, the thermal safety of the separator increases, but the resistance of the lithium secondary battery increases, and therefore the battery performance may deteriorate.

[0008] Since most traditional secondary battery separators are hydrophobic, coating them with ceramic materials is used to improve their permeability to the electrolyte. When the coating is formed as described above, the thermal safety and mechanical properties of the separator are improved; however, the coating also acts as a resistor in terms of the battery characteristics of the secondary battery. Therefore, as the thickness of the ceramic coating increases, there is a problem of deterioration in the battery characteristics of the secondary battery.

[0009] Patent document 1 discloses a coating apparatus for coating a flexible board 11 with a coating solution, wherein the coating apparatus includes a first coating unit 12 configured to coat the flexible board by dip coating with a first coating solution; a second coating unit 13 disposed at the rear end of the first coating unit 12 configured to coat the flexible board with a second coating solution by gravure coating; a drying unit 14 and a guide roller 15 disposed at the rear end of the second coating unit, the drying unit configured to dry the coated flexible board.

[0010] Patent Document 1 relates to a coating apparatus and coating method, wherein a second coating unit 13 presses and additionally coats a flexible plate, thereby coating the flexible plate with a coating solution to achieve a more uniform coating and greater thickness, but does not recognize the impact of the thick coating on the battery characteristics of the secondary battery.

[0011] Therefore, the technology related to coating apparatus and coating method for separators used in secondary batteries can be easily performed with a simple structure, thereby forming a uniform and thin coating, which is considered an important problem in this invention, but has not yet been proposed.

[0012] (Existing technical literature)

[0013] (Patent Document 1) Korean Patent Publication No. 10-1653347 Summary of the Invention

[0014] Technical issues

[0015] The present invention was made in view of the above-mentioned problems, and the object of the present invention is to provide a coating apparatus and coating method for a diaphragm that can stably form a coating with an extremely thin thickness without changing the operating conditions of conventional coating processes.

[0016] Technical solution

[0017] The coating apparatus according to the invention for continuously forming a coating on each surface of a substrate film (100) to achieve the above-mentioned objective comprises: a water tank (210) located on a movement path of the substrate film (100); a water tank partition (220) vertically located in the water tank (210), the water tank partition being configured to divide the interior space of the water tank (210) into two regions, a first water tank portion (211) and a second water tank portion (212); a roller unit (300) configured to continuously convey the substrate film (100); and a heating unit (400) located outside the water tank (210), wherein the water tank partition (220) is spaced apart from the inner bottom surface of the water tank (210) by a predetermined distance.

[0018] Each of the first water tank portion (211) and the second water tank portion (212) may include a polar solution (120), the second water tank portion (212) may also include a non-polar coating solution (110), the coating solution (110) located in the second water tank portion (212) may be located above the polar solution (120), the horizontal movement of the coating solution located in the second water tank portion toward the first water tank portion (211) may be restricted by the water tank partition (220), and the coating solution (110) may be coated onto each surface of the substrate film (100) that continuously passes through the first water tank portion (211) and the second water tank portion (212).

[0019] The roller unit (300) may include an outer roller unit and an inner roller unit. The outer roller unit may include a pair of outer guide rollers arranged parallel to each other and spaced apart from each other. The inner roller unit may include a pair of inner guide rollers arranged parallel to each other and spaced apart from each other. The pair of inner guide rollers may be located at a predetermined distance from the inner bottom surface of the water tank (210).

[0020] The distance between the water tank partition (220) and the inner bottom surface of the water tank (210) can be greater than the distance between the lowest end of each inner guide roller and the inner bottom surface of the water tank (210).

[0021] The pair of inner guide rollers constituting the inner roller unit can be separated from the opposite side of the vertically arranged water tank partition (220) by a predetermined distance.

[0022] A pair of outer guide rollers constituting the outer roller unit are located outside the water tank (210) to correspond to a pair of inner guide rollers constituting the inner roller unit.

[0023] The inner guide roller located in the second water tank section (212) and the outer guide roller located on the upper outer side of the second water tank section (212) corresponding to the inner guide roller can be configured such that the substrate film (100) is vertically located between the inner guide roller and the outer guide roller.

[0024] The heating unit (400) can dry a substrate film (100) having a coating formed thereon by coating, and the coating apparatus may include a gas treatment unit configured to treat gaseous materials that volatilize during the drying process.

[0025] The present invention provides a coating method using the above-described coating apparatus, the coating method comprising: (s1) injecting a polar solution (120) into a water tank (210); (s2) injecting a coating solution (110) into the upper layer of the polar solution (120) contained in a second water tank section (212); (s3) allowing a substrate film (100) supplied while being supported by an outer guide roller and an inner guide roller to pass sequentially through a first water tank section (211) and a second water tank section (212) such that each surface of the substrate film (100) is coated with the coating solution (110); and (s4) drying the substrate film (100) coated with the coating solution (110) at the rear end of the second water tank section (212).

[0026] In step (s2), the height of the coating solution (110) injected into the second water tank section (212) can be adjusted so that the thickness of the coating formed on the substrate film (100) is 1 μm or less.

[0027] In step (s3), the throughput speed of the substrate film (100) can be adjusted so that the thickness of the coating formed on the substrate film (100) is 1 μm or less.

[0028] Steps (s1), (s2), (s3) and (s4) can be executed sequentially to complete the first coating step, and steps (s3) and (s4) can be repeated to perform the second coating step, thereby forming a coating.

[0029] The coating solution in step (S3) of the second coating step can be different from the coating solution in the first coating step, thereby forming multiple coatings.

[0030] Furthermore, the present invention can provide possible combinations of the above-mentioned solutions.

[0031] Beneficial effects

[0032] As can be clearly seen from the above description, the coating apparatus according to the present invention has the effect of achieving ultra-thin coating thickness without changing the traditional operating conditions.

[0033] The process of forming a coating on a substrate film is simple and does not require additional complex processes, which is advantageous in terms of production process and manufacturing cost.

[0034] The coating is formed on the substrate film with an extremely thin thickness, thereby improving the battery characteristics of the secondary battery.

[0035] Furthermore, in this invention, a small amount of nonpolar solution for coating is placed on top of a polar solution, which is configured to enable phase separation, thereby minimizing contaminants. Attached Figure Description

[0036] Figure 1 This is a schematic diagram of a traditional coating device.

[0037] Figure 2 This is a schematic diagram of a coating apparatus according to a first embodiment of the present invention.

[0038] Figure 3 This is a schematic diagram of a coating apparatus according to a second embodiment of the present invention. Detailed Implementation

[0039] Preferred embodiments of the present invention will now be described in detail with reference to the accompanying drawings, enabling those skilled in the art to readily implement these preferred embodiments. However, in describing the operational principles of the preferred embodiments in detail, detailed descriptions of known functions and configurations included herein will be omitted where such descriptions may obscure the subject matter of the invention.

[0040] Furthermore, the same reference numerals will be used in all the accompanying drawings to refer to parts that perform similar functions or operations. Where the description throughout the specification states that one part is connected to another, this means not only that one part can be directly connected to the other, but also that one part can be indirectly connected to the other through the other. Moreover, including an element does not imply the exclusion of other elements, but rather means that, unless otherwise specified, these elements may be further included.

[0041] Furthermore, descriptions of elements by limiting or adding them can be applied to all inventions unless otherwise specified, and do not limit any particular invention.

[0042] Furthermore, in the description of this invention and the claims of this application, the singular form is intended to include the plural form, unless otherwise stated.

[0043] Furthermore, in the description of this invention and the claims of this application, unless otherwise stated, "or" includes "and". Therefore, "including A or B" refers to three cases: including A, including B, and including both A and B.

[0044] Furthermore, unless the context explicitly states otherwise, all numerical ranges include the minimum, maximum, and all intermediate values ​​in between.

[0045] The coating apparatus according to the present invention will be described below with reference to the accompanying drawings.

[0046] Figure 2 This is a schematic diagram of a coating apparatus according to a first embodiment of the present invention.

[0047] Reference Figure 2 According to the first embodiment of the present invention, the coating apparatus includes a coating unit 200, a guide roller unit 300, and a heating unit 400.

[0048] First, when describing the coating unit 200 in detail, the coating unit 200 includes a water tank 210, which defines a receiving space for receiving a solution and a water tank partition 220 located in the receiving space to separate the solution.

[0049] A plate-shaped water tank partition 220 can be located in the water tank 210 to divide the receiving space of the water tank 210 into two parts, such as a first water tank portion 211 and a second water tank portion 212. Here, the first water tank portion 211 is the area adjacent to an uncoiler (not shown) that supplies the substrate film 100, and the second water tank portion 212 is the area adjacent to a rewinder (not shown), around which the coated substrate 100 is wound.

[0050] The lower end of the water tank partition 220 and the inner bottom surface (not shown) of the water tank 210 can be spaced apart by a predetermined distance. In this invention, the distance between the lower end of the water tank partition 220 and the inner bottom surface of the water tank 210 can be 0.1m to 1.0m, specifically 0.1m to 0.5m, and more specifically 0.1m to 0.2m. This is advantageous for minimizing the size of the coating apparatus while stably passing the substrate film 100, described subsequently, between the lower end of the water tank partition 220 and the inner bottom surface of the water tank 210.

[0051] Next, the guide roller unit 300 will be described. In this invention, at least one guide roller configured to guide the movement path of the substrate film 100 will be included, and will be described below. Specifically, it may include an outer guide roller located outside the water tank 210 and an inner guide roller located in the receiving space of the water tank 210. The outer guide roller may include a first outer guide roller 310 and a second outer guide roller 320. The first outer guide roller 310 is located between the uncoiler (not shown) supplying the substrate film 100 and the water tank 210, and conveys the substrate film 100 supplied from the uncoiler to the inner guide rollers 330 and 340 located in the receiving space of the water tank 210, as will be described below. The second outer guide roller 320 is positioned facing the first outer guide roller 310 with the water tank 210 positioned between the second outer guide roller 320 and the first outer guide roller 310, and supplies the substrate film 100, which has passed through the inner guide rollers 330 and 340 in the water tank 210, to a rewinder (not shown) located at the rear end of the water tank.

[0052] The inner guide rollers can be located in the receiving space of the water tank 210. The inner guide rollers include a pair of inner guide rollers arranged parallel to each other and horizontally spaced apart by a predetermined distance, namely, a first inner guide roller 330 and a second inner guide roller 340. The first inner guide roller 330 and the second inner guide roller 340 can be positioned at a predetermined distance from the inner bottom surface of the water tank 210 and at a predetermined distance from the opposite side surface of the water tank partition 220. The substrate film 100 supplied by the rotation of the first outer guide roller 310 is conveyed through the lower end surface of the first inner guide roller 330 to the second inner guide roller 340, and then through the lower end surface of the second inner guide roller 340 to the outside of the water tank 210. The substrate film 100 located between the first outer guide roller 310 and the first inner guide roller 330, and the substrate film 100 located between the second outer guide roller 320 and the second inner guide roller 340, can be positioned vertically or at a predetermined angle. Specifically, the substrate film 100 located between the second outer guide roller 320 and the second inner guide roller 340 can be vertically positioned, which facilitates the coating solution being coated on the opposite surfaces of the substrate film 100 with the same thickness, as will be described later.

[0053] Furthermore, although the substrate film 100 located between the second outer guide roller 320 and the second inner guide roller 340 is shown as vertically positioned in the figures of this invention, the second outer guide roller 320 and the second inner guide roller 340 may be spaced apart from each other by a predetermined distance, and the substrate film 100 located between them may be at a predetermined angle to the ground. In this case, uniform coatings of different thicknesses can be formed on the opposing surfaces of the substrate film 100.

[0054] Next, the heating unit 400 will be described in detail.

[0055] The substrate film 100, which has been coated, has passed through the second inner guide roller 340 located in the water tank 210 and can be dried simultaneously with passing through the heating unit 400. In the heating unit 400, the substrate film 100 having the coating 101 formed by coating can be dried at a temperature of 40°C to 100°C.

[0056] Here, the heating unit 400 can be located between the second inner guide roller 340 and the second outer guide roller 320. The heating unit 400 is configured to dry the coating formed on the substrate film 100 by injecting high-temperature hot air into the coating formed on the opposing surfaces of the substrate film 100 to dry the coating. Additionally, although not shown, a gas refining unit may also be provided to prevent secondary contamination caused by gas components generated during the hot air drying process.

[0057] The heating unit 400 can be a UV curing agent, and there are no particular restrictions on the type of heating unit, as long as it can stably and effectively dry the substrate film 100 on which the coating is formed by coating.

[0058] Next, the substrate film 100 will be described in detail.

[0059] Here, the substrate film 100 can be a separator substrate. A separator substrate that electrically isolates the positive and negative electrodes of the secondary battery from each other to prevent short circuits and provides a path for lithium ion movement can be used, without particular limitation, as long as the separator substrate can function normally as a separator for the secondary battery. The substrate film can be a polyolefin-based separator commonly used in the art to which this invention pertains. For example, the substrate film can be made from any one or a mixture of two or more of the following: high-density polyethylene, low-density polyethylene, linear low-density polyethylene, ultra-high molecular weight polyethylene, polypropylene, polyethylene terephthalate, polybutylene terephthalate, polyester, polyacetal, polyamide, polycarbonate, polyimide, polyetheretherketone, polyethersulfone, polyphenylene ether, polyphenylene sulfide, polynaphthalene, and mixtures thereof; however, the invention is not particularly limited thereto. Furthermore, a film or nonwoven fabric can be used alone or in combination as the substrate film 100.

[0060] In this invention, the thickness of the separator substrate can be in the range of 5 to 50 μm. However, the thickness of the substrate film is not particularly limited to the above range. Nevertheless, if the thickness of the substrate film is much smaller than the lower limit, the mechanical properties of the substrate film deteriorate, and the separator may be easily damaged during battery use. Simultaneously, the pore size of the substrate film can be in the range of 0.01 μm to 50 μm, and the porosity of the substrate film can be in the range of 10% to 95%, although the pore size and porosity of the substrate film are not particularly limited.

[0061] Here, the substrate film 100 can be an electrode current collector. The electrode current collector can be the positive electrode current collector or the negative electrode current collector of a secondary battery.

[0062] Positive electrode current collectors are typically manufactured with a thickness ranging from 3 μm to 500 μm. There are no particular limitations on the type of positive electrode current collector, as long as it exhibits high conductivity and does not cause any chemical changes in the battery in which it is used. For example, the positive electrode current collector can be made of stainless steel, aluminum, nickel, titanium, or sintered carbon. Alternatively, it can be made of aluminum or stainless steel with a surface treated with carbon, nickel, titanium, or silver. Furthermore, microscale non-uniform patterns can be formed on the surface of the positive electrode current collector to increase adhesion to the positive electrode active material. The positive electrode current collector can be constructed in any of a variety of forms, such as films, sheets, foils, meshes, porous bodies, foams, and nonwoven fabrics.

[0063] Negative electrode current collectors are typically manufactured with a thickness ranging from 3 μm to 500 μm. There are no particular limitations on the type of negative electrode current collector, as long as it exhibits high conductivity and does not cause any chemical changes in the battery in which it is used. For example, the negative electrode current collector can be made of copper, stainless steel, aluminum, nickel, titanium, or sintered carbon. Alternatively, it can be made of copper or stainless steel with its surface treated with carbon, nickel, titanium, silver, or an aluminum-cadmium alloy. Furthermore, similar to positive electrode current collectors, microscale non-uniform patterns can be formed on the surface of the negative electrode current collector to increase the adhesion of the negative electrode active material. The negative electrode current collector can be constructed in any of a variety of forms, such as films, sheets, foils, meshes, porous bodies, foams, and nonwoven fabrics.

[0064] Next, the polar solution 120 and the coating solution 110 received in the water tank 210 will be described.

[0065] The polar solution 120 can be water. The polar solution 120 is contained in a water tank 210, namely a first water tank portion 211 and a second water tank portion 212, and a first inner guide roller 330 and a second inner guide roller 340 are located within the solution 120. In addition, a portion of the vertically arranged water tank partition 220 is located within the polar solution 120.

[0066] The coating solution 110, being a non-polar solution, can be contained in a second tank section 212 separated by a tank partition 220. Specifically, the coating solution 110 is contained in the second tank section 212 and is not contained in the first tank section 211. Furthermore, the movement of the coating solution 110 contained in the second tank section 212 is blocked by the tank partition 220, so the coating solution does not move to the first tank section 211.

[0067] The coating solution 110 forms a non-polar solution layer that floats on the polar solution 120 in a state separate from the polar solution 120. The substrate film 100 passes through the coating solution 110 formed on the polar solution 120 contained in the second tank portion 212 via a first outer guide roller 310, a first inner guide roller 330, and a second inner guide roller 340, thereby applying the coating solution 110 to the surface of the substrate film 100, and thus forming a coating 101 on the surface of the substrate film. The thickness of each coating 101 can be adjusted by the height of the coating solution 110 contained in the second tank portion 212 and / or the transport speed of the substrate film 100. In this invention, the thickness of each coating 101 can be 4 μm or less, specifically 1 μm or less.

[0068] Here, the coating solution 110, which is a nonpolar solution, may include a nonpolar solvent, such as methyl ethyl ketone (MEK), toluene, or pentane.

[0069] Although not required, it may include adhesives, such as acrylates or PVdF, and fluoro-based nonionic surfactants as additives to form a coating solution 110 together with a nonpolar solvent.

[0070] In this invention, the adhesive can be used together with the inorganic material to form a coating of the diaphragm, wherein the adhesive can maintain the bond between the inorganic particles and improve the adhesion between the electrode and the diaphragm.

[0071] Furthermore, there are no particular restrictions on the type of adhesive, as long as the adhesive does not chemically alter the coating of the diaphragm. For example, the adhesive may be made from a selection of substances including: polyolefins, such as polyethylene or polypropylene; fluorinated resins, such as polyvinylidene fluoride or polytetrafluoroethylene; fluorinated rubbers, such as vinylidene fluoride-hexafluoropropylene-tetrafluoroethylene copolymers, ethylene-tetrafluoroethylene copolymers; styrene-butadiene copolymers and their hydrides; (meth)acrylate copolymers, such as methacrylate copolymers, acrylonitrile acrylate copolymers, or styrene acrylate copolymers; rubbers, such as ethylene propylene rubber; polyvinyl acetate; resins with a melting point or glass transition temperature of 180°C or higher, such as polyphenylene ether, polysulfone, polyethersulfone, polyphenylene sulfide, polyetherimide, polyamide, polyimide, polyamide-imide, polyetheramide, polyester, aromatic polyester, or polyetheretherketone; polycarbonate; polyacetal; water-soluble resins, such as carboxyl cellulose, alkyl cellulose, hydroxyalkyl cellulose, starch, polyvinyl alcohol, sodium alginate, polyethylene glycol, cellulose esters, polyacrylic acid, polyacrylamide, or polymethacrylic acid; or copolymers containing two or more of these substances.

[0072] The adhesive may include a PVdF-based adhesive, which is configured to enable phase separation, and the content of the PVdF-based adhesive may be 80% by weight or more, based on the total weight of the adhesive. If the content of the PVdF-based adhesive is less than 80% by weight, it is difficult to increase the porosity of the inorganic coating to the desired level, which is undesirable.

[0073] Specifically, the PVdF-based adhesive can be at least one selected from the group consisting of PVdF and PVdF copolymers. More specifically, each PVdF copolymer can be configured such that the content of PVdF monomer is 92 mol% or more based on the total molar number of monomers constituting the copolymer. If the content of PVdF monomer is less than 92 mol%, phase separation is reduced, making it difficult to increase the porosity of the inorganic coating to the desired level.

[0074] In the present invention, the inorganic particles are not particularly limited as long as they are electrochemically stable. The inorganic particles are not particularly limited as long as oxidation and / or reduction do not occur within the operating voltage range of the electrochemical device to which the inorganic particles are applied. In particular, when inorganic particles having ion transfer ability are used, ion conductivity in the electrochemical device is improved, which is beneficial for performance improvement. In the present invention, the inorganic material may be selected from the group consisting of BaTiO3, Pb(Zr,Ti)O3 (PZT), Pb 1-x La x Zr 1- y Ti y O3 (PLZT) (0<x<1, 0<y<1), PB(Mg3Nb 2 / 3 )O3-PbTiO3 (PMN-PT), hafnium oxide (H f O2), SrTiO3, SnO2, CeO2, MgO, NiO, CaO, ZnO, ZrO2, Y2O3, Al2O3, TiO2, SiC, (LiAlTiP) x O y -based glass (0<x<4, 0<y<13), lithium germanium thiophosphate (Li x Ge y P z S w , 0<x<4, 0<y<1, 0<z<1, 0<w<5), lithium nitride (Li x N y , 0<x<4, 0<y<2), SiS2-based glass (Li x Si y S z , 0<x<3, 0<y<2, 0<z<4), P2S5-based glass (Li x P y S z , 0<x<3, 0<y<3, 0<z<7) and mixtures thereof. However, the present invention is not limited thereto.

[0075] The coating solution 110 according to the present invention may include an additive, wherein the additive may be a fluorine-based nonionic surfactant.

[0076] The fluorine-based nonionic surfactant may be, for example, a fluoroalkylethylene oxide adduct, a fluoroalkenylethylene oxide adduct, a fluoroalkylpropylene oxide adduct, a fluoroalkenylpropylene oxide adduct, a perfluoroalkylethylene oxide adduct, or a perfluoroalkenylethylene oxide adduct.

[0077] In the present invention, when the substrate film 100 is an electrode current collector, the coating solution 110 may include a primer material.

[0078] The primer is used to increase the adhesion of the positive electrode active material to the metal substrate while minimizing the increase in internal resistance. Specifically, it can include conductive materials and polymer materials in a weight ratio of 1:10 to 10:1. If the content of conductive material is too low, the battery's operating characteristics will deteriorate due to increased internal resistance. If the content of polymer material is too low, it will be impossible to provide the required level of adhesion. Therefore, the content of conductive material and polymer material can be appropriately selected within the above range.

[0079] The conductive material can be at least one selected from the group consisting of graphite, carbon black, acetylene black, Ketjen black, channel black, furnace black, lamp black, thermal cracking black, carbon fiber, and fluorinated carbon; however, the invention is not limited thereto. Carbon black is particularly preferred. The particle size of the conductive material is preferably from 10 nm to 100 nm.

[0080] The polymer material can be at least one selected from the group consisting of polyimide copolymers, acrylate copolymers, polyvinylidene fluoride, polyvinyl alcohol, carboxymethyl cellulose (CMC), starch, hydroxypropyl cellulose, regenerated cellulose, polyvinylpyrrolidone, tetrafluoroethylene, polyethylene, polypropylene, ethylene propylene diene monomer (EPDM), sulfonated ethylene propylene diene monomer (EPDM), styrene-butadiene rubber, and fluororubber; however, the invention is not limited thereto. Polyimide copolymers are particularly preferred.

[0081] In the coating apparatus according to the first embodiment of the present invention, as described above, the polar solution 120 and the non-polar coating solution 110 are contained in a water tank 210 separated by a water tank partition 220. The coating solution 110 is applied to the surface of the substrate film 100, and the substrate film 100 on which the coating is formed is dried by a heating unit 400, thereby forming a coating 101 on the surface of the substrate film 100.

[0082] Figure 3 This is a schematic diagram of a coating apparatus according to a second embodiment of the present invention.

[0083] In addition to the coating apparatus according to the first embodiment being continuously provided to form multiple coatings using a coating solution, the second embodiment of the present invention is similar to the one described above. Figure 2 The first embodiment of the present invention described herein is identical. Therefore, in the following text, only the technical structure for forming multiple coatings will be described.

[0084] like Figure 3 As shown, the coating apparatus according to the second embodiment of the present invention can also be configured to have a structure in which the coating apparatus according to the first embodiment is continuously provided.

[0085] The substrate film 1100 supplied to the first outer guide roller 1310 passes through the interior of the first water tank 1210. A first coating solution 1110 is applied to each surface of the substrate film 1100, and drying is performed by the heating unit 1400, thereby forming a substrate film 1100 having a first coating layer 1101 formed thereon. The substrate film is then supplied to the first outer guide roller 2310 located in the second water tank 2210, which is positioned at the rear end of the first water tank. The substrate film 1100 having the first coating layer 1101 formed thereon is supplied to the first outer guide roller 2310, passes through the interior of the second water tank 2210, and a second coating solution 2110 is applied to the surface of the first coating layer. Subsequently, drying is performed by the heating unit 2400, thereby finally forming a substrate film 1100 having the first coating layer 1101 and the second coating layer 2101 formed thereon.

[0086] Here, the first coating solution 1110 and the second coating solution 2110 may include the same non-polar material or may include different non-polar materials.

[0087] Those skilled in the art will understand that, based on the above description, various applications and modifications can be made within the scope of this invention.

[0088] (Label Explanation)

[0089] 11: Flexible board

[0090] 12: First coating unit

[0091] 13: Second coating unit

[0092] 14: Drying Unit

[0093] 15: Guide roller

[0094] 100, 1100: Substrate film

[0095] 101: Coating

[0096] 1101: First coating

[0097] 2101: Second coating

[0098] 110: Coating solution

[0099] 1110: First coating solution

[0100] 2110: Second coating solution

[0101] 120, 1120, 2120: Polar solutions

[0102] 200, 1200, 2200: Coating unit

[0103] 210, 1210, 2210: Water tank

[0104] 211, 1211, 2211: First water tank section

[0105] 212, 1212, 2212: Second water tank section

[0106] 220, 1220, 2220: Water tank partition

[0107] 300, 1300, 2300: Roller Units

[0108] 310, 1310, 2310: First outer guide roller

[0109] 320, 1320, 2320: Second outer guide rollers

[0110] 330, 1330, 2330: First inner guide roller

[0111] 340, 1340, 2340: Second inner guide rollers

[0112] 400: Heating unit

Claims

1. A coating apparatus for continuously forming a coating layer on each surface of a substrate film, the coating apparatus comprising: A water tank located on the moving path of the substrate film, the water tank having a first end wall and a second end wall; A water tank partition is vertically disposed inside the water tank, the water tank partition being configured to divide the internal space of the water tank into two regions: a first water tank portion extending between the first end wall and the water tank partition, and a second water tank portion extending between the second end wall and the water tank partition; A roller unit is configured to continuously convey the substrate film and cause the substrate film to pass sequentially through the first water tank section and the second water tank section; and The heating unit is located outside the water tank. The water tank partition is spaced a predetermined distance from the inner bottom surface of the water tank. Each of the first water tank section and the second water tank section includes a polar solution. In both the first and second water tank sections, the coating solution is contained only in the second water tank section and is located above the polar solution, extending from the tank partition to the second end wall. The coating solution is a non-polar coating solution and is at the same height in the second water tank section. The polar solution mentioned therein is water.

2. The coating apparatus according to claim 1, wherein The horizontal movement of the coating solution located in the second water tank section towards the first water tank section is restricted by the water tank partition, and The coating solution is applied to each surface of the substrate film that passes continuously through the first water tank section and the second water tank section.

3. The coating apparatus according to claim 2, wherein The roller unit includes an outer roller unit and an inner roller unit. The outer roller unit includes a pair of outer guide rollers arranged in parallel and spaced apart from each other. The inner roller unit includes a pair of inner guide rollers arranged parallel to each other at intervals, and The pair of inner guide rollers are spaced a predetermined distance from the inner bottom surface of the water tank.

4. The coating apparatus of claim 3, wherein, The distance between the water tank partition and the inner bottom surface of the water tank is greater than the distance between the lowest end of the inner guide roller and the inner bottom surface of the water tank.

5. The coating apparatus of claim 3, wherein, The pair of inner guide rollers constituting the inner roller unit are separated from the opposite sides of the vertically arranged water tank partition by a predetermined distance.

6. The coating apparatus of claim 3, wherein, The pair of outer guide rollers constituting the outer roller unit are located outside the water tank to correspond to the pair of inner guide rollers constituting the inner roller unit.

7. The coating apparatus of claim 6, wherein, The inner guide roller located in the second water tank section and the outer guide roller located on the upper outer side of the second water tank section corresponding to the inner guide roller are arranged such that the substrate film is vertically positioned between the inner guide roller and the outer guide roller.

8. The coating apparatus according to claim 1, wherein The heating unit dries the substrate film having the coating formed thereon by coating, and The coating apparatus includes a gas processing unit configured to process gaseous materials that evaporate during the drying process.

9. A coating method using the coating apparatus according to any one of claims 3 to 7, the coating method comprising: s1: Inject a polar solution into the water tank; s2: Inject the coating solution into the upper layer of the polar solution contained in the second water tank section; s3: The substrate film, simultaneously supplied and supported by the outer guide roller and the inner guide roller, passes sequentially through the first water tank section and the second water tank section, such that each surface of the substrate film is coated with the coating solution; and s4: Dry the substrate film coated with the coating solution at the rear end of the second water tank section.

10. The coating method of claim 9, wherein, In step s2, the height of the coating solution injected into the second water tank is adjusted so that the thickness of the coating formed on the substrate film is 1 μm or less.

11. The coating method according to claim 9, wherein, In step s3, the throughput speed of the substrate film is adjusted so that the thickness of the coating formed on the substrate film is 1 μm or less.

12. The coating method according to claim 9, wherein Steps s1, s2, s3, and s4 are executed sequentially to complete the first coating step, and Repeat steps s3 and s4 to perform the second coating step, thereby forming a coating.

13. The coating method according to claim 12, wherein, The coating solution in step s3 of the second coating step is different from the coating solution in the first coating step, thereby forming multiple coatings.

Citation Information

Patent Citations

  • Apparatus for applying coating solution to flexible substrate

    KR101653347B1

  • Process of making colored sheets of cellulose esters, synthetic resins, and the like

    US2078214A

  • Device for formation and deposition of monomolecular layers of amphiphilic molecules on a substrate

    US4224896A