Method of manufacturing a radio frequency assembly
By using laser annealing technology on the semiconductor substrate of the RF component to form a trap enrichment layer, the problem of induced current interference is solved, and the performance of the RF component is improved.
Patent Information
- Application Number
- CN202210966830.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2022-08-03
- Filing Date
- 2022-08-11
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2042-08-11
AI Technical Summary
In existing radio frequency (RF) components, induced current interferes with their normal operation, leading to performance degradation. Existing technologies struggle to effectively reduce this interference.
A trap enrichment layer is formed on a semiconductor substrate using laser annealing technology. By laser annealing the upper surface of the substrate and forming radio frequency components on the insulating layer, the generation of induced current is reduced.
By forming a surface layer with high trap density, parasitic currents in the substrate are significantly reduced, thereby improving the performance of RF components.
Smart Images

Figure CN115881648B_ABST
Abstract
Description
Technical Field
[0001] This disclosure generally relates to the field of electronic components, such as radio frequency components.
[0002] Related technical specifications
[0003] Known radio frequency components include active components (such as amplifiers, mixers, and data converters) and passive components (such as capacitors, inductors, and antennas). Summary of the Invention
[0004] There is a need to improve known radio frequency components and their manufacturing methods.
[0005] The embodiments provide a method for fabricating an apparatus including at least one radio frequency component on a semiconductor substrate, the method comprising:
[0006] a) Laser annealing is performed on the upper surface side of the substrate to achieve a first thickness;
[0007] b) Forming an insulating layer on the upper surface of the substrate; and
[0008] c) Form the at least one radio frequency component on the insulating layer.
[0009] According to one embodiment, the resistivity of the substrate is greater than 3kΩ.
[0010] According to one embodiment, the method includes the step of forming an oxide layer on the upper surface side of the substrate prior to step a).
[0011] According to one embodiment, during step a), the laser power is 4 J / cm². 2 Order of magnitude.
[0012] According to one embodiment, the substrate is made of silicon or gallium nitride.
[0013] According to one embodiment, the wavelength of the laser is in the range of 300nm to 700nm.
[0014] According to one embodiment, during step a), the first thickness of the substrate is melted.
[0015] According to one embodiment, step a) is followed by a step of cooling the substrate.
[0016] According to one embodiment, the first thickness is in the range of 0.5 μm to 2 μm (e.g., on the order of 1 μm). Attached Figure Description
[0017] The above features and advantages, as well as others, will be described in detail in the following description of specific embodiments given by way of illustration, and are not limited to the accompanying drawings, wherein:
[0018] Figure 1 This is a cross-sectional view showing an example of a device including radio frequency components;
[0019] Figure 2 This is a cross-sectional view showing the structure obtained at the end of a step in an example method of manufacturing a device including radio frequency components, according to one embodiment;
[0020] Figure 3 This is a cross-sectional view showing the structure obtained at the end of another step in an example of a method for manufacturing a device including radio frequency components, according to one embodiment;
[0021] Figure 4 This is a cross-sectional view showing the structure obtained at the end of another step in an example of a method for manufacturing a device including radio frequency components, according to one embodiment;
[0022] Figure 5 This is a cross-sectional view showing the structure obtained at the end of another step in an example of a method for manufacturing a device including radio frequency components, according to one embodiment; and
[0023] Figure 6 This is a cross-sectional view showing the structure obtained at the end of another step in an example of a method for manufacturing a device including radio frequency components, according to one embodiment. Detailed Implementation
[0024] Similar features are designated by similar reference numerals in different figures. In particular, structural and / or functional features common in various embodiments may have the same reference numerals and may be configured with the same structure, dimensions, and material properties.
[0025] For clarity, only steps and elements that aid in understanding the embodiments described herein have been detailed and described. In particular, the formation of radio frequency components has not been described in detail; based on the instructions in this specification, the formation of these components is within the capabilities of those skilled in the art. Furthermore, the applications that may use such components have not been described in detail, and the described embodiments are compatible with common applications of radio frequency components.
[0026] Unless otherwise stated, when referring to two elements connected together, it means a direct connection without any intermediate elements other than conductors, and when referring to two elements coupled together, it means that the two elements can be connected or coupled via one or more other elements.
[0027] In the following disclosure, unless otherwise specified, when referring to absolute position qualifiers such as the terms “front,” “back,” “up,” “down,” “left,” “right,” etc., or relative position qualifiers such as the terms “above,” “below,” “over,” “under,” etc., or direction qualifiers such as “horizontal,” “vertical,” etc., refer to the direction shown in the figure.
[0028] Unless otherwise specified, the expressions “approximately,” “around,” “basically,” and “on the order of magnitude of” indicate within 10%, preferably within 5%.
[0029] The term radio frequency component typically refers to components that operate in the range of 3 kHz to 30 GHz.
[0030] Figure 1 This is a cross-sectional view showing an example of a device including the radio frequency component 15.
[0031] Figure 1 The illustrated device includes a semiconductor substrate 11 coated with a passivation layer 13, on which radio frequency components 15 are disposed. For example, the passivation layer 13 contacts the upper surface of the semiconductor substrate 11 through its lower surface. For example, the passivation layer 13 extends continuously over the entire surface of the semiconductor substrate 11. Figure 1 In the example shown, the device includes two radio frequency components 15. In practice, the device may include any number of radio frequency components 15, such as a single radio frequency component 15 or two or more radio frequency components 15.
[0032] Substrate 11 corresponds, for example, to a semiconductor wafer or a piece of a semiconductor wafer. Substrate 11 is made of, for example, silicon or gallium nitride (GaN). For example, substrate 11 is a high-resistivity material, such as a material with a resistivity greater than 3 kΩ. Substrate 11 is made of, for example, high-resistivity silicon. Substrate 11 can be a solid semiconductor substrate, such as a solid high-resistivity silicon substrate or an SOI (semiconductor on insulator) type substrate, such as a substrate made of high-resistivity silicon on insulator.
[0033] The passivation layer 13 is an electrically insulating layer. The passivation layer 13 is, for example, made of silicon dioxide.
[0034] In practice, due to the high operating frequency of the RF component 15, induced currents may appear in the upper portion 17 of the substrate 11, known as the parasitic surface conduction (PSC) region. These induced currents may interfere with the normal operation of the RF component 15 and degrade its performance.
[0035] According to one embodiment, a trap-rich layer is provided in the upper portion of the substrate 11. In practice, the presence of traps can reduce the mobility of electrons and holes, thereby reducing induced current, which leads to a degradation in the performance of the radio frequency components.
[0036] Various techniques have been provided for forming trap-rich surface layers in semiconductor substrates, particularly laser texturing, chemical etching, electron irradiation, nanocavity formation, thermal stress, or mechanical texturing. To increase trap density, multiple of these techniques can be combined, for example. A more readily implementable alternative technique is desired for forming trap-rich surface layers in semiconductor substrates used to support radio frequency components.
[0037] In the embodiments described below, a trap-enriched layer is created using a laser annealing technique. This technique, currently used to activate or propagate dopants in semiconductor layers, is intentionally used in this embodiment in an unusual manner to create defects in the semiconductor layer.
[0038] Figures 2 to 6 This is a cross-sectional view illustrating the sequential steps of an example method for manufacturing an apparatus including radio frequency components according to one embodiment.
[0039] Figure 2 An initial structure formed from a semiconductor substrate 21 is shown. The substrate 21 is, for example, a wafer of semiconductor material. For example, the substrate 21 is made of silicon or gallium nitride. For example, the substrate 21 is made of a high resistivity material. The substrate 21 can be a solid-state semiconductor substrate or an SOI-type substrate.
[0040] For example, the thickness of substrate 21 is between 300 μm and 800 μm, such as around 725 μm.
[0041] For example, substrate 21 is undoped or very lightly doped. The doping concentration in substrate 21 is, for example, less than about 10 times that of phosphorus atoms. 12 atoms / cm 3 And, for example, smaller than a boron atom by about 4.10. 12 atoms / cm 3 For example, the dopants present in substrate 21 may be different from phosphorus and boron, and may be arsenic or antimony.
[0042] Figure 3 The structure obtained at the end of the step of forming the insulating layer 23 on the upper surface side of the substrate 21 is shown.
[0043] For example, layer 23 is an oxide layer.
[0044] exist Figure 3 In the example shown, the upper portion of substrate 21 is oxidized to form layer 23. Layer 23 then corresponds to the upper portion of substrate 21. Layer 23 has the same chemical composition as substrate 21, except that it contains a higher concentration of oxygen atoms. In this example, the thickness e1 of layer 23 is in the range of 5 nm to 30 nm, for example, in the range of 15 nm to 20 nm.
[0045] For example, layer 23 is formed by thermal or chemical oxidation of the upper part of substrate 21. For example, layer 23 is formed during cleaning of the upper surface of substrate 21 in a mixture of sulfuric acid and hydrogen peroxide. As a variant, layer 23 is a natural oxide layer present on the surface of substrate 21.
[0046] Figure 4 This shows the process from the end of the laser annealing step. Figure 3 The structure obtained from the upper surface of the structure shown.
[0047] Figure 3 The laser annealing process shown consists of two consecutive steps.
[0048] In the first step, the upper surface of the structure is exposed to radiation from laser 25 (e.g., a pulsed laser). For example, the upper surface of the structure is exposed to radiation from layer 25 to melt the upper portion of the semiconductor material of substrate 21. Reference numeral 27 indicates the upper layer of the structure with a thickness of e2, which melts under the effect of laser radiation. The thickness e2 depends in particular on the power of laser 25, the wavelength of laser 25, the material of substrate 21, and, in the case of a pulsed laser, on the pulse duration and frequency of laser 25. For example, the power of laser 25 is approximately 4 J / cm². 2 The wavelength of laser 25 can be selected according to the material of substrate 21. For example, it is in the range of 300 nm to 700 nm. For example, for silicon substrate 21, the wavelength of laser 25 can be less than 500 nm, and for gallium nitride substrate 21, the wavelength of laser 25 can be less than 400 nm. The thickness e2 is, for example, in the range of 0.5 μm to 2 μm (e.g., about 1 μm). For example, in the first step, oxygen atoms in oxide layer 23 diffuse into layer 27, and it is said that layer 23 is the source of oxygen atoms diffused into layer 27. Therefore, layer 27 contains a higher concentration of oxygen atoms than the lower part of substrate 21.
[0049] In the second step, the structure, especially the upper layer 27, is cooled, preferably rapidly. The cooling rate is preferably greater than the crystallization rate of the substrate 21 material so that layer 27 does not recrystallize and remains in an amorphous state.
[0050] At the end of the laser annealing step, substrate 21 has defects in its upper part 27 due to the incorporation of oxygen atoms (particularly from oxide layer 23 and the atmosphere of the annealing chamber) into the substrate material. For example, in the case of a silicon substrate, the defects formed in layer 27 exist in the form of complexes between carbon and silicon atoms and complexes between carbon and oxygen atoms. These defects are suitable for trapping charge carriers that may be present in layer 27.
[0051] During the annealing step, the defect density generated in the upper part 27 of the substrate 21 depends particularly on the heating and cooling rates of the substrate 21. Specifically, the higher the heating rate and the faster the cooling rate, the greater the defect density.
[0052] During the laser annealing step, another layer 29 of the substrate 21, located below and in contact with the molten layer 27, also undergoes a transformation. Specifically, during cooling, crystal structure defects tend to propagate across the thickness of the substrate 21 below layer 27. Unlike layer 27, layer 29 of the substrate 21 does not melt and remains crystalline. Layer 29 extends across a thickness e3 from the lower surface of portion 27 within the substrate 21. For example, the thickness e3 is in the range of 0.5 μm to 2 μm (e.g., on the order of 1 μm). Layer 29 contains defects of the hole or interstitial type, suitable for trapping charge carriers that may be present in layer 29.
[0053] As an example, the laser annealing step mentioned above is performed on the entire plate, that is, it is formed on the entire surface of substrate 21.
[0054] As a variation, the laser annealing step described above is performed locally on the surface of substrate 21. In this variation, the precision or resolution of the laser is, for example, around a few micrometers.
[0055] exist Figure 4 In the example shown, laser annealing does not produce texture on the surface of substrate 21. In other words, the upper surface of substrate 21, especially the upper surface of layer 27, is planar at the end of the laser annealing step.
[0056] Figure 5 It shows in Figure 4 The structure obtained at the end of the deposition step of the electrically insulating layer or passivation layer 31 on the surface of the structure shown.
[0057] For example, layer 31 is made of oxide (e.g., silicon oxide).
[0058] For example, in Figure 4 The device surface shown has a full-plate deposition layer 31, meaning the deposition layer completely covers the upper surface of the substrate 21. For example, the thickness of layer 31 is between 0.5 μm and 2 μm (e.g., about 1.2 μm).
[0059] Figure 6 The device obtained at the end of the step of forming the radio frequency component 33 on the insulating layer 31 is shown.
[0060] exist Figure 6 In the example shown, the device includes two radio frequency components 33. In particular, the device can support any number of radio frequency components 33, for example, a single radio frequency component 33 or more than two radio frequency components 33.
[0061] For example, the radio frequency component 33 is a passive component, such as an inductor or an antenna. The radio frequency component 33 is made of a metallic material, such as copper or aluminum.
[0062] For example, the radio frequency component 33 is configured to operate in a frequency range between several kilohertz and several megahertz (e.g., from 3 kHz to 30 GHz).
[0063] Combination Figures 2 to 6 The described method has the advantage of enabling the formation of a trap-rich surface layer in a semiconductor substrate used to support radio frequency (RF) components through a relatively simple laser annealing technique. The provided method achieves high trap density at low cost, thereby significantly reducing parasitic currents induced in the substrate and improving the performance of the RF components.
[0064] Various embodiments and variations have been described. Those skilled in the art will understand that certain features of these different embodiments and variations can be combined, and that other variations will be conceived by those skilled in the art. In particular, the described embodiments are not limited to the examples of materials and dimensions mentioned in this disclosure.
[0065] Furthermore, although only examples of high resistivity substrates have been detailed above, the described embodiments are not limited to this specific case.
[0066] Finally, based on the functional indications given above, the actual implementation of the embodiments and variations is within the capabilities of those skilled in the art.
[0067] A method of manufacturing an apparatus can be summarized as including at least one radio frequency component (33) on a semiconductor substrate (21), comprising A) laser annealing a first thickness (27) of the substrate on the upper surface side of the substrate; b) forming an insulating layer (31) on the upper surface of the substrate; and c) forming the at least one radio frequency component on the insulating layer.
[0068] The resistivity of the substrate (21) can be greater than 3kΩ.
[0069] Prior to step a), the method may include the step of forming an oxide layer (23) on the upper surface side of the substrate (21).
[0070] The laser power in step a) is approximately 4 J / cm². 2 .
[0071] The substrate (21) can be made of silicon or gallium nitride.
[0072] The wavelength range of lasers is 300nm to 700nm.
[0073] During step a), the first thickness (27) of the fusible substrate (21) is achieved.
[0074] Step a) can be followed by a cooling step of the substrate (21).
[0075] The first thickness (27) can be in the range of 0.5 μm to 2 μm, for example, about 1 μm.
[0076] The various embodiments described above can be combined to provide further embodiments. If it is necessary to use concepts from various patents, applications, and publications to provide further embodiments, various aspects of the embodiments can be modified.
[0077] These and other modifications can be made to the embodiments based on the detailed description above. Generally, the terminology used in the following claims should not be construed as limiting the claims to the specific embodiments disclosed in the specification and claims, but should be interpreted to include all possible embodiments and all equivalents entitled to be obtained by those claims. Therefore, the claims are not limited to this disclosure.
Claims
1. A method of manufacturing an apparatus including radio frequency components, comprising: An oxide layer is formed on the surface of the substrate; A first defect layer is formed on the substrate by laser annealing using a laser. The first defect layer includes defects of a first complex type between carbon atoms and a first atom, and defects of a second complex type between carbon atoms and oxygen atoms. The first defect layer has a first thickness and is located at the surface of the substrate. A second defect layer is formed on the substrate by laser annealing. The second defect layer includes hole-type second defects, which are different from the first complex type and the second complex type. The second defect layer has a second thickness and is located between the first defect layer and a first portion of the substrate, and is located on the first portion of the substrate. The formation of the first defect layer and the second defect layer by laser annealing of the substrate includes: By exposing a second portion of the substrate to the laser, the second portion of the substrate located on the surface of the substrate and on the first portion of the substrate is melted; Cooling the second portion of the substrate and the first portion of the substrate, wherein cooling the second portion of the substrate and the first portion of the substrate includes: A first defect layer is formed, the first defect layer comprising first defects of the first complex type and the second complex type, being in an amorphous state and located on the second defect layer; and A second defect layer is formed, the second defect layer containing the hole-type second defect, in a crystalline state, located between the first defect layer and the first portion of the substrate, and the second defect layer separates the first defect layer from the first portion of the substrate; An insulating layer is formed on the first defect layer; and At least one radio frequency component is formed on the insulating layer; The first thickness and the second thickness are in the range of 0.5 μm to 2 μm, or equal to the upper and lower ends of this range.
2. The method according to claim 1, wherein the substrate has a density greater than 3kJ / m³. The resistance.
3. The method according to claim 1, wherein, Forming an oxide layer on the surface of the substrate includes forming an oxide layer with a thickness in the range of 5 nanometers to 30 nanometers, or equal to the upper and lower ends of that range.
4. The method according to claim 1, wherein the laser annealing comprises using a power of 4 J / cm². 2 Orders of magnitude of laser power.
5. The method of claim 1, wherein the substrate is made of silicon, and the first atom is a silicon atom.
6. The method of claim 1, wherein the substrate is made of gallium nitride, and the first atom is a gallium nitride atom.
7. The method of claim 1, wherein the laser annealing comprises using a laser having a wavelength in the range of 300 nm to 700 nm or equal to the upper and lower ends of that range.
8. The method of claim 1, wherein forming the first defect layer and forming the second defect layer comprises melting the substrate to the first thickness.
9. A method of manufacturing an apparatus including radio frequency components, comprising: An oxide layer is formed on the surface of the substrate; Forming a charge carrier layer and a hole layer of the substrate, comprising: By exposing the oxide layer at the surface of the substrate to a laser, a molten portion of the substrate is formed at the surface of the substrate; and Cooling the substrate and the molten portion of the substrate at the surface of the substrate, the cooling of the substrate and the molten portion of the substrate further includes: The hole layer is formed, the hole layer comprising hole-type defects configured to capture charge carriers that may be present within the hole layer in an operational state, the hole layer being crystalline and located on a first portion of the substrate; and The charge carrier layer is formed, the charge carrier layer contains complex-type defects, the complex-type defects are configured to capture charge carriers that may exist in the charge carrier layer in the working state, the charge carrier layer is amorphous, and the charge carrier layer is located above the hole layer; An insulating layer is formed on the charge carrier layer; and At least one radio frequency component is formed on the insulating layer, wherein Forming the charge carrier layer also includes forming the charge carrier layer containing the complex-type defects, the complex-type defects including a first complex between carbon atoms and silicon atoms and a second complex between carbon atoms and oxygen atoms; The first thickness of the charge carrier layer and the second thickness of the hole layer are in the range of 0.5 micrometers to 2 micrometers, or equal to the upper and lower ends of this range; The charge carrier layer has a first oxygen atom concentration that is greater than the second oxygen atom concentration in the substrate, and the hole layer has a third oxygen atom concentration that is less than the first oxygen atom concentration.
10. The method according to claim 9, wherein: Forming the molten portion of the substrate at the surface of the substrate by exposing the oxide layer at the surface of the substrate to the laser further includes: allowing oxygen atoms present in the oxide layer to diffuse through the molten portion.
Citation Information
Patent Citations
Electronic device
CN219123214U
Method of fabrication of a semiconductor element comprising a highly resistive substrate
US20180130698A1
Methods for assessing semiconductor structures
US20200058566A1