Selective silicon etch for surround gate transistors

By pre-cleaning and trimming the semiconductor material layer, a horizontally surrounding gate device is formed using selective etching technology. This solves the space limitations and threshold voltage adjustment problems caused by device miniaturization, and improves device performance and process efficiency.

CN115997291BActive Publication Date: 2026-11-20APPLIED MATERIALS INC
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202180047207.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2021-06-22
Filing Date
2021-06-25
Publication Date
2026-11-20
Estimated Expiration
2041-06-25

AI Technical Summary

Technical Problem

Existing technologies face challenges in forming horizontally wrapped gate devices, including space limitations due to device miniaturization, difficulty in adjusting threshold voltage, and the need for metal film deposition and etching.

Method used

By pre-cleaning and trimming the semiconductor material layers, a horizontally surrounding gate device is formed, reducing the thickness and width of the silicon nanoplate. Selective etching technology is used to remove the release layer, avoiding the deposition and etching of metal films, and adjusting the threshold voltage.

Benefits of technology

This technology enables adjustment of the threshold voltage without disrupting the vacuum, reducing silicon oxidation and silicon oxide removal, improving device performance, and lowering process complexity and cost.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115997291B_ABST
    Figure CN115997291B_ABST
Patent Text Reader

Abstract

Horizontal wraparound gate devices and methods of manufacturing the same are described. The hGAA device includes a tailored semiconductor material between the source region and the drain region of the device. The method includes selectively isotropically etching a semiconductor material layer between the source region and the drain region of the electronic device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] Embodiments of this disclosure generally relate to semiconductor devices, and more specifically, to horizontal all-around gate device structures and methods and apparatus for forming horizontal all-around gate device structures. Background Technology

[0002] Transistors are critical components in most integrated circuits. Since the drive current and therefore speed of a transistor are proportional to its gate width, faster transistors generally require larger gate widths. Therefore, there is a trade-off between transistor size and speed, and "fin" field-effect transistors (FFETs) have been developed to resolve this conflicting goal of achieving the maximum drive current and the smallest size. FinFETs are characterized by a fin-shaped channel region, which significantly increases the transistor's size without substantially increasing its footprint, and are now used in many integrated circuits. However, finFETs have their own drawbacks.

[0003] As the feature size of transistor devices continues to shrink to achieve greater circuit density and higher performance, there is a need to improve transistor device structures to enhance electrostatic coupling and reduce negative impacts such as parasitic capacitance and off-state leakage current. Examples of transistor device structures include planar structures, FinFET structures, and horizontal gate all-around (hGAA) structures. The hGAA device structure comprises several lattice-matched channels suspended in a stacked configuration and connected by source / drain regions. The hGAA structure provides excellent electrostatic control and is widely used in complementary metal-oxide-semiconductor (CMOS) wafer fabrication.

[0004] Logic gate performance is related to the properties of the materials used, as well as the thickness and area of ​​the structural layers. However, challenges arise as some gate characteristics are tuned to accommodate device scaling. Furthermore, the space constraints between lines on horizontal gate-all-around (hGAA) devices limit the thickness of the gate dielectric material used for I / O transistors.

[0005] Complementary metal-oxide-semiconductor (CMOS) devices need to be fabricated with multiple threshold voltages for logic applications. Threshold voltage tuning is typically achieved by depositing and etching different metal films on the gate dielectric layer. Furthermore, with the shrinking device size of gate-all-around designs and changes in device architecture, the physical space available for film deposition and etching is becoming increasingly smaller.

[0006] Therefore, there is a need for improved methods for forming horizontally wrapped gate devices. Summary of the Invention

[0007] One or more embodiments of this disclosure relate to methods of forming semiconductor devices. In one or more embodiments, the method of forming a semiconductor device includes: pre-cleaning a plurality of semiconductor material layers to remove native oxides and / or residues; and trimming the plurality of semiconductor material layers to form trimmed semiconductor material layers.

[0008] Additional embodiments of this disclosure relate to horizontal all-around gate devices. In one or more embodiments, the horizontal all-around gate device includes a plurality of horizontally trimmed semiconductor material layers between the source and drain regions.

[0009] Further embodiments of this disclosure relate to computer-readable media. In one or more embodiments, a non-transitory computer-readable medium includes instructions, when executed by a controller of a processing chamber, to cause the processing chamber to: pre-clean a plurality of semiconductor material layers to remove native oxides and / or residues; and trim the plurality of semiconductor material layers to form trimmed semiconductor material layers. Attached Figure Description

[0010] To gain a more detailed understanding of the features described above, the present disclosure, which has been briefly outlined above, can be described in more detail with reference to embodiments, some of which are shown in the accompanying drawings. However, it should be noted that the accompanying drawings illustrate only typical embodiments of the present disclosure and should therefore not be considered as limiting its scope, as the present disclosure allows for other equally effective embodiments.

[0011] Figure 1 A process flow diagram illustrating a method for forming a semiconductor device according to some embodiments of the present disclosure is shown.

[0012] Figures 2A-2I This illustration shows the substrate manufacturing stages during a method for forming a semiconductor device according to some embodiments of the present disclosure; and

[0013] Figure 3 Clustering tools according to one or more implementations are shown.

[0014] For ease of understanding, the same reference numerals are used where possible to designate common elements in the figures. The figures are not drawn to scale and may be simplified for clarity. Elements and features of one embodiment may be advantageously incorporated into other embodiments without further description. Detailed Implementation

[0015] Before describing several exemplary embodiments of this disclosure, it should be understood that this disclosure is not limited to the details of the construction or process steps set forth in the following description. This disclosure can be implemented in other ways and can be practiced or performed in various manner.

[0016] As used in this specification and the appended claims, the term "substrate" refers to a surface or portion thereof on which a process is performed. Those skilled in the art will also understand that reference to substrate may also refer only to a portion of the substrate, unless the context clearly indicates otherwise. Furthermore, reference to deposition on a substrate may mean both a bare substrate and a substrate on which one or more films or features are deposited or formed.

[0017] As used herein, “substrate” means any substrate on which a film treatment is performed during a manufacturing process, or a material surface formed on a substrate. For example, substrate surfaces on which treatment may be performed include materials such as silicon, silicon oxide, strained silicon, silicon on insulator (SOI), carbon-doped silicon oxide, amorphous silicon, doped silicon, germanium, gallium arsenide, glass, sapphire, and any other materials such as metals, metal nitrides, metal alloys, and other conductive materials, depending on the application. Substrates include, but are not limited to, semiconductor wafers. Substrates may be exposed to pretreatment processes to polish, etch, reduce, oxidize, hydroxylate, anneal, and / or bake substrate surfaces. In addition to performing film treatments directly on the surface of the substrate itself, any of the disclosed film treatment steps may also be performed on an underlayer formed on the substrate, as disclosed in more detail below, and the term “substrate surface” is intended to include such an underlayer as indicated by the context. Thus, for example, when a film / layer or a portion of a film / layer is deposited onto a substrate surface, the exposed surface of the newly deposited film / layer becomes the substrate surface.

[0018] As used in this specification and the appended claims, the terms “precursor,” “reactant,” “reactive gas,” and the like are used interchangeably to represent any gaseous species that can react with the substrate surface.

[0019] A transistor is a circuit component or element typically formed on a semiconductor device. Depending on the circuit design, transistors may be formed on the semiconductor device in addition to capacitors, inductors, resistors, diodes, wires, or other components. Generally, a transistor includes a gate formed between a source region and a drain region. In one or more embodiments, the source and drain regions include doped regions of the substrate and exhibit a doping profile suitable for a particular application. The gate is located above the channel region and includes a gate dielectric layer inserted into the substrate between the gate electrode and the channel region.

[0020] As used herein, the term "field-effect transistor" or "FET" refers to a transistor that uses an electric field to control the electrical behavior of the device. Enhancement-mode field-effect transistors generally exhibit extremely high input impedance at low temperatures. The conductivity between the drain and source terminals is controlled by an electric field in the device, generated by the voltage difference between the device body and the gate. The three terminals of an FET are the source (S), through which charge carriers enter the channel; the drain (D), through which charge carriers leave the channel; and the gate (G), which modulates the channel conductivity. Conventionally, the current entering the channel at the source (S) is designated Is, and the current entering the channel at the drain (D) is designated I. D Specify the drain-source voltage as V. DS By applying a voltage to the gate (G), the current (i.e., Id) entering the channel at the drain can be controlled. D ).

[0021] A metal-oxide-semiconductor field-effect transistor (MOSFET) is a type of field-effect transistor (FET). It has an insulated gate, the voltage of which determines the device's conductivity. This ability to change conductivity with the amount of applied voltage is used to amplify or switch electronic signals. A MOSFET is based on the modulation of charge concentration by a metal-oxide-semiconductor (MOS) capacitance between a host electrode and a gate electrode located above the host, and is insulated from all other device regions by a gate dielectric layer. Compared to a MOS capacitor, a MOSFET includes two additional terminals (source and drain), each connected to a separate, highly doped region separated by the host region. These regions can be p-type or n-type, but they are of the same type and are the opposite of the host region. The source and drain (different from the host) are highly doped, as indicated by the "+" sign after the doping type.

[0022] If the MOSFET is an n-channel or nMOS FET, then the source and drain are in the n+ region, while the bulk is in the p region. If the MOSFET is a p-channel or pMOS FET, then the source and drain are in the p+ region, while the bulk is in the n region. The source is named as such because it is the origin of charge carriers flowing through the channel (electrons for the n-channel, holes for the p-channel); similarly, the drain is where charge carriers leave the channel.

[0023] As used herein, the term "FinFET" refers to a MOSFET transistor built on a substrate where the gate is located on two or three sides of the channel, forming a dual-gate or triple-gate structure. FinFET devices are given the common name FinFET because the channel region forms "fins" on the substrate. FinFET devices feature fast switching times and high current densities.

[0024] As used herein, the term "gate all around (GAA)" is used to represent an electronic device, such as a transistor, in which gate material surrounds a channel region on all sides. The channel region of a GAA transistor may include nanowires or nanoplates, strip channels, or other suitable channel configurations known to those skilled in the art. In one or more embodiments, the channel region of a GAA device has a plurality of vertically spaced horizontal nanowires or horizontal strips, such that the GAA transistor is a stacked horizontal gate all around (hGAA) transistor.

[0025] As used in this article, the term "nanowire" refers to wires with nanometer-scale (10⁻⁶) or nanometer-scale (10⁻⁶) wires. -9 Nanowires are nanostructures with a diameter of (meters). A nanowire can also be defined as having an aspect ratio greater than 1000. Alternatively, a nanowire can be defined as a structure with a thickness or diameter limited to tens of nanometers or less and an unlimited length. Nanowires are used in transistors and some laser applications, and in one or more embodiments, are made of semiconductor materials, metallic materials, insulating materials, superconducting materials, or molecular materials. In one or more embodiments, nanowires are used in transistors of logic CPUs, GPUs, MPUs, and volatile (e.g., DRAM) and non-volatile (e.g., NAND) devices.

[0026] In one or more embodiments, a horizontally all-around gate (hGAA) transistor includes a substrate having a top surface; a source region having a source electrode and source contacts, the source region being located on the top surface of the substrate; a drain region having a drain electrode and drain contacts, the drain region being located on the top surface of the substrate; a channel located between the source and drain electrodes and having an axis substantially parallel to the top surface of the substrate; a gate surrounding the channel between the source and drain regions; a dielectric layer covering and contacting one or more of the gate, source contacts, or drain contacts; and a gate spacer covering the dielectric layer. In one or more embodiments, the spacer layer has a thickness of less than about 8 nm.

[0027] One or more embodiments of this disclosure relate to methods for forming horizontal all-around gate devices. Some embodiments advantageously provide methods for adjusting the threshold voltage of the device without depositing and etching metal films. In some embodiments, the thickness and width of the silicon nanoplates used as the channel for the GAA transistor are advantageously reduced. One or more embodiments of the method include pre-cleaning the silicon surface and performing silicon etching without breaking the vacuum.

[0028] One or more embodiments of the method advantageously eliminate the need for deposition and etching to adjust the threshold voltage. Furthermore, one or more embodiments of the method eliminate the need for silicon oxidation and silicon oxide removal, which could increase the dielectric constant (k-value) of the surrounding spacer material and degrade device performance. In some embodiments, if a Si / SiGe superlattice is used to form a gate-all-around transistor, reducing the initial silicon layer thickness during subsequent processing can lead to process runaway due to Ge diffusion into the silicon. Therefore, one or more embodiments of the method do not require changing the thickness of the deposited silicon layer in the Si / SiGe superlattice required to fabricate the GAA transistor.

[0029] In one or more embodiments, a gate-all-around transistor is fabricated using a standard process flow. After removing the sacrificial silicon-germanium (SiGe) epitaxial layer to expose the channel release of all sides of the silicon nanoplate, the substrate is masked to expose only certain portions of the substrate for selective nanoplate trimming. In one or more embodiments, the substrate undergoes an optional first pre-cleaning to remove organic residues. Subsequently, the substrate undergoes a second pre-cleaning to remove native oxides, such as silicon oxide (SiOx), located at the silicon nanoplate interface. The substrate is then silicon etched to reduce the thickness and width of the nanoplate.

[0030] Embodiments of this disclosure are described with reference to the accompanying drawings, which illustrate devices (e.g., transistors) and processes for forming transistors according to one or more embodiments of this disclosure. The illustrated processes are merely illustrative of possible uses of the disclosed processes, and those skilled in the art will recognize that the disclosed processes are not limited to the illustrated applications.

[0031] Figure 1 A process flow diagram of a method 100 for forming a semiconductor device according to some embodiments of this disclosure is shown. The following section discusses... Figures 2A-2I Description method 100, Figures 2A-2I The present disclosure describes some embodiments of the manufacturing stages of a semiconductor structure. Figures 2A-2I This is a cross-sectional view of an electronic device (e.g., an hGAA) according to one or more embodiments. Method 100 may be part of a multi-step manufacturing process for a semiconductor device. Therefore, method 100 may be performed in any suitable processing chamber coupled to a clustering tool. The clustering tool may include processing chambers for manufacturing semiconductor devices, such as chambers configured for etching, deposition, physical vapor deposition (PVD), chemical vapor deposition (CVD), oxidation, or any other suitable chamber for manufacturing semiconductor devices.

[0032] Method 100 in operation 102 involves providing a substrate 200 having a top surface 202 (e.g., ...). Figure 2A (As shown) In some embodiments, substrate 200 may be a bulk semiconductor substrate. As used herein, the term "bulk semiconductor substrate" refers to a substrate in which the entire substrate is made of a semiconductor material. A bulk semiconductor substrate may comprise any suitable semiconductor material and / or combination of semiconductor materials for forming a semiconductor structure. For example, the semiconductor layer may comprise one or more materials, such as crystalline silicon (e.g., Si). <100> or Si <111> The semiconductor material may include silicon oxide, strained silicon, silicon germanium, doped or undoped polycrystalline silicon, doped or undoped silicon wafers, patterned or unpatterned wafers, doped silicon, germanium, gallium arsenide, or other suitable semiconductor materials. In some embodiments, the semiconductor material is silicon (Si). In one or more embodiments, the semiconductor substrate 200 comprises a semiconductor material such as silicon (Si), carbon (C), germanium (Ge), silicon germanium (SiGe), germanium tin (GeSn), other semiconductor materials, or any combination thereof. In one or more embodiments, the substrate 200 comprises one or more of silicon (Si), germanium (Ge), gallium (Ga), arsenic (As), or phosphorus (P). Although several examples of materials that can form a substrate have been described herein, any material that can be used as the basis for constructing passive and active electronic devices (e.g., transistors, memories, capacitors, inductors, resistors, switches, integrated circuits, amplifiers, optoelectronic devices, or any other electronic devices) falls within the spirit and scope of this disclosure.

[0033] In some embodiments, the semiconductor material may be a doped material, such as n-doped silicon (n-Si) or p-doped silicon (p-Si). In some embodiments, any suitable process, such as ion implantation, may be used to dope the substrate. As used herein, the term "n-type" refers to a semiconductor produced during manufacturing by doping an intrinsic semiconductor with an electron donor element. The term n-type derives from the negative charge of electrons. In an n-type semiconductor, electrons are the majority carriers and holes are the minority carriers. As used herein, the term "p-type" refers to the positive charge of a well (or hole). In contrast to an n-type semiconductor, a p-type semiconductor has a hole concentration greater than the electron concentration. In a p-type semiconductor, holes are the majority carriers and electrons are the minority carriers. In one or more embodiments, the dopant is selected from one or more of boron (B), gallium (Ga), phosphorus (P), arsenic (As), other semiconductor dopant, or combinations thereof. In some embodiments, the substrate may be doped to provide a high dose of dopant at a first location on the surface of the substrate 200 to prevent parasitic bottom device activation. In one or more embodiments, the superlattice structure 204 is formed on top of the first location. For example, in some embodiments, the surface of the substrate may have about 10 18 atoms / cm 3 To about 10 19atoms / cm 3 The dopant density.

[0034] At least one superlattice structure 204 is formed on the top surface 202 of the substrate 200 (e.g., Figure 2A (As shown). The superlattice structure 204 includes a plurality of semiconductor material layers 224 arranged in alternating stacked pairs and corresponding plurality of release layers 226. In some embodiments, the plurality of stacked layer groups include silicon (Si) and silicon-germanium (SiGe) groups. In some embodiments, the plurality of semiconductor material layers 224 and corresponding plurality of release layers 226 may include any number of lattice-matching material pairs suitable for forming the superlattice structure 204. In some embodiments, the plurality of semiconductor material layers 224 and corresponding plurality of release layers 226 include about 2 to about 50 pairs of lattice-matching materials.

[0035] Typically, parasitic devices will be present at the bottom of the superlattice structure 204. In some embodiments, as described above, dopants are implanted into the substrate to suppress the on-state of parasitic devices. In some embodiments, the substrate 200 is etched such that the bottom portion of the superlattice structure 204 includes an unremoved substrate portion, thereby allowing the substrate portion to act as a bottom release layer of the superlattice structure 204.

[0036] In one or more embodiments, in some embodiments, the thicknesses of the semiconductor material layer 224 and the release layer 226 are in the range of about 2 nm to about 50 nm, about 3 nm to about 20 nm, or about 2 nm to about 15 nm. In some embodiments, the average thickness of the semiconductor material layer 224 is within 0.5 to 2 times the average thickness of the release layer 226.

[0037] In some embodiments, dielectric material 246 is deposited on substrate 200 using a conventional chemical vapor deposition method. In some embodiments, dielectric material 246 is recessed below the top surface 202 of substrate 200, such that the bottom portion of superlattice structure 204 is formed by substrate 200.

[0038] In some embodiments, an alternative gate structure (e.g., a dummy gate structure 208) is formed on and adjacent to the superlattice structure 204. The dummy gate structure 208 defines a channel region for the transistor device. The dummy gate structure 208 can be formed using any conventional deposition and patterning process known in the art.

[0039] In some embodiments, the sidewall spacers 210 are formed along the outer sidewalls of the dummy gate structure 208. In some embodiments, the sidewall spacers 210 comprise suitable insulating materials known in the art, such as silicon nitride, silicon oxide, silicon oxynitride, silicon carbide, or the like. In some embodiments, the sidewall spacers 210 are formed using any conventional deposition and patterning process known in the art, such as atomic layer deposition, plasma-enhanced atomic layer deposition, plasma-enhanced chemical vapor deposition, or low-pressure chemical vapor deposition.

[0040] In some embodiments, embedded source region 232 and drain region 234 are formed in source trench and drain trench, respectively. In some embodiments, source region 232 is formed adjacent to a first end of superlattice structure 204, while drain region 234 is formed adjacent to a second opposite end of superlattice structure. Figure 2A In the illustrated embodiment, one of the source region 232 or the drain region 234 is not shown on the front side of the superlattice structure 204. The other end of the superlattice structure 204 has the other of the source region 232 or the drain region 234. In some embodiments, the source region 232 and / or the drain region 234 are formed of any suitable semiconductor material, such as, but not limited to, silicon, germanium, silicon-germanium, or the like. In some embodiments, the source region 232 and the drain region 234 can be formed using any suitable deposition process, such as epitaxial deposition.

[0041] In some embodiments, an inter-layer dielectric (ILD) layer 220 is blanket-deposited on the substrate 200, including source / drain regions 232, 234, a dummy gate structure 208, and sidewall spacers 210. The ILD layer 220 can be deposited using conventional chemical vapor deposition methods (e.g., plasma-enhanced chemical vapor deposition and low-pressure chemical vapor deposition). In one or more embodiments, the ILD layer 220 is formed of any suitable dielectric material, such as, but not limited to, undoped silicon oxide, doped silicon oxide (e.g., BPSG, PSG), silicon nitride, and silicon oxynitride. In one or more embodiments, the ILD layer 220 is subsequently back-polished using conventional chemical mechanical planarization methods to expose the top of the dummy gate structure 208. In some embodiments, the ILD layer 220 is polished to expose the top of the dummy gate structure 208 and the top of the sidewall spacers 210.

[0042] In operation 104, such as Figure 2BAs shown, the dummy gate structure 208 is removed to expose the channel region 214 of the superlattice structure 204. The ILD layer 220 protects the source / drain regions 232, 234 during the removal of the dummy gate structure 208. The dummy gate structure 208 can be removed using any conventional etching method, such as plasma dry etching or wet etching. In some embodiments, the dummy gate structure 208 comprises polysilicon and is removed by a selective etching process. In some embodiments, the dummy gate structure 208 comprises polysilicon and the superlattice structure 204 comprises alternating layers of silicon (Si) and silicon-germanium (SiGe).

[0043] In operation 106, such as Figure 2C As shown, a release layer 226 is selectively etched between semiconductor material layers 224 in the superlattice structure 204. In one or more embodiments, the release layer 226 is isotropically etched to form one or more cavities 228 between the semiconductor material layers 224. Figure 2C As shown, each cavity 228 has a surface 229. Furthermore, each cavity 228 is disposed between the existing structure of the device (i.e., one of the sidewall spacers 210) and the bulk semiconductor portion of the semiconductor substrate 200. Therefore, each portion of the cavity 228 is located in a region inaccessible by symbol-line ion implantation technology.

[0044] The isotropic etching process of operation 106 can be selected to remove sufficient material from the superlattice structure 204, such that the cavity 228 has any suitable target width 228a. For example, in some embodiments, the isotropic etching process of operation 106 is performed such that the cavity 228 has a target width 228a of about 2 nm to about 10 nm. In other embodiments, the cavity 228 defined by surface 229 may have a target width 228a greater than 10 nm or less than 2 nm, depending on the geometry of the sidewall spacers 210, the concentration of n-dopant or p-dopant in the heavily doped regions, and other factors. For example, in some embodiments, the target width 228a can be selected such that the cavity 228 has a target width 228a that is no more than about 1 nm smaller than the width of the sidewall spacers 210.

[0045] The isotropic etching process of operation 106 may include any suitable etching process that is selective to the semiconductor material of the release layer 226. In some embodiments, the isotropic etching process of operation 106 includes one or more of a wet etching process or a dry etching process. In some embodiments, the isotropic etching process of operation 106 includes a dry etching process.

[0046] In one or more embodiments, the superlattice structure 204 comprises a silicon layer and a silicon-germanium layer, the silicon-germanium being selectively etched to form channel nanowires 240. The release layer 226, such as silicon-germanium, can be removed using any known etchant selectively applied to the semiconductor material layer 224, wherein the etchant etches the release layer 226 at a significantly higher rate than the semiconductor material layer 224. In some embodiments, selective dry etching or wet etching processes can be used. The removal of the release layer 226 leaves voids 228 between the semiconductor material layers 224. The voids 228 between the semiconductor material layers 224 have a thickness of approximately 3 nm to approximately 20 nm. The remaining semiconductor material layers 224 form a vertical array of channel nanowires 240 coupled to source / drain regions 232, 234. The channel nanowires 240 extend parallel to the top surface 202 of the substrate 200 and are aligned with each other to form a single row of channel nanowires 240. The formation of source region 232 and drain region 234, as well as the optional lateral etch stop layer (not shown), advantageously provides self-alignment and structural integrity in the formation of the channel structure.

[0047] In operation 108, such as Figure 2D As shown, a region of substrate 200 is masked by mask 245 to leave only certain portions or regions of the substrate exposed semiconductor material layer 224 for selective silicon channel trimming. Any suitable technique known to those skilled in the art can be used to mask the substrate. Any suitable mask material known to those skilled in the art can be used to mask the substrate.

[0048] In some embodiments, optional pre-treatment cleaning processes or other surface preparation processes are performed on the surface 229 of the cavity 228. The surface preparation process may be performed prior to the processes in operation 110 to remove native oxides from the surface 229 and otherwise prepare the surface 229. The surface preparation process may include a dry etching process, a wet etching process, or a combination of both.

[0049] In such implementations, the dry etching process may include conventional plasma etching or remote plasma-assisted dry etching processes, such as SiCoNi available from Applied Materials, located in Santa Clara, California. TM Etching process. In SiCoNi TM During the etching process, surface 229 is exposed to H2, NF3, and / or NH3 plasma species, such as plasma-excited hydrogen and fluorine species. For example, in some embodiments, surface 229 may be simultaneously exposed to H2, NF3, and NH3 plasmas. SiCoNi TM Etching processes can be performed on SiCoNi TMThe pre-cleaning process takes place in a chamber that can be integrated into a variety of multiprocessing platforms, including those available from Applied... of Dual ACP, GT and Platform. The wet etching process may include a hydrofluoric acid (HF) post-process, the so-called "HF post-process," in which HF etching of surface 229 is performed, leaving hydrogen-terminated surface 229. Alternatively, any other liquid-based pre-epitaxial pre-cleaning process may be employed. In some embodiments, this process includes sublimation etching for the removal of native oxides. The etching process may be plasma-based or thermal-based. The plasma process may be any suitable plasma (e.g., conductively coupled plasma, inductively coupled plasma, microwave plasma).

[0050] In some embodiments, the apparatus or process tool is configured to hold the substrate under vacuum conditions to prevent oxide layer formation after the pre-conditioning cleaning process. In such embodiments, the process tool is configured to move the substrate from the pre-conditioning cleaning chamber to the etching process chamber without exposing the substrate to atmospheric conditions.

[0051] In one or more embodiments, during operation 110, the channel nanowires 240 are trimmed via an isotropic etching process performed on the semiconductor material layer 224. One of the isotropic etching processes in various embodiments increases the vertical thickness / width of the cavity 228 and reduces the horizontal width of the semiconductor material layer 224. For example... Figure 2C As shown, each cavity 228 has a surface 229. Furthermore, each cavity 228 is disposed between the existing structure of the device (i.e., one of the sidewall spacers 210) and the bulk semiconductor portion of the semiconductor substrate 200.

[0052] The isotropic etching process of operation 110 can be selectively used to remove sufficient material from the semiconductor material layer 224, thereby increasing the size of the cavity 228 and giving it a suitable target thickness T2. For example, in some embodiments, the isotropic etching process of operation 110 is performed such that the cavity 228 increases in size from a first thickness T1 (in the first thickness T2). Figure 2D and Figure 2E (in the middle) increase to the second thickness T2 (in Figure 2F and Figure 2G (In Chinese). As used herein, the term "thickness" refers to the vertical distance between cavities 228 defined by two semiconductor material layers 224. In one or more embodiments, the first thickness T1 of the cavity 228 is in the range of about 5 nm to about 15 nm, and the width W1 of the untrimmed semiconductor material layers 224 is in the range of about 3 nm to about 20 nm.

[0053] In one or more embodiments, after the trimming at operation 110, the thickness of cavity 228 is increased to a second thickness T2 in the range of about 6 nm to about 20 nm. After the trimming at operation 110, the width W2 of semiconductor material layer 224 is in the range of about 3 nm to about 10 nm. Therefore, in one or more embodiments, the trimming increases the thickness of cavity 228 and reduces the width of semiconductor material layer 224.

[0054] The isotropic etching process of operation 110 may include any suitable etching process that is selective for the semiconductor material layer 224. For example, an isotropic etching process available from Applied... Selectra TM The etching chamber undergoes a finishing process. In some instances, the finishing process includes a mixture of nitrogen trifluoride (NF3), nitrogen trifluoride and helium (He), or similar process chemicals.

[0055] In one or more embodiments, at operation 112, mask 245 is removed. The mask can be removed using any suitable technique known to those skilled in the art.

[0056] In one or more embodiments, operation 112 of method 100 represents one or more post-processing operations. The one or more post-processing operations can be any process known to those skilled in the art for completing an hGAA device. Reference Figure 2H and Figure 2I In some embodiments, an oxide layer 252 is formed or grown on the trimmed semiconductor material layer 224. The oxide layer 252 may be any suitable oxide formed by any suitable technique known to those skilled in the art.

[0057] In the illustrated embodiment, a high-k dielectric 254 is formed on an oxide layer 252. The high-k dielectric 254 can be any suitable high-k dielectric material deposited using any suitable deposition technique known to those skilled in the art. In some embodiments, the high-k dielectric 254 comprises hafnium oxide. In some embodiments, a conductive material 256, such as titanium nitride (TiN), tungsten (W), cobalt (Co), aluminum (Al), or the like, is deposited on the high-k dielectric 254. Any suitable deposition process can be used to form the conductive material 256, such as, but not limited to, atomic layer deposition (ALD), to ensure the formation of a layer with a uniform thickness around each doped semiconductor material layer 245.

[0058] In some embodiments, a gate electrode 242 is formed on a substrate 200 and surrounds each trimmed semiconductor material layer 225. The gate electrode 242 may be formed from any suitable gate electrode material known in the art. Any suitable deposition process, such as atomic layer deposition (ALD), is used to deposit the gate electrode material to ensure that the gate electrode 242 is formed around and between each trimmed semiconductor material layer 225. According to embodiments of this disclosure, the resulting device formed using the methods described herein is a horizontal all-around gate device. Some embodiments of this disclosure relate to horizontal all-around gate devices comprising trimmed semiconductor material layers 225 as nanowires or nanoplates in a channel between the source and drain regions.

[0059] One or more embodiments of this disclosure relate to a method of forming a semiconductor device. In one or more embodiments, a method of forming a semiconductor device includes: selectively etching a superlattice structure comprising a plurality of semiconductor material layers and corresponding plurality of release layers arranged in a plurality of stacked pairs to remove each of the semiconductor material layers or each of the release layers to form a plurality of voids in the superlattice structure and a plurality of semiconductor material layers extending between a source region and a drain region; and trimming the plurality of semiconductor material layers to form a trimmed semiconductor material layer.

[0060] Additional embodiments of this disclosure relate to a processing tool 300 for forming a GAA device and the described method, such as... Figure 3 As shown. Various multiprocessing platforms can be utilized, including those available from Applied... of DualACP, GT and Platform and other processing systems. Cluster tool 300 includes at least one central transfer station 314 with multiple sides. Robot 316 is positioned within the central transfer station 314 and configured to move robot blades and wafers to each of the multiple sides.

[0061] The cluster tool 300 includes multiple processing chambers 308, 310, and 312 connected to a central transfer station; these processing chambers are also referred to as processing stations. Each processing chamber provides a separate processing area isolated from adjacent processing stations. The processing chambers can be any suitable chamber, including but not limited to pre-cleaning chambers, deposition chambers, annealing chambers, etching chambers, selective etching chambers, and the like. The specific arrangement of the processing chambers and components may vary depending on the cluster tool and should not be considered as limiting the scope of this disclosure.

[0062] In some embodiments, the clustering tool 300 includes an isotropic etching chamber for selectively etching / trimming the semiconductor material layer 224. In some embodiments, the isotropic etching chamber comprises one or more fluorine-based dry etching chambers. In some embodiments, the clustering tool 300 includes a pre-cleaning chamber connected to a central transport station.

[0063] exist Figure 3 In the illustrated embodiment, the factory interface 318 is connected to the front of the cluster tool 300. The factory interface 318 includes a chamber 302 for loading and unloading onto the front 319 of the factory interface 318.

[0064] The size and shape of the loading chamber and unloading chamber 302 may vary depending on the substrate being processed, for example, in the clustering tool 300. In the illustrated embodiment, the loading chamber and unloading chamber 302 are sized to accommodate a wafer cassette in which multiple wafers are positioned.

[0065] Robot 304 is located within factory interface 318 and can move between loading and unloading chambers 302. Robot 304 is capable of transferring wafers from a cassette in loading chamber 302 to a loading locking chamber 320 via factory interface 318. Robot 304 is also capable of transferring wafers from loading locking chamber 320 to a cassette in unloading chamber 302 via factory interface 318.

[0066] In some embodiments, robot 316 is a multi-armed robot capable of independently moving more than one wafer at a time. Robot 316 is configured to move wafers between chambers surrounding transfer chamber 314. Individual wafers are carried on wafer transfer blades located remotely to the first robotic mechanism.

[0067] System controller 357 communicates with robot 316 and multiple processing chambers 308, 310, and 312. System controller 357 can be any suitable component capable of controlling the processing chambers and robot. For example, system controller 357 can be a computer including central processing unit (CPU) 392, memory 394, input / output 396, suitable circuitry 398, and storage.

[0068] The process can typically be stored as a software routine in the memory of system controller 357, which, when executed by the processor, causes the processing chamber to perform the process of this disclosure. The software routine can also be stored and / or executed by a second processor (not shown) remote from hardware controlled by the processor. Some or all of the methods of this disclosure can also be performed in hardware. Therefore, the process can be implemented in software and executed using a computer system in hardware implementations such as, for example, application-specific integrated circuits or other types of hardware implementations, or in hardware such as a combination of software and hardware. When executed by the processor, the software routine transforms a general-purpose computer into a dedicated computer (controller) that controls the operation of the chamber, thereby performing the process.

[0069] In some embodiments, the system controller 357 is configured to control a selective isotropic etching chamber to selectively etch a semiconductor material layer 224 on a wafer to form a trimmed semiconductor material layer 225 at a temperature ranging from about 20°C to about 300°C, in an atmosphere containing a mixture of nitrogen trifluoride (NF3), nitrogen trifluoride and helium (He) or similar process chemicals, and at a pressure ranging from about 0.05 Torr to about 10 Torr.

[0070] In one or more embodiments, a processing tool includes: a central transport station comprising a robot configured to move a wafer; a plurality of processing stations, each connected to the central transport station and providing a processing area separate from the processing areas of adjacent processing stations, the plurality of processing stations including isotropic etching chambers; and a controller connected to the central transport station and the plurality of processing stations, the controller being configured to activate the robot to move the wafer between the processing stations and to control the processes occurring in each of the processing stations.

[0071] In the context of describing the materials and methods discussed herein (especially in the context of the following claims), unless otherwise indicated herein or clearly contradicted by the context, the use of the terms “a” and “an” and “the” and similar representations is to be construed as covering both the singular and the plural. Unless otherwise indicated herein, references to numerical ranges herein are intended only as a way of individually referring to each individual value falling within that range, and each individual value is incorporated into this specification as if it were individually referenced herein. Unless otherwise indicated herein or clearly contradicted by the context otherwise, all methods described herein may be performed in any suitable order. Unless otherwise claimed, the use of any and all illustrative or exemplary language (e.g., “such as”) provided herein is intended only to better describe the materials and methods and does not constitute a limitation on the scope. No language in this specification should be construed as indicating any unclaimed element essential to the practice of the disclosed materials and methods.

[0072] Throughout this specification, references to "one embodiment," "some embodiments," "one or more embodiments," or "an embodiment" mean that a particular feature, structure, material, or characteristic described in connection with an embodiment is included in at least one embodiment of this disclosure. Therefore, the appearance of phrases such as "in one or more embodiments," "in some embodiments," "in one embodiment," or "in an embodiment" throughout this specification does not necessarily refer to the same embodiment of this disclosure. Furthermore, specific features, structures, materials, or characteristics may be combined in any suitable manner in one or more embodiments.

[0073] Although the disclosure herein has been described with reference to specific embodiments, those skilled in the art will understand that the described embodiments are merely illustrative of the principles and applications of the disclosure. It will be apparent to those skilled in the art that various modifications and variations can be made to the methods and apparatus of this disclosure without departing from the spirit and scope of the disclosure. Therefore, this disclosure may include modifications and variations within the scope of the appended claims and their equivalents.

Claims

1. A method for forming a semiconductor device, the method comprising the following steps: Selective etching is performed on a superlattice structure comprising multiple semiconductor material layers arranged in multiple stacked pairs and corresponding multiple release layers to remove each of the release layers, thereby forming multiple voids in the superlattice structure and the multiple semiconductor material layers extending between the source and drain regions. Pre-clean the multiple semiconductor material layers to remove native oxides and / or residues; and The plurality of semiconductor material layers are trimmed to form a trimmed semiconductor material layer. The step of trimming the plurality of semiconductor material layers includes the following steps: isotropic etching of the semiconductor material layers.

2. The method of claim 1, wherein the trimmed semiconductor material layer has a width in the range of 3 nm to 10 nm.

3. The method of claim 1, further comprising the step of: forming the source region adjacent to a first end of the superlattice structure and the drain region adjacent to a second opposite end of the superlattice structure.

4. The method of claim 1, further comprising the step of: forming the superlattice structure on the top surface of the substrate.

5. The method of claim 1, wherein the step of selectively etching the superlattice structure comprises the steps of: etching the release layer and leaving the semiconductor material layer.

6. The method of claim 1, wherein trimming the plurality of semiconductor material layers increases the width of the plurality of gaps from a first gap width to a second gap width.

7. The method of claim 6, wherein the width of the first gap is in the range of 5 nm to 15 nm.

8. The method of claim 6, wherein the width of the second void is in the range of 6 nm to 20 nm.

9. The method of claim 1, further comprising the step of: forming a mask on a substrate prior to trimming to expose the plurality of semiconductor material layers in a portion of the substrate.

10. The method of claim 9, further comprising the step of: removing the mask after trimming the plurality of semiconductor material layers.

11. The method of claim 1, wherein the semiconductor material layer comprises silicon (Si) and the release layer comprises silicon germanium (SiGe).

12. The method of claim 1, wherein the method is performed in a processing chamber without breaking the vacuum.

13. A horizontally all-around gate device manufactured using the method of claim 1, comprising: Multiple horizontally trimmed semiconductor material layers extending between a source region and a drain region, the source region on a substrate adjacent to a first end of a superlattice structure and the drain region adjacent to a second opposite end of the superlattice structure, the superlattice structure including the multiple horizontally trimmed semiconductor material layers arranged alternately in multiple stacked pairs and corresponding multiple voids. An oxide layer on the horizontally trimmed semiconductor material layer; A high-k dielectric layer on the oxide layer; and The conductive material on the high-k dielectric layer, The plurality of horizontally trimmed semiconductor material layers have a width in the range of 3 nm to 10 nm, and Each of the plurality of voids has a thickness in the range of 6 nm to 20 nm.

14. The device of claim 13, wherein the horizontally trimmed semiconductor material layer comprises silicon (Si).

15. A non-transitory computer-readable medium comprising instructions, when executed by a controller of a processing chamber, to cause the processing chamber to perform the following operations: Selective etching is performed on a superlattice structure comprising multiple semiconductor material layers arranged in multiple stacked pairs and corresponding multiple release layers to remove each of the release layers, thereby forming multiple voids in the superlattice structure and the multiple semiconductor material layers extending between the source and drain regions. Pre-clean the multiple semiconductor material layers to remove native oxides and / or residues; and The plurality of semiconductor material layers are trimmed to form a trimmed semiconductor material layer. The step of trimming the plurality of semiconductor material layers includes the following steps: isotropic etching of the semiconductor material layers.

16. The non-transitory computer-readable medium of claim 15, further comprising, when executed by a controller of the processing chamber, instructions to cause the processing chamber to perform the following further operations: Before finishing, a mask is formed on the substrate to expose multiple semiconductor material layers in a portion of the substrate.

Citation Information

Patent Citations

  • Horizontal gate all around and finfet device isolation

    US20160336405A1

  • Method for fabricating nanowires for horizontal gate all around devices for semiconductor applications

    US20170194430A1