Method for manufacturing a semiconductor device
By locally forming an insulating metal oxide film on the surface of the dielectric film, the problems of increased CET and inability to reduce leakage current in the prior art are solved, and leakage current can be effectively reduced without increasing CET.
Patent Information
- Application Number
- CN202180061683.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-09-15
- Filing Date
- 2021-09-01
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2041-09-01
AI Technical Summary
Existing technologies, when forming insulating metal oxide films, result in an increase in the capacitance equivalent thickness (CET) of the dielectric film and cannot effectively reduce leakage current.
An insulating metal oxide film is locally formed on the surface of the dielectric film. By selectively attaching metal and performing heat treatment, a metal oxide film is formed to reduce leakage current and suppress the increase of CET.
Without increasing the CET of the dielectric film, leakage current is significantly reduced by selectively forming metal oxide films in the periphery of the grain boundaries of the dielectric film, thereby reducing electron leakage paths.
Smart Images

Figure CN116075924B_ABST
Abstract
Description
Technical Field
[0001] This disclosure relates to a method for manufacturing a semiconductor device. Background Technology
[0002] Patent documents 1 and 2 disclose a technique for forming an insulating metal oxide film on a dielectric film that serves as a capacitor insulating film and a gate insulating film between the lower and upper electrodes during the manufacturing process of a semiconductor device, using atomic layer deposition (ALD). The insulating metal oxide film reduces the leakage current of the dielectric film.
[0003] Existing technical documents
[0004] Patent documents
[0005] Patent Document 1: Japanese Patent Application Publication No. 2007-88301
[0006] Patent Document 2: Japanese Patent Application Publication No. 2012-80095 Summary of the Invention
[0007] The problem that the invention aims to solve
[0008] This disclosure provides a technique for reducing leakage current without increasing the capacitance-equivalent thickness (CET) of the dielectric film.
[0009] Solution for solving the problem
[0010] A method for manufacturing a semiconductor device according to one aspect of this disclosure includes: a step of forming a dielectric film on a semiconductor substrate or on a lower electrode formed on a semiconductor substrate; a step of selectively attaching a metal to a predetermined area on the surface of the dielectric film; a step of forming an insulating metal oxide film on the predetermined area on the surface of the dielectric film by heat treatment of the metal; and a step of forming an upper electrode on the dielectric film while the metal oxide film is formed on the predetermined area on the surface of the dielectric film.
[0011] Invention Effects
[0012] According to this disclosure, it can reduce leakage current without increasing the CET of the dielectric film. Attached Figure Description
[0013] Figure 1 This is a diagram illustrating an example of the construction of a semiconductor device according to one embodiment.
[0014] Figure 2This is a flowchart illustrating an example of a method for manufacturing a semiconductor device according to one embodiment.
[0015] Figure 3 This is a cross-sectional view showing an example of the state of the processed object in each step of a method for manufacturing a semiconductor device according to one embodiment.
[0016] Figure 4 This is a cross-sectional view showing an example of the state of the processed object in each step of a method for manufacturing a semiconductor device according to one embodiment.
[0017] Figure 5 This is a cross-sectional view showing an example of the state of the processed object in each step of a method for manufacturing a semiconductor device according to one embodiment.
[0018] Figure 6 This is a cross-sectional view showing an example of the state of the processed object in each step of a method for manufacturing a semiconductor device according to one embodiment.
[0019] Figure 7 This is a diagram illustrating the details of the metal adhesion process in one embodiment.
[0020] Figure 8 This is a graph showing an example of the measurement results of CET and leakage current of a dielectric film.
[0021] Figure 9 This is a diagram illustrating an example of the structure of a semiconductor device according to a modified embodiment. Detailed Implementation
[0022] Hereinafter, various embodiments will be described in detail with reference to the accompanying drawings. It should be noted that the disclosed technology is not limited to the following embodiments.
[0023] In the technique of forming an insulating metal oxide film on a dielectric film by the ALD method, there is room for improvement in reducing leakage current without increasing the CET of the dielectric film.
[0024] Therefore, this disclosure provides a technique for reducing leakage current without increasing the CET of the dielectric film.
[0025] [Structure of a semiconductor device]
[0026] Figure 1 This is a diagram illustrating an example of the construction of a semiconductor device according to one embodiment. Figure 1The semiconductor device 100 shown is a metal-insulator-metal (MIM) semiconductor device. The semiconductor device 100 includes: a semiconductor substrate 101, a lower electrode 203 formed on the semiconductor substrate 101, a dielectric film 102 formed on the lower electrode 203, and an upper electrode 103 formed on the dielectric film 102. In the MIM-structured semiconductor device 100, the dielectric film 102 serves as a capacitor insulating film between the upper electrode 103 and the lower electrode 203. An insulating metal oxide film 104 is locally formed on a defined area of the surface of the dielectric film 102.
[0027] [Semiconductor device manufacturing method]
[0028] Figure 2 This is a flowchart illustrating an example of a method for manufacturing a semiconductor device according to one embodiment. Figures 3-6 This is a cross-sectional view showing an example of the state of the processed object in each step of a method for manufacturing a semiconductor device according to one embodiment.
[0029] First, a semiconductor substrate 101 having a lower electrode 203 formed thereon is provided (step S101). The semiconductor substrate 101 is, for example, a silicon substrate. The lower electrode 203 is, for example, titanium nitride (TiN).
[0030] Next, a dielectric film 102 is formed on the lower electrode 203 (step S102, see below). Figure 3 The dielectric film 102 may contain, for example, hafnium oxide (HfO2) or zirconium oxide (ZrO2).
[0031] Next, metal 104a is selectively attached to a designated area on the surface of dielectric film 102 (step S103, metal attachment process, see reference). Figure 4 Metal 104a includes, for example, aluminum (Al) or a pentavalent transition metal. A pentavalent transition metal includes, for example, niobium (Nb) or tantalum (Ta).
[0032] Here, refer to Figure 7 The details of the metal attachment process in step S103 are explained below. Figure 7 This diagram illustrates the details of the metal adhesion process in one embodiment. The dielectric film 102 includes a crystalline portion C as a crystallized portion and an amorphous material portion α as an uncrystallized portion. An aggregate containing multiple oxygen vacancies Vo is formed at the grain boundaries, which are the boundary surfaces of the crystalline portion C. A portion of the grain boundary is exposed on the surface of the dielectric film 102. In the metal adhesion process, as... Figure 7As shown, metal 104a is selectively attached to the periphery of the grain boundaries exposed on the surface of the dielectric film 102 (hereinafter referred to as the "grain boundary periphery region"). In the metal attachment process, metal 104a is selectively attached to the grain boundary periphery region on the surface of the dielectric film 102 by performing a plating process (e.g., electroplating), which utilizes electrons conducted via grain boundaries present in the dielectric film 102. That is, at the grain boundaries present in the dielectric film 102, an aggregate of oxygen vacancies Vo forms a path for electrons to conduct from the lower electrode 203 to the surface of the dielectric film 102. In the metal attachment process, metal ions in the electrolyte are reduced by utilizing electrons conducted along this path and supplied to the grain boundaries on the surface of the dielectric film 102, thereby causing metal 104a to selectively attach to the grain boundary periphery region on the surface of the dielectric film 102.
[0033] Next, by heat treating the metal 104a, an insulating metal oxide film 104 is formed on a predetermined region (i.e., the grain boundary perimeter region) on the surface of the dielectric film 102 (step S104, refer to...). Figure 5 The metal oxide film 104 is, for example, aluminum oxide (Al2O3), niobium oxide (Nb2O5), or tantalum oxide (Ta2O5). From the viewpoint of properly growing the metal oxide film 104, it is preferable that the process of step S104 is carried out at a temperature, for example, below 300°C.
[0034] In step S104, for example, if the dielectric film 102 is hafnium oxide (HfO2) and the metal oxide film 104 is niobium oxide (Nb2O5), the chemical reactions shown in the following chemical reaction formulas (1) and (2) are carried out.
[0035] [Chemical Formula 1]
[0036]
[0037] [Chemical Formula 2]
[0038]
[0039] According to the chemical reaction formula (1), two Nb atoms of niobium oxide (Nb2O5) enter the Hf atom sites in the hafnium oxide (HfO2) crystal, and four O atoms of niobium oxide enter the O atom sites in the hafnium oxide crystal. In addition, according to the chemical reaction formula (1), two electrons and one O atom remain.
[0040] According to the chemical reaction in chemical formula (2), the remaining two electrons and one O atom enter the oxygen defect Vo at the grain boundary on the surface of hafnium oxide (dielectric film 102). As a result, the oxygen defect Vo, which serves as the electron path near the surface of hafnium oxide (HfO2), disappears, and the periphery of the grain boundary on the surface of hafnium oxide is electrically sealed by the metal oxide film 104. Consequently, the leakage current of the dielectric film 102 can be reduced.
[0041] It should be noted that even when the metal oxide film 104 is tantalum oxide (Ta2O5), the same chemical reaction is presumed to occur, resulting in a reduction in the leakage current of the dielectric film 102. Furthermore, when the metal oxide film 104 is aluminum oxide (Al2O3), the Al-O bonds in aluminum oxide have strong covalent bonding and a large band gap, thus suppressing electron tunneling, which in turn reduces the leakage current of the dielectric film 102.
[0042] Furthermore, in step S104, unlike the prior art where a metal oxide film is formed on the entire surface of the dielectric film 102 using the ALD method, the metal oxide film 104 is selectively formed only in the grain boundary periphery region on the surface of the dielectric film 102. This allows for the suppression of the increase in the CET of the dielectric film 102.
[0043] Next, an upper electrode 103 is formed on the dielectric film 102 (step S105, see reference). Figure 6 The process ends here. The upper electrode 103 is, for example, titanium nitride (TiN).
[0044] [CET and leakage current of dielectric film 102]
[0045] Figure 8 This is a graph showing an example of the measurement results of CET and leakage current of dielectric membrane 102. Figure 8 The results are shown in the case where a titanium nitride (TiN) upper electrode 103 is formed on a zirconium oxide (ZrO2) dielectric film 102.
[0046] Figure 8 Comparative Example 1 shows the result of directly forming the upper electrode 103 on the dielectric film 102 without forming the metal oxide film 104. Figure 8 Example 1 shows the results of the following: under the processing conditions of processing time / current / total charge = 1 min / 3 mA / 0.2 C, metal 104a is attached to the grain boundary periphery region on the surface of dielectric film 102 by plating process to form metal oxide film 104, and then upper electrode 103 is formed. Figure 8Example 2 illustrates the following results: Under processing conditions of processing time / current / total charge = 10 min / 10 mA / 6.7 C, metal 104a is deposited onto the grain boundary periphery of the dielectric film 102 through a plating process to form a metal oxide film 104, and then the upper electrode 103 is formed. In Examples 1 and 2, metal 104a is aluminum (Al), and the metal oxide film 104 is aluminum oxide (Al2O3).
[0047] Depend on Figure 8 It can be seen that when a metal oxide film 104 is formed, compared with the case where a metal oxide film 104 is not formed, the increase in the CET of the dielectric film 102 is suppressed and the leakage current is reduced. That is, according to the semiconductor device manufacturing method of an embodiment in which a metal oxide film 104 is formed in the grain boundary periphery region on the surface of the dielectric film 102 before forming the upper electrode 103, the leakage current can be reduced without increasing the CET of the dielectric film 102. Moreover, from Figure 8 The results show that when the metal oxide film 104 is formed, the CET of the dielectric film 102 is reduced compared to when the metal oxide film 104 is not formed. That is, according to a semiconductor device manufacturing method of an embodiment in which a metal oxide film 104 is formed in the grain boundary periphery region on the surface of the dielectric film 102 before forming the upper electrode 103, the CET of the dielectric film 102 can also be reduced. The reason for the reduced CET of the dielectric film 102 can be attributed to the fact that the surface of the dielectric film 102 (ZrO2 film) is formed with oxide-based irregularities due to the plating process, and the capacitance increases with the increase of the effective surface area of the dielectric film 102.
[0048] [Variation Example]
[0049] In the above embodiments, a semiconductor device with a MIM structure was described as an example, but the disclosed technology can also be applied to semiconductor devices with a metal-oxide-semiconductor (MOS) structure. Figure 9 This is a diagram illustrating an example of the structure of a semiconductor device 100A, a modified embodiment of one implementation. Figure 9The semiconductor device 100A shown is a MOS-structured semiconductor device. The semiconductor device 100A includes a semiconductor substrate 101, a dielectric film 102 formed on the semiconductor substrate 101, and an upper electrode 103 formed on the dielectric film 102. In the MOS-structured semiconductor device 100A, the dielectric film 102 serves as a gate insulating film. An insulating metal oxide film 104 is locally formed on a defined region (i.e., the grain boundary perimeter region) on the surface of the dielectric film 102. In the MOS-structured semiconductor device 100A, the upper electrode 103 serves as the gate electrode.
[0050] Regarding the manufacturing method of the modified semiconductor device 100A, in step S101 of one embodiment, a semiconductor substrate 101 is provided. Furthermore, regarding the manufacturing method of the semiconductor device 100A, in step S102 of one embodiment, a dielectric film 102 is formed on the semiconductor substrate 101. In the manufacturing method of the modified semiconductor device 100A, the processes from the attachment of the metal 104a (step S103) to the formation of the upper electrode 103 (step S105) are the same as in one embodiment.
[0051] Thus, in the MOS-structured semiconductor device 100A, a metal oxide film 104 is formed on the grain boundary periphery region of the dielectric film 102 before the upper electrode 103 is formed. As a result, leakage current can be reduced without increasing the CET of the dielectric film 102.
[0052] [Effect]
[0053] The method for manufacturing a semiconductor device according to the above embodiments includes: a step of forming a dielectric film on a semiconductor substrate or on a lower electrode formed on the semiconductor substrate; a step of selectively attaching a metal to a predetermined area on the surface of the dielectric film; a step of forming an insulating metal oxide film on the predetermined area on the surface of the dielectric film by heat treatment of the metal; and a step of forming an upper electrode on the dielectric film while the metal oxide film is formed on the predetermined area on the surface of the dielectric film. Therefore, according to the embodiments, leakage current can be reduced without increasing the CET of the dielectric film.
[0054] Furthermore, in one embodiment, during the metal attachment process, the metal may be selectively attached to the region surrounding the grain boundaries exposed on the surface of the dielectric film. Therefore, according to this embodiment, leakage current on the surface of the dielectric film can be suppressed.
[0055] Furthermore, in one embodiment, during the metal attachment process, a plating process can be performed to selectively attach the metal to the periphery of the grain boundaries exposed on the surface of the dielectric film. This plating process utilizes electrons conducted via the grain boundaries present in the dielectric film. Therefore, according to the embodiment, it is possible to attach the metal with good precision only to the periphery of the grain boundaries exposed on the surface of the dielectric film.
[0056] Furthermore, in embodiments, the metal may comprise aluminum (Al) or a pentavalent transition metal. Additionally, in embodiments, the pentavalent transition metal may comprise niobium (Nb) or tantalum (Ta). Furthermore, in embodiments, the dielectric film may comprise hafnium oxide (HfO2) or zirconium oxide (ZrO2). Therefore, according to embodiments, using an insulating metal oxide film formed of aluminum (Al) or a pentavalent transition metal can reduce leakage current without increasing the CET of the dielectric film.
[0057] Furthermore, in one embodiment, the process of forming the metal oxide film may be performed at a temperature below 300°C. Therefore, according to the embodiment, the metal oxide film can be appropriately grown on the surface of the dielectric film.
[0058] [other]
[0059] It should be noted that the technology disclosed in this application is not limited to the above-described embodiments, and various modifications can be made within the scope of its spirit.
[0060] For example, in the above embodiment, a step of annealing the metal oxide film in an inert atmosphere may be included between the step of forming the metal oxide film (step S104) and the step of forming the upper electrode (step S105). Furthermore, in this case, it is preferable that the step of annealing the metal oxide film is performed at a temperature below 500°C. This allows the metal oxide film to grow appropriately up to the grain boundaries present in the dielectric film, and as a result, leakage current can be further reduced.
[0061] Furthermore, in the above embodiment, a step of annealing the dielectric film under an inert atmosphere may be included between the step of forming the dielectric film (step S102) and the step of attaching the metal (step S103). In this case, it is preferable that the annealing step of the dielectric film is performed at a temperature below 500°C. This allows the dielectric film to be appropriately crystallized.
[0062] It should be considered that the various embodiments disclosed herein are illustrative in all respects, and not restrictive. The above embodiments may be omitted, substituted, or modified in various forms without departing from the claims and their spirit.
Claims
1. A method for manufacturing a semiconductor device, comprising: The process of forming a dielectric film on a semiconductor substrate or on a lower electrode formed on a semiconductor substrate; A process for selectively attaching metal to a specified area on the surface of the dielectric film; The process of forming an insulating metal oxide film in a specified area on the surface of the dielectric film by heat treatment of the metal; as well as The process of forming an upper electrode on the dielectric film while the metal oxide film is formed in a designated area on the surface of the dielectric film. In the process of attaching the metal, the metal is selectively attached to the periphery of the grain boundaries exposed on the surface of the dielectric film by the reduction reaction of metal ions in the electrolyte.
2. The method for manufacturing a semiconductor device according to claim 1, wherein, The process of attaching the metal is performed using electrons conducted via grain boundaries exposed on the surface of the dielectric film.
3. The method for manufacturing a semiconductor device according to claim 2, wherein, In the process of attaching the metal, a plating process is performed to selectively attach the metal to the periphery of the grain boundaries exposed on the surface of the dielectric film. This plating process utilizes electrons conducted via the grain boundaries present in the dielectric film.
4. The method for manufacturing a semiconductor device according to any one of claims 1 to 3, wherein, The metal contains aluminum, i.e., Al, or a pentavalent transition metal.
5. The method for manufacturing a semiconductor device according to claim 4, wherein, The pentavalent transition metals include niobium (Nb) or tantalum (Ta).
6. The method for manufacturing a semiconductor device according to claim 1, wherein, The dielectric film contains hafnium oxide (HfO2) or zirconium oxide (ZrO2).
7. The method for manufacturing a semiconductor device according to claim 1, wherein, The process of forming the metal oxide film is carried out at a temperature below 300°C.
8. The method for manufacturing a semiconductor device according to claim 1, wherein, Between the process of forming the metal oxide film and the process of forming the upper electrode, there is also a process of annealing the metal oxide film in an inert atmosphere.
9. The method for manufacturing a semiconductor device according to claim 8, wherein, The annealing process of the metal oxide film is carried out at a temperature below 500°C.
10. A method for manufacturing a semiconductor device, comprising: The process of forming a dielectric film on a semiconductor substrate or on a lower electrode formed on a semiconductor substrate; A process for selectively attaching metal to a specified area on the surface of the dielectric film; The process of forming an insulating metal oxide film in a specified area on the surface of the dielectric film by heat treatment of the metal; as well as The process of forming an upper electrode on the dielectric film while the metal oxide film is formed in a designated area on the surface of the dielectric film. In the process of attaching the metal, the metal is selectively attached to the periphery of the grain boundaries exposed on the surface of the dielectric film.
11. A method for manufacturing a semiconductor device, comprising: The process of forming a dielectric film on a semiconductor substrate or on a lower electrode formed on a semiconductor substrate; A process for selectively attaching metal to a specified area on the surface of the dielectric film; The process of forming an insulating metal oxide film in a specified area on the surface of the dielectric film by heat treatment of the metal; as well as The process of forming an upper electrode on the dielectric film while the metal oxide film is formed in a designated area on the surface of the dielectric film. In the process of attaching the metal, a plating process is performed, which utilizes electrons conducted via grain boundaries present in the dielectric film.
Citation Information
Patent Citations
Semiconductor device and method for manufacturing the same
JP2007088301A
Semiconductor device and manufacturing method therefor
JP2012080095A
Nonvolatile semiconductor memory element having excellent charge retention properties and process for producing the same
CN101263595A
Manufacturing method for metal oxide film and display device comprising the metal oxide film
CN109666920A
Semiconductor device and manufacture thereof
JP1996017939A