一种真空下引连铸高纯无氧铜线材的制备方法

CN116206818BActive Publication Date: 2026-07-17SIRUI ADVANCED COPPER ALLOY TECH (FUFENG) CO LTD

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
SIRUI ADVANCED COPPER ALLOY TECH (FUFENG) CO LTD
Filing Date
2023-03-07
Publication Date
2026-07-17

AI Technical Summary

Technical Problem

Existing high-conductivity oxygen-free copper wires are prone to introducing impurities during non-vacuum smelting, resulting in high oxygen content, which affects conductivity and mechanical properties. Furthermore, the process is complex and it is difficult to control the uniformity and stability of the material.

Method used

The process employs vacuum casting, which includes vacuum melting, stepped heating, continuous casting, multi-pass drawing, and annealing. Combined with the use of grain refiners and conductive agents, it ensures the purity and uniformity of the material.

Benefits of technology

It achieves an oxygen content of less than 3 ppm, an electrical conductivity of over 100% IACS, uniform material composition, stable performance, simplified process flow, avoids the problem of coarse grains caused by forging, and improves the oxidation resistance and conductivity of the material.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116206818B_ABST
    Figure CN116206818B_ABST
Patent Text Reader

Abstract

本发明公开了一种真空下引连铸高纯无氧铜线材的制备方法,包括以下步骤:S1、真空熔炼;S2、下引连铸;S3、取样检测及表面处理;S4、一次拉拔;S5、退火处理;S6、二次拉拔;S7、盘圆及检测;本发明制备方法通过在真空环境下下引连铸获得无氧铜线材,并通过后续拉拔工序得到性能优异的高纯度、高导电线材。