Circuit board

By combining CO₂ and UV lasers to form a vertical inner cavity, and using RCC insulation and glass fiber prepreg, the problem of space waste caused by the large tilt angle of the inner wall of the conventional circuit board cavity is solved, thereby improving circuit integration and reliability, and reducing the size and cost of the circuit board.

CN116250378BActive Publication Date: 2026-11-20LG INNOTEK CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202180053271.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2020-06-29
Filing Date
2021-06-29
Publication Date
2026-11-20
Estimated Expiration
2041-06-29

AI Technical Summary

Technical Problem

Conventional circuit boards have a large tilt angle on the inner wall of the cavity, which increases the space required, reduces the circuit integration, and increases the size of the circuit board.

Method used

A cavity is formed by combining CO₂ and UV lasers, using a 1-1 metal layer as a seed layer. The inner wall of the cavity is made nearly vertical through secondary processing, reducing the need for additional stop layers. RCC insulation and glass fiber prepreg are used to improve reliability and integration.

Benefits of technology

Reduce the space occupied by cavities, improve circuit integration, reduce manufacturing costs, enhance structural reliability and product satisfaction, and reduce the overall size of the circuit board.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116250378B_ABST
    Figure CN116250378B_ABST
Patent Text Reader

Abstract

A circuit board according to an embodiment includes: a first insulating layer; a first circuit pattern disposed on one surface of the first insulating layer and including a pad; a second insulating layer disposed on one surface of the first insulating layer and including a cavity exposing the pad, wherein the first circuit pattern includes a 1-1 metal layer disposed on one surface of the first insulating layer and a 1-2 metal layer disposed on one surface of the 1-1 metal layer, wherein an area of the 1-1 metal layer is greater than an area of the 1-2 metal layer, and at least a portion of a side surface of the 1-1 metal layer is exposed through the cavity.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The embodiments relate to a circuit board and a package board including the circuit board. Background Technology

[0002] A circuit board has a structure that defines the mounting position of each component and prints and fixes the circuit patterns connecting the components on the surface of the flat plate, so as to densely mount various components on the flat plate. Such a circuit board can have an embedded structure with embedded components.

[0003] In recent years, in order to achieve miniaturization and multifunctionality of electronic components, multilayer circuit boards with high-density integration have been used.

[0004] Typically, conventional embedded circuit boards use drills to create cavities for embedding components, use auxiliary materials such as release films to mount components, or use sandblasting to create cavities for embedding components.

[0005] However, in the cavities included in conventional circuit boards, the inclination angle of the inner walls is formed to be 150° or more relative to the bottom surface of the cavity. Therefore, considering the inclination angle of the inner walls, the space required to form the cavity relatively increases in order to provide mounting space for components within the cavity. Consequently, conventional circuit boards suffer from reduced circuit integration, and the overall volume of the circuit board increases with the increase in the space required to form the cavity. Summary of the Invention

[0006] Technical issues

[0007] The embodiments relate to a circuit board, a packaging substrate, and a method for manufacturing the same, which can improve the tilt angle of the inner wall of a cavity.

[0008] In addition, this embodiment aims to provide a circuit board, a packaging substrate, and a method for manufacturing the circuit board, which can form a cavity with a desired depth in a desired area during the cavity forming process without additionally forming the required stop layer on the bottom surface of the cavity.

[0009] The technical problems to be solved by the proposed embodiments are not limited to the above-mentioned technical problems. Other technical problems not mentioned can be clearly understood by those skilled in the art to which the embodiments proposed in the following description pertain.

[0010] Technical solution

[0011] The circuit board according to an embodiment includes: a first insulating layer; a first circuit pattern disposed on one surface of the first insulating layer and including pads; and a second insulating layer disposed on one surface of the first insulating layer and including cavities exposing the pads, wherein the first circuit pattern includes a 1-1 metal layer disposed on one surface of the first insulating layer and a 1-2 metal layer disposed on one surface of the 1-1 metal layer, the area of ​​the 1-1 metal layer is larger than the area of ​​the 1-2 metal layer, and at least a portion of the side surface of the 1-1 metal layer is exposed through the cavity.

[0012] Additionally, the 1-1 metal layer includes a first portion that overlaps with the 1-1 metal layer in the vertical direction and a second portion other than the first portion, and the side surface of the second portion is exposed through a cavity.

[0013] Additionally, the second portion of the 1-1 metal layer has a closed-loop shape surrounding the outer side of the cavity and is disposed between the first insulating layer and the second insulating layer.

[0014] In addition, the 1-1 metal layer is the seed layer of the 1-2 metal layer.

[0015] In addition, the upper surface of the first part of the 1-1 metal layer is in direct contact with the lower surface of the 1-2 metal layer, and the upper surface of the second part of the 1-1 metal layer is in direct contact with the second insulating layer.

[0016] In addition, the second part of the 1-1 metal layer is spaced apart from the 1-2 metal layer by a predetermined interval.

[0017] In addition, the first circuit pattern includes a 1-1 circuit pattern disposed in a region adjacent to the cavity and a 1-2 circuit pattern other than the 1-1 circuit pattern, wherein the 1-1 metal layer of the 1-2 circuit pattern has the same area as the 1-2 metal layer of the 1-2 circuit pattern, and the area of ​​the 1-1 metal layer of the 1-1 circuit pattern is larger than the area of ​​the 1-2 metal layer of the 1-1 circuit pattern.

[0018] Additionally, the 1-1 metal layer of the 1-1 circuit pattern includes a first portion that overlaps with the 1-2 metal layer of the 1-1 circuit pattern in the vertical direction and a second portion other than the first portion, and the second portion of the 1-1 metal layer of the 1-1 circuit pattern surrounds the outside of the cavity and is disposed between the first insulating layer and the second insulating layer.

[0019] In addition, the second insulating layer includes insulating layer 2-1 and insulating layer 2-2, and the cavity passes through insulating layer 2-1 and insulating layer 2-2 together.

[0020] Additionally, the second insulating layer includes an insulating layer 2-1 and an insulating layer 2-2, and includes a second circuit pattern disposed between the insulating layers 2-1 and 2-2, wherein a cavity is formed in the insulating layer 2-1 and a second cavity is formed in the insulating layer 2-2 and has a different size from the first cavity, at least a portion of the side surface of the 1-1 metal layer is exposed through the first cavity, the second circuit pattern includes a 2-1 metal layer disposed on one surface of the insulating layer 2-1 and a 2-2 metal layer disposed on one surface of the 2-1 metal layer, the area of ​​the 2-1 metal layer is larger than the area of ​​the 2-2 metal layer, and at least a portion of the side surface of the 2-1 metal layer is exposed through the second cavity.

[0021] In addition, the second insulating layer has a thickness ranging from 5 μm to 20 μm.

[0022] In addition, the second insulating layer includes resin-coated copper (RCC).

[0023] Meanwhile, the packaging substrate according to the embodiment includes: a first insulating layer; a first circuit pattern disposed on one surface of the first insulating layer and including pads; a second insulating layer disposed on one surface of the first insulating layer and including cavities exposing the pads; a connection portion disposed on the pads; and an electronic component disposed on the connection portion, wherein the first circuit pattern includes a 1-1 metal layer disposed on one surface of the first insulating layer and a 1-2 metal layer disposed on one surface of the 1-1 metal layer, the area of ​​the 1-1 metal layer is larger than the area of ​​the 1-2 metal layer, the 1-1 metal layer includes a first portion overlapping the 1-1 metal layer in the vertical direction and a second portion other than the first portion, and the side surface of the second portion is exposed through the cavity.

[0024] Additionally, the second portion of the 1-1 metal layer has a closed-loop shape surrounding the outer side of the cavity and is disposed between the first insulating layer and the second insulating layer.

[0025] In addition, the first circuit pattern includes a 1-1 circuit pattern disposed in a region adjacent to the cavity and a 1-2 circuit pattern other than the 1-1 circuit pattern, wherein the 1-1 metal layer of the 1-2 circuit pattern has the same area as the 1-2 metal layer of the 1-2 circuit pattern, and the area of ​​the 1-1 metal layer of the 1-1 circuit pattern is larger than the area of ​​the 1-2 metal layer of the 1-1 circuit pattern.

[0026] Additionally, the 1-1 metal layer of the 1-1 circuit pattern includes a first portion that overlaps with the 1-2 metal layer of the 1-1 circuit pattern in the vertical direction and a second portion other than the first portion, and the second portion of the 1-1 metal layer of the 1-1 circuit pattern surrounds the outside of the cavity and is disposed between the first insulating layer and the second insulating layer.

[0027] Additionally, the second insulating layer comprises a resin-coated copper foil (RCC) having a thickness ranging from 5 μm to 20 μm.

[0028] Additionally, the circuit board according to the embodiment includes: a first insulating layer; a first circuit pattern disposed on one surface of the first insulating layer and including pads; a second insulating layer disposed on one surface of the first insulating layer and including cavities exposing the pads, wherein the inner wall of the cavity has an angle of inclination ranging from 90.1 degrees to 100 degrees relative to the upper surface of the first insulating layer, the second insulating layer including a prepreg, wherein glass fibers are disposed in the resin, and the glass fibers of the second insulating layer do not protrude into the cavity.

[0029] In addition, the vertical cross-section of the cavity has a rectangular or square shape.

[0030] In addition, the horizontal cross-section of the cavity includes curved surfaces.

[0031] In addition, the horizontal cross-section of the cavity includes an edge portion with a predetermined curvature.

[0032] In addition, the curvature of the edge portion of the cavity corresponds to the curvature of a circle in the range of 20μm to 80μm.

[0033] The circuit board according to an embodiment includes: a first insulating layer; and a second insulating layer disposed on the first insulating layer and including a cavity, wherein the cavity is formed through the second insulating layer, and the inner wall of the cavity contacts the upper surface of the first insulating layer and includes a first portion having a first tilt angle, a second portion extending from the first portion and having a second tilt angle different from the first tilt angle, and a third portion extending from the second portion and having a third tilt angle different from the second tilt angle.

[0034] The first tilt angle is less than the second tilt angle and the third tilt angle, the second tilt angle is greater than the first tilt angle and the third tilt angle, and the third tilt angle is greater than the first tilt angle and less than the second tilt angle.

[0035] The first tilt angle ranges from 89 to 91 degrees, the second tilt angle ranges from 130 to 160 degrees, and the third tilt angle ranges from 92 to 130 degrees.

[0036] In addition, the cavity includes a first inflection point located between the first and second portions of the inner wall and a second inflection point located between the second and third portions of the inner wall.

[0037] Additionally, the circuit board includes pads disposed on the upper surface of the first insulating layer and exposed through a cavity, wherein a second inflection point is configured to be below the upper surface of the pads.

[0038] In addition, the pad includes a first metal layer disposed on the upper surface of the first insulating layer and a second metal layer disposed on the upper surface of the first metal layer, and the first inflection point has the same height as the first metal layer.

[0039] In addition, the thickness of the second insulating layer ranges from 5 μm to 20 μm.

[0040] In addition, the second insulating layer includes resin-coated copper foil (RCC).

[0041] In addition, the surface roughness of the first part of the inner wall of the cavity is different from the surface roughness of the second or third part of the inner wall of the cavity.

[0042] Beneficial effects

[0043] An embodiment may include a first circuit pattern disposed on the upper surface of a first insulating layer. The first circuit pattern may include a 1-1 metal layer as a seed layer and a 1-2 metal layer disposed on the 1-1 metal layer as a plating layer. Furthermore, in an embodiment, the 1-1 metal layer, serving as the seed layer of the 1-2 metal layer, acts as a stop layer for the cavity C to be formed in the second insulating layer. Therefore, in an embodiment, the area of ​​the 1-1 metal layer may be larger than the area of ​​the 1-2 metal layer. Additionally, the 1-1 metal layer in the embodiment may include a first portion overlapping the 1-2 metal layer in the vertical direction and a second portion not overlapping the 1-2 metal layer. Furthermore, the side surface of the second portion of the 1-1 metal layer may be exposed through the cavity C formed in the second insulating layer. Additionally, the second portion of the 1-1 metal layer may surround the outside of the cavity C and may be disposed between the first and second insulating layers.

[0044] Therefore, in this embodiment, there is no need to form an additional stop layer in the second insulating layer required for forming the cavity using a laser process, thereby reducing manufacturing costs and simplifying the manufacturing process.

[0045] Furthermore, in this embodiment, the cavity is formed through two processing steps. For example, in this embodiment, a preliminary processing is performed using a carbon dioxide (CO2) laser and a secondary processing is performed using an ultraviolet (UV) laser to form the cavity. That is, when the cavity is formed by the CO2 laser, stepped steps are created on the inner wall of the cavity to correspond to the movement interval of the laser source during laser processing. Therefore, in this embodiment, the cavity formed by the CO2 laser can be further processed using an ultraviolet (UV) laser. Therefore, the inner wall of the cavity in this embodiment can be substantially perpendicular to the bottom surface of the cavity or the surface of the insulating layer. For example, the inner wall of the cavity can have a tilt angle of 90.01° to 100° relative to the bottom surface of the cavity or the surface of the insulating layer. For example, the inner wall of the cavity can have a tilt angle of 90.1° to 95° relative to the bottom surface of the cavity or the surface of the insulating layer. For example, the inner wall of the cavity can have a tilt angle of 91° to 93° relative to the bottom surface of the cavity or the surface of the insulating layer. Therefore, the vertical cross-sectional shape of the cavity in the embodiment can be close to that of a rectangle or a square. Thus, in the embodiment, the space occupied by the cavity in the insulating layer can be reduced, thereby improving the integration density of the circuit.

[0046] In other words, the width of the lower region of cavity C can be determined such that the size of cavity C corresponds to the size of the electronic component to be housed therein. In this case, in the comparative example, the width of the upper region of cavity C is greater than the width of the lower region of cavity C, and space waste occurs as much as the space corresponding to the width difference between the upper and lower regions. For example, when using a carbon dioxide (CO2) laser as in the comparative example, the tilt angle of the inner wall of the cavity is 110° or more. Furthermore, in the comparative example, due to the tilt angle of the inner wall of the cavity, the size of the cavity may be significantly larger than the size of the electronic component. Alternatively, in the embodiment, by making the tilt angle of the inner wall of the cavity close to a right angle, the size of the cavity can be reduced, thus solving the problem of space waste.

[0047] Furthermore, at least a portion of the cavity C in the embodiments may include rounded corners. For example, the shape of the cavity may include rounded corners. For example, at least a portion of the cavity C in the embodiments may have a curved surface. For example, the cavity C in the embodiments may have a shape in which the edge portions have curved surfaces. Therefore, in the embodiments, problems that may arise due to the edge portions of the cavity having vertical straight lines can be solved. For example, when the edge portions of the cavity have vertical straight lines, stress concentrates at the edge portions, and structural reliability problems such as cavity collapse can be solved. On the other hand, in the embodiments, by making the edge portions of the cavity include curved surfaces, structural reliability problems can be solved, thereby improving product satisfaction.

[0048] Additionally, in this embodiment, the insulating layer forming the cavity can be formed from a prepreg. The prepreg can include glass fibers in the resin to ensure rigidity. Furthermore, during the process of forming cavity C, a portion of the glass fibers may be exposed to the outside through cavity C. Moreover, various reliability issues may arise when the glass fibers are exposed through cavity C. For example, the flatness of electronic components disposed in cavity C may be affected by the glass fibers. For example, electronic components disposed in cavity C may experience electrical short circuits due to the glass fibers. Therefore, in this embodiment, after performing preliminary cavity processing using a carbon dioxide (CO2) laser, a secondary cavity processing is performed using an ultraviolet (UV) laser. In this case, the UV laser can remove the glass fibers exposed through the pre-processed cavity, while the inclination angle of the inner wall of cavity C is almost vertical. That is, in this embodiment, additional cavity processing using an ultraviolet (UV) laser is performed to improve the reliability of cavity C. In this case, the UV laser can remove any glass fibers that may be exposed through the cavity. Therefore, this embodiment can improve the structural reliability of the cavity, and thus improve the reliability of the product.

[0049] Furthermore, the circuit board of the embodiment includes a first insulating layer and a second insulating layer disposed on the first insulating layer. A cavity is formed in the second insulating layer. In this case, the inner wall of the cavity includes a first portion extending from the upper surface of the first insulating layer and having a first tilt angle, a second portion having a second tilt angle, and a third portion having a third tilt angle. In this case, the first tilt angle, the second tilt angle, and the third tilt angle are different from each other. For example, a first bend is formed between the first portion and the second portion of the inner wall of the cavity, and a second bend is formed between the second portion and the third portion. In addition, the first tilt angle of the first portion may be smaller than the second tilt angle of the second portion. In addition, the second tilt angle of the second portion may be larger than the third tilt angle of the third portion. In addition, the third tilt angle of the third portion may be larger than the first tilt angle of the first portion and smaller than the second tilt angle of the second portion. In the above embodiment, the tilt angles of the first portion and the third portion can be formed to be smaller than the tilt angles of the comparative example, therefore, compared with the comparative example, the space required to form the cavity can be minimized. Furthermore, in the embodiment, the integration density of the circuit can be improved within the same space. Furthermore, compared to the comparative example, in this embodiment, the average tilt angle of the inner wall of the cavity can be reduced. Therefore, compared to the comparative example, more circuits can be formed in the same area, thus reducing the overall volume of the circuit board.

[0050] Additionally, the packaging substrate in this embodiment includes a molded layer disposed within a cavity. In this case, the first, second, and third portions of the inner wall of the cavity are configured to contact each other. Furthermore, the first, second, and third portions of the inner wall of the cavity may have different tilt angles based on a first bend and a second bend, rather than a single tilt angle. The cavity structure of the above embodiment can increase the surface area in contact with the molded layer, thus improving the adhesion between the molded layer and the circuit board.

[0051] Additionally, in this embodiment, a mask pattern is used to form the cavity. In this case, the mask pattern includes a first mask pattern for determining the cavity depth in the lower region of the cavity and a second mask pattern configured to define the upper width of the cavity around its periphery in the upper region of the cavity. In this case, in the comparative example, separate metal layers are used to form the first and second mask patterns. Alternatively, in this embodiment, a seed layer for forming a circuit pattern can be used as both the first and second mask patterns. In this case, at least a portion of the first and second mask patterns overlaps in the vertical direction. That is, in the comparative example, the first and second mask patterns are configured not to overlap in the vertical direction. Therefore, in the comparative example, due to process deviations during laser processing, laser processing is performed on the area outside the second mask pattern, potentially resulting in a portion of the first insulating layer being processed. Alternatively, in this embodiment, as described above, reliability can be improved by precisely processing the cavity in the cavity processing region by partially overlapping the first and second mask patterns. Attached Figure Description

[0052] Figure 1 This is a view showing a circuit board according to the first embodiment.

[0053] Figure 2 It is shown Figure 1 A partial floor plan.

[0054] Figure 3 This is a view showing the packaging substrate according to the first embodiment.

[0055] Figure 4 This is a view showing the packaging substrate according to the second embodiment.

[0056] Figures 5 to 10 It is shown in the order of the processes. Figure 1 A view showing the manufacturing method of the circuit board.

[0057] Figures 11 to 13 It is shown Figure 1 A view of a modified example of a circuit board.

[0058] Figure 14 This is a view showing a circuit board according to the second embodiment.

[0059] Figure 15 yes Figure 14 A partial plan view of the circuit board configuration.

[0060] Figures 16 to 22 It is shown in the order of the processes. Figure 14 A view showing the manufacturing method of the circuit board.

[0061] Figure 23A and Figure 23B This is a view specifically illustrating the structure of the cavity according to the third embodiment.

[0062] Figure 24 This is a view used to illustrate the method of processing a cavity according to the third embodiment.

[0063] Figure 25 This is a view used to illustrate the machining method of the cavity according to the comparative example. Detailed Implementation

[0064] In the following, embodiments of the present invention will be described in detail with reference to the accompanying drawings.

[0065] However, the spirit and scope of the embodiments are not limited to the portion of the described embodiments, and may be implemented in various other forms, and one or more elements of the embodiments may be selectively combined and substituted within the spirit and scope of the invention.

[0066] Furthermore, unless otherwise explicitly defined and described, the terms (including technical and scientific terms) used in the embodiments of the present invention may be interpreted as having the same meaning as commonly understood by one of ordinary skill in the art to which this invention pertains, and terms defined, for example, in common dictionaries may be interpreted as having a meaning consistent with their meaning in the relevant technical context. Additionally, the terminology used in the embodiments of the present invention is for descriptive purposes and is not intended to limit the invention.

[0067] In this specification, unless otherwise specified in the phrase, the singular form may also include the plural form, and when describing "at least one (or more) of A (and), B and C", it may include at least one of all combinations that can be combined among A, B and C. Additionally, when describing elements of embodiments of the invention, terms such as first, second, A, B, (a) and (b) may be used.

[0068] These terms are used only to distinguish an element from other elements, and they are not limited to the nature, order, or sequence of elements. Furthermore, when an element is described as "connected" or "combined" to another element, it can include not only cases where the element is directly "connected" or "combined" to other elements, but also cases where the element is "connected" or "combined" to another element through which the element is connected or "combined" with other elements.

[0069] Furthermore, when described as being formed or disposed "above" or "below" the elements, "above" or "below" can include not only the case where two elements are directly connected to each other, but also the case where one or more other elements are formed or disposed between the two elements. Additionally, when expressed as "above" or "below," it can be based on an element including not only the upward direction but also the downward direction.

[0070] In the following, embodiments of the present invention will be described in detail with reference to the accompanying drawings.

[0071] Figure 1 This is a view showing a circuit board according to the first embodiment. Figure 2 It is shown Figure 1 A partial floor plan.

[0072] Reference Figure 1 According to the first embodiment, the circuit board 100 includes a first insulating layer 110, a second insulating layer 120, a third insulating layer 130, circuit patterns 140, 150, 160 and 170, vias V1, V2 and V3, and protective layers 180 and 185.

[0073] The first insulating layer 110 may be an insulating layer disposed at the center of the circuit board 100.

[0074] The second insulating layer 120 is disposed on the first insulating layer 110.

[0075] In addition, the third insulating layer 130 is disposed below the first insulating layer 110.

[0076] In this case, the accompanying drawings show that the first insulating layer 110 is disposed in the middle layer of the entire stacked structure of the circuit board 100, but the embodiment is not limited to this. That is, in the entire stacked structure of the circuit board 100, the first insulating layer 110 may be disposed in a position biased upward, or conversely, it may be disposed in a position biased downward.

[0077] Here, refer to Figure 1The second insulating layer 120 can be disposed on the first insulating layer 110. The second insulating layer 120 can be composed of a single layer. However, the embodiments are not limited to this. For example, the second insulating layer 120 can have a multilayer structure. However, in this embodiment, a cavity C can be formed in the second insulating layer 120. Furthermore, when the second insulating layer 120 has a multilayer structure, Figure 1 The second insulating layer shown in the first layer can represent an insulating layer with a cavity C.

[0078] Additionally, a third insulating layer 130 is disposed below the first insulating layer 110. In this case, the third insulating layer 130 may be composed of a single layer. However, the embodiments are not limited to this. For example, the third insulating layer 130 may have a multilayer structure.

[0079] Additionally, the accompanying drawings show that the circuit board 100 has a three-layer structure based on multiple insulating layers, but the embodiments are not limited thereto. For example, depending on the number of insulating layers, the circuit board 100 may have fewer than three layers or alternatively may have more than three layers.

[0080] The first insulating layer 110, the second insulating layer 120, and the third insulating layer 130 are substrates on which circuits capable of changing wiring are formed, and may include all printed circuit boards, wiring boards, and insulating boards made of insulating materials capable of forming circuit patterns on their surfaces.

[0081] For example, the first insulating layer 110 can be rigid or flexible. For example, the first insulating layer 110 can include glass or plastic. In detail, the first insulating layer 110 can include chemically tempered / semi-tempered glass (e.g., soda-lime glass or aluminosilicate glass, etc.), tempered or flexible plastics (e.g., polyimide (PI), polyethylene terephthalate (PET), polypropylene glycol (PPG), and polycarbonate (PC)), etc., or sapphire.

[0082] Additionally, the first insulating layer 110 may include an optically isotropic film. For example, the first insulating layer 110 may include cyclic olefin copolymer (COC), cyclic olefin polymer (COP), optically isotropic polycarbonate (PC), optically isotropic polymethyl methacrylate (PMMA), etc.

[0083] Furthermore, the insulating layer 110 can be partially curved while having a curved surface. That is, the insulating layer 110 can be partially planar and can be partially curved while having a curved surface. Specifically, the ends of the insulating layer 110 can be bent while having a curved surface, or bent or folded while having a surface with random curvature.

[0084] In addition, the first insulating layer 110 can be a flexible substrate with flexible properties. Furthermore, the first insulating layer 110 can be a bent or folded substrate.

[0085] Meanwhile, the second insulating layer 120 and the third insulating layer 130 can be made of resin-coated copper foil (RCC).

[0086] In other words, when each of the second insulating layer 120 and the third insulating layer 130 is composed of a single layer, each of the single-layer second insulating layer 120 and the third insulating layer 130 can be composed of RCC. Furthermore, when each of the second insulating layer 120 and the third insulating layer 130 has a multilayer structure, each layer of the multilayer second insulating layer 120 and each layer of the multilayer third insulating layer 130 can be composed of RCC.

[0087] Therefore, each of the second insulating layer 120 and the third insulating layer 130 can have a thickness of 5 μm to 20 μm. For example, each of the second insulating layer 120 and the third insulating layer 130 can have a thickness of 6 μm to 18 μm. Each of the second insulating layer 120 and the third insulating layer 130 can have a thickness of 7 μm to 15 μm.

[0088] In this case, when the second insulating layer 120 is formed of multiple layers, the thickness range can refer to the thickness range of each of the multiple layers.

[0089] In other words, the insulating layer of the circuit board in the comparative example is composed of glass fiber prepreg (PPG). In this case, based on the PPG in the circuit board of the comparative example, it is difficult to reduce the thickness of the glass fibers. This is because when the thickness of the PPG is reduced, the glass fibers contained in the PPG may electrically connect to the circuit patterns disposed on the surface of the PPG, thus inducing a risk of cracking. Therefore, in the circuit board of the comparative example, when the thickness of the PPG is reduced, dielectric breakdown and damage to the circuit patterns may occur. Therefore, due to the thickness of the glass fibers constituting the PPG, there are limitations on reducing the overall thickness of the circuit board in the comparative example.

[0090] Furthermore, since the circuit board of the comparative example is constructed from an insulating layer consisting solely of PPG containing glass fiber, it possesses a high dielectric constant. However, in the case of a dielectric with a high dielectric constant, there is a problem that it is difficult to use as a high-frequency alternative. In other words, in the circuit board of the comparative example, due to the high dielectric constant of the glass fiber, the dielectric constant is compromised in the high-frequency band.

[0091] Therefore, in this embodiment, by using RCC with a low dielectric constant to form the insulating layer, a highly reliable circuit board can be provided that minimizes signal loss even in the high-frequency band while reducing the thickness of the circuit board.

[0092] Meanwhile, since the second insulating layer 120 in this embodiment is made of RCC, the thickness of the circuit board can be significantly reduced compared to the comparative example where the insulating layer is made of PPG. Therefore, in this embodiment, by using RCC made of a low dielectric constant material, the thickness of the circuit board can be reduced by at least 5 μm compared to the comparative example.

[0093] However, even using RCC with a low dielectric constant of 2.7 (which is a 10% improvement over PPG's 3.0), the thickness reduction rate is only 10% compared to the comparative example. Therefore, in the embodiment, by using laser processing to form cavities in the portion where chips, such as electronic components, are mounted, an optimal circuit board can be provided.

[0094] In this configuration, at least one of the first insulating layer 110, the second insulating layer 120, and the third insulating layer 130 can represent electronic wiring for connecting circuit components based on a circuit design in a wiring diagram, and can reproduce electrical conductors on the insulating material. Furthermore, at least one of the first insulating layer 110, the second insulating layer 120, and the third insulating layer 130 can form wiring for mounting and connecting electronic components to create a circuit, and can mechanically fix components other than those with electrical connection functions.

[0095] For example, a first circuit pattern 140 may be disposed on the upper surface of the first insulating layer 110. For example, a second circuit pattern 150 may be disposed on the lower surface of the first insulating layer 110. For example, a third circuit pattern 160 may be disposed on the upper surface of the second insulating layer 120. For example, a fourth circuit pattern 170 may be disposed on the lower surface of the third insulating layer 130.

[0096] Each of the first circuit pattern 140, the second to 150, the third circuit pattern 160, and the fourth circuit pattern 170 can be formed as a plurality on the surface of each insulating layer while being spaced apart from each other by a predetermined interval.

[0097] Furthermore, when the second insulating layer 120 has a multilayer structure, the third circuit pattern 160 can be respectively disposed on the surfaces of the plurality of second insulating layers. Additionally, when the third insulating layer 130 has a multilayer structure, the fourth circuit pattern 170 can be respectively disposed on the surfaces of the plurality of third insulating layers.

[0098] Meanwhile, the first to fourth circuit patterns 140, 150, 160, and 170 described above can be wiring for transmitting electrical signals and can be formed from a highly conductive metallic material. Therefore, the first to fourth circuit patterns 140, 150, 160, and 170 can be formed from at least one metallic material selected from gold (Au), silver (Ag), platinum (Pt), titanium (Ti), tin (Sn), copper (Cu), and zinc (Zn). Furthermore, the first to fourth circuit patterns 140, 150, 160, and 170 can be formed from a paste or solder paste with excellent bonding strength, including at least one metallic material selected from gold (Au), silver (Ag), platinum (Pt), titanium (Ti), tin (Sn), copper (Cu), and zinc (Zn). Preferably, the first to fourth circuit patterns 140, 150, 160, and 170 can be formed from copper (Cu), which has high conductivity and relatively low cost.

[0099] The first to fourth circuit patterns 140, 150, 160 and 170 can be formed by general circuit board manufacturing processes, such as additive processes, subtractive processes, modified semi-additive processes (MSAP), semi-additive processes (SAP), etc., and detailed descriptions thereof will be omitted here.

[0100] Simultaneously, the first circuit pattern 140 may include pads 140P, which are disposed on the upper surface of the first insulating layer 110 and exposed through the cavity C. Pads 140P may be electrically connected to electronic components mounted in the cavity C (described later). For example, pads 140P may be wire bonding pads connected via wires to electronic components mounted in the cavity C. Alternatively, pads 140P may be flip-chip bonding pads directly connected to terminals of electronic components mounted in the cavity C.

[0101] Meanwhile, each of the first to fourth circuit patterns 140, 150, 160 and 170 may include via pads connected to vias for interlayer conductivity, traces for signal transmission, and mounting pads for connecting to electronic components.

[0102] Here, the first to fourth circuit patterns 140, 150, 160 and 170 can have multiple layer structures.

[0103] For example, the first circuit pattern 140 may include a 1-1 metal layer 141 and a 1-2 metal layer 142. The 1-1 metal layer 141 may be disposed on the upper surface of the first insulating layer 110. For example, the lower surface of the 1-1 metal layer 141 may be in direct contact with the upper surface of the first insulating layer 110. The 1-1 metal layer 141 may be a chemically plated copper layer. For example, the 1-1 metal layer 141 may be an electroless layer. The 1-1 metal layer 141 may be a seed layer for electroplating the 1-2 metal layer 142. The 1-2 metal layer 142 may be an electrolytically plated layer formed by electroplating with the 1-1 metal layer 141 as a seed layer. The thickness of the 1-2 metal layer 142 may be greater than the thickness of the 1-1 metal layer 141. For example, the 1-1 metal layer 141 may have a first thickness. The first thickness of the 1-1 metal layer 141 may vary depending on the electroplating method of the 1-1 metal layer 141. For example, electroless copper plating layers can be categorized based on thickness as heavy copper (over 2 μm), medium copper (1 to 2 μm), and light copper (less than 1 μm). In this case, the 1-1 metal layer 141 in the embodiment can have a first thickness of 0.5 μm to 1.5 μm through medium or light copper plating. The 1-2 metal layer 142 can have a thickness ranging from 8.5 μm to 13.5 μm. Therefore, the total thickness of the first circuit pattern 140, including the 1-1 metal layer 141 and the 1-2 metal layer 142, can be in the range of 10 μm to 14 μm.

[0104] For example, the second circuit pattern 150 may include a 2-1 metal layer 151 and a 2-2 metal layer 152. The 2-1 metal layer 151 may be disposed on the lower surface of the first insulating layer 110. For example, the upper surface of the 2-1 metal layer 151 may be in direct contact with the lower surface of the first insulating layer 110. The 2-1 metal layer 151 may be a chemically plated copper layer. For example, the 2-1 metal layer 151 may be an electroless layer. The 2-1 metal layer 151 may be a seed layer for electroplating the 2-2 metal layer 152. The 2-2 metal layer 152 may be an electrolytically plated layer formed by using the 2-1 metal layer 151 as a seed electroplating layer. The thickness of the 2-2 metal layer 152 may be greater than the thickness of the 2-1 metal layer 151.

[0105] For example, the third circuit pattern 160 may include a 3-1 metal layer 161 and a 3-2 metal layer 162. The 3-1 metal layer 161 may be disposed on the upper surface of the second insulating layer 120. For example, the lower surface of the 3-1 metal layer 161 may be in direct contact with the upper surface of the second insulating layer 120. The 3-1 metal layer 161 may be a chemically plated copper layer. For example, the 3-1 metal layer 161 may be an electroless layer. The 3-1 metal layer 161 may be a seed layer for electroplating the 3-2 metal layer 162. The 3-2 metal layer 162 may be an electrolytically plated layer formed by electroplating with the 3-1 metal layer 161 as a seed layer. The thickness of the 3-2 metal layer 162 may be greater than the thickness of the 3-1 metal layer 161.

[0106] For example, the fourth circuit pattern 170 may include a 4-1 metal layer 171 and a 4-2 metal layer 172. The 4-1 metal layer 171 may be disposed on the lower surface of the third insulating layer 130. For example, the upper surface of the 4-1 metal layer 171 may be in direct contact with the lower surface of the third insulating layer 130. The 4-1 metal layer 171 may be a chemically plated copper layer. For example, the 4-1 metal layer 171 may be an electroless layer. The 4-1 metal layer 171 may be a seed layer for electroplating the 4-2 metal layer 172. The 4-2 metal layer 172 may be an electrolytically plated layer formed by electroplating with the 4-1 metal layer 171 as a seed layer. The thickness of the 4-2 metal layer 172 may be greater than the thickness of the 4-1 metal layer 171.

[0107] Vias V1, V2, and V3, used to electrically connect circuit patterns disposed on different layers, can be disposed in the first insulating layer 110, the second insulating layer 120, and the third insulating layer 130. Vias V1, V2, and V3 can be configured to pass through at least one of the first insulating layer 110, the second insulating layer 120, and the third insulating layer 130. Furthermore, the two ends of vias V1, V2, and V3 are respectively connected to the circuit patterns disposed on the different insulating layers, thus enabling the transmission of electrical signals.

[0108] A first via V1 may be disposed on the first insulating layer 110. The first via V1 may be disposed through the upper and lower surfaces of the first insulating layer 110. The first via V1 may electrically connect a first circuit pattern 140 disposed on the upper surface of the first insulating layer 110 with a second circuit pattern 150 disposed on the lower surface of the first insulating layer 110.

[0109] The second via V2 can be disposed on the second insulating layer 120. The second via V2 can be disposed through the upper and lower surfaces of the second insulating layer 120. The second via V2 can electrically connect the first circuit pattern 140 disposed on the upper surface of the first insulating layer 110 with the third circuit pattern 160 disposed on the upper surface of the second insulating layer 120.

[0110] The third via V3 can be disposed on the third insulating layer 130. The third via V3 can be configured to pass through the upper and lower surfaces of the third insulating layer 130. The third via V3 can electrically connect the second circuit pattern 150 disposed on the lower surface of the first insulating layer 110 with the fourth circuit pattern 170 disposed on the lower surface of the third insulating layer 130.

[0111] Meanwhile, vias V1, V2, and V3 may pass through only one of the first insulating layer 110, the second insulating layer 120, and the third insulating layer 130. Multiple insulating layers may be configured to pass through together. Therefore, vias V1, V2, and V3 can connect circuit patterns disposed on surfaces spaced apart by at least two or more insulating layers, rather than on insulating layers that are adjacent to each other.

[0112] Meanwhile, vias V1, V2, and V3 can be formed by filling the interior of a via (not shown) that passes through at least one of the multiple insulating layers with a conductive material.

[0113] Through-holes can be formed by any of the following methods: mechanical, laser, and chemical processing. When forming through-holes by mechanical processing, methods such as milling, drilling, and wiring can be used. When forming through-holes by laser processing, UV or CO2 laser methods can be used. When forming through-holes by chemical processing, at least one of multiple insulating layers can be opened by using chemicals including aminosilanes, ketones, etc.

[0114] Meanwhile, laser processing is a cutting method that melts and evaporates a portion of the material by concentrating optical energy on a surface to form the desired shape. It can easily process complex shapes formed by computer programs and can process complex materials that are difficult to cut by other methods.

[0115] In addition, laser technology can achieve a cutting diameter of at least 0.005 mm and has a wide range of processable thicknesses.

[0116] Yttrium aluminum garnet (YAG) lasers, CO2 lasers, or ultraviolet (UV) lasers are preferred as laser processing drill bits. YAG lasers can process both copper foil layers and insulating layers, while CO2 lasers can only process insulating layers.

[0117] After the through-hole is formed, vias V1, V2, and V3 can be formed by filling the interior of the through-hole with a conductive material. The metal material forming vias V1, V2, and V3 can be any material selected from copper (Cu), silver (Ag), tin (Sn), gold (Au), nickel (Ni), and palladium (Pd), and the conductive material can be filled using any one or a combination of electroless plating, electroplating, screen printing, sputtering, evaporation, inkjet printing, and dispensing.

[0118] Meanwhile, protective layers 180 and 185 can be disposed on the surfaces of the uppermost and lowermost insulating layers in the first insulating layer 110, second insulating layer 120, and third insulating layer 130, respectively. For example, the first protective layer 180 can be disposed on the upper surface of the uppermost insulating layer among the multiple insulating layers. For example, the first protective layer 180 can be disposed on the upper surface of the second insulating layer 120. Furthermore, the second protective layer 185 can be disposed on the lower surface of the lowermost insulating layer among the multiple insulating layers. For example, the second protective layer 185 can be disposed on the lower surface of the third insulating layer 130.

[0119] Each of the first protective layer 180 and the second protective layer 185 may have an opening. For example, the first protective layer 180 may have an opening that exposes the surface of the third circuit pattern 160 disposed on the upper surface of the second insulating layer 120.

[0120] Additionally, the second protective layer 185 may have an opening that exposes the surface of the fourth circuit pattern 170 disposed on the lower surface of the third insulating layer 130.

[0121] The first protective layer 180 and the second protective layer 185 may include insulating materials. The first protective layer 180 and the second protective layer 185 may include various materials that can be cured by heat after coating to protect the surface of the circuit pattern. The first protective layer 180 and the second protective layer 185 may be photoresist layers. For example, the first protective layer 180 and the second protective layer 185 may be solder resist layers comprising organic polymer materials. For example, the first protective layer 180 and the second protective layer 185 may include epoxy acrylate resins. More specifically, the first protective layer 180 and the second protective layer 185 may include resins, curing agents, photoinitiators, pigments, solvents, fillers, additives, acrylic monomers, etc. However, the embodiments are not limited thereto; the first protective layer 180 and the second protective layer 185 may be any of the following: photoresist layers, capping layers, and polymer materials.

[0122] The first protective layer 180 and the second protective layer 185 can have a thickness of 1 μm to 20 μm. Alternatively, the first protective layer 180 and the second protective layer 185 can have a thickness of 1 μm to 15 μm. For example, the first protective layer 180 and the second protective layer 185 can have a thickness of 5 μm to 20 μm. When the thickness of the first protective layer 180 and the second protective layer 185 exceeds 20 μm, the thickness of the circuit board 100 increases. When the thickness of the first protective layer 180 and the second protective layer 185 is less than 1 μm, the reliability of the circuit pattern included in the circuit board 100 deteriorates.

[0123] Meanwhile, cavity C can be formed in the second insulating layer 120. In this case, cavity C can be formed in the second insulating layer 120 which consists of multiple layers, or alternatively, cavity C can be formed through the second insulating layer 120 which consists of a single layer.

[0124] Therefore, in this embodiment, the pads 140P in the first circuit pattern 140 disposed on the upper surface of the first insulating layer 110 can be exposed through the cavity C. The cavity C can provide space for mounting electronic components. Additionally, the pads 140P can be exposed through the cavity C for electrical connection to electronic components mounted within the cavity C.

[0125] The cavity C in the embodiment can be formed by a laser process. In this case, to form the cavity C by a laser process, a stop layer is required to process only the insulating layer to the desired depth. The stop layer can be formed from a metallic material that has not been laser-treated. For example, the laser can be a laser capable only of processing insulating layers. Alternatively, the laser may not be able to process metallic layers formed from metallic materials. Accordingly, in a typical circuit board, a stop layer is provided to prevent the laser from passing through the cavity formation area. In this case, the stop layer in a typical circuit board can be formed by an additional process different from the circuit pattern. Therefore, in the related art, the process of forming the stop layer and the process of removing the stop layer after forming the cavity must be performed separately, thus resulting in problems such as increased manufacturing costs and increased manufacturing complexity.

[0126] Alternatively, in an embodiment, a portion of the circuit pattern can be used as a stop layer, without forming a separate stop layer in the area where the cavity C is to be formed.

[0127] In an embodiment, a portion of the first circuit pattern 140 serves as a stop layer. Preferably, in an embodiment, the 1-1 metal layer 141 constituting the first circuit pattern 140 can be used as a stop layer for forming the cavity C.

[0128] That is, the 1-1 metal layer 141 can be removed after the 1-2 metal layer 142 is formed. In other words, the 1-1 metal layer 141 can be formed on the entire upper surface 110 of the first insulating layer before it is removed.

[0129] In addition, in a typical circuit board, after the 1-2 metal layers are formed, the 1-1 metal layer, which is formed in the area that does not overlap with the 1-2 metal layers in the vertical direction, is completely removed.

[0130] However, in the embodiment, after forming the 1-2 metal layers 142, the 1-1 metal layer 141 is not completely removed, and the 1-1 metal layer 141 remains in the region where the cavity C is to be formed.

[0131] Furthermore, in this embodiment, after the cavity C is formed, an additional step of removing the 1-1 metal layer 141 from the area exposed through the cavity C is performed. That is, in this embodiment, the 1-1 metal layer 141, which serves as the seed layer for the 1-2 metal layer 142, can be used as a stop layer for forming the cavity C. Therefore, in this embodiment, the additional step of forming a stop layer required for forming the cavity C can be omitted, thereby reducing manufacturing costs and simplifying the manufacturing process.

[0132] In this case, in the embodiment, it is difficult to accurately leave only the 1-1 metal layer 141 in the area where the cavity C is to be formed after forming the 1-2 metal layers 142. That is, there are tolerances in the laser process or product design, so it is practically impossible to leave only the 1-1 metal layer 141 in the area where the cavity C is to be formed. Therefore, the area where the 1-1 metal layer 141 is left unremoved can be larger than the actual area where the cavity C is to be formed.

[0133] Therefore, in the embodiment, the side surface of the 1-1 metal layer 141, which serves as a stop layer, can be exposed through the sidewall of the cavity C.

[0134] That is, in the embodiment, the 1-1 metal layer 141 may include a first portion disposed in a region that overlaps with the 1-2 metal layer 142 in the vertical direction.

[0135] Furthermore, in the embodiments, the 1-1 metal layer 141 may include a second portion 141a disposed in a region that does not overlap with the 1-2 metal layer 142 in the vertical direction, such as... Figure 2 As shown, the second part 141a of the 1-1 metal layer 141 may have a structure configured to surround the outer side of the cavity C.

[0136] In this case, the second portion 141a of the 1-1 metal layer 141 in the first embodiment can be separated from the 1-2 metal layer 142. In other words, the second portion 141a of the 1-1 metal layer 141 in the first embodiment can be electrically insulated from the 1-2 metal layer 142 constituting the first circuit pattern 140. In other words, the second portion 141a of the 1-1 metal layer 141 in the first embodiment can be configured to be spaced apart from the 1-2 metal layer 142 constituting the first circuit pattern 140 by a predetermined interval. Furthermore, the second portion 141a of the 1-1 metal layer 141 in the first embodiment can be configured to surround the outer side of the cavity C in a region adjacent to the cavity C.

[0137] Therefore, the area of ​​metal layer 141 1-1 in the first embodiment can be different from the area of ​​metal layer 142 1-2. That is, in a typical circuit board, the seed layer and the plating layer disposed on the seed layer can have the same area. This is because after the plating layer is formed, the seed layer in the areas where no plating layer is disposed is completely removed. Therefore, in a typical circuit board, the seed layer and the plating layer can have the same area.

[0138] Alternatively, the area of ​​metal layer 141 in the embodiment may be greater than the area of ​​metal layer 142. For example, the area of ​​metal layer 141 may be greater than the area of ​​metal layer 142 by the area of ​​the second portion 141a.

[0139] Meanwhile, in this embodiment, a Gaussian beam can be used to form the cavity C. In this case, the center point of the Gaussian beam can be used to process the outermost part of the cavity C. That is, the laser with the maximum intensity is generated at the center point of the Gaussian beam, so the tilt angle of the inner wall of the outermost cavity C can be smaller than the tilt angle of the comparative example.

[0140] As described above, in this embodiment, a first circuit pattern 140 is provided on the upper surface of the first insulating layer 110. The first circuit pattern 140 may include a 1-1 metal layer 141 as a seed layer and a 1-2 metal layer 142 provided on the 1-1 metal layer 141 as a plating layer. Furthermore, in this embodiment, the 1-2 metal layer 142 serves as a plating layer. The 1-1 metal layer 141, serving as the seed layer of the 1-2 metal layer 142, acts as a stop layer for the cavity C to be formed in the second insulating layer 120. Therefore, the area of ​​the 1-1 metal layer 141 in this embodiment can be larger than the area of ​​the 1-2 metal layer 142. Additionally, in this embodiment, the 1-1 metal layer 141 may include a first portion that overlaps with the 1-2 metal layer 142 in the vertical direction and a second portion 141a that does not overlap with the 1-2 metal layer 142 in the vertical direction. Furthermore, the side surface of the second portion 141a of the 1-1 metal layer 141 can be exposed through the cavity C formed in the second insulating layer 120. Additionally, the second portion 141a of the 1-1 metal layer 141 may surround the outer side of the cavity C and may be disposed between the first insulating layer 110 and the second insulating layer 120. Therefore, in the embodiment, it is not necessary to form an additional stop layer in the second insulating layer required for forming the cavity using a laser process, thereby reducing manufacturing costs and simplifying the manufacturing process.

[0141] In the following description, the packaging substrate including the circuit board and the method of manufacturing the circuit board will be described with emphasis on the structure of the circuit board in the first embodiment.

[0142] Figure 3 This is a view showing the packaging substrate according to the first embodiment.

[0143] Reference Figure 3 The packaging substrate 200A according to the embodiment includes Figure 1 The circuit board 100 and the electronic component 190 installed in the cavity C of the circuit board 100 are shown.

[0144] Reference Figure 1 and Figure 2 The circuit board 100 described can be used as a package board 200A for mounting electronic components 190.

[0145] In this case, since the circuit board 100 has already been described in detail above, its description will be omitted.

[0146] The circuit board 100 includes a cavity C, and pads 140P, which are part of a first circuit pattern 140, can be exposed within the cavity C. Additionally, a 1-1 metal layer 141 having a closed-loop shape surrounding the outer side of the cavity C can be provided within the cavity C. In this case, [details omitted]. Figure 2The closed-loop shape of the 1-1 metal layer 141 is quadrilateral, but the embodiments are not limited to this. For example, the closed-loop shape of the 1-1 metal layer 141 can be circular, and alternatively, it can be deformed into various shapes such as triangles, polygons and ellipses.

[0147] In this context, electronic component 190 can be an electronic part disposed in the cavity C of circuit board 100, and can be divided into active components and passive components. Furthermore, active components are components that actively utilize nonlinear characteristics, while passive components are components that do not utilize nonlinear characteristics even when both linear and nonlinear characteristics exist simultaneously. Active components can include transistors, IC semiconductor chips, etc., while passive components can include capacitors, resistors, inductors, etc. Passive components are mounted on conventional circuit boards to increase the signal processing speed of semiconductor chips that are active components, or to perform filtering functions.

[0148] Simultaneously, the connection portion 195 can be disposed on the pad 140P. The planar shape of the connection portion 195 can be quadrilateral. The connection portion 195 is disposed on the pad 140P and electrically connects the electronic component 190 to the pad 140P while fixing the electronic component 190. For this purpose, the connection portion 195 can be formed of a conductive material. As an example, the connection portion 195 can be a solder ball. The connection portion 195 can contain a heterogeneous material in the solder. The solder can be composed of at least one of SnCu, SnPb, and SnAgCu. In addition, the heterogeneous material can include any one of Al, Sb, Bi, Cu, Ni, In, Pb, Ag, Sn, Zn, Ga, Cd, and Fe.

[0149] Meanwhile, the upper surface of the electronic component 190 can be configured to be higher than the uppermost surface of the circuit board 100. However, the embodiments are not limited to this, and depending on the type of electronic component 190, the upper surface of the electronic component 190 can be configured at the same height as the uppermost surface of the circuit board 100 or lower.

[0150] Figure 4 This is a view showing the packaging substrate according to the second embodiment.

[0151] Reference Figure 4 According to an embodiment, the packaging substrate 200B includes a circuit board 100 and an electronic component 190a mounted in a cavity C of the circuit board 100.

[0152] In addition, the packaging substrate 200B is disposed in the cavity C and also includes a molding layer M covering the electronic component 190a.

[0153] The molding layer M can be selectively disposed in the cavity C to protect the electronic components 190a installed in the cavity C.

[0154] The molding layer M may be composed of a molding resin (e.g., epoxy molding compound (EMC)). However, the embodiments are not limited to this, and the molding layer M may be composed of various other molding resins besides EMC.

[0155] The circuit board 100 can be used as a packaging substrate 200B for mounting electronic components 190a.

[0156] In addition, as described above, the connection portion 195a can be disposed between the electronic component 190a and the pad 140P.

[0157] In the following description, a method for manufacturing a circuit board according to an embodiment will be described with reference to the accompanying drawings.

[0158] Figures 5 to 10 It is shown in the order of the processes. Figure 1 A view showing the manufacturing method of the circuit board.

[0159] Reference Figure 5 A first insulating layer 110 can be prepared, a first circuit pattern 140 and a second circuit pattern 150 can be formed on the surface of the first insulating layer 110, and a first through hole V1 can be formed through the first insulating layer 110 and electrically connect the first circuit pattern 140 and the second circuit pattern 150.

[0160] The first insulating layer 110 can be a prepreg. Prepreg (PPG) has good flowability and adhesion in a semi-cured state and serves as an intermediate substrate in a fiber-reinforced composite material, which acts as both an adhesive layer and an insulating layer. The prepreg is a molding material in which a matrix resin is pre-impregnated into the reinforcing fibers. A molded article is formed by stacking and heating / pressurizing the prepreg to cure the resin. In other words, prepreg refers to a material impregnated with resin (BT / Epoxy, FR4, FR5, etc.) into glass fibers and cured to grade B.

[0161] In other words, the first insulating layer 110 may be a thermosetting or thermoplastic polymer substrate, a ceramic substrate, an organic-inorganic composite substrate, or a glass fiber impregnated substrate, and when the first insulating layer 110 includes a polymer resin, it may include an epoxy insulating resin, and alternatively, it may include a polyimide resin.

[0162] In this case, the first circuit pattern 140 and the second circuit pattern 150 can be composed of multiple layers.

[0163] For example, the first circuit pattern 140 may include a 1-1 metal layer 141 and a 1-2 metal layer 142. For example, the second circuit pattern 150 may include a 2-1 metal layer 151 and a 2-2 metal layer 152.

[0164] Briefly describing the process of forming the first circuit pattern 140, in an embodiment, a process of forming a 1-1 metal layer 141 on the surface of the first insulating layer 110 by electroless plating can be performed. Subsequently, in an embodiment, a process of forming a mask on the 1-1 metal layer 141 can be performed. Subsequently, in an embodiment, the mask can be exposed and developed to form openings in areas where the 1-2 metal layer 142 is to be formed. Subsequently, in an embodiment, the 1-2 metal layer 142 filling the openings can be formed by electroplating with the 1-1 metal layer 141 as a seed layer. Simultaneously, the first circuit pattern 140 may include pads 140P, which are exposed through cavities C when later electrically connected to electronic components.

[0165] Next, refer to Figure 6 In an embodiment, after the 1-2 metal layer 142 and the 2-2 metal layer 152 are formed, a process of removing the 1-1 metal layer 141 and the 2-1 metal layer 151 used as seed crystal layers can be performed.

[0166] In this case, in the embodiment, the entire metal layer used as a seed layer is not removed, and the metal layer disposed in the region where the cavity C is to be formed is left unremoved.

[0167] Specifically, the cavity C can be formed in the second insulating layer 120 disposed on the 1-1 metal layer 141. Therefore, in the embodiment, the portion of the 1-1 metal layer 141 corresponding to the region CR where the cavity C is to be formed is left unremoved.

[0168] In other words, generally speaking, all portions of the 1-1 metal layer 141 that do not overlap with the 1-2 metal layer 142 in the vertical direction are removed. In this case, in the embodiment, the portion of the 1-1 metal layer 141 that does not overlap with the 1-2 metal layer 142 in the vertical direction and is located in the region where the cavity C is to be formed is left and not removed.

[0169] In this case, the remaining portion of the 1-1 metal layer 141 can be larger than the actual cavity C to be formed. Therefore, in this embodiment, the problem of partial removal of the surface of the first insulating layer 110 due to process errors during the process of forming the cavity C is solved.

[0170] Next, as Figure 7 As shown, in one embodiment, the second insulating layer 120 is formed on the upper surface of the first insulating layer 110. Additionally, in another embodiment, the third insulating layer 130 is formed below the lower surface of the first insulating layer 110. In this case, each of the second insulating layer 120 and the third insulating layer 130 may be constructed of RCC (Reinforcing Cylinder Carrier).

[0171] Alternatively, a process of forming a circuit pattern on the surface of the second insulating layer 120 can be performed. For example, a process of forming a third circuit pattern 160 on the upper surface of the second insulating layer 120 can be performed.

[0172] Alternatively, a process of forming a circuit pattern on the surface of the third insulating layer 130 can be performed. For example, a process of forming a fourth circuit pattern 170 on the lower surface of the third insulating layer 130 can be performed.

[0173] The third circuit pattern 160 and the fourth circuit pattern 170 can also have multi-layer structures.

[0174] For example, the third circuit pattern 160 may include a 3-1 metal layer 161 and a 3-2 metal layer 162. For example, the fourth circuit pattern 170 may include a 4-1 metal layer 171 and a 4-2 metal layer 172.

[0175] Additionally, in this embodiment, the process of forming a second via V2 in the second insulating layer 120 can be performed. Additionally, in this embodiment, the process of forming a third via V3 in the third insulating layer 130 can be performed.

[0176] Next, refer to Figure 8 In one embodiment, the process of forming cavity C can be performed by using a laser to open the second insulating layer 120.

[0177] In this case, the unremoved 1-1 metal layer 141 exists on the upper surface of the first insulating layer 110 in the region where the cavity C is to be formed.

[0178] In addition, in the embodiment, by using the 1-1 metal layer 141 left in the region where the cavity C is to be formed in the laser process as a stop layer, the process of removing the insulating layer can be performed only on the region where the 1-1 metal layer 141 is formed.

[0179] In this embodiment, the centerline of a Gaussian beam can be used to perform the process of forming cavity C. That is, in the embodiment, the outermost region of cavity C is processed using the beam along the centerline of the Gaussian beam. Alternatively, in the embodiment, the entire region of cavity C is processed while the Gaussian beam is moved a predetermined distance.

[0180] Next, refer to Figure 9 In an embodiment, a process of removing the 1-1 metal layer 141 exposed through the cavity C on its upper surface can be performed. For example, in an embodiment, a process of removing the 1-1 metal layer 141 exposed through the cavity C can be performed by etching.

[0181] Next, refer to Figure 10In the embodiments, the process of forming protective layers 180 and 185 on the upper surface of the second insulating layer 120 and the lower surface of the third insulating layer 130 can be performed respectively.

[0182] Each of the first protective layer 180 and the second protective layer 185 may have an opening. For example, the first protective layer 180 may have an opening that exposes the surface of the third circuit pattern 160 disposed on the upper surface of the second insulating layer 120.

[0183] Additionally, the second protective layer 185 may have an opening that exposes the surface of the fourth circuit pattern 170 disposed on the lower surface of the third insulating layer 130.

[0184] Figures 11 to 13 It is shown Figure 1 A view of a modified example of a circuit board.

[0185] Reference Figure 11 Circuit board 100A and according to Figure 1 The circuit board of the first embodiment is different only in the structure of the first circuit pattern 140. Therefore, the features of the first circuit pattern 140 will be mainly described below.

[0186] In the first embodiment, the 1-1 metal layer 141 disposed around the cavity C has a structure that is separate from the 1-2 metal layer 142.

[0187] Alternatively, the first circuit pattern may include a 1-1 circuit pattern 140b positioned adjacent to the cavity C. Additionally, the first circuit pattern may include a 1-2 circuit pattern other than the 1-1 circuit pattern 140b. Furthermore, the 1-1 metal layer and the 1-2 metal layer of the 1-2 circuit pattern may have the same area or width. Alternatively, the 1-1 metal layer and the 1-2 metal layer of the 1-1 circuit pattern may have different areas or widths.

[0188] That is, the 1-1 circuit pattern 140b may include a 1-1 metal layer 141b and a 1-2 metal layer 142b. In this case, the 1-1 metal layer 141b may be formed on the first insulating layer 110 and have a first width. Additionally, the 1-2 metal layer 142b may be disposed on the 1-1 metal layer 141b and have a second width. In this case, the first width may be greater than the second width. Therefore, the 1-1 metal layer 141b may include a first portion that overlaps with the 1-2 metal layer 141b in the vertical direction and a second portion that does not overlap with the 1-2 metal layer 142b in the vertical direction. In this case, the upper surface of the first portion of the 1-1 metal layer 141b may be in direct contact with the 1-2 metal layer 142b. Furthermore, unlike the first portion, the upper surface of the second portion of the 1-1 metal layer 141b may be configured to be in direct contact with the second insulating layer 120.

[0189] In addition, the second part of the 1-1 metal layer 141b can be set to be closer to the cavity C than the first part of the 1-1 metal layer 141b.

[0190] Alternatively, the side surface of the second portion of the 1-1 metal layer 141b can be exposed through the cavity C. Alternatively, the 1-2 metal layer 142b has a smaller width than the 1-1 metal layer 141b and is disposed on the 1-1 metal layer 141b at a location away from the cavity C, so the 1-2 metal layer 142b may not be exposed through the cavity C.

[0191] Reference Figure 12 The circuit board can have the same Figure 1 The circuit board has different insulating layer structures.

[0192] In other words, Figure 1 In this process, each of the second insulating layer 120 and the third insulating layer 130 is composed of a single layer, but... Figure 12 In the circuit board, each of the second insulating layer 120 and the third insulating layer 130 may have a multilayer structure.

[0193] For example, the second insulating layer may include insulating layer 120-1 (2-1) and insulating layer 120-2 (2-2). Furthermore, each of insulating layer 120-1 (2-1) and insulating layer 120-2 (2-2) may be made of RCC.

[0194] Additionally, the third insulating layer may include insulating layer 130-1 (3-1) and insulating layer 130-2 (3-2). Furthermore, each of insulating layer 130-1 (3-1) and insulating layer 130-2 (3-2) may be constructed of RCC.

[0195] Additionally, in an embodiment, the third circuit pattern may include a 3-1 circuit pattern 160-1 disposed on the upper surface of the 2-1 insulating layer 120-1 and a 3-2 circuit pattern 160-2 disposed on the upper surface of the 2-2 insulating layer 120-2.

[0196] Additionally, in an embodiment, the fourth circuit pattern may include a 4-1 circuit pattern 170-1 disposed below the lower surface of the 3-1 insulating layer 130-1 and a 4-2 circuit pattern 170-2 disposed below the lower surface of the 3-2 insulating layer 130-2.

[0197] Additionally, in an embodiment, the cavity C may be formed through a second insulating layer 120 having a multilayer structure.

[0198] In this configuration, cavities C can pass together through the second insulating layer 120 to form a single cavity. For example, cavity C may include a first cavity portion C-1 formed in the 2-1 insulating layer 120-1 and a second cavity portion C-2 formed in the 2-2 insulating layer 120-2. Furthermore, the first cavity portion C-1 and the second cavity portion C-2 may have the same width.

[0199] Therefore, the 3-2 circuit pattern 160-2 disposed on the upper surface of the 2-2 insulating layer 120-2 can be exposed without passing through the cavity C, and only the portion corresponding to the 3-1 circuit pattern 160-1 disposed on the upper surface of the 2-1 insulating layer 120-1 can be exposed.

[0200] In this case, the metal layer corresponding to the stop layer used to form cavity C in the embodiment may be located only on the first insulating layer 110 and the 2-1 insulating layer 120-1. That is, the metal layer corresponding to the stop layer may have the same characteristics as... Figure 1 and Figure 11 The structure is the same as any of the metal layers shown and may include a second part 141a of the 1-1 metal layer 141 surrounding the outside of the cavity C.

[0201] Reference Figure 13 The second insulating layer may include insulating layer 120-1 (2-1) and insulating layer 120-2 (2-2). Furthermore, each of insulating layer 120-1 (2-1) and insulating layer 120-2 (2-2) may be made of RCC.

[0202] Additionally, the third insulating layer may include insulating layer 130-1 (3-1) and insulating layer 130-2 (3-2). Furthermore, each of insulating layer 130-1 (3-1) and insulating layer 130-2 (3-2) may be constructed of RCC.

[0203] Additionally, in an embodiment, the third circuit pattern may include a 3-1 circuit pattern 160-1 disposed on the upper surface of the 2-1 insulating layer 120-1 and a 3-2 circuit pattern 160-2 disposed on the upper surface of the 2-2 insulating layer 120-2.

[0204] Additionally, in an embodiment, the fourth circuit pattern may include a 4-1 circuit pattern 170-1 disposed below the lower surface of the 3-1 insulating layer 130-1 and a 4-2 circuit pattern 170-2 disposed below the lower surface of the 3-2 insulating layer 130-2.

[0205] Additionally, in an embodiment, the cavity C may be formed through a second insulating layer 120 having a multilayer structure.

[0206] In this case, the cavity C may include two cavities, each passing through a plurality of second insulating layers 120. For example, the cavity C may include a first cavity portion C1 formed in the 2-1 insulating layer 120-1 and a second cavity C2 formed in the 2-2 insulating layer 120-2.

[0207] The first cavity C1 and the second cavity C2 may have different widths. For example, in the packaging substrate according to the embodiment, a first electronic component may be mounted in the first cavity C1 formed in the 2-1 insulating layer 120-1 and a second electronic component may be mounted in the second cavity C2 formed in the 2-2 insulating layer 120-2.

[0208] Therefore, a portion of the first circuit pattern (the pads connected to the first electronic component) can be exposed to the first cavity C1 formed in the 2-1 insulating layer 120-1, and a portion of the 3-1 circuit pattern 160-1 can be exposed to the second cavity C2 formed in the 2-2 insulating layer 120-2.

[0209] Furthermore, the first cavity C1 and the second cavity C2 can have different widths. Therefore, in the embodiments, the process of forming each cavity can be performed separately.

[0210] In this case, the metal layer corresponding to the stop layer used to form cavity C in the embodiment can be located not only between the first insulating layer 110 and the 2-1 insulating layer 120-1, but also between the 2-1 insulating layer 120-1 and the 2-2 insulating layer 120-2.

[0211] In other words, as part of the 3-1 circuit pattern 160-1 used to form the second cavity C2, the plating layer 160-1a can be disposed on the upper surface of the 2-1 insulating layer 120-1 and surround the periphery of the second cavity C2.

[0212] Figure 14 This is a view showing a circuit board according to the second embodiment. Figure 15 It is shown Figure 14 A partial plan view of the circuit board configuration.

[0213] and Figure 1 Compared to the first embodiment, the circuit board according to the second embodiment may not include the second portion 141a of the 1-1 metal layer 141. Unlike the first embodiment, the circuit board according to the second embodiment can be implemented by performing multiple processing steps to form a cavity.

[0214] However, Figure 14 The circuit board in the second embodiment may also include Figure 1 , 11 The second portion 141a of the 1-1 metal layer 141 shown in 12 and 13. However, in the following description, the second portion 141a of the 1-1 metal layer 141 will not be included in the circuit board of the second embodiment.

[0215] Reference Figure 14 The circuit board 1000 includes a first insulating layer 1100, a second insulating layer 1200, a third insulating layer 1300, circuit patterns 1400, 1500, 1600 and 1700, vias V1, V2 and V3, and protective layers 1800 and 1850.

[0216] In this case, the second insulating layer 120 of the first embodiment is formed of RCC. Alternatively, the second insulating layer 1200 of the second embodiment can be formed of the same prepreg as the first insulating layer 1100. In this case, the prepreg may contain glass fibers. In addition, when a cavity is formed in the prepreg, at least a portion of the glass fibers included in the prepreg may be exposed in the cavity. Furthermore, the exposed glass fibers may cause the various reliability problems mentioned above. Therefore, in the second embodiment, even when the second insulating layer 1200 is made of a prepreg containing glass fibers, the glass fibers exposed through the cavity can be completely removed. However, the embodiments are not limited thereto, and the second insulating layer 1200 of the second embodiment may also be formed of RCC like the second insulating layer 120 of the first embodiment.

[0217] However, in the following description, the second insulating layer 1200 of the second embodiment will be formed of prepreg.

[0218] In this case, the cavity C, described later, can be formed in the second insulating layer 1200. The cavity C can be formed through the second insulating layer 1200. Additionally, in the embodiment, the second insulating layer 1200 is formed of a prepreg. Here, the prepreg can have a structure in which glass fibers and fillers are dispersed in a resin. Furthermore, when the cavity C is formed in the second insulating layer 1200 composed of a prepreg, the glass fibers dispersed in the second insulating layer 1200 may be exposed through the cavity C. Therefore, the embodiment aims to provide a cavity forming method and cavity structure capable of effectively removing glass fibers exposed through the cavity C from the glass fibers disposed in the second insulating layer 1200.

[0219] This can be achieved through features that appear in the process of forming cavity C, as described later. For example, in an embodiment, multiple processing steps are performed to form cavity C. That is, when cavity C is formed using a laser, the shape of the cavity, processing time, etc., vary depending on the laser source. In this case, in an embodiment, while having an optimal cavity shape, a cavity in which the glass fiber is not exposed through cavity C can be formed within the process time used for optimal cavity formation.

[0220] Additionally, the first circuit pattern 1400 may be disposed on the upper surface of the first insulating layer 1100. For example, the second circuit pattern 1500 may be disposed on the lower surface of the first insulating layer 1100. For example, the third circuit pattern 1600 may be disposed on the upper surface of the second insulating layer 1200. For example, the fourth circuit pattern 1700 may be disposed on the lower surface of the third insulating layer 1300.

[0221] Meanwhile, the first circuit pattern 1400 may include pads 1400P, which are exposed through the cavity C while being disposed on the upper surface of the first insulating layer 1100.

[0222] Additionally, similar to the first embodiment, the circuit pattern in the second embodiment can have a two-layer structure. For example, the first circuit pattern 1400 may include a 1-1 metal layer 1410 and a 1-2 metal layer 1420. For example, the second circuit pattern 1500 may include a 2-1 metal layer 1510 and a 2-2 metal layer 1520. For example, the third circuit pattern 1600 may include a 3-1 metal layer 1610 and a 3-2 metal layer 1620. For example, the fourth circuit pattern 1700 may include a 4-1 metal layer 1710 and a 4-2 metal layer 1720.

[0223] Through holes V1, V2, and V3 for electrically connecting circuit patterns arranged on different layers can be provided in the first insulating layer 1100, the second insulating layer 1200, and the third insulating layer 1300.

[0224] Meanwhile, cavity C can be formed in the second insulating layer 1200. In this case, cavity C can be formed in the second insulating layer 1200 which is composed of multiple layers; alternatively, cavity C can be formed through the second insulating layer 1200 which is composed of a single layer.

[0225] Therefore, in an embodiment, the pads 1400P in the first circuit pattern 1400 disposed on the upper surface of the first insulating layer 1100 can be exposed through the cavity C.

[0226] In an embodiment, a portion of the first circuit pattern 1400 serves as a stop layer in the cavity forming process. Preferably, in an embodiment, the 1-1 metal layer 1410 constituting the first circuit pattern 1400 can be used as a stop layer for forming the cavity C.

[0227] Simultaneously, in this embodiment, a mask (not shown) is required to precisely perform laser processing only on the area where the cavity C is to be formed. The mask determines the dimensions of the area to be laser-processed. In other words, the mask determines the dimensions of the cavity C. The mask can be formed in the region corresponding to the upper region of the cavity C to determine the dimensions of the upper region. For example, the mask can have a shape surrounding the upper region of the cavity. Therefore, the mask can determine the dimensions of the upper region of the cavity and also the overall dimensions of the cavity C.

[0228] Furthermore, the stop layer determines the depth of cavity C. That is, the stop layer can be set in the region corresponding to the lower region of cavity C. Therefore, the stop layer allows the insulating layer to be processed by the laser only reaching the position corresponding to the lower region of cavity C.

[0229] In this case, the mask of the embodiment can use a circuit pattern disposed on the upper surface of the second insulating layer 1200. Preferably, the mask of the embodiment can use a seed layer of the circuit pattern disposed on the upper surface of the second insulating layer 1200. More preferably, the mask of the embodiment can use a 3-1 metal layer 1610 constituting a third circuit pattern 1600 disposed on the upper surface of the second insulating layer 1200.

[0230] In other words, in the embodiment, after the first circuit pattern 1400 and the third circuit pattern 1600 are formed, the cavity C can be formed in the second insulating layer 1200 by using the first metal layer 1410 and the 3-1 metal layer 1610 of the first circuit pattern 1400 in the region where the cavity C is to be formed.

[0231] Meanwhile, in the embodiment, laser processing can be performed in two steps to form a cavity C in the second insulating layer 1200.

[0232] Preferably, in an embodiment, the cavity can be initially formed in the second insulating layer 1200 using a carbon dioxide (CO2) laser. Compared to other lasers, the carbon dioxide (CO2) laser has the advantage of rapidly forming a cavity of the desired size in the second insulating layer 1200, but its disadvantage is that the inclination angle of the inner wall of the cavity C relative to the bottom surface of the cavity forms an obtuse angle. That is, the inner wall of the cavity formed using a carbon dioxide laser has an angle of more than 110 degrees. In addition, when the inclination angle of the inner wall of the cavity C forms an obtuse angle, a large space is required to form the cavity C of the desired size. That is, the size of the cavity C can be largely determined by the size of the lower region where the electronic components are disposed. However, when the inner wall of the cavity C has an obtuse angle, the size of the upper region of the cavity C becomes larger than the size of the lower region of the cavity C. Therefore, the space required to form the cavity C may increase the size of the upper region rather than the size of the lower region.

[0233] Therefore, in this embodiment, an ultraviolet (UV) laser can be used to perform secondary processing on the cavity formed by the carbon dioxide (CO2) laser. That is, when the cavity is formed by the carbon dioxide (CO2) laser, stepped steps are created on the inner wall of the cavity to correspond to the movement interval of the laser source during laser processing. Therefore, in this embodiment, an ultraviolet (UV) laser can be used to perform secondary processing on the cavity formed by the carbon dioxide (CO2) laser. Specifically, secondary processing of the cavity using an ultraviolet (UV) laser can be performed only on the inner wall of the cavity that has already been initially processed.

[0234] Therefore, in the embodiments, the inclination angle of the inner wall of the final cavity C after secondary processing relative to the bottom surface of the cavity or the surface of the insulating layer can be from 90.01° to 100°. For example, the inclination angle of the inner wall of the final cavity after secondary processing relative to the bottom surface of the cavity or the surface of the insulating layer can be from 90.1° to 95°. For example, the inclination angle of the inner wall of the cavity relative to the bottom surface of the cavity or the surface of the insulating layer can be from 91° to 93°. That is, the cavity in the embodiments can be substantially perpendicular (or nearly perpendicular) to the bottom surface of the cavity or the upper surface of the first insulating layer.

[0235] For example, the vertical cross-sectional shape of the cavity C formed in the second insulating layer 1200 in the embodiment can be close to that of a rectangle or a square. Therefore, in the embodiment, since the vertical cross-sectional shape of the cavity formed in the second insulating layer 1200 has a shape corresponding to a rectangle or a square, the space required to form the cavity C can be reduced, thereby improving the integration of the circuit.

[0236] Specifically, in this embodiment, the upper region of cavity C may have a first width W1. Additionally, in this embodiment, the lower region of cavity C may have a second width W2 equal to the first width W1. Therefore, in this embodiment, the space required to form cavity C can be significantly reduced.

[0237] The width of the lower region of cavity C can be determined such that the size of cavity C corresponds to the size of the electronic component to be disposed therein. In this case, in the comparative example, the width of the upper region of cavity C is greater than the width of the lower region of cavity C, and the amount of wasted space is equal to the space corresponding to the width difference between the upper and lower regions. Alternatively, in the embodiment, the widths of the lower and upper regions of cavity C are the same, thus solving the space waste problem.

[0238] Furthermore, the horizontal cross-section of the cavity C in the embodiment may have a shape in which at least a portion is circular. For example, at least a portion of the cavity C in the embodiment may have a curved surface. For example, the cavity C in the embodiment may have a shape in which the edge portions have curved surfaces.

[0239] Reference Figure 15 The horizontal cross-section of cavity C in the embodiment includes at least four straight sections.

[0240] For example, the horizontal cross-section of cavity C in the embodiment may include a first portion S1 having a straight line shape. Additionally, the horizontal cross-section of cavity C in the embodiment may include a second portion S2 having a straight line shape that is substantially perpendicular to the first portion S1. Furthermore, the horizontal cross-section of cavity C in the embodiment may include a third portion S3 having a straight line shape that is parallel to the first portion S1 and substantially perpendicular to the second portion S2. Additionally, the horizontal cross-section of cavity C in the embodiment may include a fourth portion S4 having a straight line shape that is substantially perpendicular to the third portion S3 and parallel to the second portion S2.

[0241] Additionally, the horizontal cross-section of cavity C may include a first edge E1 located between the first portion S1 and the second portion S2. In this case, the first edge E1 may be curved instead of straight. For example, the first edge E1 may be a rounded corner region. That is, the first edge E1 may include a curved surface.

[0242] Additionally, the horizontal cross-section of cavity C may include a second edge E2 located between the second portion S2 and the third portion S3. In this case, the second edge E2 may be curved instead of straight. For example, the second edge E2 may be a rounded corner region. That is, the second edge E2 may include a curved surface.

[0243] Additionally, the horizontal section of cavity C may include a third edge E3 located between the third portion S3 and the fourth portion S4. In this case, the third edge E3 may be a curve instead of a straight line. For example, the third edge E3 may be a rounded corner region. That is, the third edge E3 may include a curved surface.

[0244] Additionally, the horizontal cross-section of cavity C may include a fourth edge E4 located between the first portion S1 and the fourth portion S4. In this case, the fourth edge E4 may be curved instead of straight. For example, the fourth edge E4 may be a rounded corner region. That is, the fourth edge E4 may include a curved surface.

[0245] In this case, the curved surfaces of the first edge E1, the second edge E2, the third edge E3, and the fourth edge E4 in the embodiment can correspond to the beam size of the ultraviolet (UV) laser in the embodiment. For example, the beam size of the ultraviolet (UV) laser can be a circle with a diameter of 20 μm to 80 μm. The first edge E1, the second edge E2, the third edge E3, and the fourth edge E4 can have curved surfaces corresponding to the beam size of the ultraviolet (UV) laser. For example, the curvature of the curved surfaces of the first edge E1, the second edge E2, the third edge E3, and the fourth edge E4 can correspond to the curvature of a circle with a diameter of 20 μm to 80 μm.

[0246] Therefore, in the embodiments, since the first edge E1, the second edge E2, the third edge E3 and the fourth edge E4 have vertical straight lines, structural reliability problems such as cavity collapse can be solved, thereby improving product satisfaction.

[0247] In this embodiment, the second insulating layer 1200 can be formed from a prepreg. The prepreg may include glass fibers in the resin to ensure rigidity. Additionally, during the process of forming the cavity C, a portion of the glass fibers may be exposed to the outside through the cavity C. Furthermore, various reliability issues may arise when the glass fibers are exposed through the cavity C. For example, the flatness of electronic components disposed in the cavity C may be affected by the glass fibers. For example, electronic components disposed in the cavity C may experience electrical short circuits due to the glass fibers.

[0248] In this configuration, the carbon dioxide (CO2) laser can be used without removing the glass fibers contained in the second insulating layer 1200. Therefore, when the cavity C is formed solely by the carbon dioxide (CO2) laser, the glass fibers contained in the second insulating layer 1200 can be exposed to the outside through the cavity C.

[0249] However, in this embodiment, after performing preliminary cavity machining using a carbon dioxide (CO2) laser, a secondary cavity machining is performed using an ultraviolet (UV) laser. In this case, the UV laser can remove the glass fibers exposed by the pre-machined cavity, while the inclination angle of the inner wall of cavity C is almost vertical.

[0250] In other words, in this embodiment, an ultraviolet (UV) laser can be used to remove all glass fibers of the second insulating layer 1200 that may protrude into the cavity C. Therefore, the glass fibers of the second insulating layer 1200 will not protrude from the inner wall of the cavity C into the cavity C.

[0251] Figures 16 to 22 It is shown in the order of the processes. Figure 14 A view showing the manufacturing method of the circuit board.

[0252] Reference Figure 16 A first insulating layer 1100 can be prepared, a first circuit pattern 1400 and a second circuit pattern 1500 can be formed on the surface of the first insulating layer 1100, and a first through hole V1 can be formed through the first insulating layer 1100 and electrically connect the first circuit pattern 1400 and the second circuit pattern 1500.

[0253] Next, refer to Figure 17 In an embodiment, after the 1-2 metal layer 1420 and the 2-2 metal layer 1520 are formed, a process of removing the 1-1 metal layer 1410 and the 2-1 metal layer 1510 used as seed crystal layers can be performed.

[0254] In this case, in the embodiment, the entire metal layer used as a seed layer is not removed, and the metal layer disposed in the region where the cavity C is to be formed is left unremoved.

[0255] In this case, the 1-1 metal layer 1410 may include a 1-1 portion P1-1 that overlaps vertically with the 1-2 metal layer 1420 in the region where no cavity is formed. Alternatively, the 1-1 metal layer 1410 may include a 1-2 portion P1-2 that does not overlap vertically with the 1-2 metal layer 1420 in the region where no cavity is formed. Furthermore, the 1-1 metal layer 1410 may include a 1-3 portion P1-3 (1410a) disposed in the region where a cavity is formed.

[0256] In an embodiment, as the 1-2 metal layer 1420 is electroplated, after the first circuit pattern 1400 is manufactured, the 1-2 portion P1-2 of the 1-1 metal layer 1410 is removed, and the 1-3 portion P1-3 of the 1-1 metal layer 1410 is left and not removed.

[0257] Next, as Figure 18 As shown, in one embodiment, the second insulating layer 1200 is formed on the upper surface of the first insulating layer 1100. Additionally, in another embodiment, the third insulating layer 1300 is formed below the lower surface of the first insulating layer 1100. In this case, the second insulating layer 1200 and the third insulating layer 1300 may be made of RCC, or alternatively, may be formed of prepreg.

[0258] Alternatively, a process of forming a circuit pattern on the surface of the second insulating layer 1200 can be performed. For example, a process of forming a third circuit pattern 1600 on the upper surface of the second insulating layer 1200 can be performed.

[0259] In another embodiment, the process of forming a second via V2 in the second insulating layer 1200 may be performed. In another embodiment, the process of forming a third via V3 in the third insulating layer 1300 may be performed.

[0260] Meanwhile, in the embodiment, the third circuit pattern 1600 disposed on the upper surface of the second insulating layer 1200 includes a 3-1 metal layer 1610 and a 3-2 metal layer 1620.

[0261] In this case, during the manufacturing process of the third circuit pattern 1600, after the electroplating of the 3-2 metal layer 1620 is completed, the 3-1 metal layer 1610, which serves as the electroplating seed layer for the 3-2 metal layer 1620, is removed. In this case, in the embodiment, the 3-1 metal layer 1610, which serves as the seed layer for the 3-2 metal layer 1620, is not completely removed, and the metal layer disposed in the region where the cavity C is to be formed is left unremoved.

[0262] Specifically, in this embodiment, a portion of the 3-1 metal layer 1610 disposed in the outer region of the cavity surrounding the region where the cavity C is to be formed is left unremoved. That is, generally, after the third circuit pattern 1600 is formed, all portions of the 3-1 metal layer 1610 that do not overlap vertically with the 3-2 metal layer 1620 are removed. In this case, in this embodiment, the portion of the 3-1 metal layer 1610 that does not overlap vertically with the 3-2 metal layer 1620 located around the region where the cavity C is to be formed is left unremoved.

[0263] Specifically, the 3-1 metal layer 1610 can be formed on the entire upper surface of the second insulating layer 1200.

[0264] In this configuration, metal layer 1610 (3-1) may include a 2-1 portion P2-1 that overlaps vertically with metal layer 1620 (3-2). Additionally, metal layer 1610 (3-1) may include a portion of the region where no cavity is formed that does not overlap vertically with metal layer 1620 (3-2). In this configuration, the portion of metal layer 1610 (3-1) that does not overlap vertically with metal layer 1620 (3-2) may include a 2-2 portion P2-2 that overlaps with or is spaced apart from the region where cavity C is to be formed. Furthermore, the portion of metal layer 1610 (3-1) that does not overlap vertically with metal layer 1620 (3-2) may include a 2-3 portion P2-3 adjacent to the cavity region where cavity C is to be formed.

[0265] Here, in the general circuit board manufacturing process, as the 3-2 metal layer 1620 is electroplated, when the manufacturing of the third circuit pattern 1600 is completed, the 3-1 metal layer 1610, including the 2-2 portion P2-2 and the 2-3 portion P2-3, is removed.

[0266] Alternatively, in an embodiment, during the general circuit board manufacturing process, as the 3-2 metal layer 1620 is electroplated, when the manufacturing of the second circuit pattern 1600 is completed, portion 2-2 P2-2 of the 3-1 metal layer 1610 is removed and portion 2-3 P2-3 of the 3-1 metal layer 1610 is left unremoved.

[0267] The 2-3 portion P2-3 of the 3-1 metal layer 1610 can be located in the boundary region between the region where the cavity C is to be formed and other regions on the upper surface of the second insulating layer 1200. For example, the 2-3 portion P2-3 of the 3-1 metal layer 1610 can be formed in the remaining regions on the upper surface of the second insulating layer 1200 other than the region where the cavity C is to be formed. For example, the 2-3 portion P2-3 of the 3-1 metal layer 1610 can be configured to surround the region where the cavity C is to be formed on the upper surface of the second insulating layer 1200.

[0268] In this case, portion 2-3 P2-3 of the 3-1 metal layer 1610 can have a predetermined width. In this case, the width of portion 2-3 P2-3 of the 3-1 metal layer 1610 can be greater than the radius of the beam size in the subsequent laser process. That is, in the embodiment, a Gaussian beam corresponding to the central portion of the beam in a laser process using a carbon dioxide (CO2) laser can be used to perform the cavity processing step. Therefore, the central portion of the Gaussian beam is located in the edge region of the cavity C. Furthermore, when the width of portion 2-3 P2-3 of the 3-1 metal layer 1610 is less than the radius of the beam size, a Gaussian beam can be used to process areas other than the cavity formation region of the second insulating layer 1200. Therefore, in the embodiment, the width of portion 2-3 P2-3 of the 3-1 metal layer 1610 can be greater than the radius of the Gaussian beam.

[0269] Next, refer to Figure 19 Preliminary cavity machining of the second insulating layer 1200 can be performed using portion P2-3 of the 3-1 metal layer 1610 as the boundary line. In this case, a carbon dioxide (CO2) laser can be used to perform the preliminary cavity machining. In this case, the cavity Ca of the preliminary cavity machining can have a trapezoidal horizontal cross-section. For example, the width of the preliminary machined cavity Ca can gradually decrease from top to bottom. In addition, the glass fiber GF included in the second insulating layer 1200 can be exposed to the outside of the cavity through the preliminary machined cavity Ca.

[0270] Therefore, in the embodiments, such as Figure 20 As shown, a secondary cavity machining can be performed on a pre-machined cavity using an ultraviolet (UV) laser.

[0271] In other words, in this embodiment, an ultraviolet (UV) laser can be used to perform secondary processing on a cavity that has already been pre-processed by a carbon dioxide (CO2) laser. Specifically, when a cavity is formed by a CO2 laser, stepped steps are created on the inner wall of the cavity to correspond to the movement interval of the laser source during laser processing. Therefore, in this embodiment, an ultraviolet (UV) laser can be used to perform secondary processing on a cavity formed by a CO2 laser. Specifically, secondary processing of the cavity using an ultraviolet (UV) laser can be performed only on the inner wall of the pre-processed cavity.

[0272] Next, refer to Figure 21 After the cavity C is machined, the portions of the 1-1 metal layer 1410 and 3-1 metal layer 1610 used for machining the cavity C will be removed.

[0273] In other words, in the embodiment, for cavity machining, portions 1-3 P1-3 of the 1-1 metal layer 1410 and portions 2-3 P2-3 of the 3-1 metal layer 1610, which serve as seed layers, are left unremoved. Alternatively, in the embodiment, when the machining of cavity C is complete, a process of removing portions 1-3 P1-3 of the 1-1 metal layer 1410 and portions 2-3 P2-3 of the 3-1 metal layer 1610 can be performed. In this case, as in the first embodiment, at least a portion of portions 1-3 P1-3 of the 1-1 metal layer 1410 and portions 2-3 P2-3 of the 3-1 metal layer 1610 can be left unremoved.

[0274] Next, refer to Figure 22 In the embodiments, the steps of forming protective layers 1800 and 1850 on the upper surface of the second insulating layer 1200 and the lower surface of the third insulating layer 1300 can be performed respectively.

[0275] Alternatively, the modified example corresponding to the first embodiment can be implemented using the structure corresponding to the second embodiment. Figures 11 to 13 The structure.

[0276] Figure 23A and Figure 23B This is a view specifically illustrating the cavity structure according to the third embodiment.

[0277] Figure 23A A circuit board is shown in which the second insulating layer described in the first and second embodiments is formed by a multilayer process. Additionally, Figure 23B The circuit board is shown in the case where the second insulating layer consists of a single layer.

[0278] Reference Figure 23A and Figure 23B A cavity can be formed in the second insulating layer 2120.

[0279] A cavity can be formed by openings in multiple second insulating layers 2120 (see...) Figure 23A Alternatively, a cavity can be formed by opening a single second insulating layer 2120 (see...). Figure 23B When a cavity is formed in a plurality of second insulating layers (e.g., 2-1 to 2-3 insulating layers), the cavity may include a first portion formed on the 2-1 insulating layer, a second portion formed on the 2-2 insulating layer, and a third portion formed on the 2-3 insulating layer.

[0280] In this configuration, the cavity may include inner walls S1, S2, and S3. The inner walls S1, S2, and S3 of the cavity may have a predetermined surface roughness. In this embodiment, no additional steps are performed to give the inner walls S1, S2, and S3 of the cavity the predetermined surface roughness; however, the surface roughness may be formed during the laser process used to form the cavity.

[0281] Simultaneously, the inner wall of the cavity can be divided into multiple parts. For example, the inner wall of the cavity can be divided into a first part S3, a second part S2, and a third part S1 from its lower side. In this case, the inclination angles of each of the first part S3, the second part S2, and the third part S1 can be different from each other. Furthermore, the surface roughness of at least one of the first part S3, the second part S2, and the third part S1 can be different from the surface roughness of the other parts. For example, the surface roughness of the second part S2 can be the same as the surface roughness of the third part S1. However, the surface roughness of the second part S2 and the third part S1 can be different from the surface roughness of the first part S3. This is because at least one of the first part S3, the second part S2, and the third part S1 constituting the inner wall of the cavity is formed by a process different from the other parts. For example, the second part S2 and the third part S1 are formed by a laser process and a cleaning process. Alternatively, the first part S3 is formed by removing a portion of a circuit pattern. Therefore, the second part S2 and the third part S1 have surface roughness corresponding to the conditions of the laser process and the decontamination process, and the first part S3 may have surface roughness corresponding to the surface roughness of the side surface of a portion of the circuit pattern.

[0282] Meanwhile, in this embodiment, a Gaussian beam is used to form the cavity C. In this case, the outermost part of the cavity C is machined using the center point of the Gaussian beam. That is, a laser with maximum intensity is generated at the center point of the Gaussian beam, therefore, the tilt angle of the inner wall of the outermost cavity C can be smaller than the tilt angle of the comparative example.

[0283] In other words, the inner wall of the cavity can have a shape in which a first portion S3, a second portion S2, and a third portion S1 are connected to each other from their lower sides. The first portion S3 of the cavity can be connected to the upper surface of the first insulating layer 110. For example, the first portion S3 of the cavity can be in contact with the upper surface of the first insulating layer 110. The first portion S3 of the inner wall of the cavity can have a first tilt angle. For example, the tilt angle of the first portion S3 of the cavity can be substantially perpendicular to the reference plane BS.

[0284] The second portion S2 of the cavity may have a second tilt angle θ2. For example, the second tilt angle θ2 of the second portion S2 of the cavity may refer to the tilt angle of the dummy straight line connecting one end E1 and the other end E3 of the second portion S2 relative to the reference plane BS. For example, the reference plane BS may be the upper surface of the first insulating layer 110, but the embodiment is not limited thereto.

[0285] Furthermore, the third part S1 of the cavity may have a third tilt angle θ1. For example, the third tilt angle θ1 of the third part S1 of the cavity may be smaller than the second tilt angle θ2 of the second part S2. The third tilt angle θ1 of the third part S1 may refer to the tilt angle of the imaginary straight line connecting one end E2 of the third part S1 to the other end E1.

[0286] In other words, the third part S1 of the inner wall of the cavity is the part processed using the center point of the Gaussian beam. Therefore, the third part S1 can have a third tilt angle θ1 that is smaller than the second tilt angle θ2 of the second part S2.

[0287] The second portion S2 of the inner wall of the cavity can have an inclination angle θ2 ranging from 130 degrees to 160 degrees. In addition, the third portion S1 of the inner wall of the cavity can have a third inclination angle θ1 ranging from 92 degrees to 130 degrees, which is smaller than the second inclination angle θ2 of the second portion S2.

[0288] In other words, the inner wall of the cavity in the embodiment may have multiple inflection points. An inflection point may also be represented as a bend or a part where the angle changes.

[0289] For example, the inner wall of the cavity in the embodiment may have a first inflection point E3 and a second inflection point E2.

[0290] Additionally, in one embodiment, the cavity can be divided into a first portion S3 with a first tilt angle and a second portion S2 with a second tilt angle θ2 based on a first inflection point E3. Furthermore, in another embodiment, the cavity can be divided into a second portion S2 with a second tilt angle θ2 and a third portion S1 with a third tilt angle based on a second inflection point E2.

[0291] The first inflection point E3 can be the point where the first part S3 and the second part S2 of the inner wall of the cavity intersect each other. Additionally, the second inflection point E2 can be the point where the second part S2 and the third part S1 of the inner wall of the cavity intersect each other.

[0292] The height of the first inflection point E3 can correspond to the height of the circuit pattern 140. Preferably, the height of the first inflection point E3 can be the same as the height of a portion of the first circuit pattern 141 disposed on the upper surface of the first insulating layer 110. More preferably, the height of the first inflection point E3 can be the same as the height of the seed layer constituting the first circuit pattern 141.

[0293] In addition, the height of the second inflection point E2 can be set to be higher than the upper surface of pad 2141a.

[0294] In the above embodiment, when the cavity is formed, the outermost third part S1 of the cavity has a third tilt angle θ1, the second part S2 intersecting with the third part S1 has a second tilt angle θ2, and the first part S3 intersecting with the second part S2 has a first tilt angle.

[0295] This can be achieved by laser processing the first metal layer 2140a (which is a seed layer constituting the circuit pattern) as a stop layer to form a cavity, and further by processing the outermost part of the cavity using the center point of a Gaussian beam. Therefore, compared with the comparative example, the space required to form the cavity can be significantly reduced due to the reduced tilt angle of the outermost part of the cavity.

[0296] Therefore, in the embodiments, the cavity may include a first region having a third portion S1, a second region having a second portion S2, and a third region in addition to them.

[0297] The second part S2, which corresponds to the inner wall of the cavity in the second region, extends upward from the first part S3 and has a second tilt angle θ2. The first part S3 is one end of the third region R3 of the cavity.

[0298] In addition, the third part S1 corresponding to the first region R1 can extend upward from the second part S2, and has a third tilt angle θ1.

[0299] Figure 24 This is a view used to illustrate the method of processing a cavity according to the third embodiment. Figure 25 This is a view used to illustrate the machining method of the cavity according to the comparative example.

[0300] Reference Figure 24 In one embodiment, the outermost region of the cavity is processed using a beam along the centerline of a Gaussian beam. Alternatively, in another embodiment, the entire cavity region is processed while the Gaussian beam is moved a predetermined distance.

[0301] In this embodiment, the outermost region of the cavity is machined using the centerline of a first Gaussian beam. Furthermore, when the cavity machining using the first Gaussian beam is complete, a second Gaussian beam is provided at a predetermined distance spaced from the first Gaussian beam. In this case, since the first and second Gaussian beams are spaced apart by a predetermined distance, the cavity in this embodiment may include a third portion S1 with a third tilt angle θ1 in the outermost region and a second portion S2 extending from the third portion S1 and having a second tilt angle θ2.

[0302] At the same time, refer to Figure 25In the comparative example, the outermost edge of the laser beam is located at the outermost edge of the cavity to perform the cavity machining process.

[0303] Therefore, in the comparative example, the outermost inner wall of the cavity has an inclination angle of 160 degrees or more. On the other hand, in the embodiment, the outermost inner wall of the cavity has a third inclination angle in the range of 92 degrees to 130 degrees.

[0304] For example, in the comparative example process, when a cavity is machined in an area with a size of 600 μm, a cavity of 500 μm smaller than 600 μm is formed due to the tilt angle of the inner wall of the cavity. This is because the lower region of the cavity is used as a cavity for mounting components, and approximately 100 μm of space cannot be used due to the tilt angle of the inner wall.

[0305] On the other hand, in the embodiment, when a cavity is fabricated in a region with a size of 600 μm, a cavity of 550 μm is formed due to the improved tilt angle of the cavity's inner wall, which is larger than the cavity in the comparative example. Therefore, in the embodiment, the space required to form the cavity can be reduced, thereby improving the integration density of the circuit.

Claims

1. A circuit board, comprising: First insulating layer; A first circuit pattern is disposed on one surface of the first insulating layer and includes a 1-1 metal layer disposed on the first insulating layer and a 1-2 metal layer disposed on the 1-1 metal layer; as well as A second insulating layer is disposed on said one surface of the first insulating layer and includes a cavity. The first circuit pattern includes: 1-1 The circuit pattern is set to be closest to the cavity without overlapping the cavity in the vertical direction; The circuit pattern 1-2 is farther from the cavity than the circuit pattern 1-1 and does not overlap with the cavity in the vertical direction; Circuit patterns 1-3 are arranged in the cavity and overlap with the cavity in the vertical direction. Wherein, the width of the 1-1 metal layer of the 1-1 circuit pattern is greater than the width of the 1-2 metal layer of the 1-1 circuit pattern. Wherein, the width of the 1-1 metal layer of the 1-2 circuit pattern is equal to the width of the 1-2 metal layer of the 1-2 circuit pattern. Wherein, the width of the 1-1 metal layer of the 1-3 circuit pattern is equal to the width of the 1-2 metal layer of the 1-3 circuit pattern. Wherein, a portion of the side surface of the 1-1 metal layer of the 1-1 circuit pattern is exposed through the cavity and is not covered by the second insulating layer, and In this circuit pattern, the entire side surface of the 1-2 metal layer is covered by the second insulating layer.

2. The circuit board according to claim 1, wherein, The 1-1 metal layer of the first circuit pattern is the seed layer of the 1-2 metal layer of the first circuit pattern, and The 1-2 metal layer of the first circuit pattern is an electroplated layer formed by using the 1-1 metal layer of the first circuit pattern as a seed layer.

3. The circuit board according to claim 1, wherein, The 1-1 metal layer of the 1-1 circuit pattern includes a first portion that overlaps with the 1-2 metal layer of the 1-1 circuit pattern in the vertical direction and a second portion other than the first portion. The second portion of the 1-1 metal layer of the 1-1 circuit pattern is positioned closer to the cavity than the first portion of the 1-1 metal layer of the 1-1 circuit pattern.

4. The circuit board according to claim 3, wherein, The second portion of the 1-1 metal layer of the 1-1 circuit pattern surrounds the outer periphery of the cavity and is disposed between the first insulating layer and the second insulating layer.

5. The circuit board according to claim 1, wherein, The second insulating layer includes an insulating layer 2-1 disposed on the first insulating layer and an insulating layer 2-2 disposed on the insulating layer 2-1, and The cavity includes a first cavity passing through the 2-1 insulating layer and a second cavity passing through the 2-2 insulating layer.

6. The circuit board according to claim 5, wherein, The first cavity and the second cavity overlap in the vertical direction and have the same width as each other.

7. The circuit board according to claim 5, wherein, The first cavity and the second cavity overlap in the vertical direction and have different widths.

8. The circuit board according to claim 7, wherein, The width of the first cavity is smaller than the width of the second cavity.

9. The circuit board according to claim 8, wherein the circuit board includes a second circuit pattern disposed between the 2-1 insulating layer and the 2-2 insulating layer. The second circuit pattern includes: 2-1 Metal layer, disposed on one surface of the 2-1 insulating layer, and Metal layer 2-2 is disposed on one surface of metal layer 2-1, and The area of ​​the 2-1 metal layer is greater than the area of ​​the 2-2 metal layer.

10. The circuit board according to claim 9, wherein, At least a portion of the side surface of the 2-1 metal layer is exposed through the second cavity.

11. The circuit board according to claim 1, wherein, The inner wall of the cavity is perpendicular to the upper surface of the first insulating layer.

12. The circuit board according to claim 11, wherein, The horizontal cross-section of the cavity includes a curved surface.

13. The circuit board according to claim 12, wherein, The surface has a predetermined curvature and is located at the edge portion of the cavity.

14. The circuit board according to claim 13, wherein, The curvature at the edge portion of the cavity corresponds to the curvature of a circle in the range of 20 μm to 80 μm.

Citation Information

Patent Citations

  • Printed-circuit board and manufacturing method thereof

    JP2019046860A