Packaging structure and packaging method for avoiding adhesive contamination of components
By setting grooves and steps of specific sizes on the substrate and heat sink, combined with specific adhesives and thermal adhesives, the bridging and bridging problems caused by adhesive overflow during component packaging are solved, thereby achieving component protection and improving circuit reliability.
Patent Information
- Application Number
- CN202211730181.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-12-30
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2042-12-30
AI Technical Summary
In existing technologies, components are prone to bridging or open circuit risks due to glue overflow during the packaging process, and the glue fixes the shape, causing the components to be suspended, which affects the reliability of the circuit.
The design employs a heat sink groove and barrier step, which limits the spread of adhesive by setting grooves and steps of specific sizes on the substrate and heat sink, preventing adhesive from contaminating components. In the packaging process, a barrier is formed by using specific adhesives and heat-dissipating adhesives to avoid adhesive overflow.
It effectively prevents glue from contaminating components, avoids the risks of component bridging or open circuits, simplifies the packaging process, reduces costs, and improves circuit reliability.
Smart Images

Figure CN116314064B_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of integrated circuit technology, specifically relating to a packaging structure and packaging method that avoids adhesive contamination of components. Background Technology
[0002] Currently, FCBGA substrates are treated with SR (Surface Refill) for oxygen isolation and protection. The industry standard for SR is 5-20μm. Excessive SR thickness carries the risk of SR cracking. Furthermore, the secondary packaging thickness of WLCSP / Cowos wafers in the industry is around 910μm, and the thickness of the chip packaged in normal products is around 870μm. The industry standard for bottom filler is 50% of the standard chip corner height. This results in a wider spread of adhesive on the substrate, which compresses the space for component placement. If components come into contact with underfill / AD glue / Tim glue (thermal adhesive), these glues will maintain their shape during ball reflow soldering, causing components to adhere to the glue and resulting in components being suspended, creating a risk of circuit bridging / opening. This risk is significant and can be fatal to the product. Summary of the Invention
[0003] To address the technical problems existing in the prior art, the purpose of this invention is to provide a packaging structure and packaging method that avoids adhesive contamination of components.
[0004] To achieve the above objectives and technical effects, the technical solution adopted by this invention is as follows:
[0005] A packaging structure for preventing adhesive contamination of components includes a substrate and a heat sink. The heat sink covers the substrate and forms a cavity. A chip is disposed on the substrate and within the cavity. An SR groove is formed on the surface of the substrate near the chip. A plurality of heat sink grooves are formed on the heat sink in the contact area with the chip. A heat sink blocking step is provided on the edge of the heat sink, which is adapted to the SR step on the substrate. An AD adhesive is provided on the edge of the substrate, which can be held in place by the heat sink blocking step and the SR step. A filler adhesive is provided at the bottom of the chip, and a Tim adhesive is provided at the top of the chip, which can be embedded in the heat sink groove.
[0006] In the packaging structure provided by the present invention for avoiding adhesive contamination of components, the depth of the heat sink groove is 100-150 μm, which does not exceed 1 / 2 of the thickness of the heat sink.
[0007] In the packaging structure provided by the present invention for avoiding adhesive contamination of components, the width of the SR groove is 80-120μm and the depth is ≤20μm.
[0008] In the packaging structure provided by the present invention to avoid adhesive contamination of components, the width of the heat sink cover blocking step is 50-100μm, and the inward distance of the heat sink cover blocking step is consistent with the height of the SR step.
[0009] In the packaging structure provided by this invention to avoid adhesive contamination of components, the height of the SR step is ≤20μm when it exceeds the functional area of the substrate.
[0010] This invention also provides a packaging method for avoiding adhesive contamination of components, comprising the following steps:
[0011] Step 1: First, use a laser to burn SR grooves on the substrate, and remove the SR from the edge of the substrate;
[0012] Step 2: Perform SMT packaging and chip mounting as usual. Then, apply X23 adhesive around the SR groove to form an X23 heat dissipation barrier. Then, apply filler adhesive directly. During this process, the barrier must not be touched. Then, cure together.
[0013] Step 3: After curing, wash away the X23 heat dissipation barrier, and do not cover the capacitors on the substrate;
[0014] Step 4: First, a heat sink groove is made in the contact area between the copper layer inside the heat sink 10 and the chip. A heat sink blocking step is punched out at the edge of the heat sink, and its inward distance is consistent with the height of the SR step. Then, a nickel layer is electroplated on the overall surface.
[0015] Step 5: Apply Tim adhesive to the chip surface, embedding a portion of it into the groove of the heat sink cover. Then apply AD adhesive to the edge groove of the substrate. Cover the heat sink cover and use it to block the steps and SR steps to hold the AD adhesive in place, preventing it from overflowing and touching the components.
[0016] Step 6: Finally, apply the backing sticker, print the image, and attach the bulbs.
[0017] In step 1, the process parameters for grooving are: current 10-60A; speed 100-1000mm / s; frequency 50-500KHZ.
[0018] In step 4, the process parameters for grooving are: current 10-60A; speed 100-1000mm / s; frequency 50-500KHZ.
[0019] Compared with the prior art, the beneficial effects of the present invention are as follows:
[0020] This invention discloses a packaging structure and method for avoiding adhesive contamination of components. It employs thermal adhesive as a barrier, a heat sink groove as an adhesive expansion layer, and a stepped design at the edges of the substrate and heat sink to prevent contamination of components by filler adhesive, thermal adhesive, and other adhesives, significantly improving the adhesive overflow problem present in existing technologies. This invention requires no design modifications from the substrate supplier and can be implemented at the packaging plant. The entire process does not require complex design; appropriate modifications are made to the existing packaging structure without affecting other product functionalities. It avoids the risk of open circuits caused by solder overflow or component overhang during subsequent reflow processes, achieving cost savings and process improvement. Attached Figure Description
[0021] Figure 1 This is a schematic diagram of the structure of the present invention;
[0022] Figure 2 This is a schematic diagram of step 1 in a method for avoiding adhesive contamination of components according to the present invention;
[0023] Figure 3-4 This is a schematic diagram of step 2 in a method for avoiding adhesive contamination of components according to the present invention;
[0024] Figure 5 This is a schematic diagram of step 3 in a method for avoiding adhesive contamination of components according to the present invention;
[0025] Figure 6-7 This is a schematic diagram of step 4 in a method for avoiding adhesive contamination of components according to the present invention;
[0026] Figure 8-9 This is a schematic diagram of step 5 in a method for avoiding adhesive contamination of components according to the present invention;
[0027] Among them, 1. AD adhesive; 2. substrate; 3. SR; 4. capacitor; 5. SR groove; 6. filler adhesive; 7. chip; 8. Tim adhesive; 9. heat sink groove; 10. heat sink; 11. heat sink blocking step. Detailed Implementation
[0028] The present invention will now be described in detail so that its advantages and features can be more easily understood by those skilled in the art, thereby providing a clearer and more explicit definition of the scope of protection of the present invention.
[0029] The following provides a brief overview of one or more aspects to offer a basic understanding of them. This overview is not an exhaustive summary of all conceived aspects, nor is it intended to identify key or decisive elements of all aspects, nor to define the scope of any or all aspects. Its sole purpose is to present some concepts of one or more aspects in a simplified form to prepare for the more detailed descriptions that follow.
[0030] like Figure 1-9 As shown, a packaging structure to avoid adhesive contamination of components includes a substrate 2 and a heat sink 10. The heat sink 10 covers the substrate 2 and forms a cavity. A chip 7 is disposed on the substrate 2 and located within the cavity. An SR groove 5 is formed on the surface of the substrate 2 near the chip 7. Several heat sink grooves 9 are formed on the heat sink 10 in the contact area with the chip 7. A heat sink blocking step 11 is provided on the edge of the heat sink 10, which is adapted to the SR step on the substrate 2. An AD adhesive 1 is provided on the edge of the substrate 2. The AD adhesive 1 can be held in place by the heat sink blocking step 11 and the SR step. A filler adhesive 6 is provided at the bottom of the chip 7. A Tim adhesive 8 is provided at the top of the chip 7. The Tim adhesive 8 can be embedded in the heat sink groove 9.
[0031] The width of the SR groove 5 is 80-120μm and the depth is ≤20μm.
[0032] The depth of the groove 9 in the heat sink cover is 100-150μm, which does not exceed 1 / 2 of the thickness of the heat sink cover.
[0033] The width of the heat dissipation cover blocking step 11 is 50-100μm. The inward distance of the heat dissipation cover blocking step 11 is consistent with the height of the SR step. When it exceeds the functional area of the substrate, the height is ≤20μm. If it does not exceed the functional area of the substrate, it is not required.
[0034] A packaging method for a packaging structure that avoids adhesive contamination of components includes the following steps:
[0035] A substrate 2 and a heat sink 10 are provided. The surface of the substrate 2 is provided with an SR groove 5 and the edge of the substrate 2 is not punched with an SR 3. The heat sink 10 has a heat sink blocking step 11.
[0036] First, use thermal adhesive to cover the adhesive area in the SR groove 5 (the thermal adhesive used in this invention is X23 adhesive, which is commonly used in encapsulation processes. Its characteristics are: the pattern will not deform due to heat and it is not very sticky. It is easy to remove after curing and can be removed by washing with water and brushing. X23 adhesive can touch the components, but it will be washed off later). Then, apply filler adhesive 6 without contacting the components. Next, use the heat sink 10 to create several 100μm deep heat sink grooves 9 (which can be irregular grooves) in the area where the heat sink 10 and the chip 7 on the substrate 2 come into contact. In this way, the heat sink 10 itself can expand its volume to absorb and contain the thermal adhesive, preventing the thermal adhesive from overflowing onto the components. Finally, the heat sink blocking step 11, together with the SR step, holds the AD adhesive 1 in place, preventing excess adhesive from overflowing and achieving the effect of protecting the components and the circuit.
[0037] The packaging method for avoiding adhesive contamination of components provided by this invention specifically includes the following steps:
[0038] Step 1: First, use a laser to burn SR grooves 5 into substrate 2. The process parameters for grooving are: current 10-60A, speed 100-1000mm / s, frequency 50-500KHZ. Remove SR 3 (width consistent with the width of the heat sink foot) from the edge of substrate 2. This step can be done directly by the substrate supplier, or the supplier can be instructed not to plate SR by providing the width. See [link to documentation]. Figure 2 ;
[0039] Step 2: Perform normal SMT packaging and install chip 7. Then, apply X23 adhesive, making a circle around the SR groove 5 to form the X23 heat dissipation barrier 12. Next, apply filler adhesive 6 directly. During this process, the X23 heat dissipation barrier 12 should be located around the chip 7 and should not touch the chip 7 in any way. Then, cure together. See [link to documentation]. Figure 3-4 ;
[0040] Step 3: After curing, wash away the X23 heat sink 12, do not wrap the capacitor 4. If the glue residue can support the components, it needs to be washed again with water or removed with a brush. As long as there is no large area of glue residue, it is acceptable. See Figure 5 ;
[0041] Step 4: First, create heat sink grooves 9 in the contact area between the copper layer inside the heat sink 10 and the chip 7. These grooves can be created at irregular locations, and the number of grooves 9 should be as large as possible. The process parameters for creating the grooves are: current 10-60A, speed 100-1000mm / s, frequency 50-500kHz. Then, stamp out heat sink blocking steps 11 with a width of 50-100μm at the edge of the heat sink 10. The inward distance of these steps should be consistent with the height of the SR steps. Finally, electroplate a nickel layer onto the entire surface. See [link to relevant documentation]. Figure 6-7 ;
[0042] Step 5: Apply Tim adhesive 8 to the surface of chip 7, embedding a portion of it into the heat sink groove 9. Then, apply AD adhesive 1 to the edge groove of substrate 2. Cover with heat sink 10, using the heat sink to block the steps 11 and SR steps to hold AD adhesive 1 in place, preventing it from overflowing and touching components. See [link to relevant documentation]. Figure 8-9 ;
[0043] Step 6: Finally, perform backing adhesive, printing, and ball-planting processes to obtain the desired result. Figure 1 The structure shown.
[0044] Example 1
[0045] like Figure 1-9 As shown, a packaging structure to avoid adhesive contamination of components includes a substrate 2 and a heat sink 10. The heat sink 10 covers the substrate 2 and forms a cavity. A chip 7 is disposed on the substrate 2 and located within the cavity. An SR groove 5 is formed on the surface of the substrate 2 near the chip 7. Several heat sink grooves 9 are formed on the heat sink 10 in the contact area with the chip 7. A heat sink blocking step 11 is provided on the edge of the heat sink 10, which is adapted to the SR step on the substrate 2. An AD adhesive 1 is provided on the edge of the substrate 2. The AD adhesive 1 can be held in place by the heat sink blocking step 11 and the SR step. A filler adhesive 6 is provided at the bottom of the chip 7. A Tim adhesive 8 is provided at the top of the chip 7. The Tim adhesive 8 can be embedded in the heat sink groove 9.
[0046] The width of SR groove 5 is 100μm.
[0047] The depth of the heat sink groove 9 is 100μm.
[0048] The width of the heat dissipation cover blocking step 11 is 50-100μm, and the inward distance of the heat dissipation cover blocking step 11 is consistent with the height of the SR step, both being 20μm.
[0049] A packaging method for a packaging structure that avoids adhesive contamination of components includes the following steps:
[0050] A substrate 2 and a heat sink 10 are provided. The surface of the substrate 2 is provided with an SR groove 5 and the edge of the substrate 2 is not punched with an SR 3. The heat sink 10 has a heat sink blocking step 11.
[0051] First, use thermal adhesive to cover the adhesive area in the SR groove 5 (the thermal adhesive used in this invention is X23 adhesive, which is commonly used in encapsulation processes. Its characteristics are: the pattern will not deform due to heat and it is not very sticky. It is easy to remove after curing and can be removed by washing with water and brushing. X23 adhesive can touch the components, but it will be washed off later). Then, apply filler adhesive 6 without contacting the components. Next, use the heat sink 10 to create several 100μm deep heat sink grooves 9 (which can be irregular grooves) in the area where the heat sink 10 and the chip 7 on the substrate 2 come into contact. In this way, the heat sink 10 itself can expand its volume to absorb and contain the thermal adhesive, preventing the thermal adhesive from overflowing onto the components. Finally, the heat sink blocking step 11, together with the SR step, holds the AD adhesive 1 in place, preventing excess adhesive from overflowing and achieving the effect of protecting the components and the circuit.
[0052] The packaging method for avoiding adhesive contamination of components provided by this invention specifically includes the following steps:
[0053] Step 1: First, use a laser to burn a 100μm wide SR groove 5 into substrate 2. The process parameters for grooving are: current 10A, speed 100mm / s, frequency 50kHz. Remove SR 3 (width consistent with the width of the heat sink foot) from the edge of substrate 2. This step can be done directly by the substrate supplier, or the supplier can be instructed not to plate SR by providing the width. See [link to documentation]. Figure 2 ;
[0054] Step 2: Perform normal SMT packaging and install chip 7. Then, apply X23 adhesive, making a circle around the SR groove 5 to form the X23 heat dissipation barrier 12. Next, apply filler adhesive 6 directly. During this process, the X23 heat dissipation barrier 12 should be located around the chip 7 and should not touch the chip 7 in any way. Then, cure together. See [link to documentation]. Figure 3-4 ;
[0055] Step 3: After curing, wash away the X23 heat sink 12, do not wrap the capacitor 4. If the glue residue can support the components, it needs to be washed again with water or removed with a brush. As long as there is no large area of glue residue, it is acceptable. See Figure 5 ;
[0056] Step 4: First, create a 100μm deep heat sink groove 9 in the contact area between the copper layer inside the heat sink 10 and the chip 7. The process parameters for creating the groove are: current 10A, speed 100mm / s, frequency 50kHz. The heat sink groove 9 can be created at irregular locations, and the number of heat sink grooves 9 should be as large as possible. A 100μm wide heat sink blocking step 11 is stamped at the edge of the heat sink 10. The inward distance of this step should be consistent with the height of the SR step, which should be 20μm. Then, electroplate a nickel layer onto the entire surface. See [link to relevant documentation]. Figure 6-7 ;
[0057] Step 5: Apply Tim adhesive 8 to the surface of chip 7, embedding a portion of it into the heat sink groove 9. Then, apply AD adhesive 1 to the edge groove of substrate 2. Cover with heat sink 10, using the heat sink to block the steps 11 and SR steps to hold AD adhesive 1 in place, preventing it from overflowing and touching components. See [link to relevant documentation]. Figure 8-9 ;
[0058] Step 6: Finally, perform backing adhesive, printing, and ball-planting processes to obtain the desired result. Figure 1 The structure shown.
[0059] Any parts or structures not specifically described in this invention can be made using existing technologies or products, and will not be elaborated upon here.
[0060] The above description is merely an embodiment of the present invention and does not limit the patent scope of the present invention. Any equivalent structural or procedural transformations made based on the content of the present invention specification, or direct or indirect applications in other related technical fields, are similarly included within the patent protection scope of the present invention.
Claims
1. A packaging structure that avoids adhesive contamination of components, characterized in that, The device includes a substrate and a heat sink. The heat sink covers the substrate and forms a cavity. A chip is disposed on the substrate and within the cavity. An SR groove is formed on the surface of the substrate near the chip. The width of the SR groove is 80~120μm and the depth is ≤20μm. Several heat sink grooves are formed on the heat sink in the contact area with the chip. The depth of the heat sink grooves is 100~150μm and does not exceed 1 / 2 of the thickness of the heat sink. A heat sink blocking step is provided on the edge of the heat sink, which is adapted to the SR step on the substrate. The width of the heat sink blocking step is 50~100μm and the inward distance of the heat sink blocking step is consistent with the height of the SR step. An AD adhesive is provided on the edge of the substrate. The AD adhesive can be held in place by the heat sink blocking step and the SR step. A filler adhesive is provided at the bottom of the chip. A Tim adhesive is provided at the top of the chip. The Tim adhesive can be embedded in the heat sink groove.
2. The packaging structure for avoiding adhesive contamination of components according to claim 1, characterized in that, When the SR step extends beyond the functional area of the substrate, its height is ≤20μm.
3. A packaging method for a packaging structure that avoids adhesive contamination of components according to claim 1 or 2, characterized in that, Includes the following steps: Step 1: First, use a laser to burn SR grooves on the substrate, and remove the SR from the edge of the substrate; Step 2: Perform SMT packaging and chip mounting as usual. Then, apply X23 adhesive around the SR groove to form an X23 heat dissipation barrier. Then, apply filler adhesive directly. During this process, the barrier must not be touched. Then, cure together. Step 3: After curing, wash away the X23 heat dissipation barrier, and do not cover the capacitors on the substrate; Step 4: First, a heat sink groove is made in the contact area between the copper layer inside the heat sink 10 and the chip. A heat sink blocking step is punched out at the edge of the heat sink, and its inward distance is consistent with the height of the SR step. Then, a nickel layer is electroplated on the overall surface. Step 5: Apply Tim adhesive to the chip surface, embedding a portion of it into the groove of the heat sink cover. Then apply AD adhesive to the edge groove of the substrate. Cover the heat sink cover and use it to block the steps and SR steps to hold the AD adhesive in place, preventing it from overflowing and touching the components. Step 6: Finally, apply the backing sticker, print the image, and attach the bulbs.
4. The packaging method for a packaging structure that avoids adhesive contamination of components according to claim 3, characterized in that, In step 1, the process parameters for grooving are: current 10~60A; speed 100~1000mm / s; frequency 50~500KHZ.
5. The packaging method for a packaging structure that avoids adhesive contamination of components according to claim 3, characterized in that, In step 4, the process parameters for grooving are: current 10~60A; speed 100~1000mm / s; frequency 50~500KHZ.
Citation Information
Patent Citations
Chip packaging structure and packaging method thereof
CN113451152A
Radiating fin device for preventing radiating fin glue spilling in semi conductor packaging parts
CN1549337A