Method of manufacturing electronic component assembly on front surface of semiconductor wafer
By using a marker mask and adjusting the lithography parameters in the photolithography step, a marker specific to each field region is formed, solving the cost and time problems of tracing the position of components in the prior art, and realizing efficient component position tracking and mass production.
Patent Information
- Application Number
- CN202180070643.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-10-16
- Filing Date
- 2021-10-18
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2041-10-18
AI Technical Summary
In existing methods for manufacturing electronic components on semiconductor wafers, tracing the location of components requires additional photolithography steps and manual operations, resulting in high costs and extended production time, and making it unsuitable for mass production.
In the photolithography step, a marker mask is used to create a marker specific to each field area by adjusting photolithography parameters such as exposure dose and focus, thus avoiding additional photolithography steps and mask application.
It enables accurate tracking of component positions without adding photolithography steps, reducing production costs and time, and is suitable for mass production.
Smart Images

Figure CN116348818B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of semiconductors. More specifically, this invention relates to a method for manufacturing an assembly of electronic components on a semiconductor wafer, the method being capable of positioning all or part of these components on the wafer. Background Technology
[0002] In the semiconductor industry, a common method for manufacturing large quantities of electronic components is to finely fabricate assemblies of identical electronic components on semiconductor wafers. To form a stack of layers on the wafer (which together form the electronic components), photolithography is typically used. The principle of these techniques is well-known: a layer of material is deposited over the entire wafer, and then a photoresist is deposited on that layer. A photomask is then applied above the photoresist at a level called the first exposure field, representing a portion of the surface area of the semiconductor wafer. In the first exposure field, the portion not covered by the mask is then exposed, locally changing the photoresist. This sequence of applying the photomask and exposure is repeated sequentially in each subsequent exposure field. The changed resin is then removed, and the layer is locally etched across the entire surface of the semiconductor wafer according to the pattern of the mask before the remaining photoresist is removed in turn. Thus, this process is repeated for each layer in the stack by using a different photomask each time.
[0003] When all electronic components are formed on a wafer, the wafer is diced around each component to form a chip, and then the chips are individually packaged in a package. Typically, chip pick-and-place equipment uses calculations to ensure a match between each chip (component) and the semiconductor wafer from which it originated.
[0004] However, in the event of component failure, it may be desirable to trace the exact location of the electronic component on the wafer to verify the physical parameters of the layers manufactured in the corresponding area of the wafer, and to aid in failure analysis.
[0005] Traceability of electronic components can be achieved during assembly, i.e., when the component is packaged, there is a specific marking on the package. However, this operation, which is usually performed manually by operators, results in significant costs and production time. Furthermore, if the component is not packaged in a package, it is unsuitable and not suitable for mass production.
[0006] Some assembly lines offer semi-manual solutions, under operator supervision, for sampling, mapping the location of components on the wafer to wafer numbers, and serializing packages. However, all of these operations require human intervention, which can be a source of error.
[0007] Document US8187897 discloses a method for fabricating an assembly of electronic components on a semiconductor wafer. A single pattern is attached to a layer of the electronic component, forming a unique identifier for the component, making it possible to trace the wafer from which it originated and its location on the wafer.
[0008] However, this method has the drawback of certain implementation complexity, especially compared to traditional methods of manufacturing components, as it requires the application of additional photolithography masks to generate specific patterns for each component. Such application leads to additional costs and production time. Summary of the Invention
[0009] This invention relates to a solution that replaces the prior art and is designed to overcome all or some of the aforementioned disadvantages. It particularly relates to a method for manufacturing assemblies of electronic components on a semiconductor wafer, a method that enables the positioning of each electronic component on the wafer after dicing without requiring additional photolithography steps during the fine fabrication of the electronic component assembly.
[0010] To achieve this objective, the present invention aims to provide a method for fabricating an assembly of electronic components on the front surface of a semiconductor wafer, the assembly including a plurality of field regions, each region including at least one field, and each field including at least one electronic component, the method including a plurality of photolithography steps to form a stack of layers that form each electronic component, each photolithography step including the continuous application of a mask to each field in a photolithography apparatus.
[0011] A significant feature of the manufacturing method according to the invention is that one of the masks further includes a marking pattern, the mask being referred to as a marking mask, and is characterized in that, in the photolithography step associated with the marking mask, at least one photolithography parameter of the photolithography apparatus is different for each field region, so as to expose the marking pattern differently in each field region.
[0012] Therefore, at the end of the photolithography step associated with the identification mask, identification marks specific to each field region are formed because the spatial resolution of the identification pattern from which the marks originate is different between each field region.
[0013] Other advantageous and non-limiting features according to the invention, individually or in any technically feasible combination:
[0014] • The plurality of photolithography steps include a contact opening step for electronic components, wherein the marking mask is a mask applied in the contact opening step;
[0015] • The lithography parameters are selected from the exposure dose and focus;
[0016] • Exposure dose of 5 mJ / cm 2 and 1000mJ / cm 2 Changes between;
[0017] • The focus change is + / - 10 μm;
[0018] • The marking pattern has at least one dimension on the order of several μm, typically in the range of 1 micrometer to 20 micrometers;
[0019] Electronic components include high electron mobility transistors based on III-N materials;
[0020] • At least one field area includes multiple fields;
[0021] Each area comprises multiple fields.
[0022] The present invention also relates to an electronic structure formed by an assembly of electronic elements disposed on the front surface of a semiconductor wafer, the assembly of electronic elements comprising a plurality of field regions, each region comprising at least one field, and each field comprising at least one electronic element, each element being formed by a stack of layers. A significant feature of the electronic structure is that the electronic elements include identification markings specific to each field region, because the spatial resolution of the identification markings derived from the identification pattern differs between each field region. Attached Figure Description
[0023] Other features and advantages of the invention will become apparent from the following detailed description in conjunction with the accompanying drawings, wherein:
[0024] [ Figure 1 ] Figure 1 A semiconductor wafer comprising electronic components obtained by the manufacturing method according to the invention is shown;
[0025] [ Figure 2 ] Figure 2 Different examples of the logo patterns according to the present invention are shown;
[0026] [ Figure 3 ] Figure 3 Different markings obtained from different marking patterns and for different photolithographic parameters according to the present invention are shown.
[0027] These figures are simplified representations and are not necessarily to scale for readability purposes. The same reference numerals in the figures may be used for elements of the same nature. Different possibilities (variations and embodiments shown and / or detailed in the description below) should be understood as non-exclusive to each other and may be combined together. Detailed Implementation
[0028] This invention relates to assemblies of electronic components. An electronic component refers to any component ranging in size from micrometers to millimeters, formed by a stack of layers, capable of transmitting, processing, or storing information using electric current. Therefore, each electronic component may be formed or comprised of, for example, resistors, capacitors, coils, transistors, integrated circuits, any combination or assembly of these components, or other components or assemblies of components known to those skilled in the art.
[0029] Preferably, but not limiting of the invention, the electronic components may specifically include high electron mobility transistors formed on a substrate based on III-N material.
[0030] More generally, electronic component 3 is formed on the front surface of semiconductor wafer 1. Figure 1 The semiconductor wafer 1 preferably takes the form of a circular substrate with a diameter ranging from 100 mm to 450 mm and a thickness of 100 to 1500 micrometers. The semiconductor wafer 1 can be formed from any semiconductor material, such as silicon, and more specifically from a stack of III-N materials as previously discussed.
[0031] Of course, the present invention is by no means limited to this shape, size or composition of semiconductor wafer 1.
[0032] The front surface of semiconductor wafer 1 defines an (x, y) plane, and a stack of layers forming electronic components is formed along the z-axis perpendicular to this (x, y) plane. The formation of this stack requires a series of steps, known as manufacturing steps, namely, layer deposition steps, photolithography steps to determine the structure of the layers, etching steps to structure the layers, surface treatment steps, etc.
[0033] As noted in the introductory section of this application, during the photolithography process, a photomask is applied and light is exposed at the level of field 2 (also referred to as exposure field 2). Field 2 may include a single electronic component or multiple electronic components 3, typically between two and several hundred. In order to... Figure 1 In a simplified version, element 3 is shown only on four fields 2. In the case of points, there are nine elements 3 in each field 2.
[0034] like Figure 1 As shown, the front surface of the semiconductor wafer 1 includes multiple field regions 4 ( Figure 1The example schematically illustrates five field regions 41, 42, 43, 44, and 45. Each region 4 includes at least one field 2, preferably multiple fields 2. The number and distribution of fields in each region 4 can be the same for all regions 4, or they can differ from one region to another. As will be described later, the present invention provides the possibility of clustering multiple fields 2 into field regions 4, such that fields 2 in the same region 4 have similar properties, while fields 2 in different regions 4 have different identifiable properties.
[0035] Therefore, in Figure 1 In the simplified example, the first region 41 includes a single field 2 located at the center of the semiconductor wafer 1. The second region 42 includes eight fields 2, the third region 43 includes sixteen fields 2, the fourth region 44 includes twenty-four fields 2, and the fifth region 45 includes twenty fields 2. For simplicity, the element 3 of each field 2 is shown only on two fields of the second region 42 and on one field of the third region 43 and the fourth region 44.
[0036] The shape and size of region 4 can be freely chosen. Preferably, when the semiconductor wafer 1 is a circular substrate, region 4 can be selected to be concentric, as shown in... Figure 1 In the example, region 4 can represent a portion of semiconductor wafer 1, such as half or a quarter of the wafer. Region 4 can also be a portion of semiconductor wafer 1 along one or the other of the x-axis and y-axis, and the invention is not limited in any way to the distribution of such regions.
[0037] Returning to the manufacturing method according to the invention, this method includes multiple photolithography steps to form a stack of layers that form each electronic component 3. These photolithography steps are separated from other known steps capable of forming the stack, such as heat treatment, deposition, etching, cleaning, doping, or polishing steps. The various formation steps for forming the stack of electronic components are very conventional and known to those skilled in the art, and will only be briefly discussed.
[0038] Therefore, the heat treatment step is carried out in a furnace, typically at a temperature range of 400 to 1200°C, to form a silicon nitride or oxide layer, or to rearrange the crystal lattice.
[0039] The deposition process can be performed using a variety of known physical or chemical techniques, depending on the type of layer required and the compatibility of the stack, particularly in terms of temperature. The deposited layer can have a variety of properties: semiconductor, insulating, or conductive.
[0040] In each photolithography step, a semiconductor wafer 1 is arranged in a photolithography apparatus (not shown). After a resist layer is typically deposited on the entire surface of the wafer 1, each photolithography step includes successively applying a mask to each field 2. When applied to the field 2, the field 2 is exposed to a low-wavelength light source, typically ultraviolet or X-rays, to project the image of the mask onto the resist layer, forming a structure within the resist layer.
[0041] The etching step can be performed by wet etching or dry etching to replicate the structure of the resist layer located in the underlying material layer. This structure can, for example, include an arrangement of fingers that cross-form the gate, source, and drain of a transistor, an arrangement of an open network forming conductive interconnect vias, or an arrangement of multiple contact pads connecting each element 3. In all cases, the structure here is functional; that is, its shape and layout are defined to enable the electronic element 3 to function.
[0042] Typically, when electronic component 3 includes a transistor, the resulting stack includes an active semiconductor layer on which multiple interconnect layers are stacked, and finally includes an upper passivation layer.
[0043] Once all electronic components 3 have been formed on wafer 1, wafer 1 is cut around each component 3 to form a chip, which is then individually packaged in a package.
[0044] In the manufacturing method according to the invention, one of the masks used during one of the photolithography steps includes, in addition to the so-called functional patterns used to form the stacked functional structures, an identifier pattern. Because it has this additional pattern, the mask is referred to in this disclosure as an "identifier mask".
[0045] According to the invention, in the photolithography step associated with the marking mask, at least one photolithography parameter of the photolithography apparatus is different for each field region 4, so as to expose the marking pattern differently in each field region 4. In other words, in the photolithography step associated with the mask having the marking pattern, the marking mask is continuously applied over each field 2; and when the mask leaves field region 4 and enters another field region, at least one photolithography parameter of the photolithography apparatus is modified. Of course, the variation of the photolithography parameter is controlled, and its value is associated with the region 4 in question.
[0046] Therefore, the shape of the marking pattern on the resist and the shape of the marking marks subsequently formed in the underlying layer differ from one region 4 to another. Thus, after dicing the electronic component 3, the region 4 of the wafer 1 from which the component 3 originates can be identified by analyzing the shape of the marking marks, which are associated with the photolithographic parameters capable of forming the component 3, and therefore with the region 4 of the semiconductor wafer 1 from which the component 3 originates. Therefore, the manufacturing method according to the invention enables the identification of the location of the component 3 in each region 4 of the semiconductor wafer 1 through a simple, controlled variation of the photolithographic parameters from one region 4 to another without performing additional photolithography steps (i.e., by performing only manufacturing photolithography), particularly without applying additional masks.
[0047] Therefore, in Figure 1 In the example shown, the elements 3 of the two fields in the second region 42 will have the same identification mark, but unlike the elements of the fields in the third region 43 and the fourth region 44, they are different from each other.
[0048] Although the shape and size of the marking pattern can be freely chosen, for each region 4, it is necessary to be able to identify and characterize the deformation of the marking according to the photolithographic parameters.
[0049] Examples of logo patterns are as follows Figure 2 As shown. Therefore, the marking pattern can be a linear opening of a given thickness drawn on the mask (as shown). Figure 2 (a) Two rods with given thickness and spacing ( Figure 2 (b) Multiple disks of decreasing diameter aligned in one direction and spaced at fixed or variable distances. Figure 2 (c) Multiple bars spaced further apart in one direction ( Figure 2 (d)). However, the invention is certainly not limited to examples of this pattern.
[0050] The characteristics of the marking pattern (the size and shape of the pattern mentioned above) depend on the type of resin used in the photolithography step associated with the marking mask. To be sensitive to modifications of the photolithography parameters, the marking pattern advantageously has a size on the order of the resist thickness.
[0051] The lithographic parameters that vary from one region to another are parameters that modify the exposure of the marking pattern from one region to another. They can be selected, in particular, from exposure dose or focus. Exposure dose corresponds to the light energy received by the resin, and focus corresponds to sharpness adjustment. Of course, multiple parameters can be varied simultaneously or alternately, and other parameters that modify the exposure can be envisioned. In all cases, the value of this parameter or these parameters will be associated with each region 4 of the semiconductor wafer 1.
[0052] When the varying photolithography parameters are exposure doses, the latter can typically reach 5 mJ / cm². 2 and 1000mJ / cm 2 The changes between them.
[0053] When the lithography parameter is changed to focus, the latter can typically be changed by + / -10μm.
[0054] These variations in dosage and focus are wide enough to envision significant changes between fields.
[0055] Therefore, for each component in a field area, the spatial resolution of the identification pattern from which the identification mark originates will be specific and will differ between one field area and another.
[0056] Depend on Figure 2 The example of the logo pattern formed in the illustration is shown in Figure 3 The diagram shows three regions 42, 43, and 44 (denoted by points ii, iii, and iv, respectively). The lithographic parameter that varies from one region to another is the exposure dose, which decreases from region 42 to region 43, and then from region 43 to region 44.
[0057] Therefore, if from Figure 2 Starting with the marking pattern in (a), a straight opening can be observed, which is completely replicated when the exposure dose is at its maximum. Figure 3 (a)ii), incomplete replication when exposure dose is moderate ( Figure 3 (a)iii), no replication occurs when the exposure dose is minimal. Figure 3 (a)iv).
[0058] The maximum exposure dose may correspond to a nominal value of exposure dose, which decreases relative to the nominal value for other areas. Of course, this does not limit the invention, and the nominal exposure dose may correspond to an intermediate value, which varies above or below the value depending on the area, or it may correspond to a minimum value, where the exposure dose increases relative to the nominal value for other areas.
[0059] According to another example, when from Figure 2 (b) When the marking pattern begins, it can be observed that when the exposure dose is at its maximum ( Figure 3 (b)ii) The two completely replicated bars are superimposed, and at the same time when the exposure dose is moderate ( Figure 3 (b)iii) can distinguish between two different shapes, and when the exposure dose is minimal ( Figure 3 (b)iv) Form a single strip.
[0060] Similarly, if from Figure 2 Starting with the marking pattern in (c), it can be observed that when the exposure dose is at its maximum ( Figure 3 (c)ii) Multiple disks are perfectly defined, each disk being completely different, and the different shapes partially overlap when the exposure dose is moderate. Figure 3 (c)iii) When the exposure dose is minimum, the disk with the smallest diameter will not repeat. Figure 3 (c)iv).
[0061] Based on yet another example, from Figure 2 Starting with the marking pattern in (d), it can be observed that when the exposure dose is maximum, multiple bars are completely replicated. Figure 2 (d)ii). When the exposure dose is moderate, three stripes with the smallest spacing are superimposed ( Figure 2 (d)iii). Finally, when the exposure dose is minimum, the four bars with the smallest spacing are superimposed.
[0062] Therefore, by identifying the shape of the mark for each component, the shape can be associated with a given exposure dose, and more generally with a given lithography parameter, and thus the shape can be associated with the field region 4 of the wafer 1 from which the element 3 originates.
[0063] Of course, the size of the marking pattern must be small enough, and the marking pattern must be far enough away from the functional pattern of the marking mask so that the marking formed by the marking pattern does not affect the integrity of the layer under consideration and the functional structure of the lower and upper layers.
[0064] Typically, although the surface size of the functional structure of the active layer of the element in the plane formed by the front surface of the semiconductor wafer 1 is 10 nm 2 Up to 10 5 μm 2 The order of magnitude, or the size of the contact of the component at the surface of the upper passivation layer, is typically in the range of 10. 6 μm 2 The order of magnitude, but the size of the marking pattern can be as small as 20 μm. 2 The distance between the structural pattern and the marking pattern on the marking mask is typically chosen to be greater than 1 μm.
[0065] For example, one could mention contact openings in the range of 500μm to 2000μm and markings in the range of 5 to 10μm, which originate from marking patterns present on the contact opening mask.
[0066] Therefore, to avoid affecting the stacked, more complex, and functional layers, it is preferable that the marking mask is a mask used to form layers away from the active layer. Furthermore, it is preferable that the selected layer receiving the marking pattern is detectable on the electronic component after its fabrication. Therefore, the photolithography step, typically performed on the upper passivation layer, corresponding to the openings of the electrical contacts of the electronic component, is particularly suitable for the implementation of the marking mask. The markings are then arranged on the upper passivation layer, which has the advantage of being visible under visual inspection. Then, observing the bare component with an optical microscope will allow identification of its original position on the wafer. Of course, in addition to simple optical microscopy, other optical methods can be used to analyze the markings, such as optical analysis using pattern recognition software.
[0067] Therefore, the manufacturing method according to the invention enables the production of a semiconductor wafer having electronic components disposed on its front surface. The semiconductor wafer has multiple field regions, each electronic component occupying a field on the front surface of the wafer, each region including at least one field, and each electronic component formed by a stack of layers. Each component includes an identification mark derived from an identification pattern. The spatial resolution and shape of these identification marks are different between each field region. Therefore, the identification mark is different for each region 4, so that once the electronic structure surrounding each electronic component 3 has been cut, the region 4 of the wafer 1 from which the electronic component 3 originates can be identified.
[0068] Of course, the present invention is not limited to the described embodiments, and alternative embodiments may be introduced without departing from the framework of the invention as defined by the claims.
Claims
1. A method for fabricating an assembly of electronic components (3) on the front surface of a semiconductor wafer (1), the front surface of the semiconductor wafer (1) comprising a plurality of field regions (4), each region (4) comprising at least one field (2), and each field (2) comprising at least one electronic component (3), the method comprising a plurality of photolithography steps to form a stack of layers, the stack of layers forming each electronic component (3), each photolithography step comprising sequentially applying a mask to each field (2) in a photolithography apparatus; The method is characterized in that one of the masks includes an identification pattern, the mask being referred to as an identification mask, and is characterized in that, in the lithography step associated with the identification mask, at least one lithography parameter of the lithography apparatus is different for each field region (4) to expose the identification pattern differently in each field region (4).
2. The method according to claim 1, wherein the plurality of photolithography steps include a contact opening step of the electronic component (3), and the marking mask is a mask applied in the contact opening step.
3. The method according to claim 1, wherein the lithography parameters are selected from exposure dose and focus.
4. The method according to claim 3, wherein the exposure dose is 5 mJ / cm 2 and 1000mJ / cm 2 The changes between them.
5. The method of claim 3, wherein the focus change is + / - 10 µm.
6. The method according to claim 1, wherein the marking pattern has at least one size on the order of several µm.
7. The method of claim 1, wherein the size of the marking pattern is in the range of 1 micrometer to 20 micrometers.
8. The method of claim 1, wherein the electronic component (3) comprises a high electron mobility transistor based on a III-N material.
9. The method according to claim 1, wherein each field region (4) comprises a plurality of fields (2).
10. An electronic structure formed from an assembly of electronic elements (3) finely processed by the method of any one of the preceding claims, the electronic elements including identification marks specific to each field region, since the spatial resolution of the identification marks derived from the identification pattern is different between each field region.
Citation Information
Patent Citations
Fabricating product chips and die with a feature pattern that contains information relating to the product chip
US8187897B2
Product Chips and Die With a Feature Pattern That Contains Information Relating to the Product Chip, Methods for Fabricating Such Product Chips and Die, and Methods for Reading a Feature Pattern From a Packaged Die
US20100044858A1
Method and device for marking objects
US20100279231A1