Semiconductor device and method of manufacturing the same
By designing alternating first and second well regions in a semiconductor device and adjusting the doping concentration and interface shape, the contradiction between increasing breakdown voltage and reducing on-resistance in high-voltage devices was resolved, thus realizing a method for fabricating semiconductor devices with high breakdown voltage and low resistance.
Patent Information
- Application Number
- CN202111674077.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-12-31
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2041-12-31
AI Technical Summary
Existing high-voltage devices have a contradictory relationship: while increasing the breakdown voltage, it is difficult to effectively reduce the on-resistance. Current technologies typically increase the breakdown voltage by increasing the ion concentration in the drift region and repeatedly inserting implantation regions with the opposite conductivity type, but this narrows the current path and makes it difficult to reduce the on-resistance.
In semiconductor devices, by alternating first and second well regions along the width of the conductive channel in the drift region, setting the upper surface size of the second well region to be smaller than the lower surface size, and adjusting the doping concentration and interface shape during the fabrication process, the current path width is increased and the on-resistance is reduced.
This method effectively reduces on-resistance while increasing breakdown voltage. By inserting a second well region in the drift region and adjusting the doping concentration and interface shape, the current path of the device is optimized, achieving the effect of high breakdown voltage and low resistance.
Smart Images

Figure CN116417499B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of semiconductor technology, and in particular to a semiconductor device and its fabrication method. Background Technology
[0002] High-voltage devices are widely used in integrated circuits due to their high input resistance, low noise, low power consumption, and high flexibility. For high-voltage devices, turn-on voltage, on-resistance, saturation current, and breakdown voltage are key parameters. Among these, the specific on-resistance (Ron,sp) in the drift region has a contradictory relationship with the device's breakdown voltage (BV): Ron,sp ∝ BV. β How to alleviate the contradiction between on-resistance and breakdown voltage, that is, how to effectively improve the withstand voltage while reducing the on-resistance, has become a difficult problem that needs to be solved by those skilled in the art. Summary of the Invention
[0003] Therefore, it is necessary to provide a semiconductor device with high breakdown voltage and low on-resistance, and a method for fabricating the same.
[0004] A semiconductor device, comprising:
[0005] The substrate has a first type of conductivity;
[0006] A drift region, located on the upper surface of the substrate, includes at least two first well regions having a second conductivity type and at least one second well region having a first conductivity type, arranged alternately and adjacently along the width direction of the device conductive channel, wherein the first conductivity type and the second conductivity type are electrically opposite; the upper surface of at least one second well region has a smaller dimension in the width direction of the device conductive channel than the lower surface of the second well region in the width direction of the device conductive channel.
[0007] In one embodiment, the doping concentration of the upper surface of the second well region is greater than the doping concentration of the lower surface of the second well region.
[0008] In one embodiment, the upper surfaces of the first well region and the second well region are coplanar with the upper surface of the substrate, the lower surfaces of the first well region and the second well region are coplanar, and the thickness of the first well region is equal to the thickness of the second well region.
[0009] In one embodiment, the second well region includes a first doped region and a second doped region located below the first doped region, wherein the doping concentration of the first doped region is greater than the doping concentration of the second doped region.
[0010] In one embodiment, at least one of the interfaces between the first well region and the second well region is inclined to the plane of the substrate.
[0011] In one embodiment, the cross-sectional shape of both the first well region and the second well region along the width direction of the conductive channel of the device is trapezoidal.
[0012] In one embodiment, the semiconductor device further includes:
[0013] The source region is located on the upper surface of the substrate and is spaced apart from the drift region, and has the second conductivity type;
[0014] A body region, which surrounds the source region and is adjacent to or spaced apart from the drift region;
[0015] A body lead-out region is located on the upper surface of the body region and is disposed adjacent to the source region, and the body lead-out region has the first conductivity type;
[0016] A gate is located on the upper surface of the substrate and extends to cover the drift region, the body region and the source region;
[0017] The drain region is located on the upper surface of the drift region and is spaced apart from the gate.
[0018] In one embodiment, the doping concentration of the body region is greater than the doping concentration of the second well region of the first conductivity type.
[0019] A method for fabricating a semiconductor device, comprising:
[0020] A substrate is provided, the substrate having a first conductivity type;
[0021] A drift region is formed on the upper surface of the substrate. The drift region includes at least two first well regions having a second conductivity type and at least one second well region having a first conductivity type, which are alternately and adjacently contacted along the width direction of the device conductive channel. The first conductivity type and the second conductivity type are electrically opposite.
[0022] At least one of the upper surfaces of the second well region has a dimension smaller than that of the lower surface of the second well region in the same direction as the conductive channel of the device.
[0023] In one embodiment, the drift region formed on the upper surface of the substrate includes at least two first well regions of a second conductivity type and at least one second well region of a first conductivity type arranged alternately and adjacently along the width direction of the device conductive channel, comprising:
[0024] A third well region having the second conductivity type is formed on the upper surface layer of the substrate;
[0025] The third well region is formed by performing a first conductivity type doping process, and the remaining third well region that has not undergone the first conductivity type doping process serves as the first well region.
[0026] In one embodiment, the first conductivity type doping process is performed in the third well region to form the second well region, and the remaining third well region that has not undergone the first conductivity type doping process serves as the first well region, including:
[0027] A first ion implantation of the first conductivity type is performed to form a first ion implantation region, which is formed within the third well region and extends from the upper surface of the third well region to the interior of the third well region.
[0028] A second ion implantation of the first conductivity type is performed to form a second ion implantation region. The second ion implantation region is formed within the third well region and located below the first ion implantation region. The projected area of the second ion implantation region on the substrate is larger than the projected area of the first ion implantation region on the substrate.
[0029] Heat treatment is performed to expand the first ion implantation region into a first doped region, and the second ion implantation region into a second doped region adjacent to and in contact with the first doped region. The lower surface of the second doped region is coplanar with the lower surface of the third well region. The first doped region and the second doped region are combined to form the second well region. The remaining third well region, which has not undergone the first conductivity type ion implantation treatment, is used as the first well region.
[0030] In one embodiment,
[0031] The process of performing the first ion implantation of the first conductivity type to form the first ion implantation region includes:
[0032] A mask layer with a first opening pattern is formed on the surface of the substrate, the first opening pattern exposing a portion of the upper surface of the third well region; a first conductivity type ion implantation is performed to form a first ion implantation region extending from the upper surface of the third well region into the interior of the third well region; and / or
[0033] The second ion implantation of the first conductivity type to form the second ion implantation region includes:
[0034] A mask layer with a second opening pattern is formed on the substrate surface, the second opening pattern exposing the upper surface of the first ion implantation region and a portion of the upper surface of the third well region surrounding the first ion implantation region. A second first conductivity type ion implantation is performed to form the second ion implantation region located within the third well region and below the first ion implantation region.
[0035] In one embodiment, when forming a mask layer with a first opening pattern on the substrate surface, forming a mask layer with a second opening pattern on the substrate surface includes:
[0036] The mask layer with the first opening pattern is etched back, and the first opening pattern is enlarged to expose the upper surface of a portion of the third well region surrounding the first ion implantation region, thereby obtaining the mask layer with the second opening pattern on the substrate surface.
[0037] In one embodiment, the ion implantation energy for performing the first first conductivity type ion implantation is lower than the ion implantation energy for performing the second first conductivity type ion implantation.
[0038] In one embodiment, the ion implantation dose for performing the first first conductivity type ion implantation is higher than the ion implantation dose for performing the second first conductivity type ion implantation.
[0039] The aforementioned semiconductor device improves its breakdown voltage by inserting a second well region between the first well regions. Simultaneously, the upper surface of the second well region is made smaller in the direction of the device's conductive channel width than its lower surface in the same direction. This increases the size of the adjacent upper surface of the first well region in the same direction, thereby increasing the path width of the current flowing through the upper surface of the drift region when the device is turned on, and reducing the device's on-resistance. Ultimately, this achieves both an increase in the device's breakdown voltage and an effective reduction in its on-resistance. Attached Figure Description
[0040] To more clearly illustrate the technical solutions in the embodiments of this application or the conventional technology, the drawings used in the description of the embodiments or the conventional technology will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0041] Figure 1 This is a schematic diagram of an exemplary semiconductor device.
[0042] Figure 2 This is a schematic diagram of the structure of a semiconductor device according to an embodiment;
[0043] Figure 3 This is a schematic cross-sectional view of a semiconductor device along the width of its conductive channel, according to one embodiment.
[0044] Figure 4 This is a schematic cross-sectional view of a semiconductor device along the width of its conductive channel, according to another embodiment.
[0045] Figure 5 This is a schematic cross-sectional view of a semiconductor device along the width of its conductive channel, according to another embodiment.
[0046] Figure 6 This is a schematic cross-sectional view of a semiconductor device along the width of its conductive channel, according to another embodiment.
[0047] Figure 7 This is a schematic cross-sectional view of a semiconductor device along the width of its conductive channel, according to another embodiment.
[0048] Figure 8 This is a schematic cross-sectional view of a semiconductor device along the width of its conductive channel, according to another embodiment.
[0049] Figure 9 This is a schematic cross-sectional view of a semiconductor device along the width of its conductive channel, according to another embodiment.
[0050] Figure 10 This is a schematic diagram of the structure of a semiconductor device according to another embodiment;
[0051] Figure 11 This is a schematic flowchart of a semiconductor device fabrication method according to an embodiment;
[0052] Figure 12 This is a schematic cross-sectional view of a semiconductor device along the width of its conductive channel, according to another embodiment.
[0053] Figure 13 This is a schematic cross-sectional view of a semiconductor device along the width of its conductive channel, according to another embodiment.
[0054] Figure 14 This is a schematic cross-sectional view of a semiconductor device along the width of its conductive channel, according to another embodiment.
[0055] Figure 15 This is a schematic cross-sectional view of a semiconductor device along the width of its conductive channel, according to another embodiment.
[0056] Figure 16 This is a schematic cross-sectional view of a semiconductor device along the width of its conductive channel, according to another embodiment. Detailed Implementation
[0057] To facilitate understanding of this application, a more complete description will be provided below with reference to the accompanying drawings, which illustrate embodiments of the present application. However, the present application can be implemented in many different forms and is not limited to the embodiments described herein. Rather, these embodiments are provided so that the disclosure of this application will be thorough and complete.
[0058] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this application belongs. The terminology used herein is for the purpose of describing particular embodiments only and is not intended to be limiting of the application.
[0059] It should be understood that when an element or layer is referred to as "on," "adjacent to," "connected to," or "coupled to" other elements or layers, it may be directly on, adjacent to, connected to, or coupled to other elements or layers, or there may be intervening elements or layers. Conversely, when an element is referred to as "directly on," "directly adjacent to," "directly connected to," or "directly coupled to" other elements or layers, there are no intervening elements or layers. It should be understood that although the terms first, second, third, etc., may be used to describe various elements, parts, regions, layers, doping types, and / or portions, these elements, parts, regions, layers, doping types, and / or portions should not be limited by these terms. These terms are only used to distinguish one element, part, region, layer, doping type, or portion from another element, part, region, layer, doping type, or portion. Therefore, without departing from the teachings of this invention, the first element, component, region, layer, doping type, or portion discussed below may be represented as a second element, component, region, layer, or portion; for example, the first doping type may be referred to as the second doping type, and similarly, the second doping type may be referred to as the first doping type; the first doping type and the second doping type are different doping types, for example, the first doping type may be P-type and the second doping type may be N-type, or the first doping type may be N-type and the second doping type may be P-type.
[0060] Spatial relation terms such as “below,” “under,” “below,” “under,” “above,” “above,” etc., are used herein to describe the relationship between one element or feature shown in the figure and other elements or features. It should be understood that, in addition to the orientation shown in the figure, spatial relation terms also include different orientations of the device in use and operation. For example, if the device in the figure is flipped, the element or feature described as “below,” “under,” or “below” will be oriented “above” the other element or feature. Therefore, the exemplary terms “below” and “under” can include both above and below orientations. Furthermore, the device may also include other orientations (e.g., rotated 90 degrees or other orientations), and the spatial descriptive terms used herein will be interpreted accordingly.
[0061] When used herein, the singular forms of “a,” “an,” and “the” may also include the plural forms unless the context clearly indicates otherwise. It should also be understood that the terms “comprising / including” or “having,” etc., specify the presence of the stated features, wholes, steps, operations, components, parts, or combinations thereof, but do not preclude the possibility of the presence or addition of one or more other features, wholes, steps, operations, components, parts, or combinations thereof. Meanwhile, in this specification, the term “and / or” includes any and all combinations of the associated listed items.
[0062] Embodiments of the invention are described herein with reference to cross-sectional views illustrating ideal embodiments (and intermediate structures) of the invention, thus allowing for variations in the illustrated shape due to, for example, manufacturing techniques and / or tolerances. Therefore, embodiments of the invention should not be limited to the specific shapes of the regions shown herein, but rather include shape deviations due to, for example, manufacturing techniques. For instance, implantation regions shown as rectangular typically have rounded or curved features at their edges and / or implantation concentration gradients, rather than a binary change from implantation regions to non-implantation regions. Similarly, the buried regions formed by implantation can result in some implantation in the region between the buried region and the surface traversed during implantation. Therefore, the regions shown in the figures are substantially schematic, and their shapes do not represent the actual shapes of regions of the device and do not limit the scope of the invention.
[0063] The applicant's research found that existing high-voltage devices typically increase the ion concentration in the drift region to improve the breakdown voltage while reducing the on-resistance. In order to ensure the high breakdown voltage of the device, ion implantation regions with the opposite conductivity type to the drift region are repeatedly inserted into the drift region to enhance the depletion of the drift region, thereby ultimately achieving the goal of improving the breakdown voltage of the device while reducing the on-resistance of the device.
[0064] However, since the current flows through the surface of the drift region when the device is turned on, inserting an injection region with the opposite conductivity type into the drift region will reduce the proportion of the drift region and narrow the current path, so a sufficiently low on-resistance cannot be obtained.
[0065] Figure 1 This is a schematic cross-sectional view of an exemplary semiconductor device, such as... Figure 1As shown, the semiconductor device includes a P-type substrate 100 and a drift region 110, wherein the drift region 110 includes sequentially adjacent N-type well regions 111 and P-type well regions 112. Both the P-type well regions 112 and N-type well regions 111 are cuboid structures, with the P-type well region 112 interspersed between the N-type well regions 111. The inventors discovered that while this enhances the overall depletion of the drift region 110 and increases the device's breakdown voltage, it sacrifices the proportion of the N-type well regions 111 within the drift region 110, narrowing the current path during device conduction and making it difficult to reduce the device's on-resistance. To reduce the device's on-resistance, the proportion of the N-type well regions 111 needs to be increased, but this cannot effectively enhance the overall depletion of the drift region, thus failing to increase the device's breakdown voltage. Therefore, Figure 1 The exemplary semiconductor device shown still cannot effectively overcome the contradictory relationship between increasing the breakdown voltage of the device and reducing the turn-on voltage of the device.
[0066] Figure 2 This is a schematic diagram of the structure of a semiconductor device provided in one embodiment, such as... Figure 2 As shown, the semiconductor device includes a substrate 210 and a drift region 220. The substrate 210 has a first conductivity type; the drift region 220 is located on the upper surface of the substrate 210, and includes at least two first well regions 221 with a second conductivity type and at least one second well region 222 with a first conductivity type, arranged alternately and adjacently along the width direction of the device conductive channel, wherein the first and second conductivity types are electrically opposite; the upper surface of at least one second well region 222 has a dimension in the width direction of the device conductive channel smaller than the lower surface of the second well region 222 in the width direction of the device conductive channel.
[0067] The width direction of the conductive channel is parallel to the upper surface of the substrate 210 and perpendicular to the length direction of the conductive channel, where the length direction of the conductive channel is the direction from the source to the drain of the device. For example... Figure 2 As shown, the width direction of the conductive channel of the device can be represented by S1, and the length direction of the conductive channel of the device can be represented by direction S2.
[0068] It is understandable that when the device is turned on, majority carriers move within the conductive channel formed by the source region, drift region 220, and drain region. The majority carriers flowing between the source region and drift region 220 move above the first well region 221 within the drift region 220. The second well region 222 between the two first well regions 221 can enhance the depletion of the drift region 220, thereby increasing the device breakdown voltage. In this embodiment, the second well region 222 is fabricated such that the size of its upper surface is reduced to be smaller than the size of its lower surface in the width direction of the conductive channel. Given a fixed upper surface size for the drift region 220 (i.e., a fixed sum of the upper surface sizes of the first well region 221 and the second well region 222), the size of the upper surface of the first well region 221 increases, thereby increasing the path width of the current flowing through the drift region 220 and reducing the overall on-resistance of the device. Ultimately, this improves both the device breakdown voltage and reduces the device on-resistance.
[0069] There can be multiple first well regions 221 and multiple second well regions 222, with each second well region 222 located between two first well regions 221 (see reference). Figures 7 to 9 In this configuration, the dimension of the upper surface of at least one second well region 222 in the direction of the device conductive channel width is smaller than the dimension of its lower surface in the direction of the device conductive channel width. For example, consider a configuration with three first well regions 221 and two second well regions 222. In one embodiment, only one second well region 222 may have an upper surface dimension in the direction of the device conductive channel width that is smaller than its lower surface dimension in the direction of the device conductive channel width; alternatively, both second well regions 222 may have upper surfaces dimension in the direction of the device conductive channel that are smaller than their lower surfaces dimension in the direction of the device conductive channel width. It is understood that by repeatedly and alternately arranging multiple first well regions 221 and multiple second well regions 222, a more ideal depletion state of the drift region 220 can be achieved, increasing the device breakdown voltage while reducing the on-resistance.
[0070] The semiconductor device in this embodiment improves the breakdown voltage of the device by inserting a second well region 222 between the first well regions 221. At the same time, the upper surface of the second well region 222 is set to have a smaller dimension in the direction of the device's conductive channel width than its lower surface in the direction of the device's conductive channel width. This increases the dimension of the upper surface of the adjacent first well region 221 in the direction of the device's conductive channel width, that is, increases the path width of the current flowing through the upper surface of the drift region 220 when the device is turned on, and reduces the on-resistance of the device. Ultimately, this achieves the goal of effectively reducing the on-resistance of the device while improving the breakdown voltage.
[0071] In one embodiment, the doping concentration of the upper surface of the second well region 222 may be greater than the doping concentration of the lower surface of the second well region 222.
[0072] It is understood that the second well region 222 has different doping concentrations, with the doping concentration on the upper surface being greater than that on the lower surface. This enhances the depletion of the drift region 220, thereby increasing the breakdown voltage. The second well region 222 can employ the same type of dopant ions.
[0073] In one embodiment, the upper surface of the first well region 221 and the upper surface of the second well region 222 are coplanar with the upper surface of the substrate 210, the lower surface of the first well region 221 and the lower surface of the second well region 222 are coplanar, and the thickness of the first well region 221 is equal to the thickness of the second well region 222.
[0074] refer to Figures 3 to 5 As shown, it can be understood that the first well region 221 and the second well region 222 have the same thickness, and the upper and lower surfaces of the first well region 221 and the second well region 222 are coplanar. The upper surface of the first well region 221 and the second well region 222 is also the upper surface of the substrate 210. Therefore, when the device is turned on, majority carriers can flow on the upper surface of the substrate 210, ensuring a sufficiently wide current path on the upper surface, while also reducing the on-resistance. The thickness of the first well region 221 and the thickness of the second well region 222 are the dimensions of the first well region 221 and the second well region 222 in the direction from the lower surface of the substrate 210 to the upper surface of the substrate 210, respectively.
[0075] In one embodiment, the second well region 222 may include a first doped region and a second doped region located below the first doped region, wherein the doping concentration of the first doped region is greater than the doping concentration of the second doped region.
[0076] by Figure 4 Taking a cross-sectional view of the semiconductor device in the embodiment as an example, the structure of the second well region 222, including a first doped region and a second doped region located below the first doped region, can be as follows: Figure 6 As shown, the first doped region 222a is located on the upper surface of the drift region 220, and the second doped region 222b is located below the first doped region and in contact with the lower surface of the first doped region 222a. The doping concentration of the first doped region 222a is greater than that of the second doped region 222b, which enhances the depletion of the drift region 220 and thus increases the breakdown voltage. It can be understood that the first doped region 222a and the second doped region 222b are doped with the same type of ions and have the same conductivity type.
[0077] In one embodiment, at least one interface at the interface between the first well region 221 and the second well region 222 may be inclined to the plane where the substrate 210 is located.
[0078] It is understood that during the fabrication process, by making at least one interface of the first well region 221 and the second well region 222 inclined to the plane of the substrate 210, the size of the upper surface of at least one second well region 222 in the direction of the conductive channel width of the device is smaller than the size of the lower surface of the second well region 222. Compared with existing semiconductor devices where the interface of the two well regions is planar and perpendicular to the plane of the substrate 210, the area of the inclined interface in this embodiment is increased, which makes the second well region 222 more fully deplete the first well region 221, further enhances the depletion of the drift region 220, improves the breakdown voltage of the device, and at the same time ensures that there is a sufficiently wide current path on the upper surface, reducing the on-resistance.
[0079] Taking an example where there are two first well regions 221 and one second well region 222, a cross-sectional schematic diagram of the first well region 221 and the second well region 222 along the width direction of the conductive channel of the device can be referenced. Figures 3 to 5 As shown. At the interface between the first well region 221 and the second well region 222, when only one interface is inclined to the plane of the substrate 210, the cross-sectional shape of one of the first well regions 221 and the second well region 222 can be a right-angled trapezoid, as shown. Figure 3 As shown; in one embodiment, when both interfaces are inclined to the plane of the substrate 210, both first well regions 221 can be right-angled trapezoids, while the second well region 222 is a non-right-angled trapezoid, that is, the cross-sectional shape of both the first well region 221 and the second well region 222 along the width direction of the device conductive channel is trapezoidal, as shown. Figure 4 As shown; or both first well regions 221 are right-angled trapezoids, while the second well region 222 is an irregular shape, such as... Figure 5 As shown. It is understood that the cross-sectional shape of the first well region 221 and the second well region 222 in the direction of the conductive channel width of the device is only shown as an example. In fact, it may have other shapes if the size of the upper surface of the second well region 222 is smaller than the size of the lower surface of the second well region 222. These are not listed here.
[0080] When there are multiple first well regions 221 and multiple second well regions 222, for example, taking three first well regions 221 and two second well regions 222 as an example, if only one second well region 222 has a lower dimension on its upper surface in the direction of the device conductive channel width than its lower surface in the direction of the device conductive channel width, in one embodiment, if only one interface is inclined to the plane of the substrate 210, the cross-sectional structure of each well region can be referred to as follows. Figure 7 As shown; in one embodiment, when both interfaces are inclined to the plane of the substrate 210, both first well regions 221 are right-angled trapezoids, as shown. Figures 8 to 9As shown. The dimensions of the upper surfaces of the two second well regions 222 in the direction of the device conductive channel width are both smaller than the dimensions of their lower surfaces in the direction of the device conductive channel width. The cross-sectional shapes of the two second well regions 222 can be referenced. Figures 3 to 5 The cross-sectional shape of the second well region 222 in the embodiment is described, wherein the cross-sectional shapes of the two second well regions 222 may be the same or different. In one embodiment, the cross-sectional shapes of the first well region 221 and the second well region 222 along the width direction of the device conductive channel are both trapezoidal, for example, both may be trapezoidal. Figure 4 In the trapezoidal shape, the dimensional difference between the upper and lower surfaces of the second well region 222 in the direction of the conductive channel width, as well as the larger interface area between the first well region 221 and the second well region 222, makes the depletion of the first well region 221 by the second well region 222 more complete, further enhancing the depletion of the drift region 220 and increasing the breakdown voltage of the device. It also maximizes the current path width on the upper surface, effectively reducing the on-resistance.
[0081] In one embodiment, the interface between the first well region 221 and the second well region 222 may also be a curved surface. It is understood that when the interface is a curved surface, the second well region 222 may have a gradually changing (e.g., when the curved surface is concave or convex) or non-gradual (e.g., when the curved surface is wavy) size in the direction perpendicular to the width of the conductive channel of the device, such as the direction from the lower surface of the drift region 220 to the upper surface.
[0082] In one embodiment, the first conductivity type and the second conductivity type can be either P-type or N-type, wherein the first conductivity type and the second conductivity type have opposite electrical properties.
[0083] In one embodiment, the semiconductor device may further include a source region 230, a body region 240, a body lead-out region 250, a gate region 260, and a drain region 270, so as to Figure 2 Taking the semiconductor device in the embodiment as an example, such as Figure 10 As shown, the source region 230 is located on the upper surface of the substrate 210 and is spaced apart from the drift region 220, and has a second conductivity type; the body region 240 surrounds the source region 230 and is adjacent to or spaced apart from the drift region 220; the body lead-out region 250 is located on the upper surface of the body region 240 and is adjacent to the source region 230, and the body lead-out region 250 has a first conductivity type; the gate 260 is located on the upper surface of the substrate 210 and extends to cover the drift region 220, the body region 240 and the source region 230; the drain region 270 is located on the upper surface of the drift region 220 and is spaced apart from the gate 260.
[0084] It is understandable that arranging the body region 240 and the drift region 220 adjacently may slightly reduce the device's breakdown voltage, but it can also reduce the device's on-resistance, decrease the device's size, and optimize the device's volume. The positional distribution of the body region 240 and the drift region 220 when arranged adjacently is referenced. Figure 10 As shown; while separating the body region 240 and the drift region 220 may slightly increase the on-resistance of the device and fail to optimize the device size, it can improve the breakdown voltage of the device. In one embodiment, the body region 240 and the drift region 220 can be arranged adjacent to each other.
[0085] In one embodiment, body region 240 may have a first conductivity type.
[0086] In one embodiment, the drain region 270 may have a second conductivity type, which in one embodiment may be, for example, N-type.
[0087] In one embodiment, the doping depth of the body region 240 is greater than the doping depth of the drift region 220, which can enhance the depletion of the drift region 220 and achieve a higher breakdown voltage.
[0088] This embodiment also provides a method for fabricating a semiconductor device, such as... Figure 11 As shown, the method includes steps S110 to S120.
[0089] Step S110: Provide a substrate having a first conductivity type.
[0090] Step S120: A drift region is formed on the upper surface of the substrate. The drift region includes at least two first well regions with a second conductivity type and at least one second well region with a first conductivity type that are alternately and adjacently arranged along the width direction of the device conductive channel. The first conductivity type and the second conductivity type are electrically opposite. The upper surface of at least one second well region has a smaller dimension in the width direction of the device conductive channel than the lower surface of the second well region in the width direction of the device conductive channel.
[0091] The drift region can be formed on the upper surface of the substrate using an ion implantation process. In one embodiment, the first conductivity type and the second conductivity type can be either P-type or N-type.
[0092] The specific structures of the first and second well regions within the drift region have been described. Figure 2 The specific details in the embodiments are not repeated here.
[0093] This invention improves the breakdown voltage of a device by preparing at least two first well regions with a second conductivity type and at least one second well region with a first conductivity type that are alternately arranged and adjacent to each other along the width of the conductive channel of the device. At the same time, the upper surface of the second well region is set to have a smaller dimension in the width of the conductive channel of the device than the lower surface of the second well region in the width of the conductive channel of the device, thereby increasing the dimension of the upper surface of the adjacent first well region in the width of the conductive channel of the device. This increases the path width of the current flowing through the upper surface of the drift region when the device is turned on, thereby reducing the on-resistance of the device. Ultimately, this achieves both an increase in the breakdown voltage of the device and an effective reduction in the on-resistance of the device.
[0094] In one embodiment, the step of forming a drift region on the upper surface of the substrate includes at least two first well regions having a second conductivity type and at least one second well region having a first conductivity type arranged alternately and adjacently along the width direction of the device conductive channel. The step also includes forming a third well region having a second conductivity type on the upper surface of the substrate, and then performing a first conductivity type doping process in the third well region to form a second well region. The remaining third well regions that have not undergone the first conductivity type doping process serve as first well regions.
[0095] Specifically, a second type of conductivity impurity can be implanted into the upper surface layer of the substrate to form a third well region. Then, a first type of conductivity impurity is implanted into the third well region to form a second well region. The first type of conductivity impurity can be implanted in the middle between the two edges of the third well region along the width direction of the conductive channel of the device. The portion of the third well region that is not doped with the first type of conductivity impurity, i.e., only doped with the second type of conductivity impurity, is considered as the first well region. The first well region and the second well region together constitute the drift region. The number of first well regions can be multiple. The shape and size of each first well region can be the same as each other, or at least one first well region can be different in shape and size from the other first well regions.
[0096] It is understandable that a third well region of the second conductivity type is first formed in the substrate, and then a first conductivity type doping process is directly performed in the third well region to form a second well region of the first conductivity type. The remaining third well region that has not undergone the first conductivity type doping process is used as the first well region. The method is simple and easy to implement.
[0097] In one embodiment, the step of performing a first conductivity type doping process in the third well region to form a second well region, and the remaining third well region that has not undergone the first conductivity type doping process as the first well region includes: performing a first first conductivity type ion implantation to form a first ion implantation region, the first ion implantation region being formed in the third well region and extending from the upper surface of the third well region to the interior of the third well region;
[0098] Then, a second ion implantation of the first conductivity type is performed to form a second ion implantation region. The second ion implantation region is formed in the third well region and is located below the first ion implantation region. The projected area of the second ion implantation region on the substrate is larger than the projected area of the first ion implantation region on the substrate.
[0099] Finally, heat treatment is performed to expand the first ion implantation region into a first doped region, expand the second ion implantation region into a second doped region adjacent to and in contact with the first doped region, and make the lower surface of the second doped region coplanar with the lower surface of the third well region. The first doped region and the second doped region are combined to form the second well region, and the remaining third well region that has not undergone the first conductivity type ion implantation treatment is used as the first well region.
[0100] Also refer to Figure 6 , Figures 12 to 14 When forming the second well region, firstly, ions of the first conductivity type are implanted into the region extending from the upper surface of the third well region into its interior, forming the first ion implantation region 300. Then, ions of the first conductivity type are implanted again into the region within the third well region located below the first ion implantation region, forming the second ion implantation region 400. The positional relationship between the first ion implantation region 300 and the second ion implantation region 400 can be referenced. Figure 12 As shown; then heat treatment is performed to push the first ion implantation region 300 and the second ion implantation region 400 into the first doped region 222a at a preset temperature, so that the first implantation region 300 expands into the first doped region 222a (combined with Figure 6 As shown in the diagram, the first doped region 222a and the second doped region 222b are expanded to form the second doped region 222b. The first doped region 222a and the second doped region 222b are adjacent and in contact, and the lower surface of the second doped region is coplanar with the lower surface of the third well region, thus obtaining a second well region composed of the first and second doped regions. Since the projected area of the second ion-implanted region on the substrate is larger than that of the first ion-implanted region on the substrate, after heat treatment, the dimension of the second doped region 222b in the direction of the device's conductive channel width will be larger than that of the first doped region 222a in the same direction. This increases the path width of the current flowing through the drift region, improving the device's withstand voltage while reducing its on-resistance. It can be understood that the third well region is first formed, and then processed to obtain the first well region 221 and the second well region 222, which together form the drift region 220.
[0101] Understandable. Figure 12The positional relationship between the first ion implantation region 300 and the second ion implantation region 400 is only illustrated by way of example. In this embodiment, the orthographic projection of the second ion implantation region 400 on the substrate 200 completely covers the orthographic projection of the first ion implantation region 300 on the substrate 200. In fact, in some embodiments, the orthographic projection of the second ion implantation region 400 on the substrate 200 may also partially cover the orthographic projection of the first ion implantation region 300 on the substrate 200, such as... Figure 13 or Figure 14 As shown; in other embodiments, the orthogonal projection of the second ion implantation region 400 on the substrate 200 may not cover the orthogonal projection of the first ion implantation region 300 on the substrate 200, but the distance between the two ion implantation regions in the direction of the width of the device conductive channel should be set such that after the push-well process is performed on the first ion implantation region 300 and the second ion implantation region 400, the first doped region 222a formed by the expansion of the first ion implantation region 300 and the second doped region 222b formed by the expansion of the second ion implantation region 400 can be adjacent to each other to form the second well region 222.
[0102] Among them, the push-pit process can be carried out under high temperature conditions.
[0103] In one embodiment, such as Figure 15 As shown, performing the first first conductivity type ion implantation to form the first ion implantation region includes: forming a mask layer with a first opening pattern on the substrate surface, the first opening pattern exposing a portion of the upper surface of the third well region, and performing the first first conductivity type ion implantation to form the first ion implantation region extending from the upper surface of the third well region to the interior of the third well region.
[0104] It is understood that by coating a mask layer 500 and etching a portion of the mask layer 500 to form a first opening pattern, the first opening pattern exposes a portion of the upper surface of the third well region, and then ion implantation of a first conductivity type is performed from the exposed upper surface of the third well region, thereby enabling the formation of an ion implantation region of a specific area and size, preventing other areas from being contaminated.
[0105] In one embodiment, such as Figure 16 As shown, performing a second first conductivity type ion implantation to form a second ion implantation region includes: forming a mask layer with a second opening pattern on the substrate surface, the second opening pattern exposing the upper surface of the first ion implantation region and the upper surface of a portion of the third well region surrounding the first ion implantation region; and performing a second first conductivity type ion implantation to form a second ion implantation region located within the third well region and below the first ion implantation region.
[0106] It is understood that after the first ion implantation region is formed, a mask layer with a second opening pattern can be formed on the substrate surface to expose the upper surface of the first ion implantation region and the surrounding part of the third well region. Thus, after performing the second first conductivity type ion implantation, the orthogonal projection area of the second ion implantation region on the substrate can be larger than the orthogonal projection area of the first ion implantation region on the substrate. Finally, after heat treatment, the upper surface of the second well region has a smaller dimension in the direction of the device conductive channel width than the lower surface of the second well region in the direction of the device conductive channel width. Therefore, it is possible to increase the breakdown voltage while reducing the on-resistance.
[0107] In one embodiment, when forming a mask layer with a first opening pattern on the substrate surface, forming a mask layer with a second opening pattern on the substrate surface includes etching back the mask layer with the first opening pattern, enlarging the first opening pattern to expose the upper surface of a portion of the third well region surrounding the first ion implantation region, thereby obtaining a mask layer with a second opening pattern on the substrate surface.
[0108] It is understandable that a small area can first be exposed on the mask layer 500 using photoresist, and then a first ion implantation region 300 can be formed by low-energy ion implantation. After that, the mask layer 500 around the region can be etched to expose the upper surface areas on both sides of the region, thereby expanding the exposed area of the drift region 220. Then, ion implantation is performed on the exposed area to form a second ion implantation region 400 with a projected area on the substrate that is larger than the projected area of the first ion implantation region on the substrate. Subsequently, a push-in process can be performed to prepare a second well region 222. The size of the upper surface of the second well region 222 in the direction of the device conductive channel width is smaller than the size of the lower surface of the second well region 222 in the direction of the device conductive channel width.
[0109] In this process, the upper surface of a portion of the third well region surrounding the first ion implantation region is etched back, and ion implantation continues to form the second ion implantation region 400. This is followed by heat treatment, and the final structure of the second well region 222 can be referenced. Figure 6 As shown.
[0110] This method embodiment only requires coating a mask layer once. Without adding a mask layer, an alternating drift region morphology is formed through two injections. The method is simple and easy to implement. The semiconductor device prepared can not only ensure a sufficiently wide current path on the surface of the drift region, but also increase the interface between the first well region and the second well region in the drift region, so that the second well region depletes the first well region more fully, thus achieving a lower on-resistance.
[0111] In addition, when forming the second ion implantation region, wet etching can be used to expose the upper surface area.
[0112] In one embodiment, during the second etch-back process, only one side of the third well region surrounding the first ion implantation region may be etched, so that the cross-sectional shape of the second well region formed in the direction of the device conductive channel width can be a right trapezoid.
[0113] In one embodiment, the ion implantation energy for performing the first first conductivity type ion implantation may be lower than the ion implantation energy for performing the second first conductivity type ion implantation; in another embodiment, the ion implantation dose for performing the first first conductivity type ion implantation may be higher than the ion implantation dose for performing the second first conductivity type ion implantation, so that after obtaining the first doped region and the second doped region through heat treatment, the doping concentration of the first doped region may be greater than the doping concentration of the second doped region.
[0114] The above embodiments only illustrate the fabrication method of a semiconductor device that includes only two first well regions and one second well region. When there are multiple first well regions and multiple second well regions, the fabrication method is similar to the above embodiments, and will not be described in detail here.
[0115] In one embodiment, the fabrication method further includes forming a body region on the upper surface of a substrate, wherein the body region is adjacent to or separated from the drift region; then forming a gate extending to cover the drift region and the body region on the upper surface of the substrate; further forming a source region within the body region, the source region extending to contact the lower surface of the gate; then forming a drain region located on the upper surface of the drift region and spaced from the gate; and finally forming a body lead-out region located on the upper surface of the body region and adjacent to the source region.
[0116] In one embodiment, the body region is prepared to have a doping concentration greater than that of the second well region of the first conductivity type, thereby ensuring that the breakdown voltage of the device can be further improved.
[0117] In one embodiment, the body region is prepared such that its doping depth is greater than that of the drift region.
[0118] It should be understood that, although Figure 11 The steps in the flowchart are shown sequentially as indicated by the arrows, but these steps are not necessarily executed in the order indicated by the arrows. Unless otherwise specified herein, there is no strict order in which these steps are executed, and they can be performed in other orders. Figure 11 At least some of the steps in the process may include multiple steps or multiple stages. These steps or stages are not necessarily completed at the same time, but may be executed at different times. The execution order of these steps or stages is not necessarily sequential, but may be executed in turn or alternately with other steps or at least some of the steps or stages in other steps.
[0119] In the description of this specification, references to terms such as "some embodiments," "other embodiments," and "ideal embodiments" indicate that a specific feature, structure, material, or characteristic described in connection with that embodiment or example is included in at least one embodiment or example of the invention. In this specification, the illustrative descriptions of the above terms do not necessarily refer to the same embodiments or examples.
[0120] The technical features of the above embodiments can be combined in any way. For the sake of brevity, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0121] The embodiments described above are merely illustrative of several implementations of the present invention, and while the descriptions are relatively specific and detailed, they should not be construed as limiting the scope of the invention patent. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of the present invention, and these all fall within the protection scope of the present invention. Therefore, the protection scope of this invention patent should be determined by the appended claims.
Claims
1. A semiconductor device, characterized in that, include: The substrate has a first type of conductivity; A drift region, located on the upper surface of the substrate, includes at least two first well regions having a second conductivity type and at least one second well region having a first conductivity type, which are alternately and adjacently arranged along the width direction of the device conductive channel. The first conductivity type and the second conductivity type are electrically opposite. The upper surface of at least one second well region has a smaller dimension in the width direction of the device conductive channel than the lower surface of the second well region in the width direction of the device conductive channel. The formation of a drift region on the upper surface of the substrate includes: A third well region having the second conductivity type is formed on the upper surface layer of the substrate; A first ion implantation of the first conductivity type is performed to form a first ion implantation region, which is formed within the third well region and extends from the upper surface of the third well region to the interior of the third well region. A second ion implantation of the first conductivity type is performed to form a second ion implantation region. The second ion implantation region is formed within the third well region and located below the first ion implantation region. The projected area of the second ion implantation region on the substrate is larger than the projected area of the first ion implantation region on the substrate. Heat treatment is performed to expand the first ion implantation region into a first doped region, and the second ion implantation region into a second doped region adjacent to and in contact with the first doped region. The lower surface of the second doped region is coplanar with the lower surface of the third well region. The first doped region and the second doped region are combined to form the second well region. The remaining third well region, which has not undergone the first conductivity type ion implantation treatment, is used as the first well region.
2. The semiconductor device according to claim 1, characterized in that, The doping concentration on the upper surface of the second well region is greater than the doping concentration on the lower surface of the second well region.
3. The semiconductor device according to claim 1, characterized in that, The upper surfaces of the first well region and the second well region are coplanar with the upper surface of the substrate, the lower surfaces of the first well region and the second well region are coplanar, and the thickness of the first well region is equal to the thickness of the second well region.
4. The semiconductor device according to claim 1, characterized in that, The second well region includes a first doped region and a second doped region located below the first doped region, wherein the doping concentration of the first doped region is greater than the doping concentration of the second doped region.
5. The semiconductor device according to claim 1, characterized in that, At least one of the interfaces between the first well region and the second well region is inclined to the plane of the substrate.
6. The semiconductor device according to claim 5, characterized in that, Both the first well region and the second well region have trapezoidal cross-sectional shapes along the width of the conductive channel of the device.
7. The semiconductor device according to claim 1, characterized in that, The semiconductor device further includes: The source region is located on the upper surface of the substrate and is spaced apart from the drift region, and has the second conductivity type; A body region, which surrounds the source region and is adjacent to or spaced apart from the drift region; A body lead-out region is located on the upper surface of the body region and is disposed adjacent to the source region, and the body lead-out region has the first conductivity type; A gate is located on the upper surface of the substrate and extends to cover the drift region, the body region and the source region; The drain region is located on the upper surface of the drift region and is spaced apart from the gate.
8. The semiconductor device according to claim 7, characterized in that, The doping concentration of the body region is greater than the doping concentration of the second well region of the first conductivity type.
9. A method for fabricating a semiconductor device, characterized in that, include: A substrate is provided, the substrate having a first conductivity type; A drift region is formed on the upper surface of the substrate. The drift region includes at least two first well regions having a second conductivity type and at least one second well region having a first conductivity type, which are alternately and adjacently contacted along the width direction of the device conductive channel. The first conductivity type and the second conductivity type are electrically opposite. At least one of the upper surfaces of the second well region has a dimension in the width direction of the device conductive channel that is smaller than the dimension of the lower surface of the second well region in the width direction of the device conductive channel. The formation of a drift region on the upper surface of the substrate includes: A third well region having the second conductivity type is formed on the upper surface layer of the substrate; A first ion implantation of the first conductivity type is performed to form a first ion implantation region, which is formed within the third well region and extends from the upper surface of the third well region to the interior of the third well region. A second ion implantation of the first conductivity type is performed to form a second ion implantation region. The second ion implantation region is formed within the third well region and located below the first ion implantation region. The projected area of the second ion implantation region on the substrate is larger than the projected area of the first ion implantation region on the substrate. Heat treatment is performed to expand the first ion implantation region into a first doped region, and the second ion implantation region into a second doped region adjacent to and in contact with the first doped region. The lower surface of the second doped region is coplanar with the lower surface of the third well region. The first doped region and the second doped region are combined to form the second well region. The remaining third well region, which has not undergone the first conductivity type ion implantation treatment, is used as the first well region.
10. The method for fabricating a semiconductor device according to claim 9, characterized in that, The process of performing the first ion implantation of the first conductivity type to form the first ion implantation region includes: A mask layer with a first opening pattern is formed on the surface of the substrate, the first opening pattern exposing a portion of the upper surface of the third well region; a first conductivity type ion implantation is performed to form a first ion implantation region extending from the upper surface of the third well region into the interior of the third well region; and / or The second ion implantation of the first conductivity type to form the second ion implantation region includes: A mask layer with a second opening pattern is formed on the substrate surface, the second opening pattern exposing the upper surface of the first ion implantation region and a portion of the upper surface of the third well region surrounding the first ion implantation region. A second first conductivity type ion implantation is performed to form the second ion implantation region located within the third well region and below the first ion implantation region.
11. The method for fabricating a semiconductor device according to claim 10, characterized in that, When forming a mask layer with a first opening pattern on the substrate surface, the step of forming a mask layer with a second opening pattern on the substrate surface includes: The mask layer with the first opening pattern is etched back, and the first opening pattern is enlarged to expose the upper surface of a portion of the third well region surrounding the first ion implantation region, thereby obtaining the mask layer with the second opening pattern on the substrate surface.
12. The semiconductor device fabrication method according to claim 9, characterized in that, The ion implantation energy for the first first conductivity type ion implantation is lower than the ion implantation energy for the second first conductivity type ion implantation.
13. The method for fabricating a semiconductor device according to claim 9, characterized in that, The ion implantation dose for the first first conductivity type ion implantation is higher than the ion implantation dose for the second first conductivity type ion implantation.
Citation Information
Patent Citations
Lateral double-diffused metal oxide semiconductor device and manufacturing method thereof, and electronic device
CN112530805A
Semiconductor device and method of manufacturing the semiconductor device
US20100032754A1