LED chip and preparation method thereof

By preparing a temporary protective layer on the ITO current extension layer and etching to form a groove, and combining hydrogen ions to form a high-resistivity layer, the problem of insufficient current extension capability in LED chips is solved, enabling the current to extend further laterally and reach the edge of the chip.

CN116454183BActive Publication Date: 2026-11-20JIANGXI ZHAO CHI SEMICON CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202310462453.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-04-26
Publication Date
2026-11-20
Estimated Expiration
2043-04-26

AI Technical Summary

Technical Problem

Existing LED chips have insufficient current spreading capability, making it difficult to reach the edge of the chip.

Method used

A temporary protective layer is prepared on the ITO current spreading layer, and a preparation trench is etched on the temporary protective layer to expose part of the ITO current spreading layer. A high-resistivity layer is formed by the combination of hydrogen ions and oxygen atoms, which reduces the thickness of ITO and improves the current spreading capability.

Benefits of technology

By forming a high-resistance layer, the resistance of lateral current extension is reduced, allowing the current to extend further laterally and reach the edge of the chip.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116454183B_ABST
    Figure CN116454183B_ABST
Patent Text Reader

Abstract

The application provides an LED chip and a preparation method thereof. The preparation method comprises the following steps: providing a substrate; preparing an epitaxial light-emitting structure on the substrate; preparing a temporary protection layer on the ITO current spreading layer, etching the temporary protection layer to form a preparation groove; and performing a hydrogen ion blowing operation on one side of the temporary protection layer, so that oxygen atoms on the exposed surface of the ITO current spreading layer are combined with hydrogen ions to form a high-resistance layer at the preparation groove. By combining the hydrogen ions with the oxygen atoms on the surface of the ITO current spreading layer in the preparation groove, the resistance of the ITO surface can be increased, and even the ITO surface can be disabled to form a high-resistance layer, thereby indirectly reducing the thickness of the ITO, reducing the resistance of the current lateral expansion, and locating the electrode spreading layer inside the high-resistance layer, so that the current spreading has a current acceleration effect every certain distance, improves the current spreading capability, and thus realizes the current lateral expansion farther, so that the current can reach the edge position of the chip.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of LED chip technology, and in particular to an LED chip and its fabrication method. Background Technology

[0002] LEDs have many advantages, such as high luminous efficiency, low energy consumption, reliability, durability, long lifespan, safety in low-voltage applications, short response time, and environmental friendliness. In addition, people's demand for special features in display and lighting products is constantly increasing. Against this backdrop, LEDs will have broad development prospects.

[0003] In the existing technology, with the rapid development of LEDs and the continuous pursuit of chip performance and efficiency, some problems in LED chips have gradually been exposed, such as insufficient current spreading capability. Indium tin oxide (ITO) material has good current spreading capability and has been widely used in LED chips. However, in some large-size LED chips, there is still insufficient current spreading capability, that is, the current is difficult to reach the edge of the chip. Summary of the Invention

[0004] In view of the shortcomings of the prior art, the purpose of this invention is to provide an LED chip and its manufacturing method, which aims to solve the technical problem that the current extension capability is insufficient and it is difficult to reach the edge position of the chip in the prior art.

[0005] To achieve the above objectives, the present invention is implemented through the following technical solution: an LED chip fabrication method, comprising the following steps: providing a substrate; fabricating an epitaxial light-emitting structure on the substrate; sequentially fabricating a current blocking layer, an ITO current spreading layer, a metal electrode layer, and a passivation layer on the epitaxial light-emitting structure to form an electrode structure on the epitaxial light-emitting structure; wherein, the step of fabricating the metal electrode layer on the ITO current spreading layer specifically includes: fabricating a temporary protective layer on the ITO current spreading layer; etching a fabrication trench on the temporary protective layer to expose a portion of the ITO current spreading layer; the fabrication trench includes a plurality of trenches spaced apart along the outer edge of the metal electrode layer; performing a hydrogen ion purging operation on one side of the temporary protective layer to allow oxygen atoms on the exposed portion of the ITO current spreading layer surface to combine with the hydrogen ions to form a high-resistivity layer at the fabrication trench; removing all of the temporary protective layer, and fabricating the metal electrode layer on the high-resistivity layer and the ITO current spreading layer.

[0006] Compared with the prior art, the beneficial effects of the present invention are as follows: By preparing a temporary protective layer on the ITO current extension layer and etching a preparation trench on the temporary protective layer to expose part of the ITO current extension layer, the preparation trench includes a number of trenches spaced apart along the outer edge of the metal electrode layer. Further, hydrogen ions are formed by ionization, and the hydrogen ions combine with oxygen atoms on the surface of the ITO current extension layer in the preparation trench, which can increase the resistance of the ITO surface or even cause it to fail, thereby forming a high-resistance layer, namely, multiple high-resistance regions spaced apart corresponding to the trenches. This indirectly reduces the thickness of the ITO and reduces the resistance of the lateral current extension. The principle is similar to the increase in the flow rate of water when passing through a narrow passage. The electrode extension layer is located inside the high-resistance layer, so that the current extension has an acceleration effect at intervals, improving the current extension capability, thereby achieving a longer lateral current extension, so that the current can reach the edge of the chip.

[0007] According to one aspect of the above technical solution, the step of performing hydrogen ion purging on one side of the temporary protective layer to allow oxygen atoms on the exposed ITO current extension layer surface to combine with the hydrogen ions, thereby forming a high-resistivity layer at the preparation tank, specifically includes:

[0008] Through a preset preparation process, hydrogen ion gas is introduced into the machine, and the hydrogen ion gas is ionized by radio frequency to form hydrogen ions, wherein the hydrogen ion gas is silane;

[0009] A purge is performed under the influence of an electric field to allow the hydrogen ions to combine with oxygen atoms on the exposed surface of the ITO current-extended layer, thereby forming a high-resistivity layer at the preparation tank.

[0010] According to one aspect of the above technical solution, the preset preparation process includes: controlling the temperature inside the machine to be 200℃-300℃, the radio frequency power to be 70W-150W, the hydrogen ion gas injection rate to be 100sccm-150sccm, and the purging time to be 240s-500s.

[0011] According to one aspect of the above technical solution, the temporary protective layer is made of SiO2.

[0012] According to one aspect of the above technical solution, the step of removing all of the temporary protective layers specifically includes:

[0013] The SiO2 on the surface of the ITO current extension layer is removed by etching with BOE solution to remove all of the temporary protective layer.

[0014] According to one aspect of the above technical solution, an ITO transparent conductive film is fabricated on the current blocking layer using a magnetron sputtering process, and the ITO current spreading layer is formed by an annealing process.

[0015] According to one aspect of the above technical solution, the step of fabricating the current blocking layer on the epitaxial light-emitting structure specifically includes:

[0016] A SiO2 layer with a thickness of 250nm-350nm is deposited on the epitaxial light-emitting structure using PECVD process. The surface of the SiO2 layer is then subjected to photolithography, followed by spin coating, exposure, and development. A portion of the SiO2 layer at the position corresponding to the metal electrode layer is retained as a current blocking layer.

[0017] According to one aspect of the above technical solution, the step of fabricating an epitaxial light-emitting structure on the substrate specifically includes:

[0018] An N-type semiconductor layer, a light-emitting layer, and a P-type semiconductor layer are sequentially fabricated on the substrate using a preset fabrication process. The N-type semiconductor layer is an N-GaN layer, the P-type semiconductor layer is a P-GaN layer, and the light-emitting layer is a multi-quantum-well active layer.

[0019] The preset preparation process includes: using hydrogen as a carrier gas, ammonia as a nitrogen source, trimethylgallium and triethylgallium as gallium sources, trimethylindium as an indium source, silane as an N-type dopant, trimethylaluminum as an aluminum source, and magnesium thiocene as a P-type dopant.

[0020] According to one aspect of the above technical solution, the thickness of the N-GaN layer is 1μm-3μm, and the Si doping concentration is 5×10⁻⁶. 18 cm -3 -1×10 19 cm -3 The thickness of the P-GaN layer is 200nm-300nm, and the Mg doping concentration is 5×10⁻⁶. 17 cm -3 -1×10 20 cm -3 The molar proportion of In in the multi-quantum-well active layer is 10%-35%.

[0021] On the other hand, the present invention also provides an LED chip, which is prepared by the LED chip preparation method described above. Attached Figure Description

[0022] Figure 1 This is a flowchart of the LED chip fabrication method in the first embodiment of the present invention;

[0023] Figure 2 This is a schematic diagram of the cross-sectional structure of the LED chip in the second embodiment of the present invention;

[0024] Figure 3 This is a top view of the LED chip structure in the second embodiment of the present invention;

[0025] Explanation of key component symbols:

[0026] Metal electrode layer 1, passivation layer 2, ITO current spreading layer 3, current blocking layer 4, high resistance layer 5.

[0027] The following detailed description, in conjunction with the accompanying drawings, will further illustrate the present invention. Detailed Implementation

[0028] To facilitate understanding of the present invention, a more complete description will be given below with reference to the accompanying drawings. Several embodiments of the invention are illustrated in the drawings. However, the invention can be implemented in many different forms and is not limited to the embodiments described herein. Rather, these embodiments are provided so that this disclosure will be thorough and complete.

[0029] It should be noted that when a component is said to be "fixed to" another component, it can be directly on the other component or there may be an intervening component. When a component is said to be "connected to" another component, it can be directly connected to the other component or there may be an intervening component. The terms "vertical," "horizontal," "left," "right," and similar expressions used in this document are for illustrative purposes only.

[0030] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this invention pertains. The terminology used herein in the description of the invention is for the purpose of describing particular embodiments only and is not intended to be limiting of the invention. The term "and / or" as used herein includes any and all combinations of one or more of the associated listed items.

[0031] Example 1

[0032] Please see Figure 1 The image shows a method for preparing an LED chip according to the first embodiment of the present invention, which includes the following steps:

[0033] Step S100: Provide a substrate. Specifically, in this step, the substrate can be selected from one of the following: sapphire substrate, SiO2-sapphire composite substrate, silicon substrate, silicon carbide substrate, gallium nitride substrate, and zinc oxide substrate. In this embodiment, a sapphire substrate is selected. Sapphire is currently the most commonly used GaN-based LED substrate material, and most GaN-based LEDs on the market use sapphire as the substrate material. The biggest advantages of sapphire substrates are mature technology, good stability, and low production cost.

[0034] Step S200: An epitaxial light-emitting structure is prepared on the substrate.

[0035] Step S300: A current blocking layer, an ITO current spreading layer, a metal electrode layer, and a passivation layer are sequentially prepared on the epitaxial light-emitting structure to form an electrode structure on the epitaxial light-emitting structure.

[0036] Specifically, the step of fabricating the metal electrode layer on the ITO current spreading layer includes:

[0037] Step S310: A temporary protective layer is prepared on the ITO current spreading layer. Preparation trenches are etched into the temporary protective layer to expose a portion of the ITO current spreading layer. The preparation trenches include a plurality of trenches spaced apart along the outer edge of the metal electrode layer. In this embodiment, the temporary protective layer is made of SiO2, and its preparation steps specifically include: depositing a 100nm thick layer of SiO2 on the surface of the ITO current spreading layer using PECVD, followed by spin coating, exposure, development, and etching to form a temporary protective layer with preparation trenches. The portion outside the preparation trenches, i.e., the temporary protective layer remaining above the ITO current spreading layer, is used to protect the underlying ITO material.

[0038] Step S320 involves performing a hydrogen ion purging operation on one side of the temporary protective layer, causing oxygen atoms on the exposed ITO current extension layer surface to combine with the hydrogen ions, thereby forming a high-resistivity layer at the preparation tank. This high-resistivity layer includes multiple high-resistivity bands located at the outer edge of the metal electrode layer. Specifically, in this step, step S320 specifically includes:

[0039] Step S321: Using a preset preparation process, hydrogen ion gas is introduced into the instrument, and the hydrogen ion gas is ionized by radio frequency to form hydrogen ions. The hydrogen ion gas is silane. In other embodiments of this application, the hydrogen ion gas can also be ammonia, etc. The preset preparation process includes: controlling the temperature inside the instrument to 200℃-300℃, the radio frequency power to 70W-150W, the hydrogen ion gas introduction rate to 100sccm-150sccm, and the purging time to 240s-500s. Silane or ammonia is ionized into a mixture of ions, atoms, molecules, and electrons by radio frequency, and the mixture is then purged on the ITO surface under the action of an electric field to achieve the combination of H ions and surface oxygen atoms.

[0040] Step S322 involves purging under the influence of an electric field to allow the hydrogen ions to combine with oxygen atoms on the exposed surface of the ITO current extension layer, thereby forming a high-resistivity layer at the preparation tank.

[0041] Specifically, ITO is a transparent conductive material, short for Indium Tin Oxide. It is an oxide composed of indium and tin elements, possessing high transparency and excellent conductivity. ITO is widely used in electronic displays, solar cells, touch screens, LEDs, and other fields.

[0042] The conductivity of ITO is based on its unique electronic structure. ITO has a cubic crystal system, in which indium and tin form an oxide lattice, while oxygen atoms occupy vacancies in the lattice. In the ITO crystal, the valence electrons of indium and tin are attracted by oxygen atoms, forming covalent bonds and simultaneously creating holes. These holes can be excited by an external electric field, thus forming electron-hole pairs.

[0043] The conductivity of ITO primarily originates from these electron-hole pairs. When the ITO surface is excited by an electric field, electron-hole pairs form an electron cloud on the surface, creating a conductive channel. This channel is formed because the electron cloud on the ITO surface interacts with the external electric field, resulting in an electron flow. The advantages of ITO's conductivity lie in its high transparency and low resistivity. ITO's transparency can reach over 90%, while its resistivity can be below 10⁻⁴² cm⁻¹. This makes ITO an ideal transparent conductive material suitable for various applications requiring transparent conductivity.

[0044] Understandably, by ionizing to form hydrogen ions and allowing these hydrogen ions to combine with oxygen atoms on the surface of the ITO current extension layer, the surface resistance of the ITO can be increased, or even rendered ineffective. This indirectly reduces the thickness of the ITO to form a high-resistance layer, thereby reducing the resistance of the lateral current extension. The principle is similar to how the flow rate of water increases when passing through a narrow passage, so that the current extension has an acceleration effect at intervals, improving the current extension capability and thus enabling the current to extend further laterally, allowing the current to reach the edge of the chip.

[0045] Step S330: Remove all the temporary protective layers and fabricate the metal electrode layer on the high-resistivity layer and the ITO current spreading layer. Specifically, in this embodiment, the step of removing all the temporary protective layers includes: immersing the chip in a BOE solution for 20 minutes to completely remove the temporary protective layer made of SiO2. The step of fabricating the metal electrode layer includes: placing the wafer after the above step of removing all the temporary protective layers on the wafer tray of an electron beam evaporation machine, with the evaporation source emitter located below the wafer tray, and then sequentially evaporating Cr, Al, Ti, Ni, Pt, Ni, Pt, and Au layers to form the metal electrode layer.

[0046] Preferably, in this embodiment, the step of preparing the current blocking layer on the epitaxial light-emitting structure in step S300 specifically includes: depositing a SiO2 layer with a thickness of 250nm-350nm on the epitaxial light-emitting structure, performing yellow light treatment on the surface of the SiO2 layer, and then performing homogenization, exposure, and development, while retaining a portion of the SiO2 layer at the position corresponding to the metal electrode layer as a current blocking layer.

[0047] Preferably, in this embodiment, the step of preparing the ITO current extension layer on the current blocking layer in step S300 specifically includes: fabricating an ITO transparent conductive film on the current blocking layer using magnetron sputtering, and annealing to make the crystal arrangement more orderly and dense, thereby forming the ITO current extension layer. Specifically, the target material is sputtered onto the wafer surface by bombarding it with Ar gas ionization to complete the deposition of ITO; since the density of ITO after deposition is not good, annealing can make the crystal arrangement more orderly, the film layer more dense, and the conductivity more stable. The annealing process involves placing the epitaxial wafer coated with the ITO film layer into a chamber at 550°C for annealing for 15 minutes. The thickness of the SiO2 layer is preferably 300 nm.

[0048] Preferably, in this embodiment, the step of preparing the passivation layer on the metal electrode layer in step S300 specifically includes:

[0049] A SiO2 passivation layer with a thickness of 80 nm on one side was prepared on the chip surface using PECVD.

[0050] Furthermore, in this embodiment, step S200 specifically includes:

[0051] Step S210: An N-type semiconductor layer, a light-emitting layer, and a P-type semiconductor layer are sequentially fabricated on the substrate using a preset fabrication process. The N-type semiconductor layer is an N-GaN layer, the P-type semiconductor layer is a P-GaN layer, and the light-emitting layer is a multi-quantum-well active layer. Specifically, the preset fabrication process includes using hydrogen as a carrier gas, ammonia as a nitrogen source, trimethylgallium and triethylgallium as gallium sources, trimethylindium as an indium source, silane as an N-type dopant, trimethylaluminum as an aluminum source, and magnesia-dicenocene as a P-type dopant. The thickness of the N-GaN layer is 1 μm-3 μm, and the Si doping concentration is 5 × 10⁻⁶. 18 cm -3 -1×10 19 cm -3 The thickness of the P-GaN layer is 200nm-300nm, and the Mg doping concentration is 5×10⁻⁶. 17 cm -3 -1×10 20 cm -3 The molar proportion of In in the multi-quantum-well active layer is 10%-35%.

[0052] Step S220: Chip fabrication is performed on the epitaxial light-emitting structure, and the morphology of the N-GaN layer is exposed by ICP etching technology.

[0053] In summary, the LED chip fabrication method in the above embodiments of the present invention, by fabricating a temporary protective layer on the ITO current extension layer and etching a fabrication trench on the temporary protective layer to expose part of the ITO current extension layer, the fabrication trench includes a plurality of trenches spaced apart along the outer edge of the metal electrode layer. Further, hydrogen ions are formed by ionization, and these hydrogen ions combine with oxygen atoms on the surface of the ITO current extension layer in the fabrication trench. This increases the resistance of the ITO surface, or even causes it to fail, forming a high-resistance layer, i.e., multiple spaced high-resistance regions corresponding to the trenches. This indirectly reduces the ITO thickness and lowers the resistance of the lateral current extension. The principle is similar to the increased flow velocity of water when passing through a narrow passage. The electrode extension layer is located inside the high-resistance layer, so that the current extension has an acceleration effect at intervals, improving the current extension capability and thus enabling the current to extend further laterally, reaching the edge of the chip.

[0054] Example 2

[0055] The second embodiment of the present invention provides an LED chip, which is prepared by the LED chip preparation method described in the above embodiments.

[0056] For ease of understanding, such as Figure 2-3 The diagram shown is a schematic diagram of the LED chip structure in this embodiment, including a substrate, an epitaxial light-emitting structure, and an electrode structure. The epitaxial light-emitting structure includes an N-type semiconductor layer, a light-emitting layer, and a P-type semiconductor layer sequentially disposed on the substrate. The electrode structure includes a current blocking layer 4, an ITO current spreading layer 3, a metal electrode layer 1, and a passivation layer 2 sequentially disposed on the epitaxial light-emitting structure. The ITO current spreading layer 3 is provided with a high resistance layer 5, which includes a plurality of high resistance bands disposed on the outer edge of the metal electrode layer 1.

[0057] Specifically, the substrate can be selected from one of the following: sapphire substrate, SiO2-sapphire composite substrate, silicon substrate, silicon carbide substrate, gallium nitride substrate, and zinc oxide substrate. In this embodiment, a sapphire substrate is selected. Sapphire is currently the most commonly used GaN-based LED substrate material, and most GaN-based LEDs on the market use sapphire as the substrate material. The biggest advantages of sapphire substrates are mature technology, good stability, and low production cost. The aforementioned metal electrode layer 1 sequentially includes Cr, Al, Ti, Ni, Pt, Ni, Pt, and Au layers.

[0058] Specifically, the steps for fabricating the metal electrode layer 1 on the ITO current spreading layer 3 include:

[0059] A temporary protective layer is prepared on the ITO current spreading layer 3, and a preparation trench is etched on the temporary protective layer to expose part of the ITO current spreading layer 3. The preparation trench includes a plurality of trenches spaced apart along the outer edge of the metal electrode layer 1.

[0060] A hydrogen ion purging operation is performed on one side of the temporary protective layer to allow oxygen atoms on the exposed part of the ITO current extension layer 3 to combine with the hydrogen ions, thereby forming a high-resistivity layer 5 at the preparation tank.

[0061] The temporary protective layer is removed, and the metal electrode layer 1 is formed on the high-resistivity layer 5 and the ITO current spreading layer 3. The hydrogen ion gas is silane, ammonia, etc. The temporary protective layer is used to protect part of the ITO current spreading layer 3 from the influence of hydrogen ions, and the temporary protective layer is made of SiO2.

[0062] Furthermore, such as Figure 3 The figure shows a top view of the LED chip in this embodiment. As shown, the high-resistance layer 5 includes three spaced high-resistance strips, which are similar in shape to the metal electrode layer 1 to ensure that the distance between the high-resistance strips and the electrodes is the same. The metal electrode layer 1 is located inside the high-resistance layer 5, and its current flow direction is shown by the arrow in the figure. By setting the high-resistance strips, the current expansion can have an acceleration effect at intervals, improving the current expansion capability, thereby enabling the current to expand laterally further and reach the edge of the chip.

[0063] Furthermore, the steps for preparing the aforementioned ITO current spreading layer 3 specifically include: fabricating an ITO transparent conductive film on the current blocking layer 4 using magnetron sputtering, and then annealing to make the crystal arrangement more orderly and dense, thereby forming the ITO current spreading layer 3. Specifically, the target material is sputtered onto the wafer surface by bombarding it with Ar gas ionization, completing the deposition of ITO; since the density of ITO after deposition is not good, annealing can make the crystal arrangement more orderly, the film layer more dense, and the conductivity more stable. The annealing process involves placing the epitaxial wafer coated with the ITO film layer into a chamber at 550°C for annealing for 15 minutes.

[0064] Furthermore, in this embodiment, the aforementioned N-type semiconductor layer is an N-GaN layer, the P-type semiconductor layer is a P-GaN layer, and the light-emitting layer is a multi-quantum-well active layer. Specifically, during fabrication, an epitaxial layer can be grown on a substrate using metal chemical vapor deposition (MOCVD). High-purity hydrogen is used as the carrier gas, high-purity ammonia as the nitrogen source, trimethylgallium and triethylgallium as gallium sources, trimethylindium as the indium source, silane as the N-type dopant, trimethylaluminum as the aluminum source, and magnesium thiocene as the P-type dopant. The N-type semiconductor layer is an n-GaN layer, the P-type semiconductor layer is a P-GaN layer, and the light-emitting layer is a multi-quantum-well active layer. The thickness of the N-GaN layer is 1 μm-3 μm, and the Si doping concentration is 5 × 10⁻⁶. 18 -1×10 19 cm -3 The thickness of the P-GaN layer is 200-300 nm, and the Mg doping concentration is 5 × 10⁻⁶. 17 -1×10 20 cm -3 The molar proportion of In in the multi-quantum-well active layer is 10%-35%.

[0065] In summary, the LED chip in this embodiment exposes a portion of the ITO current extension layer by fabricating a temporary protective layer on the ITO current extension layer and etching a fabrication trench on the temporary protective layer. The fabrication trench includes several trenches spaced apart along the outer edge of the metal electrode layer. Further, hydrogen ions are formed by ionization, and these hydrogen ions combine with oxygen atoms on the surface of the ITO current extension layer in the fabrication trench. This increases the surface resistance of the ITO, potentially causing it to fail, thus forming a high-resistance layer—multiple spaced high-resistance regions corresponding to the trenches. This indirectly reduces the ITO thickness and lowers the resistance of the lateral current extension. The principle is similar to water flowing faster through a narrow passage. The electrode extension layer is located inside the high-resistance layer, allowing the current extension to have an acceleration effect at intervals, improving the current extension capability and enabling the current to extend further laterally, reaching the edge of the chip.

[0066] In the description of this specification, references to terms such as "one embodiment," "some embodiments," "example," "specific example," or "some examples," etc., indicate that a specific feature, structure, material, or characteristic described in connection with that embodiment or example is included in at least one embodiment or example of the invention. In this specification, the illustrative expressions of the above terms do not necessarily refer to the same embodiment or example. Furthermore, the specific features, structures, materials, or characteristics described may be combined in any suitable manner in one or more embodiments or examples.

[0067] The embodiments described above are merely illustrative of several implementations of the present invention, and while the descriptions are specific and detailed, they should not be construed as limiting the scope of the invention. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of the present invention, and these modifications and improvements all fall within the scope of protection of the present invention. Therefore, the scope of protection of the present invention should be determined by the appended claims.

Claims

1. A method for fabricating an LED chip, characterized in that, Includes the following steps: Provide a substrate; An epitaxial light-emitting structure is fabricated on the substrate; A current blocking layer, an ITO current spreading layer, a metal electrode layer, and a passivation layer are sequentially fabricated on the epitaxial light-emitting structure to form an electrode structure on the epitaxial light-emitting structure. Specifically, the step of fabricating the metal electrode layer on the ITO current spreading layer includes: A temporary protective layer is prepared on the ITO current spreading layer, and a preparation trench is etched on the temporary protective layer to expose a portion of the ITO current spreading layer. The preparation trench includes a plurality of trenches spaced apart along the outer edge of the metal electrode layer. A hydrogen ion purging operation is performed on one side of the temporary protective layer to allow oxygen atoms on the exposed ITO current extension layer surface to combine with the hydrogen ions, thereby forming a high-resistivity layer at the preparation tank. Remove all of the temporary protective layers and fabricate the metal electrode layer on the high-resistivity layer and the ITO current spreading layer; The specific steps for fabricating the current blocking layer on the epitaxial light-emitting structure include: A SiO2 layer with a thickness of 250nm-350nm is deposited on the epitaxial light-emitting structure using PECVD process. The surface of the SiO2 layer is then subjected to photolithography, followed by spin coating, exposure, and development. A portion of the SiO2 layer at the position corresponding to the metal electrode layer is retained as a current blocking layer. The steps for fabricating the epitaxial light-emitting structure on the substrate specifically include: An N-type semiconductor layer, a light-emitting layer, and a P-type semiconductor layer are sequentially fabricated on the substrate using a preset fabrication process. The N-type semiconductor layer is an N-GaN layer, the P-type semiconductor layer is a P-GaN layer, and the light-emitting layer is a multi-quantum-well active layer. The preset preparation process includes: using hydrogen as a carrier gas, ammonia as a nitrogen source, trimethylgallium and triethylgallium as gallium sources, trimethylindium as an indium source, silane as an N-type dopant, trimethylaluminum as an aluminum source, and magnesium thiocene as a P-type dopant.

2. The LED chip fabrication method according to claim 1, characterized in that, The step of performing hydrogen ion purging on one side of the temporary protective layer to allow oxygen atoms on the exposed ITO current extension layer surface to combine with the hydrogen ions, thereby forming a high-resistivity layer at the preparation tank, specifically includes: Through a preset preparation process, hydrogen ion gas is introduced into the machine, and the hydrogen ion gas is ionized by radio frequency to form hydrogen ions, wherein the hydrogen ion gas is silane; A purge is performed under the influence of an electric field to allow the hydrogen ions to combine with oxygen atoms on the exposed surface of the ITO current-extended layer, thereby forming a high-resistivity layer at the preparation tank.

3. The LED chip fabrication method according to claim 2, characterized in that, The preset preparation process includes: controlling the temperature inside the machine to be 200℃-300℃, the radio frequency power to be 70W-150W, the hydrogen ion gas injection rate to be 100sccm-150sccm, and the purging time to be 240s-500s.

4. The LED chip fabrication method according to claim 1, characterized in that, The temporary protective layer is made of SiO2.

5. The LED chip fabrication method according to claim 4, characterized in that, The step of removing all of the temporary protective layers specifically includes: The SiO2 on the surface of the ITO current extension layer is removed by etching with BOE solution to remove all of the temporary protective layer.

6. The LED chip fabrication method according to claim 1, characterized in that, The steps for fabricating the ITO current spreading layer on the current blocking layer specifically include: An ITO transparent conductive film is fabricated on the current blocking layer using a magnetron sputtering process, and then an ITO current spreading layer is formed by an annealing process.

7. The LED chip fabrication method according to claim 1, characterized in that, The thickness of the N-GaN layer is 1μm-3μm, and the Si doping concentration is 5×10⁻⁶. 18 cm -3 -1×10 19 cm -3 The thickness of the P-GaN layer is 200 nm - 300 nm, and the Mg doping concentration is 5 × 10⁻⁶. 17 cm -3 -1×10 20 cm -3 The molar proportion of In in the multi-quantum-well active layer is 10%-35%.

8. An LED chip, characterized in that, The LED chip is prepared by the LED chip preparation method according to any one of claims 1-7.

Citation Information

Patent Citations

  • LED chip and preparation method thereof

    CN109950378A

  • Light emitting diode chip and preparation method thereof

    CN114551673A